Prior art keywords
layer
composite
pot
iron
steel
Prior art date
Application number
TW94218765U
Other languages
Chinese (zh)
Inventor
Ming-Shuen Chen
Original Assignee
Ming-Shuen Chen
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ming-Shuen Chen filed Critical Ming-Shuen Chen
Priority to TW94218765U priority Critical patent/TWM288162U/en
Publication of TWM288162U publication Critical patent/TWM288162U/en

Links

Landscapes

  • Cookers (AREA)

Description

M288162 八、新型說明: 【新型所屬之技術領域】 本創作係有關一種「複合鍋之改良結構」,尤指 一種兼具鐵、鋁及不銹鋼鍋等之優點,以提高鍋具實 用價值之複合鍋結構。 【先前技術】M288162 VIII. New Description: 【New Technology Fields】 This creation is about “a modified structure of a composite pot”, especially a composite pot that combines the advantages of iron, aluminum and stainless steel pots to improve the practical value of the pot. structure. [Prior Art]

^按,鐵鍋係為我國的傳統炊具,其具有長期使用 知以獲取鐵貝之優點且無化學污染之危害,但也存在 ‘熱r艾、耗費能源、笨重且鍋底容易損壞之缺失,因 而有鋁鋼之問市’鋁鋼雖較輕巧、傳導熱的速度亦 較快’惟其卻較易產生化學之仙,長期使⑽銷烹 :’將造成對人體的傷害’是以,如何將鍋具製成既 =巧、無化學傷害且使用方便、壽命長之效果,實也 為業者所極思研發。^ Press, the iron pot is the traditional cookware of our country, which has the advantages of long-term use to obtain the advantages of iron shell and no chemical pollution, but there are also the lack of 'heat r, energy, bulky and easy to damage the bottom of the pot. In the case of aluminum steel, 'aluminum steel is lighter and conducts heat faster', but it is easier to produce chemical fairy, long-term (10) pin cooking: 'will cause harm to the human body', how to put the pot It is made with the effect of being skillful, chemically free, easy to use and long-lived.

