TW436361B - Welding guiding board - Google Patents

Welding guiding board Download PDF

Info

Publication number
TW436361B
TW436361B TW88112291A TW88112291A TW436361B TW 436361 B TW436361 B TW 436361B TW 88112291 A TW88112291 A TW 88112291A TW 88112291 A TW88112291 A TW 88112291A TW 436361 B TW436361 B TW 436361B
Authority
TW
Taiwan
Prior art keywords
welding
guide plate
solder
workpiece
guiding board
Prior art date
Application number
TW88112291A
Other languages
Chinese (zh)
Inventor
Jian-Chang Yang
Ming-Ren Chen
Original Assignee
Yang Jian Chang
Chen Ming Ren
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yang Jian Chang, Chen Ming Ren filed Critical Yang Jian Chang
Priority to TW88112291A priority Critical patent/TW436361B/en
Priority to JP23064199A priority patent/JP3251924B2/en
Application granted granted Critical
Publication of TW436361B publication Critical patent/TW436361B/en

Abstract

This invention relates to a welding guiding board, in which a declined clamping tank is provided at a lateral end of the welding guiding board, and a metallic rod is provided within the clamping tank. The welding guiding board is installed at the lateral end of a welding path of a workpiece. When filling solder to the first path, the solder is sealed at the bottom end of the welding path, while welding the metallic rod at the same time, such that the metallic rod may serve to stabilize and align the welding guiding board, thereby being sealed at the lateral end of the welding path during the whole processing of welding. Thus, the design of this invention allows the welding process to be proceeded much more easily, and can effectively enhance the quality of welding, so as to be adapted in the industry.

Description

436361 五、發明説明( 經濟部中央標準局貝工消费合作社印装 —本發明係-種谭接導焊板,尤指—種在焊龙驗衫 楫 ts~_ 計音 〇 按,焊接技術主要係利用高熱、高壓或兩者兼用,使 焊料可熱炫而填充於焊道之中,達到金屬連接之目的,又 ’焊料在填充於料的過程巾,在連接的金屬板之轉底 端—通會設置羞—片,使熱焊料存^在焊指中,不會由 縫隙/敗失[ 隹,g人速盈之金屬_板濃道iu組,在過去尚無導 =板之侧向封閉時,熱熔的焊料在焊道兩側亦會^ ·而待焊料固結後τ在成凹陷夕n現 I,為此,有心人士即設計出一種可將導焊板貼抵於焊道 側端之裝置,而可對於焊道側向形成封閉,使焊接品質得 以提昇。 配合參看第七圖所示,即為此一可侧向抵靠導焊板( 8 3 )之夹持器(8 〇 ),其係具有一磁鐵座(8丄), 且於磁鐵座(8 1 )上設置彈性片(8 2 ),而當兩工件 (84) ' (85)欲焊接時,則於焊道(841)底端 利用膠布貼設墊片,且將夾持器(8 〇 )之磁鐵座(8 i )吸附於工件(8 4 )側端,而可以II油( 8 2 ) 之^彈力-將〜導( 8 3 )央接而封Μ於惶i# (341) 傅端 一误Ut-熱熔焊料之恭备疼,焊料由(841) 兩側流失之。弊病,。 此一夾持器(8 0 )之設計,雖I將導焊板(8 3 ) 夾持抵靠於焊道(8 4 1 )兩側’然而,其實際使用上( 8 2 )卻定-易-通-為長_Η^·間使 本紙張尺度遑用中國國家標率(CNS ) A4規格(21〇 X 297公釐} (請先閲请背面之注意事項再填寫本頁) .裝' ,ιτ 旅 436361 A7 B7 五、發明説明( 用而造成-彈性疲乏’ ^ 玉 亚且,對於大 型板體之、工件焊接來說,其解焊料之填充,需經由數首 反覆程序,⑱料m固結加叫接H焊^ (8 3 )係以陶夸.粉卷中,笔:〜 抵靠,而與焊料並無篇.暴二激,著除了失持器78 〇二2 彈性片(8 2 )能提供側向抵壓力量以外,,'淳板-(83 以身與工件(8 4 )、( 8 5 )紐 止其因—iij,( 8 2 )的^力 不立,為此,該表持器_( 8 〇 )之使用,尚未完 備,而一般的工程中,則有直接_科馮( 8 3 )貼在工件(8 4 )側I者,惟,其爆接時,膠才遇熱身 谷_·^/產生起_1§: ’使位需要數次焊接填_料的_動作,可能在名 二女之-焊接^裎,導焊板即產生掉i,而必需反霜壯t, 使得業界深感困·擾。 有鑑於此,本發明者遂精心研究加以創新,其間,經 由不斷努力,終發j出一種,希能藉由本 發明之設計達到以下的創作目的。 經濟部中央梂準局貝工消资合作社印製 (請先閉讀背面之注意事項再填寫本頁) 本發明設計之..