TW491796B - Packaging container made of paper and method for producing the same - Google Patents

Packaging container made of paper and method for producing the same Download PDF

Info

Publication number
TW491796B
TW491796B TW90120499A TW90120499A TW491796B TW 491796 B TW491796 B TW 491796B TW 90120499 A TW90120499 A TW 90120499A TW 90120499 A TW90120499 A TW 90120499A TW 491796 B TW491796 B TW 491796B
Authority
TW
Taiwan
Prior art keywords
layer
inner layer
joint
bottom plate
winding
Prior art date
Application number
TW90120499A
Other languages
Chinese (zh)
Inventor
Ming-Tang Shiu
Original Assignee
Ming-Tang Shiu
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ming-Tang Shiu filed Critical Ming-Tang Shiu
Priority to TW90120499A priority Critical patent/TW491796B/en
Application granted granted Critical
Publication of TW491796B publication Critical patent/TW491796B/en

Abstract

The present invention provides a packaging container made of paper and a method for producing the same. The container comprises a base plate and a peripheral wall. The peripheral wall has an inner layer and an outside wrapping layer. The method for producing the container comprises: cutting an inner layer and an outside wrapping layer into a predetermined shape; folding the outside wrapping layer along a folding line to form inner and outer clamping plates that abuts each other and surround the inner layer; using a mold to curl and shape the plates, such that a first joint section and a second joint section of the outside wrapping layer that protrudes beyond the inner layer separately extends over inner and outer faces of the inner layer; using a adhesive binding technique to adhesively attach the joint sections on the inner and outer faces; and mounting the base plate and using a winding machine to wind and combine the peripheral wall with the base plate. The two protruded joint sections of the outside wrapping layer are separately attached to the faces of the inner layer so that the assembled container has a smoother appearance. Furthermore, the innovative winding technique does not need to use an adhesive for the joining of the base plate, while increasing the strength of the container.

Description

^+yi /y〇 A7 五、發明說明(1 ) 發明領域 蝼齊邨智慧財產局員工消費合作社印製 本發 一種利用 後可增加 【習知技 一般 環繞底板 之頂蓋, 層及一印 時,先裁 層外壁面 後之圍繞 繞壁,接 在圍繞壁 物品之容 其圍繞壁 合,因此 出之接合 用膠合之 壁之内壁 置太重之 提高容器 【發明概 因此 月疋關於_種紙製包裝容器及其製法,特 裁切成型與捲繞接合之製造方法,使其成 美觀性與強度的容器。 藝說明】 紙製谷|§為常見的包裝器物,其包含一底 周緣延伸之圍繞壁,以及一可覆蓋在圍繞 -中’該圍繞壁具有—由厚紙板材質所製 有圖案色彩之外包覆層,而習知紙製容器 切出該内層與外包覆層,續將外包覆層貼 上,再以預定模具將其捲曲定型,此時, 壁的銜接端以膠合技術將其重疊膠合而成 著將底板置於圍繞壁底端且同樣將其以膠 之内壁面上,該圍繞壁與底板即可形成一 置空間。上述習知紙製容器雖然可放置物 之接合方式乃是直接以膠水將兩銜接端 ,圍繞壁上會產生一段由該銜接端重疊接 段,造成容器美觀上的缺失,再者,其底 方式而與圍繞壁結合,兩者僅靠底板貼合 面上的接合部分做結合,其負重強度不足 物品,因此,如何改善容器的構造及製造 之美觀及整體強度,乃是本發明所欲改良要】 ’本發明之目的即在提供一種構造美觀, 別是指 型結合 板、一 壁頂端 成之内 在製造 附於内 將定型 型該圍 水貼合 可放置 品,但 重疊膠 合所突 板亦採 在圍繞 無法放 方法以 之處。 且可增 -------------裝--------訂---------線 (請先閱讀背面之注意事項再填寫本頁) 第3頁 私紙張尺度適用中酬家標準(CNS)A4規格(210 X 297公爱) 491796 A7 五、發明説明(2 加整體強度與底板結合度的容器。^ + yi / y〇A7 V. Description of the invention (1) Field of invention Printed by the Consumers' Cooperative of the Qiqi Village Intellectual Property Bureau. This method can be used to increase the [cover of the conventional technology, which usually surrounds the bottom cover of the bottom plate, and the time of printing. The outer wall surface of the layer is cut first, and then the surrounding wall is connected to the surrounding wall, and the surrounding wall is closed. Therefore, the inner wall of the glued wall is too heavy to improve the container. Packaging container manufacturing method and manufacturing method thereof, special cutting molding and winding and bonding manufacturing method, make it a beautiful and strong container. Description of the art] Paper valley | § is a common packaging utensil, which includes a surrounding wall extending from the bottom periphery, and a covering-in-the 'surrounding wall which has a pattern-color package made of cardboard material Cover, and the conventional paper container cuts out the inner layer and the outer cover layer, continues to attach the outer cover layer, and then curls it with a predetermined mold to shape it. At this time, the connecting ends of the walls are overlapped by a gluing technique. Glued to the work, the bottom plate is placed on the bottom end of the surrounding wall and the inner wall surface is also glued. The surrounding wall and the bottom plate can form a space. Although the conventional paper container can be placed, the joining method is to directly connect the two joint ends with glue, and a section overlapping the joint end will be generated around the wall, which causes the lack of aesthetic appearance of the container. Furthermore, the bottom way In combination with the surrounding wall, the two are combined only by the joints on the bonding surface of the bottom plate, and their load-bearing strength is insufficient. Therefore, how to improve the appearance and overall strength of the structure and manufacture of the container is the improvement of the invention. 】 'The purpose of the present invention is to provide an aesthetically pleasing structure, not to mention that the type of bonding plate, a wall top is built in, and the shape of the surrounding water can be placed and placed, but the protruding plates of the overlapping gluing are also used. Around where you can't put a method. And can add ------------- install -------- order --------- line (please read the precautions on the back before filling this page) The 3-page private paper scale applies the CNS A4 specification (210 X 297 public love) 491796 A7 V. Description of the invention (2 The container with the overall strength and the combination of the bottom plate.