【新型内容】 社j作之主要目的,即在提供一種複合鍋之改良 :之2鍋具達到輕巧、易導熱,安全且使用壽命較 長之效果,且其製程簡易。 别述之複合鍋,係設有一鍋體 設為鐵質居,从a 從成鍋體的内層 水平突括f、曰則設為鋁質層,並於鍋體開口設以 以供包覆不銹鋼之捲邊,使鍋體連結把手 5 M288162 後,構成複合鍋,俾藉由内、外層之鐵、鋁層,使鍋 體易於導熱、鍋底不易氧化、脫落,以增加使用壽命 ,且於長期使用得以獲得人體所需之鐵質。 前述所述之複合鍋結構,其中該内、外層係經由 擴散焊接形成一體,且該鋁質層厚度係為〇·2 —〇 5m/m ,而鐵質層厚度係為〇·8—12m/in並較佳。 如述之複合銷結構,其中該外層之鋁質層,係以 鋁粉喷塗後以高溫燒結成型。 【實施方式】 印同時參閱第一、二、三圖,本創作主要係設有 一鍋體(1),使該鍋體〇)的内層設為鐵質層(11), 而外層設為鋁質層(12),鍋體(1)開口則設有突垣 (13),於突垣(13)包覆不銹鋼之捲邊(14),使鍋體 (1)以鉚釘(15)連接把手(16)後,構成複合鍋,俾藉 由鍋體(1)内、外層之鐵、鋁層〇1)(12),使鍋體 (1)的傳熱較為快速,鍋底不易氧化、脫落,以增加 使用哥命’且長期使用得以獲取人體所需之鐵質。 前述之複合鍋,其中鍋體(丨)的内、外層之鐵質 層(11)及鋁質層02),係經由擴散焊接形成一體,且 忒铭質層(12)之厚度為〇·2-〇.5m/m ,而該鐵質體(11) 之厚度為0.8-1.2m/m為較佳。 而該外層之鋁質層,係可由鋁粉喷塗後,再以高 溫燒結成型。 M288162 综上戶斤、十、 … 延,本創作之複合鍋,至少俱備以下之優 點: •由於外層為紹質層,因此導熱快速,節省能源且使 用上更為省時。 • ^層為心層’因此較不易氧化、脫^,使用壽命 得以增長。 3.=於係為銘質層與㈣層之結合,故聽備鐵銷無 丨 α人體及鋁鶴輕巧之特點。 •此外本創作之複合锅於長期使用可獲取人體所 舄之鐵質,為一實用之崎士+ ^ 、又计,減屬一俱新穎性之創作 ’羑依法提出專利申請,新 Τ ^斫鈞局予以審杳,早曰賜 准專利,至感德便。 一 【圖式簡單說明】 圖1係為本創作之立體圖。 圖2係為本創作之剖視圖。 圖3係為本創作之部份放大剖視圖。 【主要元件符號說明】 (1)鍋體 (11)鐵質層 (12)鋁質層 (13)突垣 (14)捲邊 (15) I即釘 (16)把手[New content] The main purpose of the company is to provide a composite pot improvement: the 2 pots achieve light weight, easy heat conduction, safety and long service life, and the process is simple. In the composite pot, there is a pot body which is set as an iron residence, from a from the inner layer of the pot body to the horizontal level, and the crucible is set to the aluminum layer, and the pot body is opened to cover the stainless steel. The curling edge connects the handle to the handle 5 M288162 to form a composite pot. The inner and outer layers of iron and aluminum layer make the pot easy to conduct heat, the bottom of the pot is not easy to oxidize and fall off, so as to increase the service life and long-term use. Get the iron you need for your body. The composite pot structure described above, wherein the inner and outer layers are integrally formed by diffusion welding, and the thickness of the aluminum layer is 〇·2 - 〇 5 m / m, and the thickness of the iron layer is 〇 · 8 - 12 m / In and better. The composite pin structure as described above, wherein the aluminum layer of the outer layer is sprayed with aluminum powder and then sintered at a high temperature. [Embodiment] Simultaneously refer to the first, second and third figures. This creation mainly consists of a pot body (1), the inner layer of the pot body is set as the iron layer (11), and the outer layer is made of aluminum. The layer (12), the opening of the pot body (1) is provided with a protrusion (13), and the flange (13) is covered with a stainless steel bead (14), so that the pot body (1) is connected with a rivet (15) ( 16) After constituting the composite pot, the heat transfer of the pot body (1) is relatively fast by the iron and aluminum layer 〇1)(12) in the inner and outer layers of the pot body (1), and the bottom of the pot is not easily oxidized and peeled off. Increase the use of scorpion' and long-term use to obtain the iron needed by the human body. In the above composite pot, the inner and outer iron layers (11) and the aluminum layer 02) of the pot body are integrally formed by diffusion welding, and the thickness of the enamel layer (12) is 〇·2 - 〇. 5 m / m, and the thickness of the ferrous body (11) is preferably 0.8 - 1.2 m / m. The aluminum layer of the outer layer can be sprayed with aluminum powder and then sintered at a high temperature. M288162 In general, the composite pot of this creation has at least the following advantages: • Because the outer layer is the primary layer, it is fast in heat conduction, saves energy and is more time-saving. • The layer is the core layer, so it is less prone to oxidation and de-enhancement, and the service life is increased. 3.= The system is a combination of the inscription layer and the (four) layer, so the hearing iron is not 丨 α body and aluminum crane light features. • In addition, the composite pot of this creation can obtain the iron of the human body for long-term use. It is a practical sage + ^, and counts, and reduces the creation of a novelty. 羑 Patent application according to law, new Τ ^斫The bureau will examine it and give it a patent as soon as possible. A [simplified description of the drawings] Figure 1 is a perspective view of the creation. Figure 2 is a cross-sectional view of the creation. Figure 3 is a partial enlarged cross-sectional view of the creation. [Main component symbol description] (1) Pot body (11) Iron layer (12) Aluminum layer (13) Axle (14) Curling (15) I is nail (16) Handle

Claims (1)