目的在於:m 一種戈接^^板. 一其传 於_導焊土姻篇真矣,且^^41~也設置金屬棒, ,導焊—板工#iliat端’ _而堂第一—道@料填充時, 堪於焊違底J,同時一併焊接金jj奉,佶得全屋棒 可對於導_浮板形成穩固定位作用,而在^煤接之全程作業中 ^LMH道」則*因此,本發明之設計,可讓焊接作更 進存-且能有效的提高焊接品質,而更適於產業界加 本紙張尺度適用中围國家揉準(CNS ) Α4祝格(2ι〇χ297公釐) 436361 C7 D7 五、創作说明(今) 以利用° 為使貴審查委員能進一步了解本發明設計之結構特 徵、組合方式及其他目的,茲附以圖式詳細說明如后: (一)圖式部份: 經濟部智^,^/4/-0=工;'/1骨合作社印% .-------裝 — -------訂 — ^-----線 (请先閒讀背面之注意事項V,寫本頁) 圖 圖 圖 月'體外觀示意圖。 係本發明設置於工件之焊道兩側的外觀示意圖。 係本發明設置於工件之焊道兩側的側視實施例示 意圖('一)。 係本發明設置於工件之焊道兩側的側視實施例示 意圖(二)。 係本發明之另一型態導焊板外觀示意圖。 係本發明又一型態導焊板之實施例圖。 第七圖:係習用設置於工件之焊道兩側的外觀示意圖。 (二)圖號部份: 第 第 第 第四圖 第五圖 第六圖 (10) 導焊板 (11) 夾槽 (13)卡合槽 (21)膠布 (3 0 )工件 (4 0 )工件 (6 0 )導焊板 (6 2 )金屬棒 (6 4)金屬棒 (71)夾槽 (12)金屬棒 (2 0 )墊片 (2 2)雙面膠帶 (3 0 1 )烊道 (5 〇 )焊料 (61)夾槽 (6 3 )夾槽 _( 7 0 )導焊板 (7 2 )金屬棒 本紙张尺度適用令國國家梂準(CNS ) A4規格(210X297公釐) 436361436361 V. Description of the invention (printed by the Central Bureau of Standards, Ministry of Economic Affairs, Shellfish Consumer Cooperatives—this is the department of the present invention—special welding plates, especially—specialized in welding inspection shirts. It uses high heat, high pressure, or both to make the solder dazzle and fill the bead to achieve the purpose of metal connection, and the solder is in the process of filling the material, at the bottom of the connected metal plate— The general meeting will set up a shame-sheet, so that the hot solder is stored in the welding fingers, and will not be lost by the gap / loss. When closed, the hot-melt solder will also be on both sides of the bead ^ and τ will appear in the depression after the solder is consolidated. To this end, those who are interested in designing a solder guide can be attached to the bead The device at the side end can form a side seal to the weld bead to improve the welding quality. As shown in Figure 7 for cooperation, this is a holder (which can abut against the welding guide plate (8 3) laterally) 8 〇), which is provided with a magnet base (8 丄), and an elastic sheet (8 2) is arranged on the magnet base (8 1), and when two workers (84) '(85) When welding is to be performed, a gasket is attached to the bottom of the bead (841) with adhesive tape, and the magnet holder (8i) of the holder (80) is adsorbed on the workpiece (84). Side end, but can be the ^ elasticity of II oil (8 2)-will be connected to the guide (8 3) and sealed in 惶 i # (341) Fu Duanyi mistake Ut-hot melt solder congratulations, solder by (841) Loss on both sides. Disadvantages. The design of this holder (80), although I will hold the welding plate (8 3) against the sides of the weld bead (8 4 1). However, In actual use (8 2), it is set to be -easy-pass-long. This paper uses the Chinese National Standards (CNS) A4 specification (21〇X 297 mm). (Please read it first. Note on the back, please fill out this page again.) Installation,, ττ 436361 A7 B7 V. Description of the invention (effect caused by use-elastic fatigue) ^ Yuya, and