US20220333464A1 - Systems and methods for cathodic protection of an oil and gas well system - Google Patents
Systems and methods for cathodic protection of an oil and gas well system Download PDFInfo
- Publication number
- US20220333464A1 US20220333464A1 US17/715,621 US202217715621A US2022333464A1 US 20220333464 A1 US20220333464 A1 US 20220333464A1 US 202217715621 A US202217715621 A US 202217715621A US 2022333464 A1 US2022333464 A1 US 2022333464A1
- Authority
- US
- United States
- Prior art keywords
- sucker rod
- component
- cathode
- anode
- string
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
System, assemblies, and methods for cathodic protection of one or more components of an oil and gas well may include an anode comprising an anodic coating on a surface of at least one first component of the oil and gas well. A cathode may comprise at least one second component of the oil and gas well, where the anode is configured to at least partially inhibit corrosion of the cathode.
Description
- This application claims the benefit of the filing date of U.S. Provisional Patent Application Ser. No. 63/175,233, titled “SYSTEMS AND METHODS FOR CATHODIC PROTECTION OF AN OIL PUMPING SYSTEM,” filed Apr. 15, 2021, the disclosure of which is hereby incorporated by this reference in its entirety.
- The present disclosure relates, according to some embodiments, to systems and methods of cathodic protection of an oil and gas well system (e.g., a pumping system) using an anodic coating.
- Sucker rod pumping systems are commonly used artificial lifting systems for oil wells. Suckers rods can be used to implement a rotary or linear reciprocating motion that provides mechanical energy to lift oil from bottom-hole to surface for further processing and refinement.
- However, many downhole components including sucker rods, tubing and pumps are made of carbon steel that readily corrodes when introduced to oil compositions containing water and corrosive agents (e.g., acids, oxidizers, bases) including H2S, CO2, O2, and chlorides. Corrosion of downhole components lead to pitting that may lead to fatigue and corrosion cracking of components that is formed at the base of a corrosion pit. This fatigue can be somewhat exacerbated by the cyclic loading nature of sucker rod-driven artificial lifting where cracks often initiate at high stress points on the sucker rod and can lead to a reduction in the rod cross-section to the point where the rod cannot carry the load and fails. Further, as many oil well systems age and use up the readily available oil deposits, operators must dig deeper to find more oil. Since the deeper oil reserves tend to contain hotter and more corrosive (e.g., acids, oxidizers, bases) fluids, digging deeper leads to even more corrosion on the downhole components causing sucker rod pumping system component failure. Also as wells age and production rates decrease, operators often use enhanced recovery methods such as water and steam flooding, or cyclic steam injection to help boost production. Unfortunately, these methods also introduce large amounts of H2O which increases corrosion.
- Some known corrosion mitigation techniques involve the use of chemical corrosion inhibitors. While these inhibitors may have some effectiveness, they are often difficult to transport to the sites of corrosion and can often be incompatible with other downhole pump components such as elastomeric parts. Another strategy involves the use of metal alloys that are inherently more corrosion resistant than general carbon steel components. However, these alloys are generally not cost effective as their production cost outweighs their often incremental performance benefit.
- A third method of protecting sucker rods includes coating the sucker rods with polymeric coatings that are protective against corrosive agents. These include thermoplastic polymer coatings (e.g., polyethylene) and thermosetting fusion bonded epoxy (FBE) coatings. The thermoplastic polymer coating technique does not bond well with the sucker rod surface and is prone to disbondment. This leads to a limitation of the depth of well in which this coated coiled rod string can be installed. The deeper the well, the more squeeze pressure the injector units, which deploy and retrieve coiled sucker rod strings from wells, need to hold onto the sucker rod strings. Since the thermoplastic polymer coating does not bond well enough, the squeeze pressure strips or sloughs off the polymer coating from the sucker rod surface. This is especially true when trying to retrieve the coated sucker rod string from the well after it has been down hole for any period of time. Once the thermoplastic polymer coating strips or sloughs off, the sucker rod metal is left unprotected and will begin to corrode. Additionally, thermoplastic polymer coating that has fallen off can plug flow lines. If the coating peels while in the well bore, the loose coating can plug the pump and/or the flow lines, leading to unwanted and expensive repairs.