於是,本發明之紙製包裝容器乃包合 VL s〜底板,及一沿 底板周緣向上突伸之圍繞壁,其中,該圚 次固繞壁具有一内層 及一外包覆層,其特徵在於: 該内層,係由可撓曲之紙材所裁切而#,益具有兩反 向之内基面與外基面、位於該等基面上、下兩側之相對立 側邊,以及兩可相互對接之左、右銜接端; 該外包覆層,呈預定形狀且可撓曲之薄板體,其具有 一平行薄板體長度方向之摺線、沿摺線對折而可相互貼合 且包覆該内層之一内夾板與一外夾板,以及分別自内、外 夾板相背離之一端突伸而可相互接合之第—與第二接合 丰又’ g内、外夾板包覆該内層後’該外包覆層更具有兩突 出内層之兩側邊且相對稱的捲繞段; 經濟部中央標準局員工消費合作社印製 當該等炎板包覆該内層後’該内層之左、右銜接端會 分別突出内、外夾板背離第一、二接合段之一端,此時將 其撓曲’該第一接合段即可黏固在内層左銜接端之内基面 上’而第^一接合段則黏固在内層右銜接端之外基面上,最 後’利用捲繞機器將撓曲後之捲繞段對折捲繞至内層之兩 側邊即可成型該圍繞壁。 為了製造該容器,本發明的製造方法包含有裁切成 型、黏固内層及外包覆層、撓曲定型、膠合對接及捲繞接 合底板等加工步驟,其中: 該裁切成型步驟:利用裁切技術將内層及外包覆層裁 切成預定尺寸形狀; 頁 (請先閱讀背面之注意事項再填寫本頁) 第 本紙張尺度適用中國國家標準(CNS ) A4規格(210X297公釐) 491796 A7 B7 五、發明説明(3 ) (請先閱讀背面之注意事項再填寫本頁) 該黏固内層及外包覆層步驟:將外包覆層沿一中央摺 線對折’而形成一可相互貼合之内、外夾板,且内、外夾 板相背離之一端分別突伸一可相互接合之第一與第二接合 段,該等夾板即可沿摺線對折而黏貼該内層; ,該撓曲定型步驟:將上述黏貼後所形成之圍繞壁以預 定之成型模具使其捲曲定型,此時,内層之兩銜接端相互 抵接,外包覆層之第一、第二接合段分別伸入内層銜接端 b反向之内、外基面; 膠合對接步驟:將定型後之圍繞壁以膠合技術,使外 包覆層之第一、第二接合段分別伸入而膠合在内層銜接端 ‘反向之内、外基面上; 該捲繞接合底板步驟:把底板放置在膠合後圍繞壁所 形成之空間内,使底板之一捲繞層沿底板板體周緣向下彎 折貼合圍繞壁,再利用可捲繞機器將圍繞壁與捲繞層由其 底端捲繞對折,使圍繞壁與底板接合固定。 ,【圖式之簡單說明】 ,本發明之其他特徵及優點,在以下配合參考圖式之較 佳實施例的詳細說明中,將可清楚的明白,在圖式中: 經濟部中央標準局員工消費合作社印製 第一圖是本發明包裝容器之一較佳實施例的立體分解 圖,圖中顯示一底板、一圍繞壁與二頂蓋的相對關係; 第二圖是該較佳實施例中之圍繞壁的平面展開分解 圖’說明該圍繞壁之一外包覆層與一内層的對廡關係; 第二圖是該較佳實施例之局部縱向組合剖視圖,說明 該圍繞壁接合該底板後的對應關係; 第5頁 本紙張尺度適用中國國家標準(CNS ) A4規格(210X297夕釐) 491796 A7 B7 五、發明説明(4) 第四圖是該較佳實施例之一製造流程圖 第五圖是本發明包裝容器之另一較佳實施例的立體 Γ5Π · 園, 第六圖是第五圖中之一圍繞壁的平面展開分解圖,說 明該圍繞壁之一外包覆層與一内層的對應關係;及 第七圖是一製造流程圖,說明第五圖之容器的製造流 程。 【較佳實施例之詳細說明】 參閱第一、二圖,本發明之包裝容器1是由符合環保 之紙材加工製成,而可用來容置物品,以下說明之方向即 以第二圖之圍繞壁展開圖的方向為基準,該容器1包含: 一底板11、一圍繞壁2,以及一可覆蓋在圍繞壁2上方之 頂蓋12 〇 該底板11,為一圓盤造型,但該造型並不以本實施例 所揭示之圓形為限’其亦可為··正方形、六角形、八角形 等等的幾何形狀’所述之底板11具有一圓形之板體m , 以及一面積較板體111大且可彎折捲繞之捲繞層112,該 捲繞層11 2即具有一外緣突出該板體1丨丨之-折段丨丨3。 經濟部中央標準局員工消費合作社印製 (請先閱讀背面之注意事項再填寫本頁) 該圍繞壁2,具有一内層21及一可對折而包覆該内層 21之外包覆層22,其中’該内層21是由厚紙板裁切而成 一矩形板體’並具有兩反向之内基面211與外基面212、 位於該等基面2 11、21 2上下兩侧之相對立側邊2 1 3,以及 兩可藉由撓曲而相互對接之左銜接端214與右銜接端 2 1 5。又該圍繞壁2為了達到不需膠水即可結合内層21之 第6頁 本紙張尺度逋用中國國家標準(CNS ) A4規格(210X 297公釐) 491796 Α7 Β7 五、發明説明(5 ) 兩銜接端214、215的目的,故更具有一可結合該内層21 之左、右銜接端214、215的卡接裝置23,該卡接裝置23 具有至少一形成在左銜接端214上的卡槽231,以及至少 一形成在右銜接端215上,且可配合卡嵌入該卡槽231的 •卡嵌塊232’藉由該等卡嵌塊232卡嵌所對應之卡槽231 即可不需膠水黏合而達到結合内層2丨之目的,且結合後不 會有重疊之結合段產生更具有美觀的效果。 該外包覆層22,為一預定形狀且可撓曲之薄板體,其 具有一平行薄板體長度方向之中央摺線2 2 1、沿摺線2 2 1 對折而可相互貼合且包覆該内層21之一内夾板222與一外 失板223、分別自内、外夾板222、223相背離且對應該内 經濟部中央標準局員工消費合作社印製 (請先閱讀背面之注意事項存填寫本買) 層21之左、右銜接端214、215之一端突伸的第一接合段 224與第二接合段225,以及一自第二接合段22 5鄰近摺線 221之一端突伸的第三接合段226,其中,該第一接合段 224與第一接合段225之面積相同。再者,該外包覆層22 -更具有平行摺線221且分別位在内、外夾板222、223鄰近 ί側邊之兩平行捲繞摺線2 2 0,每一夾板2 2 2、2 2 3之兩捲繞 摺線2 2 0的最大距離恰與内層2 1兩側邊2 1 3間之最大距離 相同’當内、外夾板222、223包覆該内層21且沿該摺線 221對折時,該外包覆層22内外夾板222、223之捲繞摺 線2 2 0重疊,而内層21之兩侧邊213亦分別與捲繞摺線 220呈一直線疊合,此時,該外包覆層22對折後之上下兩 側邊即可界定出兩突出内層2 1之上下兩侧邊2 1 3且相對稱 〃的捲繞段227。 第7頁 本紙張尺度適用中國國家標準(CNS ) Α4規格(210Χ 297公釐) 491796 A7 B7 五、發明説明(6) 該頂蓋12,可覆蓋在圍繞壁2之上方,藉以防止異物 進入’或防止放置在容器丨内之物品掉落。 當該等夾板222、223包覆該内層21後,該内層21 之左、右銜接端214、215會分別突出内、外夾板222、223 遠離第一、二接合段224、225垂直摺線221之一端,且内 層21之兩側邊213分別與内、外夾板222、223之捲繞摺 線220呈一直線疊合狀態,此時將圍繞壁2撓曲定型且藉 由該卡接裝置23之卡嵌,使内層21之左、右銜接端214、 215對接,該第一接合段224即可藉由膠合技術而黏固在 内層21鄰近左銜接端214之内基面211上,而第二接合段 225則黏固在内層21鄰近右銜接端215之外基面212上, 最後將第三接合段2 2 6沿摺線2 2 0向第一接合段2 2 4方向 彎折並加以黏固,即可完成圍繞壁2之製造。 經濟部中央標準局員工消費合作社印製 (請先閲讀背面之注意事項再填寫本頁) 參閱第一、三圖,本發明為了使容器1之底板11與圍 繞壁2達到接合與具有較佳的結合強度,先將底板11之捲 繞層11 2沿板體111周緣彎折成垂直狀,續將底板11放置 在圍繞壁2底端,使底板11捲繞層11 2之彎折段11 3貼合 圍繞壁2内夾板222之内壁面,再利用捲繞機器將圍繞壁 2下端定型後之捲繞段227與彎折段113重複對折捲繞, 直至包覆住底板11板體111底面為止,其中,位於圍繞壁 2底端之捲繞段227至少重複對折捲繞二次以上,藉此達 到固結底板11與圍繞壁2之目的,相同道理,該圍繞壁2 頂端亦是採用相同技術來捲繞該捲繞段227使其定型,該 等捲繞段2 2 7經由多次折繞後,其厚度將相對增加故更具 第8頁 本紙張尺度適用中國國家標準(CNS ) A4規格(210X297公釐) 491796 經濟部中央標準局員工消費合作社印製 Α7 Β7 五、發明説明(7 ) 有增加容器1整體強度的功效。 當然’本發明之圍繞壁2亦可僅預留一結合底板i i 之捲繞段227即可,並不一定要預留兩捲繞段227來捲繞 加工’當圍繞壁2僅預留一捲繞段227時,只要將連結兩 夾板222、223之摺線221抵接内層21上方之側邊213, 使中央摺線2 2 1與側邊21 3呈一直線重疊,接著,即可利 用捲繞技術將位於下方之捲繞段227與底板11捲繞結合。 . 參閱第四圖,本發明為了製造第一圖所示的容器1, 其製造上包含以下加工步驟: 一、 裁切成型内層21及外包覆層22:利用裁切技術將内 層21及外包覆層22裁切成預定尺寸形狀,其中,該 、内層21可選用厚紙板直接裁切,該外包覆層22則可 選用列印有圖樣標籤之包裝紙。 二、 黏固内層2 1及外包覆層22 ··將外包覆層22沿一中央 摺線2 2 1對折,形成一可相互貼合之一内夾板2 2 2與 • 一外夾板223,且内、外夾板222、223相背離之一端 ί 分別突伸一可相互接合之第一接合段224與第二接合 段225,以及一自第二接合段22 5鄰近摺線221之一 端向外延伸之第三接合段226,該等夾板222、223即 可沿摺線221對折而包覆黏定該内層21,當内、外夾 板222、223包覆該内層21後,該外包覆22層更具有 兩突出内層2 1之兩側邊2 1 3且相對稱的捲繞段2 2 7。 三、 撓曲定型:將上述黏貼後所形成之圍繞壁2以預定之 成型模具使其捲曲定型,此時,内層21之兩銜接端 第9頁 本紙張尺度適用中國國家標準(CNS ) A4規格(210X 297公釐) I I I I n 批衣 I I I 1訂 n 線 (請先閲讀背面之注意事項再填寫本頁} 491796 A7 B7___ 五、發明説明(8 ) 214、215藉由卡接裝置23中之該等卡嵌塊232分別 卡嵌所對應之卡槽231而達到抵接固結,外包覆層22 之第一、第二接合段224、225分別伸入内層21鄰近 銜接端214、215之反向的内、外基面211、212上。 四、 膠合對接··將定型後之圍繞壁2以膠合技術,使外包 覆層22之第一、第二接合段224、2 2 5分別伸入而膠 合在内層 21銜接端214、215反向之内、外基面上 211、212,最後將第三接合段226朝第一接合段224 方向彎折,再將其膠合固定在第一接合段224背離内 層21之内基面上。 五、 捲繞接合底板11:把底板11放置在膠合後圍繞壁2 所形成之空間内,使底板11捲繞層丨丨2之彎折段11 3 彎折而貼合圍繞壁2内壁面,此時,該底板11捲繞層 11 2彎折後之彎折段11 3底端切齊内層2 1下端之側邊 2 1 3,即底板11稍高於圍繞壁2底端之捲繞段2 2 7, 再利用可捲繞機器將圍繞壁2由底端捲繞段2 2 7往上 捲繞對折多次,使圍繞壁2與底板11捲繞層丨丨2捲繞 接合固定。 經濟部中央標準局員工消費合作社印製 (請先閲讀背面之注意事項再填寫本頁) 六、 捲繞圍繞壁2頂端並覆蓋頂蓋12 :同樣利用可捲繞機 器將圍繞壁2頂端之捲繞段22、7朝下捲繞對折多次, 使圍繞壁2頂端定型而可增加i繞壁2頂端之強度, 最後將頂蓋12覆蓋即完成容器1。 由以上說明可知,本實施例利用外包覆層22突出之兩 接合段224、225分別貼合在内層21之該等基面211、212 第10頁 本紙張尺度適用中國國家樣準(CNS) M規格(21〇χ297公楚) " -- A7 B7 491796 五、發明説明(9 ) 上,可使結合後之容器1更具平整美觀,且藉由捲繞製造 技術的創新’不僅不需膠水接合底板π,更可增加容器之 強度’故本發明該製造方法可製造出美觀且強度較佳的容 器1 0 參閱第五、六圖,為本發明容器1之另一較佳實施例, 該今器1可配合底板u形狀而製成不同幾何形狀的外觀, 因所能成型之幾何形此π t ^ ^ 八N〜狀眾多,以下僅以一六角形外觀之容 器1來做說明,但該容器1之外觀並不以所揭示之六角形 為限。該容器1具有一六角形之底板13、頂蓋14,以及一 橫截面為六角形之圍繞壁3,其中,該圍繞壁3同樣是由 内層31及外包覆層32所組成,該内層31同樣具有反 向之内、外基面311,以及兩銜接端312,且同樣可藉由一 卡接裝置33而達到對接兩銜接端31 2之目的,該外包覆層 32亦具有一中央摺線321、兩夾板3 2 2、第一、二=合二 323、324,以及第三接合段325。 σ又 本實施例與第一實施例之差異在··該外包覆層32之兩 夾板322具有數個等距間隔且垂直中央摺線32丨 、弟一凹 摺線320,該内層31具有與該第一凹摺線32〇内外對應之 第二凹摺線310,當内層31與外包覆層32組成圍繞=3 後,沿各摺線310、320將其彎摺,再同第一實施例之牛驟 將該第一接合段323與第二接合段3'24分別黏固右咖^ q牧内層3 1 鄰近兩銜接端312之内、外基面311上,之後將笛一 、乐—*接合 段325向第一接合段321方向彎折並加以黏固,再利用上 述之捲繞技術結合底板13與成型該圍繞壁3頂端遗菩 狄盖上頂 第11頁 &張尺度適用中國國家標準(CNS ) A4規格(210X297公釐) ---------裝------訂------線 C请先閱讀背面之注意事項再填寫本頁) 經濟部中央標準局員工消費合作社印褽 491796 A7 ------ 五、發明說明(10) 蓋14’即可形成一六角形外觀之容器1。 (請先閱讀背面之注意事項再填寫本頁) 配合參閱第七圖,為了製造第六圖之容器1,本實施 例之加工步驟與第一實施例之步驟大致相同,其僅在第一 實施例之步驟二與步驟三之間增加一成型摺線的步驟,其 中’該成型摺線之加工方法為: 利用預定之模具在黏固内層31及外包覆層32後的圍 繞壁3上成型數等距間隔且垂直中央摺線32丨之凹摺線 310、32 0。接著,再重複第一實施例製造方法之步驟四、 五、六即可完成外觀為六角形之容器1。 歸納上述,本發明容器利用外包覆層突出之兩接合段 可分別貼合在内層之該等基面上,可使結合後之容器更具 平整吳觀’且藉由捲繞製造技術的創冑,不僅不需膠水接 合底板,更可增加容器之強纟,再者,本發明之容器亦可 製作成多種幾何形狀外觀以因應消費者的需求,故確實能 達到發明之目的。 經濟部智慧財產局員工消費合作社印製 惟以上所述者,僅為本發明之二較佳實施例而已,當 不能以此限定本發明實施之範圍,即大凡依本發明申請專 利範圍及發明說明書内容所作之簡單的等效變化與修飾, 皆應仍屬本發明專利涵蓋之範圍内。 第12頁 本紙張尺度適用中國國家標準(CNS)A4規格(210 X 297公釐) 491796 A7 B7 五、發明説明(η) 【元件標號對照】 經濟部中央標準局員工消費合作社印製 1 容 器 224 第 一 接 合段 11 底 板 225 第 二 接 合段 111 板 體 226 第 二 接 合段 112 捲 繞層 227 捲 繞 段 113 彎 折 段 23 卡 接 裝 置 12 頂 蓋 231 卡 槽 13 底 板 232 卡 塊 14 頂 蓋 3 圍 繞 壁 2 圍 繞 壁 31 内 層 21 内 層 310 第 二 凹 摺線 2H 内 基 面 311 基 面 212 外 基 面 312 銜 接 端 213 側 邊 32 外 包 覆 層 214 左 銜 接 端 320 第 一 凹 摺線 215 右 銜 接 端 321 中 央 摺 線 22 外 包 覆 層 322 夾 板 220 捲 繞 摺 線 323 第 一 接 合段 221 中 央 摺 線 324 第 二 接 合段 222 内 夾 板 325 第 二 接 合段 223 外 夾 板 33 卡 接 裝 置 (請先閲讀背面之注意事項再填寫本頁) 第13頁 本紙張尺度適用中國國家標準(CNS ) A4規格(210X07公釐)Therefore, the paper packaging container of the present invention includes a VL s ~ bottom plate, and a surrounding wall protruding upward along the peripheral edge of the bottom plate, wherein the secondary fixed winding wall has an inner layer and an outer coating layer, which are characterized by: The inner layer is cut from a flexible paper material. # It has two opposite inner and outer base surfaces, the opposite sides located on these base surfaces, the lower sides, and two The left and right joint ends that are butted to each other; the outer cladding layer has a predetermined shape and a flexible thin plate body, which has a fold line parallel to the length direction of the thin plate body, and can be folded and folded along the fold line to cover each other and cover the inner layer. An inner plywood and an outer plywood, and a first and a second joint which protrude from one end facing away from the inner and outer plywood, respectively, and can be joined to each other—the second and outer joints are covered by the inner and outer plywood after the inner layer is covered. The cladding layer also has two winding sections that protrude from both sides of the inner layer and are symmetrical; printed by the Consumer Cooperatives of the Central Standards Bureau of the Ministry of Economic Affairs. After the lamina covers the inner layer, the left and right joint ends of the inner layer will be respectively Protruding the inner and outer splints away from the first and second joint sections One end, at this time, it is flexed 'the first joint section can be fixed on the inner base surface of the left joint end of the inner layer' and the first joint section is fixed on the outer base surface of the right joint end of the inner layer, and finally 'Using a winding machine, the deflected winding section is folded in half to the two sides of the inner layer to form the surrounding wall. In order to manufacture the container, the manufacturing method of the present invention includes processing steps such as cutting and shaping, cementing the inner and outer cladding layers, deflection setting, gluing butt joints, and winding and bonding the bottom plate, etc., wherein: the cutting and shaping steps: Use the cutting technology to cut the inner layer and outer cladding into a predetermined size and shape; page (please read the precautions on the back before filling in this page) The paper size applies to the Chinese National Standard (CNS) A4 (210X297 mm) 491796 A7 B7 V. Description of the invention (3) (Please read the precautions on the back before filling this page) The step of cementing the inner layer and the outer coating layer: Fold the outer coating layer in half along a central fold line to form a mutual fold Laminated inner and outer plywood, and one end facing away from the inner and outer plywood, respectively, protrudes a first and a second joining section which can be engaged with each other, and the plywood can be folded along the fold line to stick the inner layer; Step: The surrounding wall formed after the pasting is curled and shaped by a predetermined molding mold. At this time, the two joint ends of the inner layer abut against each other, and the first and second joint sections of the outer cladding layer respectively extend into the inner layer. The inner and outer base surfaces of the connecting end b are reversed. The step of gluing butt jointing: the surrounding wall after shaping is glued so that the first and second joint sections of the outer cladding layer are respectively extended and glued to the inner end of the connecting layer. Inwardly and outwardly on the base surface; The step of winding and joining the bottom plate: placing the bottom plate in the space formed by the surrounding wall after gluing, so that one of the winding layers of the bottom plate is bent down along the peripheral edge of the bottom plate and fits the surrounding wall Then, a winding machine is used to wind the surrounding wall and the winding layer in half from the bottom end, so that the surrounding wall and the bottom plate are joined and fixed. [Simplified description of the drawings] Other features and advantages of the present invention will be clearly understood in the following detailed description of the preferred embodiment with reference to the drawings. In the drawings: Staff of the Central Standards Bureau of the Ministry of Economic Affairs The first picture printed by the consumer cooperative is a perspective exploded view of a preferred embodiment of the packaging container of the present invention, showing the relative relationship between a bottom plate, a surrounding wall and two top covers; the second picture is in the preferred embodiment Exploded exploded view of the plane surrounding the wall 'illustrates the opposing relationship between an outer cladding layer and an inner layer of the surrounding wall; the second figure is a partial longitudinal sectional view of the preferred embodiment, illustrating that the surrounding wall joins the bottom plate Corresponding relationship; page 5 This paper size applies the Chinese National Standard (CNS) A4 specification (210X297). 