CN101041315B - 树木年轮画制作方法 - Google Patents

树木年轮画制作方法 Download PDF

Info

Publication number
CN101041315B
CN101041315B CN200710049034XA CN200710049034A CN101041315B CN 101041315 B CN101041315 B CN 101041315B CN 200710049034X A CN200710049034X A CN 200710049034XA CN 200710049034 A CN200710049034 A CN 200710049034A CN 101041315 B CN101041315 B CN 101041315B
Authority
CN
China
Prior art keywords
tree
ring section
tree ring
ring
picture
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN200710049034XA
Other languages
English (en)
Other versions
CN101041315A (zh
Inventor
蒲正茂
蒲薪豫
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN200710049034XA priority Critical patent/CN101041315B/zh
Publication of CN101041315A publication Critical patent/CN101041315A/zh
Application granted granted Critical
Publication of CN101041315B publication Critical patent/CN101041315B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种树木年轮画制作方法,按下列步骤进行:①制作树木年轮切片,通过切削机械或手工工具锯切厚度为0.1mm-10mm的树木带年轮的断面切片备用;②年轮切片干燥,将切好的树木年轮片在20-80℃条件下干燥至含水量小于11%;③固定,将干燥好的树木年轮切片固定于底板上即可。本发明的产品适用于家庭装饰、公共场所建筑物装饰、各种家俱表面装饰、宗教场所装饰,也可直接制作成镜框画,悬挂于需装饰美化的场所,本发明制作工艺简单,艺术感染力强。风格自然典雅,能给人以较大的联想空间,本发明所用树木材料基本上是木材加工中的废弃料,有利于提高资源利用率,有利于建设节约型社会。

