WO2011078968A2 - Method and system for fracturing a pattern using charged particle beam lithography with multiple exposure passes - Google Patents
Method and system for fracturing a pattern using charged particle beam lithography with multiple exposure passes Download PDFInfo
- Publication number
- WO2011078968A2 WO2011078968A2 PCT/US2010/059345 US2010059345W WO2011078968A2 WO 2011078968 A2 WO2011078968 A2 WO 2011078968A2 US 2010059345 W US2010059345 W US 2010059345W WO 2011078968 A2 WO2011078968 A2 WO 2011078968A2
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- shots
- shot
- exposure
- dosage
- pass
- Prior art date
Abstract
Description
Claims