The method is applied in catalytical processes and ensures the derivation of mono-phasic, well-crystallised product. It is made by subjecting dealuminated clinoptilolite containing in weights %: silicon dioxide from 95.4 to 97.5 and dialuminium trioxide from 2.01to 3.45 to hydrothermal recrystallization in a solution of sodium base and piperidin, while the proportion between the organic reagent and the sodium base to the dialluminated material is from 1.4:1.0 to 0.3:1.0.