Description

树木年轮画制作方法
技术领域
本发明涉及一种木材加工方法,尤其是一种树木年轮画制作方法。
背景技术
目前室内外装饰多采用人工绘制图案或木雕来装饰,这种图案全是人工痕迹,装饰效果缺少自然美感,难以适应不同人群需要,且木雕需消耗大量木材,不利生态环境保护,直到目前为止,尚未见有能体现自然美、给人们较大联想空间的树木年轮画面世。
发明内容
本发明的目的在于克服现有技术不足,提供一种树木年轮画制作方法及该方法获得的年轮画,本发明目的通过下述技术方案来实现:
1、先用桐油、染色剂液或沥青浸泡木材3-70天,然后再行切片;
2、制作树木年轮切片,通过切削机械或手工工具锯切厚度为0.1mm-10mm带年轮的树木断面切片备用;
3、年轮切片干燥,将切好的树木年轮切片在20-80℃条件下干燥至含水量小于11%;
4、固定,将干燥好的树木年轮切片固定于底板上即可。
为增强树木年轮切片的防腐效果,可用防腐剂对切片进行浸渍、浸泡或涂刷。
考虑到树木年轮画表面细腻光亮,不变色、不开裂及防腐,可用水砂纸、细砂布等打磨器具对树木年轮切片表面进行清理打磨,并涂刷桐油或透明漆。
考虑到硬度较大的树木年轮切片不变形,可在树木年轮切片与底板间增设一层柔软织物层如纱布、棉布、丝绸等。
本发明的产品适用于家庭装饰、公共场所建筑物装饰、各种家俱表面装饰、宗教场所装饰,也可直接制作成镜框画,悬挂于需装饰美化的场所,本发明制作工艺简单,艺术感染力强。风格自然典雅,能给人以较大的联想空间,本发明所用树木材料基本上是木材加工中的废弃料,有利于提高资源利用率,有利于建设节约型社会。
具体实施方式
实施例1,选择直径大小适合的圆木置于刨床上,刨出树木横断面片即树木年轮切片,树木年轮切片的厚度根据需要而定,一般在0.1-10mm之间为佳,本实施例选用0.1mm备用,将树木年轮在自然条件下干燥至含水量小于11%,一般较薄的树木年轮切片不宜爆晒,而在较柔和的阳光下晒干或自然风干,温度以20-40℃为佳,待树木年轮切片含水量小于11%时,即可进入固定程序,所说的固定可以是通过粘接剂粘贴于底板上,也可以是直接嵌于带凹槽的底板上。首先选择好底板,底板可以是墙壁、家俱表面或纸板、玻璃板、塑胶板等任一载体均可,本实施例选择白色纸板,在纸板上刷胶粘剂,所说的胶粘剂根据需要选择,可以是乳白胶,各种化学粘结剂,如合成树脂类、聚乙烯醇及其缩醛树脂、脲醛树脂、改性环氧树脂、聚乙烯树脂及骨胶等任一种均可,本实施例选用乳白胶,刷好胶后将干燥好的树木年轮切片贴于底板上,压实即可。如果需要进行裱画处理,即按常规方法裱画,或制作画框将树木年轮画置于画框中,本实施例选择后者。
实施例2,选择直径大小适合的圆木,将圆木置于桐油或染色剂液或沥青中浸泡3-70天,以使树木切片色泽更丰富,视觉效果更好,且防腐与不开裂。本实施例选择用桐油浸泡3天,取出去除表面要桐油,用锯子锯成10mm的树木年轮切片,将树木年轮切片在烘箱中80℃条件下干燥至含水量小于11%,用细砂布对树木年轮切片进行清理打磨,并涂上透明漆,所说透明漆为清漆,Y00-8聚合清漆,Y001-3油脂漆或天然树脂漆,如TO-1-1酯胶清漆,TO-1-1虫胶清漆或FO-1酚醛清漆等任一种,本实施选用Y00-7清漆,漆干后即可进入固定程序,即选择好底板,底板可以是墙壁、家俱表面或纸板、玻璃板或塑胶板均可,本实施例选择墙壁,在墙壁上预留有与树木年轮切片大小相一致的凹槽,将树木年轮切片直接嵌于凹槽中即可。
实施例3,根据需要选择直径大小适合的圆木,将圆木在沥青中浸泡70天后去除外表沥青,再将其置于刨床上,刨出树木横断面片即树木年轮切片,树木年轮切片的厚度根据需要而定,本实施例选用2mm备用,将树木年轮切片在烘箱中50℃干燥至含水量小于11%,用CCA或ACQ防腐剂涂刷树木年轮切片,待干后即可进入固定程序,即选择好底板,本实施例选择塑胶板,在塑胶板上刷胶粘剂,所说的胶粘剂根据需要选择,可以是乳白胶,各种化学粘结剂,如合成树脂类如聚乙烯醇及其缩醛树脂、脲醛树脂、改性环氧树脂、聚乙烯树脂及骨胶等均可,本实施例选用聚乙烯树脂,刷好胶后将干燥好的树木年轮切片贴于塑胶板上,压实即可。如果需要进行裱画处理,即按常规方法裱画,或制作画框将树木年轮画置于画框中。
实施例4,根据需要选择直径大小适合的圆木,将圆木在沥青中浸泡30天后去除外表沥青,再将其置于刨床上,刨出树木横断面片即树木年轮切片,树木年轮切片的厚度根据需要而定,本实施例选用1mm备用,将树木年轮切片在烘箱中60℃干燥至含水量小于11%,用CCA防腐剂涂刷树木年轮切片,待干后即可进入固定程序,即选择好底板,本实施例选择塑胶板,在塑胶板上刷胶粘剂,本实施例选用脲醛树脂,刷好胶后辅上一层柔软织物层,再涂一次脲醛树脂,再将干燥好的树木年轮切片贴于柔软织物上,压实即可,所说柔软织物可以是纱布、棉布或丝绸任一种,本实施例选用纱布。如果需要进行裱画处理,即按常规方法裱画,或制作画框将树木年轮画置于画框中。
实施例5,根据需要选择直径大小适合的圆木,将圆木在桐油中浸泡20天后去除外表桐油,再将其置于刨床上,刨出树木横断面片即树木年轮切片,树木年轮切片的厚度根据需要而定,本实施例选用0.5mm备用,将树木年轮切片在烘箱中50℃干燥至含水量小于11%,用ACQ防腐剂涂刷树木年轮切片,待干后即可进入固定程序,即选择好底板,本实施例选择立柜外面板作底板,在立柜需贴树木年轮切片部的面板上刷胶粘剂,所说的胶粘剂根据需要选择,本实施例选用聚乙烯树脂,刷好胶后将干燥好的树木年轮切片贴于板上,压实即可。

Claims (3)

1.一种树木年轮画制作方法,按下列步骤进行:
①先用桐油、染色剂液或沥青浸泡木材3-70天,然后再行切片;
②制作树木年轮切片,通过切削机械或手工工具锯切厚度为0.1mm-10mm的树木带年轮的断面切片备用;
③年轮切片干燥,将切好的树木年轮片在20-80℃条件下干燥至含水量小于11%;
④固定,将干燥好的树木年轮切片固定于底板上即可。
2.根据权利要求1所述的树木年轮画制作方法,其特征在于:在树木年轮切片与底板间设有一层柔软织物层。
3.一种根据权利要求1或2所述方法制作的树木年轮画。
CN200710049034XA 2007-04-27 2007-04-27 树木年轮画制作方法 Expired - Fee Related CN101041315B (zh)