CN100506770C - Color stabilizer for phenol and alkylphenol and its use - Google Patents

Color stabilizer for phenol and alkylphenol and its use Download PDF

Info

Publication number
CN100506770C
CN100506770C CNB200610024186XA CN200610024186A CN100506770C CN 100506770 C CN100506770 C CN 100506770C CN B200610024186X A CNB200610024186X A CN B200610024186XA CN 200610024186 A CN200610024186 A CN 200610024186A CN 100506770 C CN100506770 C CN 100506770C
Authority
CN
China
Prior art keywords
reagent
phenol
gram
colour
stabiliser
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNB200610024186XA
Other languages
Chinese (zh)
Other versions
CN101029002A (en
Inventor
金洁
戴鸣
吴长宁
陈新
周太申
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Baoshan Iron and Steel Co Ltd
Original Assignee
Baoshan Iron and Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Baoshan Iron and Steel Co Ltd filed Critical Baoshan Iron and Steel Co Ltd
Priority to CNB200610024186XA priority Critical patent/CN100506770C/en
Publication of CN101029002A publication Critical patent/CN101029002A/en
Application granted granted Critical
Publication of CN100506770C publication Critical patent/CN100506770C/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A color stabilizer for preventing the color of phenol and alkylphenol from changing is composed of component A (hydrazine compound and/or hindered amine type photostabilizer) and component B hydroxyamine compound and/or 9,10-dihydro-9-oxa- 10-phospha phenanthrine-10-oxide (DPPO).

