A manufacturing method of foamed aluminum alloy composites comprises the following steps: a. 54~69 wt%, 50~100 #gm ore powder, 30~45 wt% inflammable resins and 1 wt% inflammable curing agent are mixed into a tank. b. Placed foamed alnminum alloy plate on the mixers and pressed under 10~50 Kg/cm2 for 1~2 hours. c. Cured and obtained foamed aluminum alloy composites.
TW084100085A1995-01-041995-01-04Manufacturing method of foamed aluminum alloy composites