M288162 九、申請專利範圍: 1. -種「複合鍋之改良結構」,主要係設有一鍋體,使 該鶴體的内層設為鐵質層,而外層則設為銘質層,並 ;鍋體開口 5又以犬垣’以供包覆不銹鋼捲邊,使鍋體 連結於把手後,構成兼具鐵、銘鋼之複合鍋。 2. 如申請專利範圍第Μ所述之「複合鋼之改良結構」 在其中,該鋼體之内、外層係經由擴散焊接形成一體 〇 3. 申請專利範圍第1項所述之「複合鋼之改良結構」, 在其中’該㈣之質層之厚度為GW.·,該鐵 質層之厚度0.8-1.2m/m為較佳者。 4. 如申請專利範圍第1項所述之「複合鋼之改良結構」 &在八中,該銷體之紹質層,係可以銘粉喷塗後,以 鬲溫燒結成型。M288162 IX. Scope of application: 1. - "Improved structure of composite pot", mainly consisting of a pot body, the inner layer of the body is set as iron layer, and the outer layer is set as inscription layer; The body opening 5 is made of a canine's for covering the stainless steel, and the body is connected to the handle to form a composite pot having both iron and Ming steel. 2. The "modified structure of composite steel" as described in the scope of the patent application, in which the inner and outer layers of the steel body are integrally formed by diffusion welding. 3. "Composite steel as described in claim 1 In the modified structure, the thickness of the layer of the (four) is GW.·, and the thickness of the iron layer is preferably 0.8-1.2 m/m. 4. If the “modified structure of composite steel” mentioned in the first paragraph of the patent application is in the middle of the eighth grade, the finished layer of the pin body can be sintered by sintering after being sprayed with powder.
TW94218765U 2005-10-31 2005-10-31 Improved structure of a composite wok TWM288162U (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
TW94218765U TWM288162U (en) 2005-10-31 2005-10-31 Improved structure of a composite wok

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
TW94218765U TWM288162U (en) 2005-10-31 2005-10-31 Improved structure of a composite wok

Publications (1)

Publication Number Publication Date
TWM288162U true TWM288162U (en) 2006-03-01

Family

ID=37432567

Family Applications (1)

Application Number Title Priority Date Filing Date
TW94218765U TWM288162U (en) 2005-10-31 2005-10-31 Improved structure of a composite wok

Country Status (1)

Country Link
TW (1) TWM288162U (en)

Similar Documents

Publication Publication Date Title
CN103705103B (en) Cast-in titanium aluminum composite pot and its manufacture method
US7960034B2 (en) Multi-ply cookware with copper-aluminum-stainless steel
JP4047878B2 (en) Inner pot for electronic induction cooker
CN100496359C (en) A cooking utensil having three-layered composite plate fitting for various stoves and its processing method
TWM288162U (en) Improved structure of a composite wok
CN205763821U (en) A kind of fork truck turns aluminum bag
WO2007085132A1 (en) Cookware with copper composite plate and manufature method thereof
CN201260613Y (en) Novel cooker body structure
CN203735976U (en) Cast iron enamel pot with inclined edge
CN206080222U (en) Pot
CN211022171U (en) Energy-saving nutrition pot
JP2002238739A (en) Casserole
CN206197732U (en) A kind of easy to operate pot
CN201219816Y (en) Novel ceramic pot
CN202775813U (en) Nanometer ceramic non-stick pan
CN201370446Y (en) Multi-pore energy-saving conditioning pot
CN202436840U (en) Electric pressure cooker cover or inner pot body with improved structure
CN209694848U (en) Electric pressure cooking saucepan titanium alloy pot gallbladder
CN216090030U (en) Novel composite pot
CN220001489U (en) Pot body with high heat transfer efficiency and iron/aluminum copper alloy/carbon steel composite plate for pot body
CN206433960U (en) A kind of heater of hair straightener ceramic wafer
CN207229226U (en) Motorcycle exhaust pipe heat-insulating shield
KR20130117014A (en) Energy saving cookpot
CN2933217Y (en) Pressure cooker
CN207544880U (en) Electromagnetic induction heating pot has and equipment of cooking

Legal Events

Date Code Title Description
MM4K Annulment or lapse of a utility model due to non-payment of fees