for large plate and workpiece welding, its solution of soldering Filling, it needs to go through several iterative procedures. The material m is consolidated and then called H welding ^ (8 3) is Tao Tao. In the powder roll, pen: ~ abut, and there is no article with solder. In addition to the displacer 78 02 02 elastic sheet (8 2) can provide lateral abutment pressure In addition, 'chunban- (83 with the body and the workpiece (8 4), (8 5) stops its cause—iij, (8 2) cannot stand. For this reason, the watch holder _ (8 〇 The use of) is not complete, and in general engineering, there are those who directly _ Ke Feng (8 3) affixed to the side of the workpiece (8 4), but when it bursts, the glue will meet the warm-up valley _ · ^ / Generated _1§: 'It takes several times to weld and fill the _ material. It may be in the second daughter-welding ^ 裎, the welding guide plate will produce i, and it must be anti-frost, which makes the industry deeply feel Sleepy and disturbing. In view of this, the present inventor has carefully studied and innovated. During this period, through continuous efforts, one will eventually be produced, hoping to achieve the following creative purposes through the design of the present invention. Printed by the Central Working Group of the Ministry of Economic Affairs, Beige Consumers Cooperatives (Please close the precautions on the back before filling out this page) The present invention is designed ... The purpose is: m a kind of connection ^^ board. The true meaning of Welding Marriage, and ^^ 41 ~ also set up metal rods. Welding guide-plate worker #iliat 端 '_ 而 堂 第一 — 道 @ 料 填 When filling, it is worth welding at the same time, and welding at the same time Jin jj Feng, won the whole house rod can form a stable fixed position for the guide _ floating board, and ^ LMH road in the entire operation of the coal connection ″ ”Therefore, the design of the present invention can make welding more advanced- And it can effectively improve the welding quality, and it is more suitable for the industry to increase the paper size. Applicable to the central countries (CNS) Α4 Zhuge (2ι〇χ297 mm) 436361 C7 D7 5. Creation instructions (today) to use ° In order to enable your review committee to further understand the structural features, combination methods and other purposes of the design of the present invention, the detailed description is attached as follows: (1) Schematic part: Ministry of Economic Affairs, ^, ^ / 4 / -0 = 工; '/ 1 Bone Cooperative Co., Ltd.