Prior art keywords
screw
tail
reaming
cracking
improvement
Prior art date
Application number
TW100206926U
Other languages
Chinese (zh)
Inventor
deng-hong Lin
Original Assignee
Fong Prean Ind Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Fong Prean Ind Co Ltd filed Critical Fong Prean Ind Co Ltd
Priority to TW100206926U priority Critical patent/TWM413770U/en
Publication of TWM413770U publication Critical patent/TWM413770U/en

Links

Landscapes

  • Connection Of Plates (AREA)

Description

M413770 五、新型說明: 【新型所屬之技術領域】 一種針對先前技術創作第98224168號(新型專利權第 M388578號)予以改進而成的防裂螺絲改良設計。 【先前技術】 -般已知岐齡所使__設計,依不⑽求效果與 ‘利的驗思想而有諸乡設計,但其猶要求不外 '· 乎鑽孔速度、排屑速度以及最終的螺固和材料不龜裂的效果。 ' 而為求達到前述目的的設計有單段敎、雙段螺紋,以 及相同螺牙導程角度或不同螺牙導程角度的變化。 本案創作人亦冑就料獅的效細不斷的技術研發出 相關的創作設計,如:公告第539〇67號、公告第56顏號、 公告第570115號、公告第575099號、公告第M259859號、公 ‘ 告第M258201號、公告第隱371號、公告第_372號、公 • 告* M299237號、公告第謂號、公告第咖27〇號及公 開第200525091號等先前技術創作成果。 在螺絲的設計上’又因螺絲的欲螺設對象的材質不同及材 質特性的不同而有別,如金屬材質用的螺絲,塑膠材質用的螺 絲以及木料材質用的螺絲。而在已知的木料材質用的螺絲設計 上’在硬質木料的材質螺設時,因硬質木料的材質特性而常發 生木料因螺絲的迫入而崩裂,所以業界亦設計出使用於木料材 質的防裂螺絲,如公告第M350622號「防裂螺絲」、公告第 3 M413770 1318270號「?方裂及防起毛邊之螺絲」。 本案創作人f針對已知獅的缺點加以設制作,而取 第98224168號「防裂螺絲」新型專利權第M388578號,胁 創作物品稍改良研發財創作物更理想的㈣效果的^提 下’該技躺作亦有再研發騎的必要。 【新型内容】 本案創作「防裂螺絲的改良」係針對先前技術創作第 9822個號(新型專利權第嶋㈣予以改進而成,= 有效的提昇原創作物所應具備的鑽孔螺入迅速、省力且防裂、 無殘餘木料功效的_獅改_,該改良之防裂螺絲包 含一螺絲頭-由螺絲頭延伸的直桿體及位於直桿體尾端的尖 錐狀螺絲尾;其創作特徵在於: 由螺絲頭延伸的直桿體上設有三段螺牙,第一段螺牙為一 計且設近於_職部,第二段螺牙接續設 一_ ""螺牙的下方’該第二段螺牙尾端距離#·螺絲尾 七66笛:^於該距離内的直桿體上設有由預定個擴孔螺牙構 立㈣^段擴孔螺牙,而尖錐狀螺絲尾上則設有雙鑽孔螺牙; ^ &螺讀第三段航螺牙為相 螺牙與第二段螺牙為獨螺旋方向。 = 及螺絲直桿體上的三段螺牙設計與位於直桿體尾 木質物W螺絲尾的雙鑽孔螺牙的整體創新設計,得構成貫穿 如硬木)a寺,能達到防裂功能以及螺絲頭與木質物體 4 M413770 間無殘餘木屑的更理想功效。 【實施方式】 請參閱同附之圖式部分第1圖及第4圖所示為本案「防裂 螺絲」之實施例㈠及㈡,該防裂螺絲包含—螺絲頭i,一 由螺絲頭i延伸的直桿體10及位於直桿體1〇尾端的尖錐狀螺 絲尾11。M413770 V. New description: [New technical field] A modified design of anti-cracking screw which was improved according to the prior art creation No. 98224168 (new patent No. M388578). [Prior Art] - It is known that 岐 _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ The final screw and the material do not crack. In order to achieve the above objectives, there are single-stage 双, double-stage threads, and the same screw lead angle or different screw lead angle changes. The creators of this case also developed relevant creative designs on the technology of the lions, such as: Announcement No. 539〇67, Announcement No. 56 No., Announcement No. 570115, Announcement No. 575099, Announcement No. M259859 , the public's notice No. M258201, Announcement No. 371, Announcement No. _372, Public Notice* M299237, Announcement No., Announcement No. 27 No. and Public Publication No. 200525091. The design of the screw is different depending on the material of the screw to be screwed and the material properties, such as screws for metal materials, screws for plastic materials, and screws for wood materials. In the screw design for the known wood material, when the material of the hard wood is screwed, the wood often breaks due to the forced insertion of the screw due to the material properties of the hard wood, so the industry has also designed the material for the wood. Anti-cracking screws, such as Bulletin No. M350622 "Fracture-Resistant Screws", Announcement No. 3 M413770 1318270 "Fractures and Flange-Resistant Screws". The creator of this case f was made to deal with the shortcomings of the known lions, and took the new patent No. M388578 of No. 98224168 "Fracture-resistant screws", and it was better to improve the research and development of the assets. This technique is also necessary to re-develop the ride. [New content] The creation of the "anti-cracking screw" in this case is based on the improvement of the previous technical creation No. 9822 (the new patent right (4), = the effective drilling of the original crop should have the drilling screw, _ lion modified _, the improved anti-cracking screw includes a screw head - a straight rod extending from the screw head and a pointed taper tail at the end of the straight rod body; It consists of: There are three sections of thread on the straight body extending from the screw head. The first section of the thread is one meter and is close to the _ position. The second section of the thread is connected with a _ "" 'The second segment of the screw end distance #· screw tail seven 66 flute: ^ in the distance of the straight body is set by a predetermined reaming screw (4) ^ segment reaming screw, and the cone The double-drilled thread is provided on the tail of the screw; ^ & the third section of the thread is the single screw and the second thread is the spiral direction. = and the three-section thread on the screw straight body The overall innovative design of the double-drilled screw with the screw tail of the wooden body W at the end of the straight rod body is constructed as a hard Wood) a temple, can achieve anti-crack function and screw head and wooden objects 4 M413770 no residual wood chips are more ideal. [Embodiment] Please refer to the drawings (1) and (4) of the "Anti-cracking screw" of the present invention as shown in the attached drawings. The anti-cracking screw includes a screw head i and a screw head i. The extended straight body 10 and the pointed tapered tail 11 at the end of the straight body 1 are.