491796 A7 B7 V. Description of the invention (4) The fourth figure is one of the preferred embodiments. The figure is a three-dimensional Γ5Π · circle of another preferred embodiment of the packaging container of the present invention. The sixth figure is an exploded plan view of a wall surrounding one of the fifth figures, illustrating an outer coating layer and an inner layer of the surrounding wall. Corresponding relationship; FIG seventh and a manufacturing flow diagram illustrating processes for producing a fifth container of FIG. [Detailed description of the preferred embodiment] Referring to the first and second drawings, the packaging container 1 of the present invention is made of environmentally-friendly paper materials and can be used for containing articles. The directions described below are shown in the second drawing. The direction of the development view of the surrounding wall is used as a reference. The container 1 includes: a bottom plate 11, a surrounding wall 2, and a top cover 12 that can cover the surrounding wall 2. The bottom plate 11 is a disc shape, but the shape It is not limited to the circular shape disclosed in this embodiment. 'It may also be a geometric shape of a square, a hexagon, an octagon, etc.' The bottom plate 11 has a circular plate body m, and an area. The winding layer 112 is larger than the plate body 111 and can be bent and wound, and the winding layer 112 has an outer edge that protrudes from the plate body 1 丨-a folded section 丨 3. Printed by the Consumer Cooperatives of the Central Standards Bureau of the Ministry of Economic Affairs (please read the precautions on the back before filling out this page) The surrounding wall 2 has an inner layer 21 and an outer covering layer 22 that can be folded in half to cover the inner layer 21, of which 'The inner layer 21 is a rectangular plate cut out of thick cardboard' and has two opposite inner base surfaces 211 and an outer base surface 212, and the opposite vertical sides located on the upper and lower sides of the base surfaces 2 11, 21 2 2 1 3, and two left joint ends 214 and right joint ends 2 1 5 which can be docked with each other by bending. And the surrounding wall 2 can be combined with the inner layer 21 on page 6 without the need for glue. This paper size uses the Chinese National Standard (CNS) A4 specification (210X 297 mm) 491796 Α7 Β7 5. Description of the invention (5) For the purpose of the ends 214 and 215, there is a latching device 23 which can be combined with the left and right ends 214 and 215 of the inner layer 21. The latching device 23 has at least one slot 231 formed on the left engaging end 214. And at least one of the card inserting blocks 232 'formed on the right connecting end 215 and capable of cooperating with the card embedded in the card slot 231. The card slot 231 corresponding to the card inserting block 232 can be inserted without glue. To achieve the purpose of bonding the inner layer 2 丨, and there will be no overlapping bonding sections after bonding to produce a more beautiful effect. The outer cladding layer 22 is a predetermined shape and flexible thin plate body, which has a central fold line 2 2 1 parallel to the length direction of the thin plate body, and is folded in half along the fold line 2 2 1 to be able to be attached to each other and cover the inner layer. One of the 21 inner plywood 222 is separated from an outer plywood 223, which is separated from the inner and outer plywoods 222 and 223 respectively and printed in accordance with the Consumer Cooperatives of the Central Standards Bureau of the Ministry of Internal Economics (please read the precautions on the back and fill in this purchase ) The first joint section 224 and the second joint section 225 protruding from one of the left and right joint ends 214 and 215 of the layer 21, and a third joint section protruding from the second joint section 22 5 adjacent to one end of the polyline 221 226, wherein the first joint section 224 has the same area as the first joint section 225. Furthermore, the outer cladding layer 22 further has parallel fold lines 221 and two parallel winding fold lines 2 2 0 located on the inner and outer plywood 222 and 223 adjacent to the side, each plywood 2 2 2, 2 2 3 The maximum distance between the two winding fold lines 2 2 0 is exactly the same as the maximum distance between the two sides 2 1 3 of the inner layer 2 'When the inner and outer plywood 222, 223 cover the inner layer 21 and fold along the fold line 221, the The winding fold lines 2 2 0 of the inner and outer plywood 222 and 223 of the outer covering layer 22 overlap, and the two sides 213 of the inner layer 21 also overlap with the winding fold line 220 in a straight line. At this time, the outer