%. -------- Installation -------- Order-^ ----- line (please read the precautions on the back first, write this page ) Figure Figure Figure Moon's appearance. It is a schematic diagram of the appearance of the present invention provided on both sides of a bead of a workpiece. The side view of the embodiment of the present invention is provided on both sides of the bead of the workpiece ('a). The side view of the embodiment of the present invention is provided on both sides of the bead of the workpiece. It is a schematic diagram of the appearance of another type of welding guide plate of the present invention. It is a diagram of an embodiment of another type of welding guide plate of the present invention. Figure 7: This is a schematic diagram of the appearance of the two sides of a weld bead that is commonly used. (2) Part No .: Figures No.4, No.5, No.6, No.6 (10) Welding plate (11), clamping groove (13), engaging groove (21), adhesive tape (3 0), work piece (4 0) Workpiece (6 0) Welding plate (6 2) Metal rod (6 4) Metal rod (71) Clamping slot (12) Metal rod (2 0) Gasket (2 2) Double-sided tape (3 0 1) (5) solder (61) clamping groove (6 3) clamping groove _ (7 0) solder guide plate (7 2) metal rod This paper is applicable to national standards (CNS) A4 specification (210X297 mm) 436361

創作説明( 7 3 )墊片 7 5 )工件 8 〇 )爽持器 8 2 )彈性片 8 4 )工件 (7 4 )膠布 (7 6 )工件 (請先閱讀背面之注意事項,/寫本頁} (8 1 )磁鐵座 C 8 3 )導焊板 ^ ( 8 5 )工件 訂 首先,請配合參看第一圖及第二圖所示,其分別為本 :月之導焊板(1〇)的外觀示意圖,及設置於工件(3 )、(4 0 )側端而封閉於焊道(3 〇丄)兩側之外觀 ,,其中’導焊板(1 〇 ) 一側設置傾斜的失槽(丄丄) 山爽槽(11)在導焊板(1〇)抵靠於工件(3〇)側 端時’正好對應於焊道(3 〇丄)位置,爽槽(工工)側 形成缺口,且於夾槽(11)中設置金屬棒(12)。 導焊板(1 0 )上對應於墊片(2〇)設置處設置卡 合槽(13),卡合槽(13)之端面形態與墊片(20 )端面相同,而可令墊片(2〇)可插入卡掣於卡合槽( 1 3 )中。 經濟部^!ί--ι··ΗΑ^9 丄·γί2^'合作社印製 其實際操作之使用上,墊片(2 0 )藉由膠布貼設於 工件(30) 、(40)之焊道(301)底端,而導焊 板(1 0)之卡合槽(1 3 )則可以套設於墊片(2 0 ) 側端加以夾持,而令夾槽(1 2 端’並且,在導焊板(10)上可典莫婪帶(2 2 ) ’使其可以黏結於工神-(3 0 )側端,而能增加_導」淳板( 1 0 )在遲_接„缸座^定4ϋ,如第三圖所示,而當焊道( 30 1)進行焊接時,第一次之熱熔焊料(50)的填充 本紙張尺度速用中國闺家梯準(CNS > Α4規格(210 X 297公釐) C7 D7 436361 五、創作説明(ς·) 、,即可以連同夹槽(i丄)中所設置的金屬榛( — 併熱熔,使得金屬棒(丄2 )下側融入焊料(5 〇 充於焊道(3 0 1)中,而將導焊板(1〇)谭接定= 工件(3 0)之焊道(3 〇 1 )側端。 此% ’即使墊片(2〇)底端的膠布(2 1 )遇熱脫 離’或墊片(2〇)因重力而向下掉落,在焊道 己底端已具有一道初步封閉之焊料(5〇),而能封閉在 谭道(3 0 1 )底端’並且,導焊板(工〇 )中的金屬棒 (1 2 )與焊料(5 0)的溶接,可讓導谭板(! 0)形 成-種側蚊位之卡f,因此,如第四圖所示,而在隨後 的烊料(5 0 )填充程序中,導焊板(工〇 )依然可也穩 固的封閉在¥道(3 Q 1 )兩·,而能有效的播止焊料( 5 0 ),避免其側向滲漏,直到焊接完畢後,導焊i (工 0)因金屬棒(12)完全熱您而充填於焊4 3 〇工) 中’使得導焊板(1 〇 ) GU可脫離輿合_ (1 1 )的未掣,而將導焊板(_工〇 )加私取」^ ’或者, 在焊接過程中,夾槽(1 1 )的缺口可隨著高熱的焊料( 5 0 )之重覆焊接而逐―漸破損,使得導焊板(i 〇 )於工 件(3 0 ) 、( 4 0 )之幕接完成時即自梓满^,完成^焊 接工作。 上與 _ L5.J1)孫·;热 束,而當工件(3 0 ) 、( 4 〇 )在_焊接過程中,高熱的 焊接溫度,可使兩者熱熔一起,而且,金屬棒(12)埋 設於爽槽(1 1 )—沖的長_度,係於導焊板(丄〇 )靠合後 ----裝---ii——訂 (請先閣讀背面之泣意事項^"本頁) I I 11- tfn . 部 y. Hi A ii x Ά ff Λ. ft 社 印 % 本紙张尺度通用 t ( CNS ) A4ii^- ( 2l"〇x 297^t~ C7 D7 436361 五、創作説明(厶) ’金屬2 )位身·焊道(3 0 1 )觝與逍备-度_以不超 過厚度馬丰.」一—並且,該金屬棒(12)的長 度’可依此原則而視工件(3 0 )板材的厚度予以規格化 設置,使其在焊接過程中,可隨同熱熔的焊料(5 〇 )完 全融入焊道(3 〇 1 )中,因此,本、創―作之設激,在焊接 工d完_成蓋,完全不-會_澎響爆it ( 3 0 1 )外熟.」—而具在 極佳的一致性。 再如第五圖所示,耳係本發明之另一型態導焊板(6 0 )結構’其係於導焊板(6 〇 )兩側設置斜向的夾槽( 6 1 ) 、(6 3 ),且夾槽(6 1 ) 、( 6 3 )中分別設 置金屬棒(62)'(64),而可於一側使用之後,再 將導焊板(6 0 )另側抵靠於焊道側-端―,而對於另一金屬 棒加以利用。 如第六圖所示,係本發明之又一型態導焊板(7 0 ) 結構,其係應用於平行焊〜接之工4牛(7 5 )、( 7 6 ), 而同樣在..導骂板(7 〇 )側端設詈类槽(7 1 ),.且於夾 槽.