TWM512491U - Thermoplastic one-piece metal shell injection burying device - Google Patents

Thermoplastic one-piece metal shell injection burying device Download PDF

Info

Publication number
TWM512491U
TWM512491U TW104211135U TW104211135U TWM512491U TW M512491 U TWM512491 U TW M512491U TW 104211135 U TW104211135 U TW 104211135U TW 104211135 U TW104211135 U TW 104211135U TW M512491 U TWM512491 U TW M512491U
Authority
TW
Taiwan
Prior art keywords
metal shell
thermoplastic
plastic
embedding device
groove
Prior art date
Application number
TW104211135U
Other languages
Chinese (zh)
Inventor
Zhi-Jia Wei
Original Assignee
Zhi-Jia Wei
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhi-Jia Wei filed Critical Zhi-Jia Wei
Priority to TW104211135U priority Critical patent/TWM512491U/en
Publication of TWM512491U publication Critical patent/TWM512491U/en

Description

熱塑一體成型之金屬殼埋射裝置Thermoplastic one-piece metal shell embedding device

本創作熱塑一體成型之金屬殼埋射裝置,主要是應用於熱塑一體成型之金屬殼埋射塑料的成型技術上。The metal shell embedding device of the invention is mainly used for forming the metal shell embedded plastic of thermoplastic molding.

按,傳統習用金屬殼並非一體成型,而是分成若干片製作之後,再予以組合成一體,同時傳統習用金屬殼埋射塑料的方式,主要是先將金屬殼粗胚先經過CNC加工出凹槽,再經過陽極處理,完成之後,再將金屬殼拿去射出塑料,不但製作成本高,而且加工刀具經過一段時間之後,即會產生磨損,造成加工精確度上的公差增加,而導致瑕疵品的產生;同時,陽極處理後的化學藥劑亦會侵蝕金屬與塑料;而且,在射出塑料時,塑料容易高出金屬殼的凹槽甚多,用手摸起來,觸感不佳,為其既存尚待克服解決的問題與缺失。According to the traditional metal shell, it is not formed in one piece, but is divided into several pieces and then combined into one. At the same time, the traditional method of embedding the plastic in the metal shell is mainly to first process the metal shell rough embryo through the CNC. After the anode treatment, the metal shell is taken out to shoot the plastic, which is not only expensive to manufacture, but also wears after a period of time, causing the machining tolerance to increase in tolerance, resulting in defective products. At the same time, the anodized chemical also erodes the metal and the plastic; moreover, when the plastic is shot, the plastic is easily raised from the metal shell, and the hand is touched, and the touch is not good. Problems and lacks to be solved.

本創作人目前從事相關產品的製造、設計,累積多年的實務經驗與心得,針對傳統習用金屬殼埋射塑料的所既存的問題與缺失,積極地投入創新與改良的精神,所完成的熱塑一體成型之金屬殼埋射裝置。The creator is currently engaged in the manufacture and design of related products, accumulated many years of practical experience and experience, and has actively invested in the spirit of innovation and improvement in response to the existing problems and lacks of traditional metal shell embedded plastics. One-piece metal shell embedding device.

新型解決問題所應用的技術手段以及對照先前技術的功效係在於:熱塑一體成型之金屬殼成品經由陽極處理後,於金屬殼內凹槽形的弧面以CNC加工做絕緣,再將內層所須位置上以蝕刻處理或雷射雕刻 加工,並於金屬殼內層蝕刻處理或雷射雕刻加工處做上膠,金屬殼的凹槽內預留間距相同之通孔,將凹槽兩側邊角加工成微小平面,於平面上設置與金屬殼外形相同之弧形模具,該弧形模具的兩側略大於凹槽兩側,而模具後方放置彈簧,射出成型時,塑料匯流至金屬殼預留之通孔,經由凹槽向外流出埋射熱塑一體成型,當塑料碰觸於弧形模具後向外推動,此時弧形模具藉由後方彈簧之彈性,使塑料能向外推動距離受到限制,進而達成塑料溢出容許量之可接受範圍內,用手摸起來,觸感極佳,具有功效上的增進,為其主要目的成者。The technical means applied by the new problem solving and the effect of the prior art are as follows: the thermoplastic molded one-piece metal shell finished through the anode, and the grooved arc surface in the metal shell is insulated by CNC machining, and then the inner layer is Etching or laser engraving at the required location Processing, and sizing in the inner layer etching process or laser engraving processing of the metal shell, the through holes of the same spacing are reserved in the grooves of the metal shell, and the sides of the groove are processed into a micro plane, which is set on the plane An arc-shaped mold having the same shape as the metal shell, the two sides of the curved mold are slightly larger than the two sides of the groove, and a spring is placed behind the mold, and when the injection molding is performed, the plastic is merged to the through hole reserved by the metal shell, and the outer hole is outward through the groove The effluent and the embedded thermoplastic are integrally formed, and when the plastic touches the curved mold, the plastic is pushed outward. At this time, the elastic shape of the curved mold is restricted by the elasticity of the rear spring, thereby achieving the plastic overflow tolerance. Within the acceptable range, the hand is touched, the touch is excellent, and the effect is improved, which is the main purpose.

