Solid-Phase Diffusion Into Metallic Material Surfaces
(AREA)
Abstract
A method for hardening parts from high-alloyed heat resistant steel VKS-5 includes chemical-thermal treatment, which is carried out by a method of gas carbonitriding in the furnace at a temperature of 850- for 6-8 hours. At that during all the process of treatment the control and holding of the carbon potential of saturating gas mixture are carried out.
UAU201403489U2014-04-042014-04-04Method for hardening parts from high-alloyed heat resistant steel VKS-5
UA92672U
(en)
Process gas treatment device for the treatment of process gas for an industrial furnace installation, and industrial furnace installation for gas carburizing and for hardening of metallic workpieces