Description

Phenol and alkylphenol colour(ing)stabiliser and application thereof
Technical field
The present invention relates to a kind of phenols colour(ing)stabiliser, more specifically relate to a kind of inhibition phenol and alkylphenol discoloration, improve the composition of its appearance color stability.The invention still further relates to the application of this colour(ing)stabiliser.
Background technology
Phenol and alkylphenol are a kind of important organic synthesis raw materials, are widely used in the production of pharmacy, fuel, synthetic resins, insullac etc.The phenol and the variable color of alkylphenol product appearance of domestic production at present are very fast, and the situation of appearance color change often occurs, cause phenol and alkylphenol product memory cycle very short, are unfavorable for product application.
Prior art is studied utilizing stable reagent inhibition phenol and the variable color of alkylphenol product, it is reported that Japan adopts antioxidant that adds the 0.001-2.0% that accounts for phenol and alkylphenol product weight or the storage period that azanol class compositions and methods prolongs phenol products.For example add 9 in phenol, cresols and xylenol, the 10-dihydro-9-oxy is mixed-10-phospho hetero phenanthrene-10-oxide compound (DPPO), can store nondiscoloration in 60 days; The salt reagent that in phenol and alkylphenol product, adds diethyl hydroxylamine (DEHA), diethyl hydroxylamine also can reach identical effect (fuel and chemical industry, 1986,2:36).Chinese invention patent application 02132533.2 discloses a kind of compound colour(ing)stabiliser that suppresses phenol and alkylphenol discoloration, this stablizer is made up of P contained compound and sequestrant, in phenol and alkylphenol, add this compound colour(ing)stabiliser and can suppress variable color, improve the color stability of phenol and alkylphenol, and the inhibition color changeable effect of this compound colour(ing)stabiliser is not subjected to product purity, moisture, the influence of factors such as metallic impurity kind, but this compound colour(ing)stabiliser contains P contained compound, and more inapplicable required phenol and the alkylphenol product of technology that P contained compound is had the side effect reaction.
The existing colour(ing)stabiliser that is used for phenol and alkylphenol product exists and keeps the product appearance colour stable time shorter, and certain defectives such as side effect are arranged.
Summary of the invention
The purpose of this invention is to provide a kind of phenol and alkylphenol colour(ing)stabiliser, use preservation that this stablizer can make phenol and alkylphenol product effectively more than 90 days and nondiscoloration, thereby overcome the deficiencies in the prior art.Another object of the present invention provides the purposes of this stablizer.
Colour(ing)stabiliser of the present invention is made up of the A reagent of 1-1000 weight part and the B reagent of 0-500 weight parts, wherein said A reagent refers to carbohydrazide or hindered amine light stabilizer or their mixture, wherein the preferred Tinuvin-622 reagent of hindered amine light stabilizer, Tinuvin-770 reagent, Tinuvin-5178 reagent or their mixture; Said B reagent refers to hydroxylamine compound, 9, and the 10-dihydro-9-oxy is mixed-10-phospho hetero phenanthrene-10-oxide compound (DPPO) or their mixture, the wherein preferred diethyl hydroxylamine of hydroxylamine compound.A reagent and B reagent are promptly got colour(ing)stabiliser of the present invention by above-mentioned formula rate mixing.
According to the present invention, this colour(ing)stabiliser is used for suppressing by resulting phenol of industrial production and alkylphenol product, and its consumption is every processing 1000 gram phenol or alkylphenols, and the colour(ing)stabiliser that is consumed is made up of 0.01-10 gram A reagent and 0-5 gram B reagent.The usage of colour(ing)stabiliser of the present invention is: make phenol and alkylphenol product keep liquid state by the heat tracing mode, add colour(ing)stabiliser of the present invention after, mix.
Beneficial effect
1, colour(ing)stabiliser of the present invention can suppress phenol and the variable color of alkylphenol product effectively, improves the stability of its appearance color, uses behind the colour(ing)stabiliser of the present invention to keep appearance white storing more than 90 days.
2, colour(ing)stabiliser of the present invention does not contain P contained compound substantially, uses simply, and side effect is low.
Embodiment
Below by embodiment the inventive method is further elaborated, but does not limit the present invention:
Among the following embodiment, the look of phenol or alkylphenol number mensuration is undertaken by BG 605; The measuring method of its outward appearance is: pouring the sample of fusing into internal diameter is in 22 millimeters the colourless transparent glass test tube, in transmitted light its color of range estimation down.
Embodiment 1
Take by weighing 1000 gram phenol, keep liquid state with 40-50 ℃ of water-bath insulation, add 5 gram carbohydrazides while stirring, churning time is not shorter than 5 minutes, and the outward appearance of gained sample be a white, and its mensuration look number is 10.The sample of being prepared is positioned in the free warehouse preserved 91 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 20.
Embodiment 2
Take by weighing 1000 gram ortho-cresols, keep liquid state with 40-50 ℃ of water-bath insulation, add 1 gram carbohydrazide while stirring, churning time is not shorter than 5 minutes during interpolation, and the outward appearance of gained sample be a white, and its mensuration look number is 10.The sample of being prepared is positioned in the free warehouse preserved 91 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 10.
Embodiment 3
Take by weighing 1000 gram phenol, keep liquid state with 40-50 ℃ of water-bath insulation, add 1 gram Tinuvin-622 reagent while stirring, churning time is not shorter than 5 minutes during interpolation, and the outward appearance of gained sample be a white, and its mensuration look number is 20.The sample of being prepared is positioned in the free warehouse preserved 91 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 40.
Embodiment 4
Take by weighing 1000 gram ortho-cresols, keep liquid state with 40-50 ℃ of water-bath insulation, add 1 gram Tinuvin-622 reagent while stirring, churning time is not shorter than 5 minutes during interpolation, and the outward appearance of gained sample be a white, and its mensuration look number is 10.The sample of being prepared is positioned in the free warehouse preserved 91 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 20.
Embodiment 5
Take by weighing 1000 gram ortho-cresols, keep liquid state with 40-50 ℃ of water-bath insulation, add 1 gram Tinuvin-770 reagent while stirring, churning time is not shorter than 5 minutes during interpolation, and the outward appearance of gained sample be a white, and its mensuration look number is 10.The sample of being prepared is positioned in the free warehouse preserved 91 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 10.
Embodiment 6
Take by weighing 1000 gram ortho-cresols, keep liquid state with 40-50 ℃ of water-bath insulation, add 1 gram Tinuvin-5178 reagent while stirring, churning time is not shorter than 5 minutes during interpolation, and the outward appearance of gained sample be a white, and its mensuration look number is 10.The sample of being prepared is positioned in the free warehouse preserved 91 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 20.
Embodiment 7
Take by weighing 1000 gram ortho-cresols, keep liquid state with 40-50 ℃ of water-bath insulation, add 5 gram Tinuvin-5178 reagent while stirring, churning time is not shorter than 5 minutes during interpolation, and the outward appearance of gained sample be a white, and its mensuration look number is 10.The sample of being prepared is positioned in the free warehouse preserved 91 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 30.
Embodiment 8
Take by weighing 1000 gram phenol, keep liquid state with water-bath 40-50 ℃ of insulation, add the colour(ing)stabiliser of forming by 0.3 gram carbohydrazide, 0.03 gram diethyl hydroxylamine and 0.03 gram DPPO reagent while stirring, churning time is not shorter than 5 minutes during interpolation, the outward appearance of gained sample is a white, and it measures look number is 10.The sample of being prepared is positioned in the free warehouse preserved 116 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 20.
Embodiment 9
Take by weighing 1000 gram phenol, keep liquid state with water-bath 40-50 ℃ of insulation, add the colour(ing)stabiliser of being made up of 0.4 gram carbohydrazide and 0.04 gram DPPO reagent while stirring, churning time is not shorter than 5 minutes during interpolation, the outward appearance of gained sample is a white, and it measures look number is 10.The sample of being prepared is positioned in the free warehouse preserved 116 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 30.
Embodiment 10
Take by weighing 1000 gram phenol, keep liquid state with water-bath 40-50 ℃ of insulation, add the colour(ing)stabiliser of being made up of 0.5 gram carbohydrazide, 0.05 gram diethyl hydroxylamine while stirring, churning time is not shorter than 5 minutes during interpolation, the outward appearance of gained sample is a white, and it measures look number is 10.The sample of being prepared is positioned in the free warehouse preserved 116 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 20.
Embodiment 11
Take by weighing 1000 gram ortho-cresols, keep liquid state with water-bath 40-50 ℃ of insulation, add the colour(ing)stabiliser of being made up of 0.5 gram carbohydrazide, 0.2 gram diethyl hydroxylamine while stirring, churning time is not shorter than 5 minutes during interpolation, the outward appearance of gained sample is a white, and it measures look number is 10.The sample of being prepared is positioned in the free warehouse preserved 116 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 30.
Embodiment 12
Take by weighing 1000 gram ortho-cresols, keep liquid state with water-bath 40-50 ℃ of insulation, add the colour(ing)stabiliser of being made up of 0.5 gram carbohydrazide, 0.2 gram Tinuvin-5178 reagent while stirring, churning time is not shorter than 5 minutes during interpolation, the outward appearance of gained sample is a white, and it measures look number is 10.The sample of being prepared is positioned in the free warehouse preserved 116 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 20.
Embodiment 13
Take by weighing 1000 gram ortho-cresols, keep liquid state with water-bath 40-50 ℃ of insulation, add the colour(ing)stabiliser of forming by 0.2 gram Tinuvin-770 reagent, 0.2 gram Tinuvin-5178 reagent while stirring, churning time is not shorter than 5 minutes during interpolation, the outward appearance of gained sample is a white, and it measures look number is 10.The sample of being prepared is positioned in the free warehouse preserved 116 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 20.
Embodiment 14
Take by weighing 1000 gram ortho-cresols, keep liquid state with water-bath 40-50 ℃ of insulation, add the colour(ing)stabiliser of forming by 0.2 gram carbohydrazide, 0.1 gram diethyl hydroxylamine, 0.1 gram Tinuvin-770,0.1 gram Tinuvin-5178 reagent while stirring, churning time is not shorter than 5 minutes during interpolation, the outward appearance of gained sample is a white, and it measures look number is 10.The sample of being prepared is positioned in the free warehouse preserved 116 days, it is fixed to measure its look number and carry out External Observation, and after measured, its outward appearance be a white, and the mensuration look number is 20.

