A method for delignification of raw material with production of fiber half-finished product includes addition of chaff of non-wooden plant raw material and boiling solution followed by chaff boiling at given modes. Chaff boiling is carried out with sodium-based neutral-sulfite solution, with decreased content of total SOfrom 20 to 25 g/dm, at a temperature of 180 and 190 °C, hydro-module of 5:1, for 110-150 minutes.