睛參閱第1圖至第3圖所示本案創作實施例㈠,其中該 螺、糸頭1本體物為上大下小設計’並在螺絲頭1的上周緣具 有一平環12 ’平環12底緣設有環狀棘齒13,螺絲頭丨底緣亦 設有環狀棘齒14。See Fig. 1 to Fig. 3 for the creation example (1) of the present case, wherein the body of the screw and the head 1 is of a large upper and lower design and has a flat ring 12' flat ring 12 at the upper periphery of the screw head 1. The bottom edge is provided with an annular ratchet 13 and the bottom edge of the screw head is also provided with an annular ratchet 14.

=參閱第1圖及第4圖所示,螺絲頭i向下延伸的直桿體 5 Μ4Ϊ3770 -該第三段航斷4於直雛1G上均猶不足—圏且 第切擴孔螺牙4所包含的擴孔螺相上牙面4A下傾角度a 小於下牙面4B的上揚角度B,而上牙面4Ατ傾角度a與下牙 面4B的上揚角度β的和敍於或等於⑽度角。 藉由本案「防裂螺絲的改良」之螺絲頭的不同設計運用及=Refer to Figure 1 and Figure 4, the straight rod body 5 Μ4Ϊ3770 with the screw head i extending downwards - the third section of the trajectory 4 is still insufficient on the straight 1G - and the first cut reamer thread 4 The included angle of the upper surface 4A of the countersunk spiral surface is smaller than the upward angle B of the lower tooth surface 4B, and the sum of the inclination angle a of the upper tooth surface 4Α and the upward angle β of the lower tooth surface 4B is equal to or equal to (10) degrees. angle. With the different design and application of the screw head of the "improvement of crack-proof screws" in this case