(7 1 )中設置金屬棒(7 2 ),而利用会屈樓(72 )束( 7 0 ) ,並且,工 件(75) 、(7 6)之焊道底端,亦可以利用膠布(7 4)黏貼塾片(7 3 ),而對於烊道進行焊擠作業。 因此,經由上述結構特徵及組合方^式之詳細說明,可 清兔看出本發明設計之特點在於: 提供一種,其 -由的_灰it ’夾槽,藉此設計.,而可在革 本紙張尺度適用中國國家標準(CNS ) Μ規格-- .---^-------^1;-----0 f靖先閱讀背面之注意事項 \寫本頁〕 j 經濟部智总!1ί減,/;ίπ:丄^货合作社印製 436361 C7 D7 五、創作説明(了) 斧件填^夺,使得焊料可里基,泰舍ϋΐΜ 態穩_—位1屢」,因此’本發明孓設.計 ,可讓龙接作業易於進行’上能.達真提真 ,而"妥適於產貴界加以科—用。 綜上所述,本發.日月『焊接導焊板』,.係..利用自態J去則 抜術思-德之高度創作,if合發明專^牛’爰依涂俱 又展出申請。 ------]--t------ΐτ—·-----^ < (請先閱讀背面之注意事項i /寫本頁) . 經濟部智u)HA^:Hx;/i'^合作社印焚 本紙張尺度適用中國國家標準(CNS ) A4規格(21〇X297公釐)Creation instructions (7 3) Gasket 7 5) Workpiece 8 〇) Holder 8 2) Elastic sheet 8 4) Workpiece (7 4) Tape (7 6) Workpiece (Please read the precautions on the back first, / write this page } (8 1) Magnet holder C 8 3) Welding plate ^ (8 5) Workpiece order First, please refer to the first and second pictures, which are: Welding plate of the month (1〇) Schematic diagram of the appearance, and the appearance of the workpiece (3), (40) side ends and closed on both sides of the weld bead (300 丄), where the 'lead plate (1 〇) side is provided with an inclined loss slot (丄 丄) When the welding slot (11) abuts on the side end of the workpiece (30), the slot (11) corresponds to the position of the bead (30 °), and the slot (worker) side is formed. A notch, and a metal rod (12) is arranged in the clamping groove (11). An engagement groove (13) is provided on the welding guide plate (10) corresponding to the place of the gasket (20). The end surface of the engagement groove (13) has the same shape as the end surface of the gasket (20), and the gasket (20) 2) The latch can be inserted into the engaging slot (1 3). Ministry of Economic Affairs ^! Ί--ι ·· ΗΑ ^ 9 丄 · γί2 ^ 'For the printing of the actual operation of the cooperative, the gasket (20) is attached to the workpiece (30) and (40) by adhesive tape. The bottom end of the channel (301), and the engaging groove (1 3) of the soldering plate (1 0) can be sleeved on the side end of the gasket (20) to be clamped, so that the clamping groove (1 2 end 'and On the soldering plate (10), the greed band (2 2) can be used to make it adhere to the side of God- (3 0), and it can increase the ”guide” Chun plate (1 0) in the late_connection „Cylinder seat 定 定 4ϋ, as shown in the third figure, and when the welding bead (30 1) is being welded, the first time the hot-melt solder (50) is filled in this paper is quickly used by Chinese girl ladder standards (CNS > Α4 size (210 X 297 mm) C7 D7 436361 V. Creation instructions (ς ·), that is, the metal hazel (— 热) set in the clamping slot (i 丄) can be melted together to make the metal rod (丄2) The lower side is filled with solder (50 filled in the bead (301), and the welding plate (10) Tan is set = the side end of the bead (301) of the workpiece (30). This % 'Even if the adhesive tape (2 1) at the bottom of the gasket (20) comes off with heat' or the gasket (2) Falling down by gravity, there is already a preliminary closed solder (50) at the bottom end of the welding bead, and it can be closed at the bottom end of Tan Dao (3 0 1). The dissolution of the metal rod (1 2) and the solder (50) can make the guide plate (! 