- Fusion bonded epoxy coatings provide a modest protection against corrosion caused by contact with down well chemicals, but such coatings are also subject to abrasion. Additionally, application of fusion bonded epoxy coating systems involves complicated, timely, and costly procedures. As these coatings are worn, corrosion protection is lost and repairs to such systems are problematic and expensive.
- Another downfall of known sucker rod corrosion protection methods is that they generally protect only the sucker rods and leave other downhole components prone to corrosion and degradation. Therefore, systems and methods are needed that not only protect the sucker rods, but that also protect other system components against corrosive agents. Additionally, systems and methods are needed that are operable to protect downhole components even after both physical wear and corrosion has occurred on the sucker rods.
- In some aspects, the techniques described herein relate to a sucker rod pumping system for cathodic protection of components, the system including: an anode including an anodic coating on a surface of a body of a sucker rod string including one or more sucker rods; and a cathode including one or more of: a tubing string including a cylinder and configured to concentrically contain the sucker rod string, a polished rod, and a pump; the polished rod configured to be connected to a polished rod clamp above ground and to be connected to a top end of the sucker rod string contained below the ground; or the pump mechanically connected to a bottom end of the sucker rod string, wherein the anode is configured to at least partially inhibit corrosion of the cathode.
- In some aspects, the techniques described herein relate to a method for cathodic protection using the sucker rod pumping systems discussed in this section.
- In some aspects, the techniques described herein relate to a system for cathodic protection of one or more components of an oil and gas well, the system including: an anode including an anodic coating on a surface of at least one first component of the oil and gas well; a cathode including at least one second component of the oil and gas well that is connected to and configured to be positioned in a location that is uphole or downhole from the at least one first component; and at least one electrically conductive connection line electrically coupling the at least one first component and the at least one second component, wherein the anode is configured to at least partially inhibit corrosion of the cathode.
- In some aspects, the techniques described herein relate to a method for cathodic protection of components of a sucker rod pumping system, the method including: applying an anodic coating on a surface of at least one first component of the oil and gas well to form an anode component; electrically connecting, via a conductive connection, the anode component to a cathode component including at least one second component of the oil and gas well; and at least partially inhibiting corrosion of the cathode component with the anode component.
- Features from any of the disclosed embodiments may be used in combination with one another, without limitation. In addition, other features and advantages of the present disclosure will become apparent to those of ordinary skill in the art through consideration of the following detailed description and the accompanying drawings.
- The drawings illustrate several embodiments of the present disclosure, wherein identical reference numerals refer to identical or similar elements or features in different views or embodiments shown in the drawings.
-
FIG. 1 is an elevational view of a pumping system according to embodiments of the disclosure. -
FIG. 2 is an elevational view of a pumping system according to embodiments of the disclosure. -
FIG. 3 illustrates a cross-sectional view of a coating on at least one component of an oil and gas well according to embodiments of the disclosure. -
FIG. 4 illustrates a cross-sectional view of a coating on at least one component of an oil and gas well according to embodiments of the disclosure. - As used herein, relational terms, such as “first,” “second,” “top,” “bottom,” etc., are generally used for clarity and convenience in understanding the disclosure and accompanying drawings and do not connote or depend on any specific preference, orientation, or order, except where the context clearly indicates otherwise.
- As used herein, the term “and/or” means and includes any and all combinations of one or more of the associated listed items.
- As used herein, the terms “vertical,” “upper,” “lower,” and “lateral” refer to the orientations as depicted in the figures. Further, when used herein in reference to a location in, or relative to, a wellbore, the terms “above,” “upper,” and “uphole” mean and include a relative position proximate the surface of the well, whereas the terms “below,” “lower” and “downhole” mean and include a relative position distal the surface of the well.
- The term “surface” may indicate the surface of the Earth on which a portion of pumping assembly for a well is positioned where the well or borehole extending through and below the surface.
- The present disclosure relates to the application of an anodic coating (e.g., metal anodic coating) on a portion of either a coiled or conventional sucker rod that synergistically provides for a cathodic protection against corrosion for downhole and above-well components of a sucker rod pumping system. The anodic coating (e.g., aluminum, zinc, and/or magnesium) may act as a sacrificial anode that will corrode in place of sucker rod pumping system components acting as a cathode, thereby protecting the cathodic components from corrosion. Each of the sucker rod pumping system components may be electrically connected in a continuous circuit so that the corrosion protection provided to the sucker rod by the anodic coating will also provide similar protection to all other system components.