covering layer 22 is folded in half. The upper and lower sides can define two protruding winding layers 227 protruding from the inner layer 21 and the upper and lower sides 2 1 3 and are relatively symmetrical. Page 7 This paper size applies the Chinese National Standard (CNS) A4 specification (210 × 297 mm) 491796 A7 B7 V. Description of the invention (6) The top cover 12 can be covered above the surrounding wall 2 to prevent foreign matter from entering ' Or prevent items placed in the container from falling. After the splints 222 and 223 cover the inner layer 21, the left and right joint ends 214 and 215 of the inner layer 21 will protrude from the inner and outer splints 222 and 223 away from the first and second joint sections 224 and 225 of the vertical folding line 221 One end, and the two sides 213 of the inner layer 21 and the winding fold lines 220 of the inner and outer plywood 222, 223 are in a straight line overlapping state, at this time, the wall 2 will be bent and shaped and the card device 23 will be used to engage. To make the left and right joint ends 214 and 215 of the inner layer 21 abut, the first joint section 224 can be fixed on the inner base surface 211 of the inner layer 21 adjacent to the left joint end 214 by a gluing technique, and the second joint section 225 is cemented on the inner surface 21 adjacent to the right joint end 215 outside the base surface 212, and finally the third joint segment 2 2 6 is bent along the fold line 2 2 0 in the direction of the first joint segment 2 2 4 and fixed, that is, The manufacture of the surrounding wall 2 can be completed. Printed by the Consumer Cooperatives of the Central Standards Bureau of the Ministry of Economic Affairs (please read the precautions on the back before filling this page). Refer to the first and third figures. In order to achieve the joint between the bottom plate 11 and the surrounding wall 2 of the container 1 and the better Combining strength, first bend the winding layer 11 2 of the bottom plate 11 along the periphery of the plate body 111 to be vertical, and then continue to place the bottom plate 11 at the bottom end of the surrounding wall 2 to make the bending section 11 3 of the winding layer 11 2 of the bottom plate 11 3 The inner wall surface of the inner plywood 222 of the surrounding wall 2 is adhered, and the winding section 227 and the bending section 113 after shaping the lower end of the surrounding wall 2 are repeatedly folded in half by a winding machine until the bottom surface of the plate body 111 of the bottom plate 11 is covered. Among them, the winding section 227 located at the bottom end of the surrounding wall 2 is repeatedly folded at least twice, thereby achieving the purpose of consolidating the bottom plate 11 and the surrounding wall 2. For the same reason, the top of the surrounding wall 2 also uses the same technology. The winding section 227 is wound to shape it. After the winding sections 2 2 7 are folded several times, the thickness will be relatively increased. Therefore, the page size of this paper applies the Chinese National Standard (CNS) A4. (210X297 mm) 491796 Central Bureau of Standards, Ministry of Economic Affairs Consumer cooperative work five printed Α7 Β7 described (7) an overall strength of the invention increase the effectiveness of the container. Of course, 'the surrounding wall 2 of the present invention can also reserve only one winding section 227 combined with the bottom plate ii, and it is not necessary to reserve two winding sections 227 for winding processing'. When the surrounding wall 2 only reserves one roll When winding the segment 227, as long as the fold line 221 connecting the two plywood plates 222 and 223 abuts the side edge 213 above the inner layer 21 so that the central fold line 2 2 1 and the side edge 21 3 overlap in a straight line, then the winding technology can be used to The winding section 227 located below is wound and combined with the bottom plate 11. Referring to the fourth figure, in order to manufacture the container 1 shown in the first figure, the present invention includes the following processing steps: 1. Cutting and forming the inner layer 21 and the outer cladding layer 22: The inner layer 21 and The outer cladding layer 22 is cut into a predetermined size. Among them, the inner layer 21 can be directly cut with a thick cardboard, and the outer cladding layer 22 can be a wrapping paper printed with a pattern label. Second, cement the inner layer 21 and the outer cladding layer 22 ·· Fold the outer cladding layer 22 along a central fold line 2 2 1 to form an inner plywood 2 2 2 and an outer plywood 223 that can be attached to each other, And the inner and outer splints 222 and 223 are facing away from one end, respectively. A first joint section 224 and a second joint section 225 that can be engaged with each other are protruded, and a second joint section 225 extends outward from an end adjacent to the fold line 221 The third joint section 226, the plywood 222, 223 can be folded along the fold line 221 to cover and fix the inner layer 21, and when the inner and outer plywood 222, 223 cover the inner layer 21, the outer cover 22 layer has more Two protruding sides 2 1 3 of two protruding inner layers 2 1 and symmetrical winding sections 2 2 7. III. Deflection setting: The surrounding wall 2 formed after the pasting is curled and shaped by a predetermined molding mold. At this time, the two connecting ends of the inner layer 21 page 9 This paper applies the Chinese National Standard (CNS) A4 specification (210X 297 mm) IIII n batch III III order n line (please read the precautions on the back before filling this page) 491796 A7 B7___ V. Description of the invention (8) 214, 215 After the card inserting blocks 232 are respectively engaged with the corresponding card slots 231 to achieve abutment and consolidation, the first and second joint sections 224 and 225 of the outer covering layer 22 respectively protrude into the inner layer 21 adjacent to the connecting ends 214 and 215. Facing the inner and outer base surfaces 211 and 212. 