Abstract
This invention relates to a method for joining golf club head wherein metal molding is employed to form two or more components, which are joined by means of brazing, characterized in that: a layer of another metal is applied first on the welding surface of the material for joining.
Description
1288011 叫y fI 6 十、申請專利範圍: 1.一種高爾夫桿頭接合方法,是以金屬材料成型出二或 二以上之構件,然後在各構件的相對接合部位塗佈硬焊焊 料,將該等構件送入加熱爐中加熱,使硬焊焊料在各構件 的塗佈面上形成一金屬層,而形成具有金屬保護層的待接 5合構件備料,之後再將具有金屬保護層的對應構件以硬焊 方式接合。1288011 Called y fI 6 X. Patent application scope: 1. A golf club head joining method, in which two or more members are formed by metal materials, and then brazing solder is applied to the opposite joint portions of the members, and the like The member is sent to the heating furnace for heating, so that the brazing solder forms a metal layer on the coated surface of each member, and the prepared 5-member member with the metal protective layer is prepared, and then the corresponding member having the metal protective layer is Bonded by brazing.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW95116404A TWI288011B (en) | 2006-05-09 | 2006-05-09 | Method for joining golf club head |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW95116404A TWI288011B (en) | 2006-05-09 | 2006-05-09 | Method for joining golf club head |
Publications (2)
Publication Number | Publication Date |
---|---|
TWI288011B true TWI288011B (en) | 2007-10-11 |
TW200742598A TW200742598A (en) | 2007-11-16 |
Family
ID=39202854
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW95116404A TWI288011B (en) | 2006-05-09 | 2006-05-09 | Method for joining golf club head |
Country Status (1)
Country | Link |
---|---|
TW (1) | TWI288011B (en) |
-
2006
- 2006-05-09 TW TW95116404A patent/TWI288011B/en not_active IP Right Cessation
Also Published As
Publication number | Publication date |
---|---|
TW200742598A (en) | 2007-11-16 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
AT502103B8 (en) | Method for bonding by soldering two parts made of thermoplastic composite material | |
ATE423892T1 (en) | REPAIR PROCEDURES FOR COATED ITEMS | |
WO2009046699A3 (en) | Joining and material application method for a workpiece having a workpiece region comprising a titanium aluminide alloy | |
WO2007109416A8 (en) | Method for joining or repairing metal surface parts | |
JP2009532296A5 (en) | ||
BRPI0413148A (en) | welding method and adhesive bonding method for joining metal components | |
JP2007507355A5 (en) | ||
EP1605068A3 (en) | Homogeneous welding via pre-heating for high strength superalloy joining and material deposition | |
WO2008115696A3 (en) | Metal-ceramic composite air braze with ceramic particulate | |
WO2009010934A3 (en) | Method for joining sic-diamond | |
JP2011514947A5 (en) | Exhaust turbocharger | |
JP2009503002A5 (en) | ||
DE602007009589D1 (en) | A friction stir welding method for bonding a coated metal element to another metal element with pre-heating the coating prior to friction stir welding | |
WO2009077735A8 (en) | Joining metal pipes | |
ATE417691T1 (en) | METHOD FOR JOINING WORKPIECES MADE OF STAINLESS STEEL, NICKEL OR NICKEL ALLOYS USING A JOINING LAYER CONSISTING OF A NICKEL-PHOSPHORUS ALLOY; METHOD FOR PRODUCING A MICROSTRUCTURED COMPONENT USING SUCH A METHOD | |
TWI455817B (en) | Joined belt and method for producing joined belt | |
GB2463214A (en) | Method for preventing void formation in a solder joint | |
TWI456017B (en) | Method of manufacturing bonded member and bonded member manufacturing apparatus | |
SE0501199L (en) | Procedure for soldering stainless steel objects | |
TWI288011B (en) | Method for joining golf club head | |
JP2007127649A5 (en) | ||
JP2008218953A5 (en) | ||
AU2015243024A1 (en) | Bonding dissimilar ceramic components | |
DE502007002956D1 (en) | Method for connecting an aluminum fin to a steel pipe and heat exchanger with a unit produced in this way | |
ATE554877T1 (en) | METHOD FOR PRODUCING A LOW-DRAGON WELDED JOINT |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
MM4A | Annulment or lapse of patent due to non-payment of fees |