- In some embodiments, in addition to providing corrosion protection to the sucker rod, an anodic coating may improve (e.g., decrease) the coefficient of friction by up to 25% in comparison to the underlying metal alone, where the metal alone would exhibit a coefficient of friction that is greater than the coefficient of friction of the anodic coating. The relatively more soft, ductile, and malleable anodic coating may provide surfaces having a relatively lower coefficient of friction, more desirable wear, and self-healing characteristics as is discussed below.
- Besides providing corrosive protection for down-well components, embodiments of the disclosed anodic coated sucker rods may advantageously exhibit self-healing properties in response to wear. As previously described, wear ruins the polymeric protective barriers of previously known systems by causing the barriers to slough off in chunks, thereby exposing the underlying metals. Instead of being removed in chunks, the disclosed anodic coating wears in small portions, which then self-heals through a smearing action of the coating to cover the sucker rod portions that were exposed through wear. Additionally, even when localized damage to portions of the anodic coating occurs, corrosion protection of system components is not disrupted since the anodic coating contacts the entire sucker rod string so that the electrical circuit created through galvanic coupling of the cathode and anode is not disrupted. For example, full cathodic protection may be provided by a system where from 30% to 40% of the anodic coating has been worn off.
- Application of an anodic coating on a coiled or conventional sucker rod as is presented herein includes coating a portion of an entirety of sucker rod. For example, a sucker rod may have a surface that is about 0.1% coated with the anodic coating, or about 5% coated, or about 10% coated, or about 15% coated, or about 20% coated, or about 25% coated, about 30% coated, or about 35% coated, or about 40% coated, or about 45% coated, about 50% coated, or about 55% coated, or about 60% coated, or about 65% coated, or about 70% coated, or about 75% coated, or about 80% coated, or about 85% coated, or about 90% coated, or about 95% coated, or about 100% coated, where about includes plus or minus 2.5%. A coating may include any geometric design. A coating may be applied on a sucker rod as a longitudinal strip and as multiple longitudinal strips. For example, a coating may be applied on a sucker rod as two longitudinal strips that are diametrically opposed to each other. A coating may be applied circumferentially around a sucker rod. For example, a coating may be applied at one or more circumferential strips around a sucker rod. In some embodiments, coated sucker rods and non-coated sucker rods are connected in an alternative series along a sucker rod string.
- A self-healing capability of disclosed cathodic protection methods and systems is in part driven by an inclusion of anodic coatings containing soft metals including aluminum, zinc, magnesium, and/or alloys thereof. Soft metal anodic coating compositions smear in the presence of heat and friction to recoat exposed sucker rod surfaces. Additionally, anodic coating made of relatively soft metals (e.g., aluminum) may wear away instead of spalling off in larger pieces or splinters as do conventional polymeric coatings (e.g., FBE and thermoplastic polymer coatings). Therefore, anodic coatings used herein will not generally plug up flow lines or contaminate production fluids. Additionally, anodic coatings according to embodiments disclosed herein do not tend to as readily spall off of the sucker rod surfaces while being serviced as compared to either fusion bonded epoxy or thermoplastic polymer coatings.
- In some embodiments, a cathodic protection system disclosed herein may include a sealant on a portion of an anodic coating. For example, a sucker rod may include an anodic coating on a surface of the sucker rod and a sealant on a surface of the anodic coating. A sealant may be organic, inorganic, or a mixture thereof. An organic sealant may include an epoxy, a silicone, and a phenol resin. A sealant may include a moisture cured urethane, a urethane, a clear single component moisture cured urethane, a clear two components (2k) aliphatic polyurethane, and combinations thereof.
