AR205378A1 - Mejoras en un metodo para la fabricacion de vidrio que comprende los pasos de descargar una capa de vidrio fundido sobre la superficie de un charco de metal fundido de soporte - Google Patents
Mejoras en un metodo para la fabricacion de vidrio que comprende los pasos de descargar una capa de vidrio fundido sobre la superficie de un charco de metal fundido de soporteInfo
- Publication number
- AR205378A1 AR205378A1 AR258812A AR25881275A AR205378A1 AR 205378 A1 AR205378 A1 AR 205378A1 AR 258812 A AR258812 A AR 258812A AR 25881275 A AR25881275 A AR 25881275A AR 205378 A1 AR205378 A1 AR 205378A1
- Authority
- AR
- Argentina
- Prior art keywords
- glass
- cast
- puddle
- unloading
- manufacture
- Prior art date
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03B—MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03B18/00—Shaping glass in contact with the surface of a liquid
- C03B18/02—Forming sheets
- C03B18/04—Changing or regulating the dimensions of the molten glass ribbon
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03B—MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03B18/00—Shaping glass in contact with the surface of a liquid
- C03B18/02—Forming sheets
- C03B18/18—Controlling or regulating the temperature of the float bath; Composition or purification of the float bath
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Re-Forming, After-Treatment, Cutting And Transporting Of Glass Products (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US483508A US3926605A (en) | 1974-06-27 | 1974-06-27 | Method and apparatus for forming a ribbon of glass on a molten metal bath |
Publications (1)
Publication Number | Publication Date |
---|---|
AR205378A1 true AR205378A1 (es) | 1976-04-30 |
Family
ID=23920337
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
AR258812A AR205378A1 (es) | 1974-06-27 | 1975-01-01 | Mejoras en un metodo para la fabricacion de vidrio que comprende los pasos de descargar una capa de vidrio fundido sobre la superficie de un charco de metal fundido de soporte |
Country Status (14)
Country | Link |
---|---|
US (1) | US3926605A (nl) |
JP (1) | JPS5130218A (nl) |
AR (1) | AR205378A1 (nl) |
AU (1) | AU8046375A (nl) |
BE (1) | BE830703A (nl) |
BR (1) | BR7503705A (nl) |
DE (1) | DE2528240A1 (nl) |
DK (1) | DK284175A (nl) |
ES (2) | ES436951A1 (nl) |
FR (1) | FR2276272A1 (nl) |
IT (1) | IT1036147B (nl) |
NL (1) | NL7506804A (nl) |
NZ (1) | NZ177272A (nl) |
ZA (1) | ZA752440B (nl) |
Families Citing this family (25)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5375213A (en) * | 1976-12-17 | 1978-07-04 | V Nauchinooisusuredobuaterusuk | Production of plate glass |
US4360373A (en) * | 1981-04-02 | 1982-11-23 | Ppg Industries, Inc. | Method of and apparatus for controlling erosion of a refractory threshold |
JPH0529589Y2 (nl) * | 1987-11-07 | 1993-07-28 | ||
CN1923734B (zh) * | 2003-02-10 | 2010-11-03 | 日本电气硝子株式会社 | 生产玻璃产品的方法 |
JP4968631B2 (ja) * | 2003-02-10 | 2012-07-04 | 日本電気硝子株式会社 | 溶融ガラス供給装置及びガラス成形品の製造方法 |
KR101483918B1 (ko) * | 2006-06-30 | 2015-01-16 | 코닝 인코포레이티드 | 유리리본으로부터 생산되는 유리시트의 응력변화를 감소시키는 방법 및 장치 |
US8627684B2 (en) * | 2007-10-29 | 2014-01-14 | Corning Incorporated | Pull roll apparatus and method for controlling glass sheet tension |