螺絲直桿體上的球螺牙設計與位於直龍尾端的尖雜狀螺 絲尾的雙觀财的整體鑛設計,得構㈣?木質物飢如 硬木)時’能達到防裂功能以及螺絲頭與木質物體間無殘餘木 屑的更理想功效。 【圖式簡單說明】 第1圖:本創作之實施例(一)。 第2圖:第1圖之2-2剖視圖。 第3圖:本創作擴孔螺牙之上、下牙面角度示意圖。The design of the ball screw on the straight shaft of the screw and the overall design of the double-viewing of the tip of the twisted screw tail at the end of the straight dragon (4)? When woody food is hungry like hardwood, it can achieve the anti-cracking function and the ideal effect of no residual wood chips between the screw head and the wooden object. [Simple description of the drawing] Fig. 1: Example (1) of the present creation. Fig. 2 is a cross-sectional view taken along line 2-2 of Fig. 1. Figure 3: Schematic diagram of the angle of the upper and lower teeth of the created reaming screw.

第4圖:本創作之實施例(二) 【主要元件符號說明】 1螺絲頭 10直桿體 U0尾尖 12平環 14環狀棘齒 2第一段螺牙 4第三段擴孔螺牙4Α上牙面 11尖錐狀螺絲尾 13環狀棘齒 3第二段螺牙 4Β下牙面 3鑕孔螺牙 Α擴孔螺牙上牙面下傾角度 B擴孔螺牙下牙面上揚角度 6Figure 4: The embodiment of the creation (2) [Description of the main components] 1 screw head 10 straight rod U0 tail tip 12 flat ring 14 ring ratchet 2 first segment screw 4 third segment reaming screw 4Α Upper tooth surface 11 Tip-shaped screw tail 13 Ring ratchet 3 Second stage thread 4 Β Lower tooth surface 3 螺 螺 螺 Α Α Α 螺 螺 上 上 上 上 上 上 B B B B B B B B Angle 6

Claims (1)