- A sealant may advantageously fill the porosity of the anodic coating and may provide physical wear protection of the anodic coating. In some embodiments, a sealant may negate a portion of a cathodic protection provided by an anodic coating until it is worn off of the anodic coating. A sealant may be applied to all or only a portion of the anodic coating contained on a surface of the sucker rod. For example, a sucker rod may have a surface of the anodic coating that is 0.1% sealed with a sealant, or about 5% sealed, or about 10% sealed, or about 15% sealed, or about 20% sealed, or about 25% sealed, about 30% sealed, or about 35% sealed, or about 40% sealed, or about 45% sealed, about 50% sealed, or about 55% sealed, or about 60% sealed, or about 65% sealed, or about 70% sealed, or about 75% sealed, or about 80% sealed, or about 85% sealed, or about 90% sealed, or about 95% sealed, or about 100% sealed, where about includes plus or minus 2.5%.
- Disclosed in the present application are methods and systems for cathodic protection of a pumping system (e.g., a sucker rod pumping system for an oil and gas well). As shown in
FIG. 1 , a suckerrod pumping system 100 includes an anode and a cathode. For example, as discussed below, existing components of thesystem 100 may be used as the anode and/or the cathode, such that these components perform their traditional functions while providing or benefiting from added protective features (e.g., corrosion protection) provided by existing component of the suckerrod pumping system 100. By way of example, and as discussed below, an anode may be provided with an anodic coating on one or more components of the suckerrod pumping system 100. For example, a surface of a body of asucker rod string 115 that has one or more sucker rods may have theanodic coating 101 applied thereto (e.g., theanodic coating 101 applied on one or more of the sucker rods of the sucker rod string 115). In additional embodiments, other components of the suckerrod pumping system 100 may function as the anode and may include theanodic coating 101. - The
system 100 may include on or more components (e.g., positioned uphole or downhole relative to the anode) that may be cathodes, including, for example, a progressive cavity (PC)pump 125, atubing string 105, asucker rod string 115, apolished rod 120, acasing head 180, atubing head 170, a composite pumping tee (CPT) 110, a surfacecasing vent line 190, aflow line 140, aflow tee 150, atubing hanger 160, apolished rod clamp 130, and asurface drive unit 135. In additional embodiments, other components of the suckerrod pumping system 100 may function as the cathode. - In some embodiments, and as discussed above, the components acting as the anode and cathode may be electrically connected to one another. Such electrical connection may be an electrically conductive connection line that connects the components. As a depicted example in
FIG. 1 , asimplified connection line 145 is shown extending between thesucker rod string 115 and theprogressive cavity pump 125. Thesimplified connection line 145 may be internal to, external to, and/or integral with the components acting as the anode and cathode and any intervening components. - By way of example, in use, a positive charge may be applied to
anodic coating 101 such that at least a portion of the sucker rod string 115 (e.g., or other selected components) acts as an anode. An opposite charge may be applied to another component or components that are selected as one or more cathodes to be protected (e.g., theprogressive cavity pump 125 or other selected components). For example, a negative charge may be applied to theprogressive cavity pump 125 such that at least a portion of theprogressive cavity pump 125 acts as a cathode. - A sucker rod
rotary pumping system 100 includes a string oftubing 105 containing cylinder and is configured to concentrically contain asucker rod string 115, apolished rod 120, and aPC pump 125. Asystem 100 may include aproduction casing 185 that is located below ground that includes a cylindrical interior cavity that is configured to surround thetubing 105 in a cylindrical manner (e.g., cylindrically surround in a lateral or radially direction). Aproduction casing 185 may have acasing head 180 at the top of theproduction casing 185. Acasing head 180 may mechanically connect aproduction casing 185 to atubing head assembly 170. Additionally, acasing head 180 may include a surfacecasing vent line 190 that is mechanically connected to thecasing head 180 and extends from the casing head and end above ground. The surfacecasing vent line 190 permits gas migration from below ground to the surface. Each of atubing string 105, asucker rod string 115, apolished rod 120, aproduction casing 185, acasing head 180, atubing head assembly 170, and a surfacecasing vent line 190 may be a cathode that is protected from corrosion through inclusion of an anodic coating surface on a body of asucker rod string 115. - As shown in
