TWI561677B - - Google Patents
Info
- Publication number
- TWI561677B TWI561677B TW103135839A TW103135839A TWI561677B TW I561677 B TWI561677 B TW I561677B TW 103135839 A TW103135839 A TW 103135839A TW 103135839 A TW103135839 A TW 103135839A TW I561677 B TWI561677 B TW I561677B
- Authority
- TW
- Taiwan
Links
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW103135839A TW201615891A (en) | 2014-10-16 | 2014-10-16 | Plated steel sheet and fuel tank |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW103135839A TW201615891A (en) | 2014-10-16 | 2014-10-16 | Plated steel sheet and fuel tank |
Publications (2)
Publication Number | Publication Date |
---|---|
TW201615891A TW201615891A (en) | 2016-05-01 |
TWI561677B true TWI561677B (en) | 2016-12-11 |
Family
ID=56508457
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW103135839A TW201615891A (en) | 2014-10-16 | 2014-10-16 | Plated steel sheet and fuel tank |
Country Status (1)
Country | Link |
---|---|
TW (1) | TW201615891A (en) |
Families Citing this family (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
WO2022014645A1 (en) * | 2020-07-14 | 2022-01-20 | 日本製鉄株式会社 | Hot stamped member and manufacturing method therefor |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN101395300A (en) * | 2006-03-01 | 2009-03-25 | 日本油漆株式会社 | Composition for metal surface treatment, metal surface treatment method, and metal material |
TW201035376A (en) * | 2009-01-16 | 2010-10-01 | Nippon Steel Corp | Hot-dip zn-al-mg-si-cr alloy coated steel material with excellent corrosion resistance |
TW201200604A (en) * | 2010-06-24 | 2012-01-01 | Nippon Steel Corp | Hot-dip Al-coated steel sheet with excellent thermal blackening resistance and method of making the same |
-
2014
- 2014-10-16 TW TW103135839A patent/TW201615891A/en not_active IP Right Cessation
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN101395300A (en) * | 2006-03-01 | 2009-03-25 | 日本油漆株式会社 | Composition for metal surface treatment, metal surface treatment method, and metal material |
TW201035376A (en) * | 2009-01-16 | 2010-10-01 | Nippon Steel Corp | Hot-dip zn-al-mg-si-cr alloy coated steel material with excellent corrosion resistance |
TW201200604A (en) * | 2010-06-24 | 2012-01-01 | Nippon Steel Corp | Hot-dip Al-coated steel sheet with excellent thermal blackening resistance and method of making the same |
Also Published As
Publication number | Publication date |
---|---|
TW201615891A (en) | 2016-05-01 |
Similar Documents
Legal Events
Date | Code | Title | Description |
---|---|---|---|
MM4A | Annulment or lapse of patent due to non-payment of fees |