A method for preparation of charge for the continuous melting of titanium slags includes pelletizing of mixture of titanium concentrate, reducing agent, and binding agent, loading into the recirculating furnace of the pellets with addition of coal. Gas coal is loaded into the furnace for creation of reducing atmosphere. The ratio of pellets and gas coal amounts to 1:(0.22-0.36).
UAU200906102U2009-06-152009-06-15METHOD For PREPARATION OF CHARGE FOR CONTINUOUS MELTING OF TITANIum SLAGS