10‧‧‧金屬殼10‧‧‧Metal shell

11‧‧‧凹槽11‧‧‧ Groove

111‧‧‧弧面111‧‧‧ curved surface

112‧‧‧蝕刻處理或雷射雕刻加工處112‧‧‧ etching treatment or laser engraving processing

113‧‧‧膠113‧‧‧ glue

12‧‧‧通孔12‧‧‧through hole

13‧‧‧平面13‧‧‧ plane

14‧‧‧弧形模具14‧‧‧Arc mould

20‧‧‧塑料20‧‧‧ plastic

S‧‧‧彈簧S‧‧ ‧ spring

第一圖:係射出成型時,塑料匯流至金屬殼預留的通孔,經由凹槽向外流出之動作示意圖。The first figure is a schematic diagram of the action of the plastic flowing to the reserved through hole of the metal shell when the injection is formed, and flowing out through the groove.

第二圖:係射出成型時,塑料碰觸到弧形模具後向外推動,此時弧形模具藉由後方彈簧的彈性,使得塑料能向外推動距離受到限制之動作示意圖。The second picture: when the plastic is shot and molded, the plastic pushes outward after pushing the curved mold. At this time, the curved mold is driven by the elasticity of the rear spring, so that the plastic can push the distance to be restricted.

第三圖:係金屬殼之立體示意圖。Third figure: a three-dimensional schematic diagram of a metal shell.

第四圖:係金屬殼射埋塑料之立體示意圖。The fourth picture: a three-dimensional schematic diagram of a metal shell embedded plastic.

第五圖:係完成品之斷面組合示意圖。Figure 5: Schematic diagram of the cross-section of the finished product.

為使專精熟悉此項技藝之人仕業者易於深入瞭解本創作的構造內容以及所能達成的功能效益,茲列舉一具體實施例,並配合圖式詳細介紹說明如下:一種熱塑一體成型之金屬殼埋射裝置,敬請參閱第一圖至第 五圖所示。主要包括:金屬殼10、塑料20;其中:該熱塑一體成型之金屬殼10表面的上方與下方設有二凹槽11,該金屬殼10對應於二凹槽11的內面突出形成二弧面111,該金屬殼10成品經由陽極處理後,於金屬殼10的二弧面111以CNC加工做絕緣,再將內層所須位置上以蝕刻處理或雷射雕刻加工,並於金屬殼10內層蝕刻處理或雷射雕刻加工處112做上膠113,該二凹槽11內預留複數個間距相同的通孔12,並將凹槽11兩側邊角加工成微小的平面13,且在平面13上設置與金屬殼10外形相同的弧形模具14,該弧形模具14的兩側略大於凹槽11兩側,同時在弧形模具14的後方放置彈簧S,射出成型時,塑料20匯流至金屬殼10預留的通孔12,經由凹槽11向外流出(如第一圖所示),當塑料20碰觸到弧形模具14後向外推動,此時弧形模具14藉由後方彈簧S的彈性,使得塑料20能向外推動距離受到限制,藉以控制塑料20溢出的容許量達到可以接受的範圍內(如第二圖所示),射出成型後,即可以在金屬殼10上方與下方的凹槽11中一體成型二塑料20(如第三、四、五圖所示),該塑料20的材料可以選擇塑膠者。In order to make it easier for those who are familiar with the art to understand the construction content of the creation and the functional benefits that can be achieved, a specific embodiment will be listed, and the detailed description will be given as follows: a thermoplastic molding Metal shell embedding device, please refer to the first figure to the first The five figures are shown. The utility model mainly comprises: a metal shell 10 and a plastic 20; wherein: the surface of the metal shell 10 of the thermoplastic integrally formed is provided with two grooves 11 above and below the surface of the metal shell 10, and the metal shell 10 protrudes from the inner surface of the two grooves 11 to form two arcs. After the surface of the metal shell 10 is processed through the anode, it is insulated by CNC machining on the two curved surfaces 111 of the metal shell 10, and the inner layer is processed by etching or laser engraving at the position of the inner layer, and the metal shell 10 is processed. The inner layer etching process or the laser engraving processing portion 112 is smeared 113, and a plurality of through holes 12 having the same pitch are reserved in the two grooves 11, and the two corners of the groove 11 are processed into a minute plane 13 and An arc-shaped mold 14 having the same outer shape as that of the metal shell 10 is disposed on the flat surface 13, and both sides of the curved mold 14 are slightly larger than both sides of the groove 11, while a spring S is placed behind the curved mold 14, and plastic is formed during injection molding. 20, the through hole 12 which is reserved to the metal shell 10, flows outward through the groove 11 (as shown in the first figure), and is pushed outward when the plastic 20 touches the curved mold 14, and the curved mold 14 is now pushed. By the elasticity of the rear spring S, the plastic 20 can be pushed outwardly to be limited, thereby controlling The allowable amount of plastic 20 overflow is within an acceptable range (as shown in the second figure). After injection molding, two plastics 20 can be integrally formed in the groove 11 above the metal shell 10 (such as the third and fourth The figure of the plastic 20 can be selected from plastics.

