TWI308076B - - Google Patents

Download PDF

Info

Publication number
TWI308076B
TWI308076B TW95137016A TW95137016A TWI308076B TW I308076 B TWI308076 B TW I308076B TW 95137016 A TW95137016 A TW 95137016A TW 95137016 A TW95137016 A TW 95137016A TW I308076 B TWI308076 B TW I308076B
Authority
TW
Taiwan
Prior art keywords
paint
carbon fiber
layer
transparent
golf club
Prior art date
Application number
TW95137016A
Other languages
Chinese (zh)
Other versions
TW200711687A (en
Inventor
xiang-zhen Hou
Original Assignee
xiang-zhen Hou
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by xiang-zhen Hou filed Critical xiang-zhen Hou
Priority to TW095137016A priority Critical patent/TW200711687A/en
Publication of TW200711687A publication Critical patent/TW200711687A/en
Application granted granted Critical
Publication of TWI308076B publication Critical patent/TWI308076B/zh

Description

1308076 九、發明說明: 【發明所屬之技術領域】 本發明係提供一種且古也主麻_採Λ 、 具冗先表層及多樣色之高爾夫球桿 製法,尤指其技術上提供碳纖材質經過濺鍍及烘烤而具有 光亮效果,並可經多樣色漆,而達到豐富色彩高爾夫球桿 〇 【先前技術】 習用之问爾夫球桿之表面加工方式,主要採用球桿之 表面形成-層透明的底彡黍,其後再於透明的底漆上著一層 色漆,其後在色漆之上再上—層的保護漆,據以完成高爾 夫球桿表面之塗裝。 准,其上述習用之高爾夫球桿,仍存在有下列缺失: 碳纖之材料結構較為粗糙,所以無論如何的喷塗 亡色’都是沒有辦法改變其暗沉狀態,如此將使得碳纖球 #在視覺效果表現上相當S ’且給人直接的觀感就是次級 品的感受,所以品質再好也無法提升買氣。 一、不論是以何種方式噴塗或刷塗球桿,其色漆之色 澤㈣達到均句,且無法使得顏色多樣化。 —疋以,針對上述習知結構所存在之問題點,如何開發 /、里心實用性之創新結構,實消費者所殷切企盼, 亦係相關業者須努力研發突破之目標及方向。 有i於此’冑明人本於多年從事相關產品之製造開發 與設計經驗,針對上t τ上这之目b ’詳加設計與審慎評估後’ 終得一確具實用性之本發明。 1308076 【發明内容】 欲解決之技術問題點: 垅鏞,装士 L 阿爾夫球才干之材質如果為 、’ 土本上均可達到質輕與強倉τι夕*<· a 也較為粗糖,I論如何 ^ ,^碳纖材質 颧;=§你” 研磨再上漆,其表面給人的 觀感仍疋相當暗淡粗糙而會 ^ ^ s . 先 &成妷纖高爾夫球桿 之購貝使用意願低落。 解決問題之技術特點:提供— 古 種具冗光表層及多樣色 之间爾夫球桿製法,其係 ^ ^ , 反紙坺扣表面先以透明打底塗 料塗佈,再利用濺鍍設備 冑濺鍍&後以相各濺鍍材質之保 4材質塗於濺鍍構诰> k . . ^ ’打底塗料、測鍍構造及保護材 、並經洪烤結合—冑’於球桿之特定區域並經表面粗化, 並上漆各種顏色之色漆,最後以透明金油塗裝保護顏色, 使其碳纖球桿表面具右意出 、 儿光表面之質感,而同時達到碳纖 質輕強韌及金屬光赛、, 鏡面美麗外觀,據以提升整體品質 者0 對照先前技術之功效: 、先剛技術對於高爾夫球桿之塗裝,僅係利用喷或 塗漆方式’但對於&纖材質之高爾夫球桿,則仍無法提升 其質感,造成高爾夫球桿呈現暗淡顏色,而本發明藉由濺 鍍之方式,將靶材之材質濺鍍至碳纖高爾夫球桿上,使碳 纖高爾夫球桿具有亮光表層’得以提升其質感與視覺感受 者。 二、高爾夫運動, 以無論是場地與球具, 一般定位在高階層人員的運動,所 都是一種高責象徵,所以球具均不 6 1308076 便宜,而如習用取碳纖製作高爾夫球桿,費用雖不便宜, 但卻沒有質感,造成人們不願意購買,而本發明相同之碳 纖球桿,卻具有亮光表面而深得喜愛,材質又輕又具強韌 性’提升整體品質與購買意願者。 有關本發明所採用之技術、手段及其功效,兹舉一較 佳實施例並配合圖式詳細說明於后,相信本發明上述之目1308076 IX. Description of the invention: [Technical field to which the invention pertains] The present invention provides a method for making a golf club with an ancient and a hemp, a redundant surface layer and a plurality of colors, in particular, a technically provided carbon fiber material is splashed. Polished and baked to have a bright effect, and can be used in a variety of colors to achieve a rich color golf club 〇 [Prior Art] The surface processing method of the conventional Wolff club is mainly formed by the surface of the club - transparent The bottom layer is then coated with a layer of lacquer on the transparent primer, and then a layer of protective lacquer is applied over the lacquer to complete the coating of the golf club surface. Quite, the above-mentioned golf clubs still have the following defects: The carbon fiber material structure is rough, so no matter how the paint is dead, there is no way to change its dull state, so that the carbon fiber ball # in the visual The effect is quite S' and the direct perception is the feeling of the secondary product, so the quality is not good enough to improve the buying. 