AT511686A1 - Asche-wärmedämmungsplatte - Google Patents
Asche-wärmedämmungsplatte Download PDFInfo
- Publication number
- AT511686A1 AT511686A1 AT9362011A AT9362011A AT511686A1 AT 511686 A1 AT511686 A1 AT 511686A1 AT 9362011 A AT9362011 A AT 9362011A AT 9362011 A AT9362011 A AT 9362011A AT 511686 A1 AT511686 A1 AT 511686A1
- Authority
- AT
- Austria
- Prior art keywords
- ash
- insulation panel
- plate
- ashes
- tried
- Prior art date
Abstract
Die Erfindung betrifft eine Wärmedämmplatte, wobei Asche mit einem Bindemittel vermengt und zu einer Platte geformt wird.
Description
Erfindung Aschenwärmedämmplatte
Kurze Erklärung wie es dazu gekommen ist:
Bel meiner Holzheizung habe ich die Asche immer ausgelehrt und im Freien auf ein Häufchen geschüttet. Da ich am Land lebe habe ich diese im Frühjahr mit dem Traktor in den Wald geführt. Jedes Mal ist mir aufgefallen, dass der Schnee schon lange überall weg war.
Unter der Asche war der Schnee aber noch Schön weiß nicht einmal Matschig.
Jetzt zur Idee oder (Erfindung)
Ich habe versucht eine Aschenplatte zu konstruieren, es ist mir aber nicht gleich gelungen das richtige Bindemittel zu finden.
Als ersten Schritt habe ich die Asche nur lose ca. 4-5cm in eine Zwischenwand gefüllt und Im Vergleich 8-1 Ocm Porozell oder(Styropor).
Mit zwei Funkthermometern habe ich den Unterschied festgestellt.
Bei diesem Versuch hält die Asche um 5'C länger, wie auch bei den anderen Versuchen mit der Aschenplatte in 12-24 Std.(Kälte oder Wärme) Also ein extremer Unterschied, die Platte ist zwar schwerer als Porozell, aber sie muss nicht stärker sein als 4-5 cm.
Zur Herstellung einer kleinen Versuchsplatte habe ich versucht die Asche mit Melaminharz zu mischen, dieses wäre aber in der Produktion zu teuer. Probiert habe ich es auch mit Harnstoffharz dieses wäre die günstigere Variante gegenüber Melaminharz, und funktioniert auch. Dieses wäre dann In der Herstellung (Wenn es Umsetzbar wäre) variabel und müsste sowieso in Labors getestet werden, aber die Grundidee mit Asche wäre nicht schlecht, ich weiß zwar nicht wie viel Asche überall zur Verfügung steht, aber die Hersteller könnten Sammelstellen einrichten.( Vielleicht geht es auch mit Vulkanasche, das habe ich zwar nicht versucht.)
Die Versuchsplatten habe ich mit einem Gasflämmer angeheitzt. Sie brennen auch nicht, wäre vielleicht in verschiedenen Einsatzbereichen ein Vorteil. Der Verputz hält auch auf der Platte. 25.06.2011
Schoby Michael am