CN100420723C - Free formaldehyde trapping agent and process for preparing same - Google Patents

Free formaldehyde trapping agent and process for preparing same Download PDF

Info

Publication number
CN100420723C
CN100420723C CNB2006100750465A CN200610075046A CN100420723C CN 100420723 C CN100420723 C CN 100420723C CN B2006100750465 A CNB2006100750465 A CN B2006100750465A CN 200610075046 A CN200610075046 A CN 200610075046A CN 100420723 C CN100420723 C CN 100420723C
Authority
CN
China
Prior art keywords
urea
free formaldehyde
trapping agent
raw materials
weight
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CNB2006100750465A
Other languages
Chinese (zh)
Other versions
CN1827710A (en
Inventor
于红卫
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang A&F University ZAFU
Original Assignee
Zhejiang Forestry College
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhejiang Forestry College filed Critical Zhejiang Forestry College
Priority to CNB2006100750465A priority Critical patent/CN100420723C/en
Publication of CN1827710A publication Critical patent/CN1827710A/en
Application granted granted Critical
Publication of CN100420723C publication Critical patent/CN100420723C/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to a preparation method for a free formaldehyde trapping agent. The present invention is characterized in that the free formaldehyde trapping agent is prepared from the following raw materials: 90 to 110 portions by weight of phosphoric acid, 55 to 75 portions by weight of urea, 55 to 75 portions by weight of water and 0.05 to 0.15 portion by weight of catalyst. The preparation method comprises the following steps: firstly, all prepared phosphoric acid and all prepared urea are added in a reaction kettle to be stirred; then the catalyst is added, and water equal to the urea measured by weight portion is simultaneously added to be heated to 120 to 130 DEG C, and heat is preserved; when a pH value of a reaction liquid is from 6.0 to 6.5, temperature naturally drops to at most 40 DEG C, and a pH value is regulated by ammonia water to obtain the free formaldehyde trapping agent. The trapping agent prepared by the method can be widely used for the production of products needing a urea-formaldehyde resin adhesive in timber industry, etc.; the trapping agent has the advantages of easy acquirement of raw materials, simple preparation method, low cost and high rate of formaldehyde removal.

