A refractory concrete mix of high strength and thermal resistance contains: 64.0-71.0 % by weight ofelectrocorundum, 12.0-18.0 % by weight of silicon carbide, 4.0-6.0 % by weight of alumina, 2.0-4.0 % by weight of crystalline silicon, 2.0-4.0 % by weight of aluminate cement, 0.1-0.3 % by weight of metal aluminum, 2.0-9.0 % by weight of carbide-silicon-containing waste of electrode production graphitization and 0.1-1.5 % by weight of plasticizer. It is designed for making lining for discharge of cast iron in blast furnaces, hot-metal ladle cars, other metallurgical equipment.