Claims (4)

1. phenol and alkylphenol colour(ing)stabiliser, it is characterized in that forming by the A reagent of 1-1000 weight part and the B reagent of 0-500 weight parts, wherein said A reagent refers to carbohydrazide or hindered amine light stabilizer or their mixture, said B reagent refers to hydroxylamine compound, 9, and the 10-dihydro-9-oxy is mixed-10-phospho hetero phenanthrene-10-oxide compound (DPPO) or their mixture.
2. phenol according to claim 1 and alkylphenol colour(ing)stabiliser is characterized in that said hindered amine light stabilizer is Tinuvin-622 reagent, Tinuvin-770 reagent, Tinuvin-5178 reagent or their mixture.
3. phenol according to claim 1 and alkylphenol colour(ing)stabiliser is characterized in that said hydroxylamine compound is a diethyl hydroxylamine.
4. described phenol of claim 1 and alkylphenol is characterized in that every processing 1000 gram phenol or alkylphenols with the application of colour(ing)stabiliser, and the colour(ing)stabiliser that is consumed is made up of 0.01-10 gram A reagent and 0-5 gram B reagent.
CNB200610024186XA 2006-02-28 2006-02-28 Color stabilizer for phenol and alkylphenol and its use Expired - Fee Related CN100506770C (en)