0) form a card f of the species side, so as shown in the fourth figure, 50) In the filling procedure, the solder guide plate (work 0) can still be firmly enclosed in the ¥ channel (3 Q 1), and can effectively stop the solder (50) to avoid its lateral leakage, Until the welding is completed, the welding guide i (work 0) is filled in the welding 430 work because the metal rod (12) completely heats you so that the welding guide plate (1 〇) GU can be separated from the consensus_ (1 1) The soldering plate (_ 工 〇) is taken privately ^^ or in the welding process, the gap of the clamping groove (1 1) can be followed by the repeated welding of the hot solder (50) One by one-gradually broken, so that the welding guide plate (i 〇) is completed at the completion of the workpiece (3 0), (4 0), and completed the welding work. ^ L5.J1) Sun ·; Heat beam, and when the workpiece (30), (400) In the process, the high heat welding temperature can make the two hot-melt together, and the metal rod (12) is buried in the flute (1 1)-the length of the punch is tied to the welding guide plate (丄 〇). ---- Equipment --- ii——Order (please read the Weep on the back ^ " this page) II 11- tfn. Department y. Hi A ii x Ά ff Λ. Ft General dimensions t (CNS) A4ii ^-(2l " 〇x 297 ^ t ~ C7 D7 436361 V. Creation instructions (厶) 'Metal 2) niche · weld bead (3 0 1) 逍 and free preparation-degree_ to No more than the thickness of Ma Feng. ”—- Moreover, the length of the metal rod (12) can be standardized according to the thickness of the workpiece (30) according to this principle, so that during the welding process, it can be accompanied by hot melting. The solder (50) is completely integrated into the weld bead (301). Therefore, the original and creative design is stimulated when the welder d finishes _ forming a cover, not at all-will _ Pengxiang burst it (3 0 1 ) Outside cooked. "— And with excellent consistency. As shown in the fifth figure, the ear is a structure of another type of welding plate (60) of the present invention, which is provided with oblique clamping grooves (61) at both sides of the welding plate (60), ( 6 3), and metal rods (62) '(64) are respectively set in the clamping grooves (6 1) and (6 3), and can be used on one side, and then the other side of the welding guide plate (60) is abutted against On the bead side-end-while another metal rod is used. As shown in the sixth figure, the present invention is another type of welding plate (7 0) structure, which is used in parallel welding ~ 4G (7 5), (7 6), and the same. The side of the scolding board (70) is provided with a trough (7 1), and a metal rod (7 2) is arranged