CA2459031A1 - High torque battery terminal and method of making same - Google Patents
High torque battery terminal and method of making same Download PDFInfo
- Publication number
- CA2459031A1 CA2459031A1 CA002459031A CA2459031A CA2459031A1 CA 2459031 A1 CA2459031 A1 CA 2459031A1 CA 002459031 A CA002459031 A CA 002459031A CA 2459031 A CA2459031 A CA 2459031A CA 2459031 A1 CA2459031 A1 CA 2459031A1
- Authority
- CA
- Canada
- Prior art keywords
- battery terminal
- slug
- die
- punch
- finished
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
A battery terminal with high torque resistance utilizing three sided frusto-conical recesses and mating protrusions extending from the battery terminal and method of making the terminal by a cold forming process that forms a finished battery terminal from a preworked lead slug by driving one end of a punch through the slug to remove excess material and form an axial through hole, a second and third portion of the punch to close the die chamber and a fourth portion of the punch to radially expand the lead slug into a finished battery terminal. The dies for forming the battery terminal include a movable multiple-segmented die for collapsing radially inward around the slug and a frusto-conical die for forming the top portion of the battery terminal. An ejector sleeve removes the finished battery terminal after the cold forming process. In one method of the invention includes a cold-forming method of making a finished battery terminal with a necked down flange by first expanding the metal radially outward until the battery terminal die cavity is partially filled with metal and then upsetting the metal to complete the deformation filling of the battery terminal die cavity and to simultaneously form a necked down region in the flange on the battery terminal.
Applications Claiming Priority (7)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US07/940,391 | 1992-09-03 | ||
US07/940,391 US5296317A (en) | 1992-09-03 | 1992-09-03 | High torque battery terminal and method of making same |
US08/016,370 | 1993-02-11 | ||
US08/016,370 US5349840A (en) | 1992-09-03 | 1993-02-11 | Method of making a high torque battery terminal |
US08/029,869 US5373720A (en) | 1992-09-03 | 1993-03-11 | Method of making battery terminal with necked flange |
US08/029,869 | 1993-03-11 | ||
CA002103759A CA2103759C (en) | 1992-09-03 | 1993-08-10 | High torque battery terminal and method of making same |
Related Parent Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CA002103759A Division CA2103759C (en) | 1992-09-03 | 1993-08-10 | High torque battery terminal and method of making same |
Publications (2)
Publication Number | Publication Date |
---|---|
CA2459031A1 true CA2459031A1 (en) | 1994-03-04 |
CA2459031C CA2459031C (en) | 2005-11-01 |
Family
ID=32475443
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CA002459031A Expired - Fee Related CA2459031C (en) | 1992-09-03 | 1993-08-10 | High torque battery terminal and method of making same |
Country Status (1)
Country | Link |
---|---|
CA (1) | CA2459031C (en) |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP2460216A4 (en) * | 2009-07-31 | 2017-02-22 | Water Gremlin Company | Battery parts and associated systems and methods |
US9748551B2 (en) | 2011-06-29 | 2017-08-29 | Water Gremlin Company | Battery parts having retaining and sealing features and associated methods of manufacture and use |
US9917293B2 (en) | 2009-04-30 | 2018-03-13 | Water Gremlin Company | Battery parts having retaining and sealing features and associated methods of manufacture and use |
US9954214B2 (en) | 2013-03-15 | 2018-04-24 | Water Gremlin Company | Systems and methods for manufacturing battery parts |
US11038156B2 (en) | 2018-12-07 | 2021-06-15 | Water Gremlin Company | Battery parts having solventless acid barriers and associated systems and methods |
CN113680879A (en) * | 2021-08-25 | 2021-11-23 | 东莞市松正五金制品有限公司 | Terminal shell machining process |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6701998B2 (en) | 2002-03-29 | 2004-03-09 | Water Gremlin Company | Multiple casting apparatus and method |
US7338539B2 (en) | 2004-01-02 | 2008-03-04 | Water Gremlin Company | Die cast battery terminal and a method of making |