1. Regardless of the way in which the club is sprayed or brushed, the color of the paint (4) reaches a uniform sentence and does not diversify the color. In view of the problems in the above-mentioned conventional structure, how to develop / and the innovative structure of the practicality of the heart, the consumers are eagerly awaiting, and the relevant industry must strive to develop the goal and direction of breakthrough. In view of the fact that the company has been engaged in the manufacturing development and design of related products for many years, the invention has been put into practical use for the purpose of designing and prudently evaluating the purpose of the above. 1308076 [Summary of the Invention] Technical problems to be solved: 垅镛, the material of the L. Alf Ball can be as good as the material, and the material can reach the light and strong position τι 夕*<· a is also relatively coarse sugar, I on how ^, ^ carbon fiber material 颧; = § you" grinding and lacquer, the surface of the human face is still quite faint and rough will ^ ^ s. First & 妷 妷 fiber golf clubs Technical characteristics of the problem: provide - ancient method with a redundant surface layer and a variety of colors between the golf clubs, the system ^ ^, anti-paper buckle surface coated with a transparent primer, then use sputtering The equipment is sputtered & and then coated with the sputter material of the sputter material. Sprinkle texture 诰> k . . ^ 'Bottom coating, plating structure and protective material, and combined with flooding - 胄' The specific area of the club is roughened by the surface, and the paint of various colors is painted, and finally the color is coated with transparent gold oil to make the surface of the carbon fiber club have the texture of the right and the light surface, and at the same time Carbon fiber light and strong and metal light race, mirror beautiful appearance, according to The overall quality of the 0 compared to the efficacy of the prior art: First, the technology for the golf club painting, only by spraying or painting method 'but for the & fiber material of the golf club, it still can not improve its texture, resulting in The golf club presents a dim color, and the present invention sputters the material of the target onto the carbon fiber golf club by sputtering, so that the carbon fiber golf club has a bright surface layer to enhance its texture and visual sensation. Golf, whether it is the venue and the ball, generally positioned in the movement of high-level personnel, is a high-responsibility symbol, so the clubs are not cheaper than 6 1308076, and the golf clubs are used for carbon fiber, although the cost is It is not cheap, but it has no texture, which makes people unwilling to buy, and the carbon fiber club of the same invention has a bright surface and is deeply loved, and the material is light and strong and toughened to improve the overall quality and purchase intention. The technology, the means and the effects thereof adopted by the invention are described in detail with reference to the drawings. EYES