Description

Catching agent for free formaldehyde and production method thereof
Technical field
The invention belongs to bamboo and wood, the bonding production method of using the catching agent for free formaldehyde of urea-formaldehyde resin of paper product.
Background technology
Urea-formaldehyde resin is widely used in timber industry, inexpensive with it, bonding strength is high, production technique is simple, cost is low welcome, but all can release formaldehyde in aging in the raw material of this glue before production, when producing in the condensation of methylol, after using, be free state, serious environment pollution is detrimental to health.Extensive and deep research has been carried out at the content that reduces free formaldehyde, removing free formaldehyde in countries in the world.CN93121419 discloses " catching agent for free formaldehyde and production technique thereof " patented technology of Mr. of Liu Ding, with urea, bean powder, blood meal, gelatin, resol etc. is raw material, it is mould to produce urea in copolymerizing and blending, add emulsifying agent and form microcapsule, the removing of PARA FORMALDEHYDE PRILLS(91,95) also has positive effect, but bean powder, blood meal, gelatin easily produce and go mouldy, and causes the variation of color and luster and smell, the adding of resol will influence the stability of urea glue and make color curved dark, and production cost also increases.
Summary of the invention
The technical problem to be solved in the present invention is: provide a kind of and can overcome above-mentioned defective, technology is simple, with low cost, the aldehyde rate that disappears is high catching agent for free formaldehyde and production method thereof, produce a kind of novel formaldehyde-trapping agent, with urea glue with mixing with being used for eliminating free formaldehyde.
Technical solution of the present invention is: be made up of following raw materials according and weight part thereof: 90-110 part phosphoric acid, 55-75 part urea, 55-75 part water, 0.05-0.15 part are made ethylenediamine tetraacetic acid (EDTA) and/or its sodium salt of catalyzer; Its technical process be earlier will the amount of getting the raw materials ready whole phosphoric acid and whole urea of the amount of getting the raw materials ready add in the reactors, stir, the water that adds catalyzer, adding simultaneously and urea equal weight part again, be heated to 120-130 ℃, insulation, as reaction solution PH=6.0-6.5, be cooled to naturally≤40 ℃, with ammoniacal liquor accent PH=7.0-7.5.
The formaldehyde-trapping agent that aforesaid method is produced, this trapping agent outward appearance is faint yellow or colourless liquid, PH=7.0-7.5, solid content 50 ± 2%, viscosity 13-18 second (being coated with one 4 glasss of mensuration), storage period 〉=3 month.
The formaldehyde-trapping agent that aforesaid method is produced evenly stirs the back with joining with usefulness with 90-110 weight part urea-formaldehyde resin adhesive and this catching agent for free formaldehyde of 4-8 weight part during application in container.
Embodiment
The present invention will now be further detailed embodiment: in the raw material, phosphoric acid and urea are all used technical pure, their more satisfactory mol ratios are 1: 1.05, catalyzer is at least a with ethylenediamine tetraacetic acid (EDTA), disodium ethylene diamine tetraacetate, tetrasodium ethylenediamine tetraacetate, and the amount of adding is the 0.05-0.15% of phosphoric acid and urea add-on sum.For easy to operate raw material and weight part thereof are listed six kinds of embodiment such as following table 1 (wherein ethylenediamine tetraacetic acid (EDTA) is represented with EDTA):
Figure C20061007504600041
Consult the listed 6 kinds of embodiment of table, now illustrate with embodiment 1: earlier 90 weight parts (hereinafter to be referred as part) phosphoric acid and 55 parts of urea are added reactors, stir, add EDTA and 55 parts of water, be heated to 120-130 ℃, be incubated, when reaction solution PH=6.0-6.5,
Naturally be cooled to≤40 ℃, transfer PH=7.0-7.5 with ammoniacal liquor, blowing is gone into bucket, and this trapping agent is promptly made.
All the other embodiment 2-6 make with embodiment 1 same procedure by each routine parts by weight of raw materials proportioning.Wherein preferential with embodiment 2,5.
With the catching agent for free formaldehyde that present method makes, its outward appearance is faint yellow or colourless liquid, PH7.0-7.5, solid content 50 ± 2%, viscosity 13-18 second (being coated with-4 glasss of mensuration), storage period 〉=3 month.
This trapping agent using method be with urea-formaldehyde resin adhesive with joining with usefulness, the general requirement preparation is finished the back and was used up in 4-8 hour.Proportioning is that urea-formaldehyde resin 90-110 weight part is joined this trapping agent 4-8 weight part, mixes the back thoroughly and uses.Preferred weight part proportioning is 100: 6, and like this, the aldehyde rate that disappears is stated more than 90%.
The present invention has compared to existing technology that raw material is easy to get, technology is simple, with low cost, aldehyde disappears Effective advantage.

Claims (3)

1. catching agent for free formaldehyde production method, it is characterized in that being made up of following raw materials according and weight part thereof: 90-110 part phosphoric acid, 55-75 part urea, 55-75 part water, 0.05-0.15 part are made ethylenediamine tetraacetic acid (EDTA) and/or its sodium salt of catalyzer; Its technical process be earlier will the amount of getting the raw materials ready whole phosphoric acid and whole urea of the amount of getting the raw materials ready add in the reactors, stir, the water that adds catalyzer, adding simultaneously and urea equal weight part again, be heated to 120-130 ℃, insulation, as reaction solution PH=6.0-6.5, be cooled to naturally≤40 ℃, with ammoniacal liquor accent PH=7.0-7.5.
2. the catching agent for free formaldehyde produced of the method for claim 1, during its feature application be outward appearance be faint yellow or colourless liquid, PH=7.0-7.5, solid content 50 ± 2%, with being coated with-4 glasss of mensuration viscosity 13-18 seconds, storage period 〉=3 month.
3. the catching agent for free formaldehyde produced of method according to claim 1, when it is characterized in that using with 90-110 weight part urea-formaldehyde resin adhesive and this catching agent for free formaldehyde of 4-8 weight part in container evenly stirring afterwards with joining with usefulness.
CNB2006100750465A 2006-03-30 2006-03-30 Free formaldehyde trapping agent and process for preparing same Expired - Fee Related CN100420723C (en)