CN101380624B - Flush lettering painting treatment method - Google Patents

Flush lettering painting treatment method Download PDF

Info

Publication number
CN101380624B
CN101380624B CN2008102329003A CN200810232900A CN101380624B CN 101380624 B CN101380624 B CN 101380624B CN 2008102329003 A CN2008102329003 A CN 2008102329003A CN 200810232900 A CN200810232900 A CN 200810232900A CN 101380624 B CN101380624 B CN 101380624B
Authority
CN
China
Prior art keywords
bas
relief
character cut
lettering
flush
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2008102329003A
Other languages
Chinese (zh)
Other versions
CN101380624A (en
Inventor
何金杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2008102329003A priority Critical patent/CN101380624B/en
Publication of CN101380624A publication Critical patent/CN101380624A/en
Application granted granted Critical
Publication of CN101380624B publication Critical patent/CN101380624B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a processing method for painting a character cut in bas-relief, which comprises the following steps: firstly, an anti-sticking film is coated on the periphery of the character cut in bas-relief; then, dope is coated on the surface of the character cut in bas-relief, after the dope is dried and solidified, the dope on the periphery of the character cut in bas-relief is removed; finally, the anti-sticking film on the periphery of the character cut in bas-relief is removed. With the method, the surface of a printing product is effectively prevented from being damaged when the character cut in bas-relief is painted, thereby facilitating the improvement of working efficiency and reducing the production cost.

Description

A kind of flush lettering painting treatment method
Technical field
The present invention relates to the flush lettering painting print field, relate in particular to a kind of flush lettering painting treatment method.
Background technology
Mashed plate printing is a kind of technology that product surface need stamp special marking that is applied to, and can solve general planographic requirement basically, but along with the development of society and the continuous variation of the market demand, is had higher requirement in the print product surface.Particularly for electroplated, the irregular product of flatness, as on the character cut in bas-relief of cambered surface, carrying out special marking with color, often to the character cut in bas-relief surface coloring time, also can coat color to the character cut in bas-relief periphery, to remove the color of character cut in bas-relief periphery after the printing, in the prior art, great majority adopt the shovel of band cutting edge or the color that scraper is removed the character cut in bas-relief periphery, and are so easy of the surface tear of print product, cause product surface not attractive in appearance, and operating efficiency is extremely low.
Summary of the invention
In view of this, the invention provides a kind of flush lettering painting treatment method, when carrying out the flush lettering painting processing on the surface of product, can effectively protect the surface of print product.
A kind of flush lettering painting treatment method provided by the invention comprises the steps:
A, apply one deck antiadhesion barrier at character cut in bas-relief periphery;
B, at character cut in bas-relief surface-coated coating, after treating the coating drying, solidifying, remove the coating of character cut in bas-relief periphery;
C, remove the antiadhesion barrier of character cut in bas-relief periphery;
Further, described antiadhesion barrier adopts and mixing, the materials of different colors mutually of tinting;
Further, described antiadhesion barrier is solid wax or soft wax;
Further, among the described step b, the coating of removing the character cut in bas-relief periphery adopts the coarse cloth that is stained with alcohol to wipe;
Further, among the described step c, the antiadhesion barrier of removing the character cut in bas-relief periphery adopts the cotton that is stained with alcohol to wipe.
Beneficial effect of the present invention is: can effectively prevent to damage when flush lettering painting from handling the surface of print product, help increasing work efficiency, reduce production costs.
The specific embodiment
In order to make the purpose, technical solutions and advantages of the present invention clearer, describe below in conjunction with specific embodiments.
As tinting to spcial character at the product surface after electroplating well, at first apply one deck antiadhesion barrier at product surface character cut in bas-relief periphery, then coating is coated in the surface of the spcial character that need tint with writing brush, after treating coating drying, curing, wipe the coating of spcial character periphery with the coarse cloth that is stained with alcohol, be stained with the antiadhesion barrier that wipes of alcohol is removed the print product surface with muslin at last.
When selecting antiadhesion barrier for use, preferably adopt with flush lettering painting do not mix mutually, the solid wax or the soft wax of different colours, in order to avoid obscure, when the usefulness coarse cloth that is stained with alcohol is wiped the coating of character cut in bas-relief periphery again, avoid wiping antiadhesion barrier, wiping because of coarse cloth can the scratch product surface behind the antiadhesion barrier as far as possible.The antiseized rete of product surface is wiped with the muslin that is stained with alcohol, can not damage the surface of print product.
Explanation is at last, above embodiment is only unrestricted in order to technical scheme of the present invention to be described, those of ordinary skill in the art can make amendment or is equal to replacement technical scheme of the present invention, and not breaking away from the aim and the scope of the technical program, it all should be encompassed in the middle of the claim scope of the present invention.

Claims (5)

1. a flush lettering painting treatment method is characterized in that: comprise the steps:
A, apply one deck antiadhesion barrier at character cut in bas-relief periphery;
B, at character cut in bas-relief surface-coated coating, after treating the coating drying, solidifying, remove the coating of character cut in bas-relief periphery;
C, remove the antiadhesion barrier of character cut in bas-relief periphery.
2. a kind of flush lettering painting treatment method according to claim 1 is characterized in that: described antiadhesion barrier adopts and mixing, the materials of different colors mutually of tinting.
3. a kind of flush lettering painting treatment method according to claim 1 and 2 is characterized in that: described antiadhesion barrier is solid wax or soft wax.
4. a kind of flush lettering painting treatment method according to claim 1 is characterized in that: among the described step b, the coating of removing the character cut in bas-relief periphery adopts the coarse cloth that is stained with alcohol to wipe.
5. a kind of flush lettering painting treatment method according to claim 1 is characterized in that: among the described step c, the antiadhesion barrier of removing the character cut in bas-relief periphery adopts the cotton that is stained with alcohol to wipe.
CN2008102329003A 2008-10-21 2008-10-21 Flush lettering painting treatment method Expired - Fee Related CN101380624B (en)