綜合上述所陳,本創作係在提供一種熱塑一體成型之金屬殼埋射裝置,經過本創作人實際製做完成以及反覆操作測試之後,證實的確可以達到本創作所預期的功能效益,同時又為目前坊間尚無見聞之首先創作,具有產業上的利用價值,誠然已經符合新型專利實用性與進步性之成立要義,爰依專利法之規定,向 鈞局提出新型專利之申請。In summary, the present invention provides a thermoplastic integrated molded metal shell embedding device. After the actual fabrication and repeated operation tests of the creator, it is confirmed that the functional benefits expected by the creation can be achieved. For the first time in the world, there is no such thing as the creation of the industry, and it has the industrial use value. It has already met the important requirements of the practicability and progress of the new patent, and has filed a new patent application with the bureau.

10‧‧‧金屬殼10‧‧‧Metal shell

11‧‧‧凹槽11‧‧‧ Groove

111‧‧‧弧面111‧‧‧ curved surface

112‧‧‧蝕刻處理或雷射雕刻加工處112‧‧‧ etching treatment or laser engraving processing

113‧‧‧膠113‧‧‧ glue

12‧‧‧通孔12‧‧‧through hole

13‧‧‧平面13‧‧‧ plane

14‧‧‧弧形模具14‧‧‧Arc mould

20‧‧‧塑料20‧‧‧ plastic

S‧‧‧彈簧S‧‧ ‧ spring

Claims (4)

一種熱塑一體成型之金屬殼埋射裝置,主要在於:熱塑一體成型之金屬殼外部設有凹槽,該金屬殼對應於凹槽內面突出形成的弧面,該金屬殼成品經由陽極處理後,於金屬殼的弧面以CNC加工做絕緣,再將內層所須位置上以蝕刻處理或雷射雕刻加工,並於金屬殼內層蝕刻處理或雷射雕刻加工處做上膠,該凹槽內預留間距相同的通孔,射出成型時,塑料匯流至金屬殼預留的通孔,經由凹槽向外流出埋射熱塑一體成型者。The utility model relates to a metal shell embedding device which is integrally formed by thermoplastic molding, which mainly comprises: a groove formed outside the metal shell of the thermoplastic molding, the metal shell corresponding to a curved surface formed by the inner surface of the groove, the finished metal shell is processed through the anode After that, the inner surface of the metal shell is insulated by CNC machining, and the inner layer is etched or laser-engraved, and the metal shell is etched or laser-engraved. The through holes with the same spacing are reserved in the grooves. When the injection molding is performed, the plastics flow to the through holes reserved for the metal shells, and the buried thermoplastics are formed outward through the grooves. 如請求項1所述之熱塑一體成型之金屬殼埋射裝置,其中:該金屬殼係由熱塑成型者。The thermoplastic integrally formed metal shell embedding device of claim 1, wherein the metal shell is formed by a thermoformer. 如請求項1所述之熱塑一體成型之金屬殼埋射裝置,其中:該塑料的材料可以選擇塑膠者。The thermoplastic integrated molded metal shell embedding device according to claim 1, wherein the plastic material is selected from plastics. 如請求項1所述之熱塑一體成型之金屬殼埋射裝置,其中:該金屬殼的凹槽兩側邊角加工成微小平面,於平面上設置與金屬殼外形相同之弧形模具,該弧形模具的後方放置彈簧,當塑料碰觸於弧形模具後向外推動,此時弧形模具藉由後方彈簧之彈性,使塑料能向外推動距離受到限制,進而達成塑料溢出容許量之可接受範圍內者。The thermoplastic integrated molded metal shell embedding device of claim 1, wherein: the sides of the groove of the metal shell are processed into a micro plane, and an arc-shaped mold having the same shape as the metal shell is disposed on the plane, A spring is placed behind the curved mold, and when the plastic touches the curved mold, the plastic is pushed outward. At this time, the elastic shape of the curved mold is restricted by the elasticity of the rear spring, thereby achieving the plastic overflow tolerance. Acceptable range.
TW104211135U 2015-07-10 2015-07-10 Thermoplastic one-piece metal shell injection burying device TWM512491U (en)