YU36637B - Method for the manufacture of a stretched oriented foil from polyethylene terephthalate of an electrical surface resistance of about 105
- Google Patents
Method for the manufacture of a stretched oriented foil from polyethylene terephthalate of an electrical surface resistance of about 105
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Priority claimed from DE1704766Aexternal-prioritypatent/DE1704766C3/en
Application filed by Hoechst AgfiledCriticalHoechst Ag
Publication of YU204668ApublicationCriticalpatent/YU204668A/en
Publication of YU36637BpublicationCriticalpatent/YU36637B/en
YU204668A1967-09-041968-09-02Method for the manufacture of a stretched oriented foil from polyethylene terephthalate of an electrical surface resistance of about 105
YU36637B
(en)