的、構造及特徵,當可由之得一深入而具體的瞭解。 【實施方式】 參閱第一圖所示,本創作係提供-種具亮光表層及多 樣色之高爾夫球桿製法,其步驟為: 夕 步驟r取碳纖球桿1G ••取碳纖高爾夫球桿,於球桿表面 喷塗透明底漆,並細研磨該透明底漆; 步驟b :濺鑛1 1 :以激妒古、土 濺鍍方法,將靶材材質濺鍍至碳 爾夫球桿之透明底漆表面; 门 步驟c :保護處理賤錢芦彳? 12 .以保遵漆喷塗於碳纖高爾 球桿之濺鍍後类& ^ ^ 尺 表面保濩濺鍍層,保護漆為相定 於濺鍍層,且徂增、* 4 A ^ 1保濩漆為透明保護漆; 步驟d :烘烤13 :烘烤使锈 巧使透明底漆、滅鍍層及保護漆結人 一體。 α 明之碳纖球桿,該碳纖球 高爾夫球桿之形狀;該碳 干系1成 ,該打底塗料可為透明=夫打底塗料喷塗 滑,*此在後續製作上二1τ底塗料製作後表面會报平 光,以利繼續施作之之&打底塗料進行細研磨拋 之附者力;再以減鍍的方法在打底塗 7 1308076 料外部形成1鍍層;#後於濺鏟層外嘴塗保護漆,該保 護漆係保4處理賤鐘層,保護漆以相容於濺鍍層之材料為 之,保護漆為—透明塗料,保護漆並具有光澤,也可利用 喷塗的方式製作;其後得藉由烘烤硬化的方式使其結合在 一起。 另外,參閱第二圖所示,—種具亮光表層及多樣色之 南爾夫球桿另一製法,其步驟為: 步驟a:取碳纖球桿2ϋ :取碳纖高爾夫球桿,於球桿表面 喷塗透明底漆,並細研磨該考明底漆; ^ 以濺鍍方法,將靶材材質濺鍍至碳纖高 爾夫球桿之透明底漆表面; :蒦處理濺鍍層22 :以保護漆噴塗於碳纖高爾夫 球椁之滅鍍後表面’保護減鍍層; 供烤2 3 :供烤你读日日泛、未 使透明底漆、濺鍍層及保護漆社合 一體; 、。 特定區域粗化2 4 :特宕F梡、,. 特疋區域以研磨方式製作表面 租化; 上色漆 2 5 ·· l& 化位置; 、斤鸿顏色漆於特定區域之表面粗 μ & 26: *高_夫球桿上塗佈透明金$ 上述從步驟e後+ 3金油。 # ^ , 4[ 要針對碳纖球桿之特定區域方 付以藉由利用研麼 c人] 二如田 式’在特定區域内,#i甚斗矣 面粗化效果;其後特定 使,、產生表 ,該色漆包括不同之—面粗化位置’施以色漆喷塗 ",完全依照需求,而得以讓顏色 步驟 步驟 步驟d 步 步 步驟g 面 8 1308076 多變化;其後再塗佈透明金油,以透明金油除可展 外,更使色漆產生光亮質感。 精由上述之製法’本發明之碳纖球桿經過打底 保護漆’使得碳纖球桿具有金屬光亮質感, 油塗:於特定區域利用表面粗化研磨、色漆喷塗及 ’使得球桿表面顏色多變化,以之製成具有 鏡面質感球桿。 之較佳實施例為本發明之技 熟悉此項技術之人士當可在 積神與原則下對本發明進行變更與修改 修改1應涵蓋於如下申請專利範圍所界 【圖式簡單說明】 圖:係本發明其-製法步驟流程圖 圖:係'本發明另一製法步驟流程圖 王要7〇件符號說明】 0 )取碳纖球桿 2 )保護處理濺鍍層 0 )取碳纖球桿 2 )保護處理濺鍵層 4 )特定區域粗化 6 )塗佈金油 現色漆 塗料、 並該碳 透明金 金屬光 術特徵 不脫離 而該等 之範_ 前 進行具 本發明 變更與 中。, structure and characteristics, when you can get an in-depth and specific understanding. [Embodiment] Referring to the first figure, the author provides a golf club manufacturing method with a bright surface and a variety of colors. The steps are as follows: Take the carbon fiber club 1G in the evening step r • Take the carbon fiber golf club, Spray the transparent primer on the surface of the club and finely grind the transparent primer; Step b: Splashing 1 1 : Sputtering the target material to the transparent bottom of the carbon ball by exciting ancient and soil sputtering methods Paint surface; door step c: protection treatment of money reed? 12. Apply the varnish to the carbon fiber golf clubs after the sputtering & ^ ^ ruler surface protection splash, the protective paint is set to the sputtering layer, and increase, * 4 A ^ 1 protection The paint is a transparent protective paint; Step d: Baking 13: Baking makes the rust make the transparent primer, the de-plating layer and the protective lacquer one.明 明的碳纤维球杆, the shape of the carbon fiber golf club; the carbon dry system is 10%, the primer can be transparent = the base paint is sprayed, *This is the surface after the second 1τ primer is produced in the subsequent production Will report Pingguang, in order to continue to apply the & primer to carry out the fine grinding and polishing of the attached force; then by the method of deplating in the primer 7 1308076 material to form a plating outside; # after the splash layer The mouth is coated with a protective lacquer, which is used to protect the enamel layer. The protective lacquer is made of a material compatible with the sputter layer. The protective lacquer is a transparent paint, a protective lacquer and a gloss, and can also be produced by spraying. Then it can be combined by bake hardening. In addition, as shown in the second figure, another method for producing a Nelph cue with a bright surface layer and a plurality of colors is as follows: Step a: Take a carbon fiber club 2: Take a carbon fiber golf club on the surface of the club Spray a clear primer and finely grind the test primer; ^ Sputter the target material to the transparent primer surface of the carbon fiber golf club; 蒦 Treat the sputter layer 22: Spray with a protective paint Carbon fiber golf ball 灭 镀 镀 ' ' ' ' ' ' ' ; ; ; 供 供 供 供 供 供 供 供 供 供 供 供 供 供 供 供 供 供 供 供 供 2 2 2 2 2 2 2 2 2 2 2 2 Specific area roughening 2 4 : Special 宕F梡,,. Special area to make surface renting by grinding; Paint lacquer 2 5 ·· l&Position; jinhong color lacquered on a specific area surface μ &; 26: * High _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ # ^ , 4[To pay for a specific area of the carbon fiber club by using the researcher] The second type is in the specific area, #i甚斗矣面粗化的效果; Produce the table, the color paint includes different - surface roughening position 'painting paint', completely in accordance with the requirements, and the color step step d step by step step g face 8 1308076 more changes; The cloth is transparent gold oil, which can be used in addition to transparent gold oil to make the paint produce a bright texture. The above method of 'the carbon fiber club of the present invention is subjected to a primer protection paint' to make the carbon fiber club have a metallic bright texture, oil coating: using surface roughening, color paint spraying and 'making the surface color of the club surface in a specific area Changed to make a mirror-like club. The preferred embodiment of the present invention is a person skilled in the art. The present invention can be modified and modified in accordance with the principle of the invention. The modification 1 should be covered by the following patent application scope. The flow chart of the method of the invention is as follows: "The flow chart of another process step of the invention is illustrated by a symbol of 7". 0) Take the carbon fiber rod 2) Protect the sputter layer 0) Take the carbon fiber rod 2) Protection treatment The splash-bonding layer 4) the specific region is roughened 6) the gold-oil lacquer coating is applied, and the carbon-transparent gold-metal glazing feature is not detached, and the invention is modified.