-
1993
- 1993-08-10 CA CA002459031A patent/CA2459031C/en not_active Expired - Fee Related
Cited By (14)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US10283754B2 (en) | 2004-01-02 | 2019-05-07 | Water Gremlin Company | Battery parts and associated systems and methods |
US10910625B2 (en) | 2009-04-30 | 2021-02-02 | Water Gremlin Company | Battery parts having retaining and sealing features and associated methods of manufacture and use |
US9917293B2 (en) | 2009-04-30 | 2018-03-13 | Water Gremlin Company | Battery parts having retaining and sealing features and associated methods of manufacture and use |
US9935306B2 (en) | 2009-04-30 | 2018-04-03 | Water Gremlin Company | Battery parts having retaining and sealing features and associated methods of manufacture and use |
US11942664B2 (en) | 2009-04-30 | 2024-03-26 | Water Gremlin Company | Battery parts having retaining and sealing features and associated methods of manufacture and use |
EP2460216A4 (en) * | 2009-07-31 | 2017-02-22 | Water Gremlin Company | Battery parts and associated systems and methods |
US9748551B2 (en) | 2011-06-29 | 2017-08-29 | Water Gremlin Company | Battery parts having retaining and sealing features and associated methods of manufacture and use |
US10181595B2 (en) | 2011-06-29 | 2019-01-15 | Water Gremlin Company | Battery parts having retaining and sealing features and associated methods of manufacture and use |
US10217987B2 (en) | 2013-03-15 | 2019-02-26 | Water Gremlin Company | Systems and methods for manufacturing battery parts |
US9954214B2 (en) | 2013-03-15 | 2018-04-24 | Water Gremlin Company | Systems and methods for manufacturing battery parts |
US11038156B2 (en) | 2018-12-07 | 2021-06-15 | Water Gremlin Company | Battery parts having solventless acid barriers and associated systems and methods |
US11283141B2 (en) | 2018-12-07 | 2022-03-22 | Water Gremlin Company | Battery parts having solventless acid barriers and associated systems and methods |
US11804640B2 (en) | 2018-12-07 | 2023-10-31 | Water Gremlin Company | Battery parts having solventless acid barriers and associated systems and methods |
CN113680879A (en) * | 2021-08-25 | 2021-11-23 | 东莞市松正五金制品有限公司 | Terminal shell machining process |
Also Published As
Publication number | Publication date |
---|---|
CA2459031C (en) | 2005-11-01 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CA2103759A1 (en) | High torque battery terminal and method of making same | |
US5296317A (en) | High torque battery terminal and method of making same | |
US4166373A (en) | Method of cold forming | |
US4416141A (en) | Method and apparatus for forming an electrical connector | |
US7360388B2 (en) | Hollow stepped shaft and method of forming the same | |
EP0000438B1 (en) | Process for producing tubular articles | |
JPH03242408A (en) | Manufacture of hollow engine-valve | |
CA2459031A1 (en) | High torque battery terminal and method of making same | |
US2751676A (en) | Method of cold working metal | |
US4217771A (en) | Method of cold forming | |
US1623059A (en) | Method of manufacturing seamless wrought-iron annealing boxes | |
US2874460A (en) | Process for manufacturing shells for spark plugs and the like | |
US3501790A (en) | Method of making blind rivet assemblies | |
US4271240A (en) | Lobed preparatory blank for cold extruding a cup-shaped article with hollow polygonal interior | |
JP2002346690A (en) | Method for forging metal part | |
US1480843A (en) | Method for the cold spurting of tubes and thin-walled metal pipes of lead, tin, and especially aluminium | |
EP0036050B1 (en) | Method of forming spark plug bodies | |
EP0080791A3 (en) | Method of and apparatus for shaping neck and providing terminal curl on can end | |
US1783261A (en) | Process and apparatus for making bullets | |
SU489564A1 (en) | Method for making thin-walled mold sleeves | |
JPS6229132B2 (en) | ||
JPH05277617A (en) | Method for forging flange product with step having long shaft | |
JPS6257414B2 (en) | ||
SU1303241A1 (en) | Method of cold extrusion of hollow taper articles | |
SU499916A1 (en) | Method of making hollow nipples |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
EEER | Examination request | ||
MKLA | Lapsed |