FIG. 1 , a suckerrod pumping system 100 may include apolished rod 120 that connects to apolished rod clamp 130 both located above ground. The bottom of thepolished rod 120 may mechanically connect to a top end of asucker rod string 115. Apolished rod 120 may partially protrude above ground from a center of atubing head assembly 170 and may be partially housed below ground within the interior cavity of theproduction casing 185. The bottom end of thesucker rod string 115 may mechanically connect to a top end of aprogressive cavity pump 125 that is located towards the bottom of theproduction casing 185. In some embodiments, aprogressive cavity pump 125 or plunger pump may be switched out for an electric submersible pump (ESP) artificial lift system. - The
system 100 may include asucker rod string 115 containing one or more sucker rods. Each sucker rod in thesucker rod string 115 includes a first threaded end, a second threaded end, a solid cylinder, and ananodic coating 101 on a surface of a body of the sucker rod. Application of theanodic coating 101 onto a sucker rod or coiledsucker rod string 115 surface includes a surface preparation and blasting step and a thermal anodic coating spray step. The thermal anodic coating spray step may involve a process where melted or heated anodic coating is sprayed onto the sucker rod surface. Ananodic coating 101 may be applied onto an outside surface of the sucker rod individually or onto a coiledsucker rod string 115. Theanodic coating 101 may be applied as thin as 0.20 millimeter (0.008 in.) as thick as 0.51 millimeters (0.020 in.), or it may be applied to other thicknesses according to design needs. - In some embodiments, the
anodic coating 101 may comprise a suitable electrically conductive material, such as, for example, a metallic, semi-metallic, and/or graphitic material. For example, theanodic coating 101 may include, without limitation, copper, tungsten carbide, cobalt, aluminum, magnesium, zinc, iron, platinum, palladium, niobium, graphite, graphene, nichrome, gold, silver, alloys thereof, any suitable metallic material, and/or any other suitable electrically conductive material, without limitation. - The sucker
rod pumping system 100 may include other components such as asurface drive unit 135 attached to atubing head 170 through acomposite pumping tee 110. Atubing head 170 may be mechanically connected to atubing hanger 160. A tubing hanger may include one ormore flow lines 140 that may transfer produced oil from the well to any form of known oil collection vessel or oil transport system. Aflow line 140 may connect to acomposite pumping tee 110 through aflow tee 150. - The present disclosure relates to methods of cathodic protection of downhole components of a sucker
rod pumping system 100. A method includes a step of producing oil using a suckerrod pumping system 100 including an anode and a cathode as described herein where the anode protects the cathode from corrosion. - In some embodiments, as is shown in
FIG. 2 , a pumping system includes a reciprocating suckerrod pumping system 200 including an anodic coating on a surface of a body of asucker rod string 115. Asystem 200 includes aprime mover 205 mechanically connected to abeam pumping unit 210 including ahorsehead 215. Theprime mover 205 provides mechanical energy to thebeam pumping unit 210 and thehorsehead 215, which translates into a reciprocating motion for down well components through thepolished rod 120. Thehorsehead 215 may be mechanically connected to thepolished rod 120 through acarrier bar 220. Thepolished rod 120 is partially contained above the surface as well as below the surface and transitions through awellhead 225, which caps the top of the well.System 200 includes asurface casing 230 that concentrically contains agas flow 235, anoil flow 240, anintermediate casing 245, aproduction casing 185, aproduction tubing 105, and asucker rod string 115. As shown inFIG. 2 , anintermediate casing 245 goes deeper into the ground than thesurface casing 230 and concentrically contains aproduction casing 185. Theproduction casing 185 concentrically contains thesucker rod string 115, atubing anchor 250, apump 255 and ends atperforations 260 that may provide effective flow communication between thesystem 200 and the oil reservoir. - A
reciprocating rod system 200, as shown inFIG. 2 may include a sucker rod orsucker rod string 115 containing an anodic coating that may provide cathodic protection to one or more of apolished rod 120, awellhead 225, asurface casing 230, anintermediate casing 245, aproduction casing 185, aproduction tubing 105, atubing anchor 250, and apump 255. In some embodiments, a system includes a cathode including thepolished rod 120, thewellhead 225, thesurface casing 230, theintermediate casing 245, theproduction casing 185, theproduction tubing 105, thetubing anchor 250, and thepump 255. - The corrosion and wear associated with downhole systems reduces the lifespan of sucker rod pump systems. Embodiments of disclosed systems and methods for cathodic protection of sucker rod pump systems may relatively increase the lifespan of and therefore reduces operating costs of using the sucker rod pump systems to produce oil from an oil well.