文係針對本發明 體之說明;惟,The text is directed to the description of the invention;

(11)濺鍍 (1 3 )烘烤 (21)濺鍍 (2 3 )烘烤 (2 5 )上色漆 9(11) Sputtering (1 3) Baking (21) Sputtering (2 3) Baking (2 5 ) Coloring paint 9

Claims (1)

1308076 、申請專利範圍: 步驟為 步驟a 種具亮光表層及多樣色之高爾夫球桿製法,其 取碳纖球桿:取碳纖高爾夫球桿,於球桿表 塗透明底漆’並細研磨該透明底漆; 、 減鑛:以濺鍍方法,將 4ί“曰· 將乾材材質濺鑛至碳纖高爾 夫球#之透明底漆表面; _ 保護處理濺錢層: 以保護漆噴塗於碳纖高爾 桿之濺鍍後表面’保護濺鍍層; 火、烤烘烤使透明底漆、㈣層及保護漆 體丨 。一 特定區域粗化· ^主〜 .特疋區域以研磨方式製作表 化; 祖 色漆上漆所需顏色漆於特定區域之表面 位置; 。g塗佈金油.於高爾夫球桿上塗佈透明金油。 2 >申叫專利範圍第1項所述之具亮光表層及多揭 色之高爾夫球桿製法’其中該保護法為相容於滅鍍層。策 2如申明專利範圍第1項所述之具亮光表層及多樣 之冋爾夫球桿製法,其中該保護漆為透明保護漆。’十一、圖式: 如次頁 步驟 步驟 步驟d 步驟 步驟 101308076, the scope of patent application: The steps are step a. A golf club method with a bright surface and various colors, which takes a carbon fiber club: a carbon fiber golf club, a transparent primer on the club surface and finely grinds the transparent bottom Paint; , ore reduction: by sputtering method, 4 曰 "曰 · will dry the material to the carbon fiber golf ball # transparent primer surface; _ protection treatment splashing layer: with protective paint sprayed on the carbon fiber Gol rod After sputtering, the surface 'protects the sputter layer; fire, bake and bake to make the transparent primer, (four) layer and protect the paint body. A specific area is roughened · ^ main ~ . The special area is made by grinding; Paint the desired color to paint on the surface of a specific area; .g coating gold oil. Apply transparent gold oil to the golf club. 2 > Apply for the bright surface layer and the multiple surface mentioned in the patent scope The golf club method of the color is in which the protection method is compatible with the de-plating layer. The method of claim 2 is as follows: the bright surface layer and the various methods of the golf club according to the first claim, wherein the protective paint is transparent protection Paint. '11. Schema: Next page Step Step Step d Step Step 10
TW095137016A 2006-10-05 2006-10-05 Method for manufacturing golf club with multicolor and varnished surface layer TW200711687A (en)