4. Gluing butt jointing · The gluing technology will be applied to the surrounding wall 2 after shaping to make the first and second joint sections 224 and 2 2 5 of the outer cladding layer 22 respectively extend. Enter and glue on the inner and outer mating ends 214 and 215 of the inner layer 21 and reverse the inner and outer base surfaces 211 and 212. Finally, bend the third joint section 226 in the direction of the first joint section 224, and then glue and fix it on the first joint. The segment 224 faces away from the inner base surface of the inner layer 21. V. Coupling the bottom plate 11: Put the bottom plate 11 In the space formed by surrounding the wall 2 after gluing, the bending section 11 3 of the bottom plate 11 is wound around the inner wall surface of the surrounding wall 2 by bending the bending section 11 3. The folded section 11 3 is cut at the bottom end to align the inner layer 2 1 and the side 2 1 3 at the lower end, that is, the bottom plate 11 is slightly higher than the winding section 2 2 7 surrounding the bottom end of the wall 2. Wall 2 is wound up from the bottom winding section 2 2 7 upwards and folds in multiples, so that the winding layer around wall 2 and the bottom layer 11 are wound and fixed. Printed by the Consumer Cooperative of the Central Standards Bureau of the Ministry of Economic Affairs (please first Read the notes on the back side and fill in this page) 6. Wrap the top of the surrounding wall 2 and cover the top cover 12: Also use a windable machine to fold the winding sections 22 and 7 around the top of the wall 2 down and fold it several times. The shape of the top of the surrounding wall 2 can increase the strength of i around the top of the wall 2 and finally cover the top cover 12 to complete the container 1. As can be seen from the above description, this embodiment utilizes the two joint sections 224 and 225 protruding from the outer coating layer 22 These base surfaces 211, 212, which are attached to the inner layer 21, respectively. Page 10 This paper applies the Chinese National Standard (CNS) M specification (21〇χ). 297 公 楚) "-A7 B7 491796 5. In the description of the invention (9), the combined container 1 can be made more flat and beautiful, and through the innovation of the winding manufacturing technology, 'the glue is not required to join the bottom plate π, The strength of the container can also be increased. 'Therefore, the manufacturing method of the present invention can produce a beautiful and strong container 10. Referring to the fifth and sixth figures, this is another preferred embodiment of the container 1 of the present invention. The appearance of different geometric shapes is made according to the shape of the bottom plate u. Due to the geometric shapes that can be formed, there are many π t ^ ^ eight N ~. The following is only a description of the container 1 with a hexagonal appearance, but the container 1 The appearance is not limited to the disclosed hexagon. The container 1 has a hexagonal bottom plate 13, a top cover 14, and a hexagonal surrounding wall 3. The surrounding wall 3 is also composed of an inner layer 31 and an outer covering layer 32. The inner layer 31 It also has opposite inner and outer base surfaces 311, and two connecting ends 312, and the purpose of butting two connecting ends 31 2 can also be achieved by a snapping device 33. The outer covering layer 32 also has a central fold line 321, two plywood plates 3 2 2, first, second = two two 323, 324, and third joint section 325. σ The difference between this embodiment and the first embodiment is that the two plywoods 322 of the outer cladding layer 32 have a plurality of equidistant intervals and a vertical central fold line 32, and a dimple fold line 320. The inner layer 31 has a The first concave fold line 32, the second concave fold line 310 corresponding to the inside and the outside, when the inner layer 31 and the outer cladding layer 32 form a surrounding = 3, it is bent along each of the fold lines 310 and 320, and then the same as the first embodiment. The first joint section 323 and the second joint section 3'24 are respectively fixed to the right coffee ^ q inner layer 3 1 adjacent to the two joint ends 312 on the inner and outer base surfaces 311, and then the flute one, Le— * joint section 325 is bent in the direction of the first joint section 321 and cemented, and then the above-mentioned winding technology is used to combine the bottom plate 13 with the top of the surrounding wall 3, and the upper part of the wall 3 is placed on top. Page 11 & Zhang scales apply Chinese national standards ( CNS) A4 specification (210X297 mm) --------- install ------ order ------ line C, please read the notes on the back before filling this page) Central standard of the Ministry of Economy Bureau Consumer Consumption Cooperative Seal 491796 A7 ------ V. Description of Invention (10) A container 1 with a hexagonal appearance can be formed by the cover 14 '. (Please read the precautions on the back before filling