- As is shown in Table 1 below, a disclosed anodic coating outperforms comparative thermosetting fusion bonded epoxy (FBE) and polyethylene coatings. Even when using a thinner anodic coating (e.g., 10-20 mils), it provides for both barrier and cathodic protection whereas FBE and polyethylene coatings only provide barrier protection. Anodic coatings are generally impermeable to fluids whereas FBE and polyethylene coatings are semi-permeable. Being impermeable to fluids advantageously minimizes or prevents fluid ingress between the coating and the sucker rod metal substrate since entrapped fluid may corrode the metal substrate and lead to a detachment of the coating from the surface of the metal substrate. Anodic coatings as disclosed herein may have virtually or substantially no limit to clamping pressure of the rod injector used to either deploy or retrieve a coiled sucker rod, whereas FBE and polyethylene coatings both have limitations. Additionally, anodic coatings generally have no depth or handling equipment limitations whereas FBE and polyethylene coatings both do. As is shown in Table 1, the response to mechanical damage of an anodic coating is to smear, whereas FBE gouges off and polyethylene coatings peel off. Anodic coatings have excellent adhesion, whereas FBE has good and polyethylene coatings have fair. Additionally, anodic coatings require no special coating disposal. Also, anodic coated sucker rods may operate at temperatures of over 200 ° C. where FBE is limited to about 90° C.
-
TABLE 1 Comparison of Anodic Coatings to FBE and Polyethylene Coating Anodic Polyethylene Property coating FBE Coating Thickness (mils) 10-20 20-30 125-250 Corrosion resistance Form of protection Cathodic Barrier Barrier and barrier Permeable No Yes Yes Serviceability Clamping pressure No limit Limited Limited Depth limitation None Yes Yes Handling equipment None Yes Yes Response to Smear Gouge Peel mechanical damage Adhesion Excellent Good Fair Disposal of Standard N/A Special rod/coating Operating +200° C. ~90° C. <90° C. temperature -
FIG. 3 illustrates a cross-sectional view of a coating on at least one component of an oil and gas well (e.g., sucker rod 300). As shown inFIG. 3 , thecoating 302 may be applied about a circumference of the sucker rod 300 (e.g., an entire circumference). - As also depicted in an idealized schematic form, a
conductive element 304 may couple thesucker rod 300 to anothercomponent 306 of the oil and gas well. As above, theconductive element 304 may be internal to, external to, and/or integral with thesucker rod 300 and the anothercomponent 306 acting as the anode and cathode, respectively, and any intervening components. -
FIG. 4 illustrates a cross-sectional view of a coating on at least one component of an oil and gas well (e.g., sucker rod 400). As shown inFIG. 4 , thecoating 402 may be applied at selected locations about a circumference of thesucker rod 400. For example, as discussed above, thecoating 402 may applied as one or morelongitudinal strips 404 extending along a length of the sucker rod 400 (e.g., along a longitudinal axis of the sucker rod 400). In some embodiments, thecoating 402 may be applied onsucker rod 400 as two or more longitudinal strips 404 (e.g., two, three, four, or more) that are positioned on opposing about thesucker rod 400. - As also depicted in an idealized schematic form, a
conductive element 406 may couple thesucker rod 400 to anothercomponent 408 of the oil and gas well. As above, theconductive element 406 may be internal to, external to, and/or integral with thesucker rod 400 and the anothercomponent 408 acting as the anode and cathode, respectively, and any intervening components. - While various aspects and embodiments have been disclosed herein, other aspects and embodiments are contemplated. The various aspects and embodiments disclosed herein are for purposes of illustration and are not intended to be limiting.
- Terms of degree (e.g., “about,” “substantially,” “generally,” etc.) indicate structurally or functionally insignificant variations. In an example, when the term of degree is included with a term indicating quantity, the term of degree is interpreted to mean±10%, ±5%, or +2% of the term indicating quantity. In an example, when the term of degree is used to modify a shape, the term of degree indicates that the shape being modified by the term of degree has the appearance of the disclosed shape. For instance, the term of degree may be used to indicate that the shape may have rounded corners instead of sharp corners, curved edges instead of straight edges, one or more protrusions extending therefrom, is oblong, is the same as the disclosed shape, etc.