M413770 六、申請專利範圍: 卜-種防裂螺絲的改良,包含螺絲頭’由螺絲頭延伸的直桿 體及位於直桿體尾_尖錐狀螺絲尾;其在於:由螺絲頭 延伸的直桿體上設有三段螺牙,第一段螺牙為一圈數螺牙的設 計,第二段螺牙接續設置在第一段螺牙的下方;第二段螺牙尾 舰離直桿觀端的錄狀_尾—奴轉,於該距離内的 - 直桿體上設有由預定個擴孔螺牙構成的第三段擴孔螺牙,而位 • ☆直杯體尾端的央錐狀螺絲尾上則設有雙鑽孔螺牙。 2、 依申請專利範圍第丨項所述防裂螺絲的改良其中該螺絲 頭本體外彳:為上大下小設計,並在螺絲頭的上周緣具有一平 % ’平環底緣設有環狀棘齒,螺絲頭底緣亦設有環狀棘齒。 3、 依申請專利範圍第1項所述防裂螺絲的改良,其中該第一 段螺牙為一圈四螺牙。 4、 依申請專利範圍第1項所述防裂螺絲的改良,其中該第三 鬱 段擴孔螺牙的各擴孔螺牙於直桿體上均螺旋不足一圈,且第三 '' 段擴孔螺牙所包含的各擴孔螺牙的上牙面下傾角度A小於下 牙面的上揚角度8,而上牙面下傾角度A與下牙面的上揚角度 B的和係大於、等於90度角。 5、 依申請專利範圍第1項所述防裂螺絲的改良,其中該位於 直杯體尾端的尖錐狀螺絲尾上的雙鑽孔螺牙的尾端係延伸、不 延伸到尖錐狀螺絲尾的尾尖處。 6、 依申請專利範圍第1項所述防裂螺絲的改良,其t該第- 7 M413770 段螺牙與第二段螺牙為不同螺旋方向,第二段螺牙與第三段擴 孔螺牙為相同螺旋方向。 7、依申請專利範圍第1項所述防裂螺絲的改良,其中該第三 段擴孔螺牙係由三撇擴孔螺牙構成。M413770 VI. Scope of application: The improvement of the anti-cracking screw includes a screw head 'straight rod body extended by the screw head and a tail-shaped screw tail at the end of the straight rod body; it is: straight extending from the screw head There are three sections of thread on the rod body. The first section of the thread is designed as a number of threaded teeth. The second section of the thread is connected below the first section of the thread. The second section of the threaded tail is from the perspective of the straight rod. The end of the record _ tail - slave transfer, within the distance - on the straight body is provided with a third reaming screw consisting of a predetermined reaming screw, and the position of the ☆ straight cup end of the cone Double drilled threads are provided on the screw tail. 2. The improvement of the anti-cracking screw according to the scope of the patent application scope is as follows: the screw head is in the outer body of the screw: it is designed to be large and small, and has a flat % on the upper circumference of the screw head. The ratchet teeth are also provided with annular ratchets at the bottom edge of the screw head. 3. The improvement of the anti-cracking screw according to Item 1 of the patent application scope, wherein the first segment of the screw is a ring of four threads. 4. According to the improvement of the anti-cracking screw according to the first item of the patent application scope, wherein the reaming screw of the third-stage reaming screw has less than one turn on the straight rod body, and the third '' section The angle of the upper tooth surface of the reaming screw included in the reaming screw is smaller than the angle 8 of the lower tooth surface, and the sum of the angle D of the upper tooth surface and the angle B of the lower tooth surface is greater than Equal to 90 degrees. 5. The improvement of the anti-cracking screw according to Item 1 of the patent application scope, wherein the end of the double-drilled screw on the tip of the tapered screw tail of the straight cup extends and does not extend to the tip of the tapered tail At the tip of the tail. 6. According to the improvement of the anti-cracking screw mentioned in the first paragraph of the patent application scope, the t-stage 7 M413770 segment screw and the second segment screw are in different spiral directions, the second segment screw and the third segment reaming screw The teeth are in the same spiral direction. 7. The improvement of the anti-cracking screw according to the first item of the patent application scope, wherein the third-stage reaming screw system is composed of three reaming screw teeth.
TW100206926U 2011-04-20 2011-04-20 Improved rupture-proof screw TWM413770U (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
TW100206926U TWM413770U (en) 2011-04-20 2011-04-20 Improved rupture-proof screw

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
TW100206926U TWM413770U (en) 2011-04-20 2011-04-20 Improved rupture-proof screw

Publications (1)

Publication Number Publication Date
TWM413770U true TWM413770U (en) 2011-10-11

Family

ID=46421771

Family Applications (1)

Application Number Title Priority Date Filing Date
TW100206926U TWM413770U (en) 2011-04-20 2011-04-20 Improved rupture-proof screw

Country Status (1)

Country Link
TW (1) TWM413770U (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
TWI734312B (en) * 2019-12-21 2021-07-21 徐國泰 Screw with hole-enlarging portion

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
TWI734312B (en) * 2019-12-21 2021-07-21 徐國泰 Screw with hole-enlarging portion

Similar Documents

Publication Publication Date Title
TWI548818B (en) Screw element
TWM442418U (en) Bolting component
TWM413770U (en) Improved rupture-proof screw
US9228603B2 (en) Crack-proof screw
US8235637B2 (en) Anti-loosen self-tapping screw
TWM407970U (en) wood screw
TWM440842U (en) Drill structure
CA2708419C (en) Crack-proof screw
CN102235410A (en) Wooden screw
US9249822B2 (en) Screws
EP2395251A1 (en) Crack-proof screw
TWI352160B (en)
TWM373974U (en) Screw having spiral-type trifles-exhausting groove
CN108670448A (en) A kind of root canal conveyer
TWM439727U (en) Self-drilling screw
TWI626385B (en) Screw structure
TWM350623U (en) Self-drilling screw
TWM408623U (en) Screw
TW201013060A (en) Screw with helical trench
TWM427470U (en) Improvement of screw
TWM443787U (en) Screw head bit
TWM427469U (en) Screw
TWM406664U (en) Wood screw capable of being rapidly locked into woods
TWM414507U (en) Screw
TWM354007U (en) Screw with cone-shaped teeth section

Legal Events

Date Code Title Description
MK4K Expiration of patent term of a granted utility model