this page.) With reference to the seventh figure, in order to manufacture the container 1 of the sixth figure, the processing steps of this embodiment are approximately the same as those of the first embodiment, which is only implemented in the first embodiment. For example, a step of forming a polyline is added between step 2 and step 3, wherein the processing method of the polyline is: using a predetermined mold to form a number on the surrounding wall 3 after the inner layer 31 and the outer cladding layer 32 are fixed, etc. Concave folds 310, 32 0 spaced from the vertical central fold line 32 丨. Then, steps 4, 5, and 6 of the manufacturing method of the first embodiment are repeated to complete the container 1 with a hexagonal appearance. To sum up, the two joint sections of the container of the present invention which are protruded by the outer coating layer can be respectively attached to the base surfaces of the inner layer, which can make the combined container more flat. Alas, not only glue is not needed to join the bottom plate, but also the strength of the container can be increased. Furthermore, the container of the present invention can also be made into a variety of geometric shapes to meet the needs of consumers, so it can indeed achieve the purpose of the invention. Printed by the Consumer Cooperatives of the Intellectual Property Bureau of the Ministry of Economic Affairs, but the above are only the two preferred embodiments of the present invention. When this cannot be used to limit the scope of the present invention, that is, the scope of the patent application and the invention specification according to the present invention The simple equivalent changes and modifications made by the content should still fall within the scope of the patent of the present invention. Page 12 This paper size applies the Chinese National Standard (CNS) A4 specification (210 X 297 mm) 491796 A7 B7 V. Description of the invention (η) [Comparison of component numbers] Printed by the Consumers Cooperative of the Central Standards Bureau of the Ministry of Economic Affairs 1 Container 224 First joint section 11 Base plate 225 Second joint section 111 Plate body 226 Second joint section 112 Winding layer 227 Winding section 113 Bending section 23 Snap-in device 12 Top cover 231 Slot 13 Base plate 232 Block 14 Top cover 3 Surrounding wall 2 Surrounding wall 31 Inner layer 21 Inner layer 310 Second concave folding line 2H Inner base surface 311 Base surface 212 Outer base surface 312 Joint end 213 Side edge 32 Outer coating layer 214 Left joint end 320 First concave fold line 215 Right joint end 321 Center fold line 22 Outer coating layer 322 Plywood 220 Winding fold line 323 First joint section 221 Central fold line 324 Second joint section 222 Inner clamp plate 325 Second joint section 223 Outer clamp plate 33 Snap-in device (please read the precautions on the back first) (Fill in this page) Page 13 National Standards (CNS) A4 size (210X07 mm)

Claims (1)

491796 A8 B8 C8 D8 經濟部智慧財產局員工消費合作社印製 、申請專利範圍 i· 一種紙製包裝容器,包含一 ^ δ 底板,及一沿底板周緣向 上突伸之圍燒壁,豆φ,# 該圍繞壁具有一内層及一外 包覆層,其特徵在於: “内3係由可撓曲之紙材所裁切而成,並具有 兩反向之内基面與外基面、位於該等基面上、下兩側 之相對立側邊,以及兩可相互對接之左、右銜接端; 而 該外包覆層,呈預定形狀且可撓曲之薄板體,其 具有一平行薄板體長度方向之摺線、沿摺線對折而可 相互貼合且包覆該内層之一内夾板與一外夾板,以及 分別自内、外夾板相背離之一端突伸而可相互接合之 第一與第二接合段,當内、外夾板包覆該内層後,該 外包覆層更具有兩突出内層之兩側邊且相對稱的捲繞 段; 當該等夾板包覆該内層後,該内層之左、右銜接 端會分別突出内、外夾板背離第一、二接合段之一端, 此時將其撓曲,該第一接合段即可黏固在内層左銜接 端之内基面上,而第二接合段則黏固在内層右銜接端 之外基面上,最後,利用捲繞機器將撓曲後之捲繞段 對折捲繞至内層之兩侧邊即可成型該圍繞壁。 2 ·依據申請序利範圍第1項所述'之紙製包裝容器,其 中,該外包覆層更具有一自第一接合段鄰近摺線之一 端突伸的第三接合段。 3.依據申請專利範圍第1項所述之紙製包裝容器更包含 第14頁 本紙張尺度適用中國國家標準(CNS)A4規格(210 X 297公爱) (請先閱讀背面之注意事項再填寫本頁) P 線· 491796 喔齊卽眘慧讨轰笱員工消費合作fi印製 A8 B8 C8 D8 六、申請專利範圍 一可覆蓋在圍繞壁上方之頂蓋。 4·依據申响專利範圍第1項所述之紙製包裝容器,其 中,該圍繞壁更具有-可接合該左、右銜接端之卡接 裝置,該卡接裝置具有至少一形成在兩銜接端其中之 一上的卡槽,以及至少1成在兩銜接端其中之另一 上,且可配合卡嵌入該卡槽的卡嵌塊。 • 5.依據申請專利範圍第1項所述之.紙製包裝容器,其 | 中,該内層之兩基面可藉由滾壓而形成内外起伏的波 浪狀。 6·依據申請專利範圍第1項所述之紙製包裝容器,其 - 中,該底板具有一自其周緣向下突伸而可立於地面之 捲繞層,該捲繞層具有一可與圍繞壁貼合之外環面。 7· —種紙製包裝容器之製造方法,該容器包含一底板, 及一沿底板周緣向上突伸之圍繞壁,直中 八^ 该底板是 具有一板體及一面積較板體為大之捲繞層,該圍繞壁 具有一内層及一外包覆層,而其製造方法包括: 、裁切成型:利用裁切技術將内層及外句 。復層裁切 成預定尺寸形狀; 、黏固内層及外包覆層:將外包覆層沿— 甲央摺線 對折,而形成一可相互貼合之内、外爽板,且 外夾板相背離之一端分別突伸一可相石 立筏合之第 一與第二接合段,該等夾板即可沿摺 伯深對折而黏 貼該内層; 、撓曲定型:將上述黏貼後所形成之圍繞辟、 — 心太以預定 第15頁 本紙張尺度適用中國國家標準(CNS)A4規格(210 X 297公釐) --------------褒--------訂---------線 (iff先閱讀背面之注意事項再填寫本頁) 491796 A8 B8 C8 D8 六、申請專利範圍 之成型模具使其捲曲定型,此時,内層之兩銜接 端相互抵接,外包覆層之第一、第二接合段分別 伸入内層銜接端反向之内、外基面; 四、 膠合對接:將定型後之圍繞壁以膠合技術,使外 包覆層之第一、第二接合段分別伸入而膠合在内 層銜接端反向之内、外基面上; 五、 捲繞接合底板··把底板放置在膠合後圍繞壁所形 成之空間内,使底板之捲繞層沿板體周緣向下彎 折貼合圍繞壁,再利用可捲繞機器將圍繞壁與捲 繞層由其底端捲繞對折,使圍繞壁與底板接合固 定。 8.依據申請專利範圍第7項所述之紙製包裝容器之製造 方法,更包含:一成型摺線的加工步驟,該加工步驟 介於黏固内層及外包覆層及撓曲定型之間。 ί -------------裝-------·—訂---------線 (請先閱讀背面之注意事項再填寫本頁) 經濟部智慧財產局員工消費合作社印製 第16頁 本紙張尺度適用中國國家標準(CNS)A4規格(210 X 297公釐)491796 A8 B8 C8 D8 Printed and patented by the Consumer Cooperative of the Intellectual Property Bureau of the Ministry of Economic Affairs i. A paper packaging container containing a ^ δ bottom plate and a surrounding burning wall protruding upward along the periphery of the bottom plate, beans φ, # 该The surrounding wall has an inner layer and an outer cladding layer, which are characterized by: "Inner 3 is cut from flexible paper and has two opposite inner and outer base surfaces. The opposite sides on the base surface, the lower sides, and the two left and right joint ends that can be docked with each other; and the outer cladding layer has a predetermined shape and a flexible thin plate body having a parallel thin plate body length A fold line in the direction, a double fold along the fold line, which can be fitted to each other and cover an