in the clamp groove (7 1), and the beam (72) is bent (70) ), And the bottom end of the welding bead of the workpieces (75) and (7 6), the adhesive sheet (7 3) can also be pasted with adhesive tape (7 4), and the welding can be performed on the bead. Therefore, through the detailed description of the above structural features and combination methods, it can be seen from the rabbit that the design feature of the present invention is: provide a kind of, which is designed by the _ gray it 'clip groove, and can be used in leather This paper size applies to China National Standard (CNS) M specifications-.--- ^ ------- ^ 1; ----- 0 f Jingxian first read the notes on the back \ write this page] j Economy General Minister of Ministry! 1ί minus ,; ίπ: printed by the goods cooperative, 436361 C7 D7 V. Creation instructions (a) Axe pieces are filled, making the solder creeky and Taishe ϋΐM stable _-bit 1 repeated. " Therefore, 'the present invention is designed and designed to make the dragon connection operation easy to perform', and it is true that "it is suitable for use in the industry and industry." To sum up, this issue. Sun and Moon "Welding Welding Guide Plate", Department .. Uses the self-state J to create a high degree of creative thinking and morality. Application. ------]-t ------ ΐτ— · ----- ^ < (Please read the precautions on the back i / write this page). Ministry of Economy u) HA ^: Hx; / i '^ The size of the paper printed by the cooperative is applicable to the Chinese National Standard (CNS) A4 (21 × 297 mm)

Claims (1)

AS B8 C8 D8 436361 六、申請專利範圍 ~ 1、·、一種焊接導焊板,其中,導焊板側端設置對應於 工件焊道之夾槽,夾槽侧形成缺口,且夾槽中設置金屬棒 〇 2 如申請專利範圍第1項所述之焊接導焊板,其中 ,導知板側端所設置的夾槽,可位於導焊板兩侧。 3 ·如申請專利範圍第1項所述之焊接導焊板,其中 ,導焊板上可設置卡合槽,使得焊接用之墊片可插設於卡 合槽中。 ---------装-------:.玎—------^ (诗先閲讀背面之注意事項再项寫本頁} 經濟部智慧財產局員工消費合作社印製 紙 本 10 率 梯 家 公 7 9 2AS B8 C8 D8 436361 Sixth, the scope of patent application ~ 1, ·, a welding guide plate, wherein the side of the welding guide plate is provided with a clamping groove corresponding to the workpiece bead, a gap is formed on the clamping groove side, and a metal is arranged in the clamping groove. Rod 02 The welding guide plate as described in item 1 of the scope of the patent application, wherein the clamping grooves provided at the side ends of the guide plate can be located on both sides of the guide plate. 3 · The welding guide plate according to item 1 of the scope of the patent application, wherein the welding guide plate can be provided with an engagement groove so that a welding gasket can be inserted into the engagement groove. --------- Equipment ------- :. 玎 -------- ^ (Read the notes on the back of the poem before writing this page again} Employee Consumer Cooperatives, Intellectual Property Bureau, Ministry of Economic Affairs Printed on paper 10 Leader 7 7 2
TW88112291A 1999-07-20 1999-07-20 Welding guiding board TW436361B (en)