Claims (20)
1. A sucker rod pumping system for cathodic protection of components, the system comprising:
an anode comprising an anodic coating on a surface of a body of a sucker rod string comprising one or more sucker rods; and
a cathode comprising one or more of:
a tubing string comprising a cylinder and configured to concentrically contain the sucker rod string, a polished rod, and a pump;
the polished rod configured to be connected to a polished rod clamp above ground and to be connected to a top end of the sucker rod string contained below the ground; or
the pump mechanically connected to a bottom end of the sucker rod string,
wherein the anode is configured to at least partially inhibit corrosion of the cathode.
2. The sucker rod pumping system of claim 1 , wherein each sucker rod of the sucker rod string further comprises:
a first threaded end and a second threaded end; and
a body exhibiting a substantially cylindrical shape.
3. The sucker rod pumping system of claim 1 , wherein the anodic coating comprises at least one of aluminum, magnesium, zinc, or an alloy of aluminum, magnesium, or zinc.
4. The sucker rod pumping system of claim 1 , wherein the cathode further comprises a production casing configured to be located below the ground, the production casing comprising a cylindrical interior cavity configured to cylindrically contain the tubing string, the polished rod, at least a portion of the sucker rod string, and the pump.
5. The sucker rod pumping system of claim 4 , wherein the cathode further comprises a casing head and a tubing head assembly, the tubing head assembly configured to be located partially above the ground and mechanically connected to the production casing through the casing head.
6. The sucker rod pumping system of claim 5 , wherein the polished rod is configured to partially protrude above the ground from a center of the tubing head assembly and to be partially housed below the ground within the cylindrical interior cavity of the production casing.
7. The sucker rod pumping system of claim 5 , wherein the cathode further comprises a surface casing vent line mechanically connected to the casing head, the surface casing vent line configured to extend from the casing head and to end above the ground.
8. The sucker rod pumping system of claim 1 , wherein only a portion of the surface of the body of the sucker rod string is coated with the anodic coating.
9. The sucker rod pumping system of claim 8 , wherein the anodic coating is applied in circumferential strips around the body of the sucker rod string.
10. The sucker rod pumping system of claim 1 , wherein the anode further comprises a sealant on at least a portion of the body of the sucker rod string.
11. A method for cathodic protection of components of a sucker rod pumping system, the method comprising producing oil using the sucker rod pumping system of claim 1 .
12. A system for cathodic protection of one or more components of an oil and gas well, the system comprising:
an anode comprising an anodic coating on a surface of at least one first component of the oil and gas well;
a cathode comprising at least one second component of the oil and gas well that is connected to and configured to be positioned in a location that is uphole or downhole from the at least one first component; and
at least one electrically conductive connection line electrically coupling the at least one first component and the at least one second component,
wherein the anode is configured to at least partially inhibit corrosion of the cathode.
13. The system for cathodic protection of claim 12 , wherein the cathode and the anode comprise portions of a downhole artificial lift system.
14. The system for cathodic protection of claim 13 , wherein the anode comprises at least a portion of a rod string of the downhole artificial lift system.
15. The system for cathodic protection of claim 13 , wherein the cathode comprises at least one of a tubing string, a polished rod, a pump, a sucker rod string, a casing head, a tubing head, a composite pumping tee, a casing vent line, a flow line, a flow tee, a tubing hanger, a polished rod clamp, or a surface drive unit.
16. A method for cathodic protection of components of a sucker rod pumping system, the method comprising:
applying an anodic coating on a surface of at least one first component of the oil and gas well to form an anode component;
electrically connecting, via a conductive connection, the anode component to a cathode component comprising at least one second component of the oil and gas well; and
at least partially inhibiting corrosion of the cathode component with the anode component.
17. The method of claim 16 , further comprising forming the cathode component and the anode component with existing components of a downhole artificial lift system, each of the cathode component and the anode component configured to perform another function related to the oil and gas well.
18. The method of claim 17 , further comprising forming the cathode component with at least one of a tubing string, a polished rod, a pump, a sucker rod string, a casing head, a tubing head, a composite pumping tee, a casing vent line, a flow line, a flow tee, a tubing hanger, a polished rod clamp, or a surface drive unit.
19. The method of claim 16 , further comprising applying a sealant to a portion of the anode component.
20. The method of claim 16 , further comprising applying the anodic coating to only a portion of a rod string of a downhole artificial lift system.