inner plywood and an outer plywood of the inner layer, and a first and a second joint which protrude from one end of the inner and outer plywood facing away from each other and can be mutually joined. After the inner and outer plywood covers the inner layer, the outer cladding layer has two winding sections that protrude from both sides of the inner layer and are symmetrical; after the plywood covers the inner layer, the left and right sides of the inner layer The right joint ends will protrude from the inner and outer splints, respectively. From one end of the first and second joint sections, at this time, the first joint section can be fixed to the inner base surface of the left joint end of the inner layer, and the second joint section is fixed to the right joint end of the inner layer. On the outer base surface, finally, a winding machine is used to fold the deflected winding section in half to the two sides of the inner layer to form the surrounding wall. 2 · According to the first order of the scope of the application, The paper packaging container, wherein the outer covering layer further has a third bonding section protruding from one end of the first bonding section adjacent to one end of the fold line. 3. The paper packaging container according to item 1 of the patent application scope further includes Page 14 This paper size applies to China National Standard (CNS) A4 (210 X 297 public love) (Please read the precautions on the back before filling out this page) P-line · 491796 Oh, Qi Hui, Shen Hui, discuss employee cooperation fi printed A8 B8 C8 D8 6. The scope of patent application 1 can cover the top cover above the surrounding wall. 4. The paper packaging container according to item 1 of the scope of the patent application, wherein the surrounding wall has more- The card connecting device for engaging the left and right connecting ends, the card The device has at least one card slot formed on one of the two joint ends, and at least 10% of the card insert block on the other of the two joint ends, and can fit the card into the card slot. 5. According to the patent application The paper packaging container described in the first item of the scope, wherein | the two base surfaces of the inner layer can be rolled to form an undulating inner and outer wave shape by rolling. 6. The paper made according to the first patent application scope A packaging container, wherein the bottom plate has a winding layer protruding downward from its periphery and standing on the ground, and the winding layer has an outer torus which can be attached to the surrounding wall. 7 · —Paper A method for manufacturing a packaging container. The container includes a bottom plate and a surrounding wall protruding upward along the periphery of the bottom plate. The bottom plate is a coiled layer having a plate body and a larger area than the plate body. The wall has an inner layer and an outer cladding layer, and its manufacturing method includes: Cutting and forming: the inner layer and the outer sentence are cut by using cutting technology. The double layer is cut into a predetermined size and shape; and the inner and outer cladding layers are cemented: the outer cladding layer is folded in half along the central line of the center to form an inner and outer plate that can be fitted to each other, and the outer plywood faces away from each other. One end protrudes respectively from the first and second joint sections that can be erected by lithographic rafts, and the plywood can be folded in half along the folding depth to adhere the inner layer; and deflection setting: the surrounding formed by the pasting, Xin Tai is scheduled to page 15. This paper size applies the Chinese National Standard (CNS) A4 specification (210 X 297 mm) -------------------------- Order- -------- Thread (iff first read the precautions on the back and then fill out this page) 491796 A8 B8 C8 D8 VI. The patent application scope of the molding mold makes it curl and shape. At this time, the two connecting ends of the inner layer are against each other. The first and second joint sections of the outer cladding layer extend into the inner and outer base surfaces of the connecting ends of the inner layer, respectively. 4. Glue butt jointing: Glue the surrounding walls after shaping to make the outer cladding layer The first and second joint sections are respectively extended and glued on the inner and outer base surfaces of the inner layer connecting ends opposite; Winding and bonding the bottom plate ... Place the bottom plate in the space formed by the surrounding wall after gluing, so that the winding layer of the bottom plate is bent down along the peripheral edge of the board to fit the surrounding wall. The winding layer is folded in half from its bottom end, so that the surrounding wall and the bottom plate are joined and fixed. 8. The method for manufacturing a paper packaging container according to item 7 of the scope of the patent application, further comprising: a processing step of forming a polyline, the processing step being between the inner and outer layers of the adhesive and the shape setting of the flexure. ί ------------- install ------- · -order --------- line (please read the precautions on the back before filling this page) Ministry of Economy Printed by the Intellectual Property Bureau's Employee Cooperatives, page 16 This paper is sized for China National Standards (CNS) A4 (210 X 297 mm)
TW90120499A 2001-08-21 2001-08-21 Packaging container made of paper and method for producing the same TW491796B (en)