A method for change of specific heat conductivity of alloys, at which starting alloy and catalyst are melted in a crucible of smelting furnace at the temperature of heater of 998 °С, located on distance of from wall of crucible, provided temperature of melt of 960 °С. A starting alloy consists at least of two components, taken in the ratio 2:1. A catalyst contains mix from one mass part NaSiOand two mass part CuSO. The starting alloy and the catalyst in the ratio 5:1 are taken.
UAU200813318U2008-11-182008-11-18Method for change of specific heat conductivity of alloys