UA89736C2 - Method for deoxidatin of steel in ladle - Google Patents

Method for deoxidatin of steel in ladle

Info

Publication number
UA89736C2
UA89736C2 UAA200900713A UAA200900713A UA89736C2 UA 89736 C2 UA89736 C2 UA 89736C2 UA A200900713 A UAA200900713 A UA A200900713A UA A200900713 A UAA200900713 A UA A200900713A UA 89736 C2 UA89736 C2 UA 89736C2
Authority
UA
Ukraine
Prior art keywords
desoxidant
melt
ladle
lump
steel
Prior art date
Application number
UAA200900713A
Other languages
Russian (ru)
Ukrainian (uk)
Inventor
Эдгар Шумахер
Эвалд Шумахер
Анатолий Константинович Белитченко
Геннадий Аркадьевич Лозин
Игорь Витальевич Деревянченко
Виктор Николаевич Хлопонин
Владимир Константинович Туровский
Александр Николаевич Савьюк
Константин Филиппович Дорн
Владимир Владимирович Яковенко
Рената Францки
Александр Хешеле
Original Assignee
Техком Гмбх
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Техком Гмбх filed Critical Техком Гмбх
Priority to UAA200900713A priority Critical patent/UA89736C2/en
Publication of UA89736C2 publication Critical patent/UA89736C2/en

Abstract

The invention relates to producing a high-quality low-carbon steel. The inventive ladle steel deoxidation method consists in introducing granulated or lump desoxidant, the density of which is less than the density of a melt in a ladle, in to a said melt. Said desoxidant is introduced during the melt pouring off a production unit into the ladle by means of a concentrated high-rate flow, the impulse of which allows the desoxidant to penetrate directly inside the melt. The desoxidant is introduced into the melt stream with the aid of a shotblast machine. The desoxidant is embodied in the form of a granulated or lump aluminium of a size ranging from 0.5 to 12.0 mm. The use of the invention makes it possible to reduce the desoxidant loss by two times, to increase the recovery thereof and to improve the metal quality.
UAA200900713A 2006-06-30 2006-06-30 Method for deoxidatin of steel in ladle UA89736C2 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
UAA200900713A UA89736C2 (en) 2006-06-30 2006-06-30 Method for deoxidatin of steel in ladle

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
UAA200900713A UA89736C2 (en) 2006-06-30 2006-06-30 Method for deoxidatin of steel in ladle

Publications (1)

Publication Number Publication Date
UA89736C2 true UA89736C2 (en) 2010-02-25

Family

ID=50693017

Family Applications (1)

Application Number Title Priority Date Filing Date
UAA200900713A UA89736C2 (en) 2006-06-30 2006-06-30 Method for deoxidatin of steel in ladle

Country Status (1)

Country Link
UA (1) UA89736C2 (en)

Similar Documents

Publication Publication Date Title
UA96303C2 (en) Method and system for pouring slag and/or steel melt from tiltable vessel into receiving vessel
CN102796963B (en) Martensitic stainless steel rectangular billet continuous casting method
CN104862443A (en) Smelting method for low-carbon low-silicon wire-welding steel
CN103056343B (en) Trimetal composite cast crusher hammer production process method
PT2039785E (en) Ladle steel deoxidation method
CN105586531A (en) Production method capable of effectively controlling quality of 37Mn round pipe billet steel casting blank
TW200724263A (en) Process for producing ultra-low-carbon cast slab
UA89736C2 (en) Method for deoxidatin of steel in ladle
MY164762A (en) Method for manufacturing stainless steel
CN104152782A (en) Process method for casting corrosion-resistant heat-resistant steel by induction furnace
CN102312152B (en) Production method of steel containing boron
CN102816889A (en) Smelting method of pseudo rimmed steel H08A
Yu et al. Optimization of production process in Shougang No. 3 steel plant
CN202482353U (en) Sulfur cored wire
CN202090016U (en) Ferro-silicon-aluminum deoxidizing block
CN105861774A (en) Casting method for reducing nodulation rate during casting of aluminum steel tank for small square billet high-carbon steel
Guo et al. Production practice of 150 mm x 150 mm concasting billet of steel ML 08 Al.
He et al. Improvement of central segregation in SWRH 82 B continuous casting bloom.
CN202284211U (en) Pure aluminum rod used for deoxidization
Tian Model of prediction for end temperature of molten steel in CAS refining.
CN202090019U (en) Moss type deoxygenation aluminium block
Mukhopadhyay et al. Determination of Slag Basicity by pH Method.
UA97924C2 (en) A composition is used in the ferrous metallurgy in the steel production
UA84098C2 (en) Method for production of steel blank
Xiu Cause analysis and control measures of longitudinal cracks on the surface of continuous casting slabs.