CN102388003B (zh) | 2009-03-02 | 2014-11-19 | 苹果公司 | 用于强化用于便携式电子设备的玻璃盖的技术 |
US9778685B2 (en) | 2011-05-04 | 2017-10-03 | Apple Inc. | Housing for portable electronic device with reduced border region |
KR101377541B1 (ko) * | 2010-06-01 | 2014-03-26 | 주식회사 엘지화학 | 유리판 제조용 플로트 배스 및 플로트 유리 성형 방법 |
US10189743B2 (en) | 2010-08-18 | 2019-01-29 | Apple Inc. | Enhanced strengthening of glass |
US8824140B2 (en) | 2010-09-17 | 2014-09-02 | Apple Inc. | Glass enclosure |
US20120085130A1 (en) * | 2010-10-08 | 2012-04-12 | Hill Matthew D | Annealing of glass to alter chemical strengthening behavior |
US10781135B2 (en) | 2011-03-16 | 2020-09-22 | Apple Inc. | Strengthening variable thickness glass |
US9725359B2 (en) | 2011-03-16 | 2017-08-08 | Apple Inc. | Electronic device having selectively strengthened glass |
US9128666B2 (en) | 2011-05-04 | 2015-09-08 | Apple Inc. | Housing for portable electronic device with reduced border region |
US9944554B2 (en) | 2011-09-15 | 2018-04-17 | Apple Inc. | Perforated mother sheet for partial edge chemical strengthening and method therefor |
US9516149B2 (en) | 2011-09-29 | 2016-12-06 | Apple Inc. | Multi-layer transparent structures for electronic device housings |
US10144669B2 (en) | 2011-11-21 | 2018-12-04 | Apple Inc. | Self-optimizing chemical strengthening bath for glass |
US10133156B2 (en) | 2012-01-10 | 2018-11-20 | Apple Inc. | Fused opaque and clear glass for camera or display window |
US9946302B2 (en) | 2012-09-19 | 2018-04-17 | Apple Inc. | Exposed glass article with inner recessed area for portable electronic device housing |
US9459661B2 (en) | 2013-06-19 | 2016-10-04 | Apple Inc. | Camouflaged openings in electronic device housings |
US9593033B2 (en) | 2013-10-04 | 2017-03-14 | Corning Incorporated | Glass manufacturing apparatus and method for manufacturing glass sheet |
KR20240044359A (ko) * | 2022-09-28 | 2024-04-04 | 쇼오트 테크니컬 글래스 솔루션즈 게엠베하 | 낮은 광학 결함, 특히 낮은 근표면 굴절을 갖는 유리판, 이의 제조 방법 및 이의 용도 |
CN117970037B (zh) * | 2024-03-29 | 2024-06-07 | 昆明理工大学 | 一种基于sod变化的输电线路多重雷识别方法 |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
BE640207A (nl) * | 1962-11-20 | |||
GB1085010A (en) * | 1965-08-25 | 1967-09-27 | Ford Motor Co | Float method of manufacturing glass |
US3843346A (en) * | 1973-03-06 | 1974-10-22 | Ppg Industries Inc | Manufacture of sheet glass by continuous float process |
-
1974
- 1974-06-27 US US483508A patent/US3926605A/en not_active Expired - Lifetime
-
1975
- 1975-01-01 AR AR258812A patent/AR205378A1/es active
- 1975-04-16 ZA ZA752440A patent/ZA752440B/xx unknown
- 1975-04-18 NZ NZ177272A patent/NZ177272A/xx unknown
- 1975-04-23 AU AU80463/75A patent/AU8046375A/en not_active Expired
- 1975-04-25 ES ES75436951A patent/ES436951A1/es not_active Expired
- 1975-04-25 ES ES75436952A patent/ES436952A1/es not_active Expired
- 1975-06-03 IT IT68412/75A patent/IT1036147B/it active
- 1975-06-09 NL NL7506804A patent/NL7506804A/nl unknown
- 1975-06-12 BR BR4754/75D patent/BR7503705A/pt unknown
- 1975-06-23 DK DK284175A patent/DK284175A/da not_active Application Discontinuation
- 1975-06-24 JP JP50078534A patent/JPS5130218A/ja active Pending
- 1975-06-25 DE DE19752528240 patent/DE2528240A1/de active Pending
- 1975-06-26 FR FR7520076A patent/FR2276272A1/fr not_active Withdrawn
- 1975-06-26 BE BE157738A patent/BE830703A/xx unknown
Also Published As
Publication number | Publication date |
---|---|
IT1036147B (it) | 1979-10-30 |
ES436951A1 (es) | 1977-01-01 |
ES436952A1 (es) | 1977-01-01 |
FR2276272A1 (fr) | 1976-01-23 |
DE2528240A1 (de) | 1976-01-08 |
BE830703A (fr) | 1975-12-29 |
NL7506804A (nl) | 1975-12-30 |
US3926605A (en) | 1975-12-16 |
JPS5130218A (nl) | 1976-03-15 |
NZ177272A (en) | 1978-04-28 |
AU8046375A (en) | 1976-10-28 |
DK284175A (da) | 1975-12-28 |
BR7503705A (pt) | 1976-07-06 |
ZA752440B (en) | 1976-11-24 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
AR205378A1 (es) | Mejoras en un metodo para la fabricacion de vidrio que comprende los pasos de descargar una capa de vidrio fundido sobre la superficie de un charco de metal fundido de soporte | |
AR208084A1 (es) | Procedimiento para la manufactura de un laminado de peliculas | |
IT1062229B (it) | Metodo per ricoprire alluminio con un deposito di rame asportabile | |
IT1041222B (it) | Procedimento per indurire strati fotograici | |
SE7607950L (sv) | Elastomera reflekterande metallytor | |
IT972605B (it) | Procedimento per bonificare la superficie di elementi costut tivi costituiti di metalli leg geri | |
NO139969C (no) | Fremgangsmaate for fjerning av alkalimetallforurensninger fra smeltet aluminium | |
DK287475A (da) | Varslingsanordning til advarsel ved affladning af dek | |
FR2317348A1 (fr) | Composition adhesive applicable par extrusion en couche adhesive sur un support et procede pour sa fabrication | |
AR211814A1 (es) | Aparato para la fabricacion de vidrio plano mientras es sostenido sobre una superficie de un charco de metal en fusion | |
SE402358B (sv) | Forfarande for anbringande av ett fotopolymeriserbart kopieringsskikt pa en skiktberare av koppar resp en kopparlegering | |
AT301650B (de) | Verfahren zur Herstellung eines Hohlleiters | |
IT1047591B (it) | Metallo d apporto per giunti saldati | |
IT1070742B (it) | Metodo per preparare una composizione a base di copulante cromatico idrofilo ed elementi fotografici che la contengono | |
IT1029699B (it) | Metodo per controllare la planarita di una striscia in movimento | |
IT1047388B (it) | Procedimento per la fabbricazione di materiali metallici in nastro mediante colata | |
TR18572A (tr) | Karayolu satih kaplama malzemesinin imali icin usul | |
AR217084A1 (es) | Procedimiento para la aplicacion de un revestimiento reflectante sobre una superficie metalica y superficie reflectiva obtenida mediante el mismo | |
SE418076B (sv) | Forfarande for framstellning av en vidheftande tunn metalloxidfilm pa en glasyta | |
SE402653B (sv) | Forfarande for anbringande av ett fotopolymeriserbart kopieringsskikt pa en skiktberare av koppar resp en kopparlegering | |
AR198958A1 (es) | Dispositivo para medir los defectos opticos de un cuerpo | |
AT358067B (de) | Asbestfreie filterschicht fuer schichtenfilter | |
IT1038413B (it) | Metodo e complesso per riparare lingottiere | |
NO144596C (no) | Fremgangsmaate ved laminatfremstilling | |
SU497231A1 (ru) | Способ получени бората алюмини |