TW326420B - Process for the preparation of re-usable bottles starting from modified PET - Google Patents

Process for the preparation of re-usable bottles starting from modified PET

Info

Publication number
TW326420B
TW326420B TW084104877A TW84104877A TW326420B TW 326420 B TW326420 B TW 326420B TW 084104877 A TW084104877 A TW 084104877A TW 84104877 A TW84104877 A TW 84104877A TW 326420 B TW326420 B TW 326420B
Authority
TW
Taiwan
Prior art keywords
acid
units
moles
hydroxy
preparation
Prior art date
Application number
TW084104877A
Other languages
Chinese (zh)
Inventor
Occhiello Ernesto
Po Riccardo
Original Assignee
Enichem Spa
Inca Internat S P A
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Enichem Spa, Inca Internat S P A filed Critical Enichem Spa
Application granted granted Critical
Publication of TW326420B publication Critical patent/TW326420B/en

Abstract

A process for the preparation of transparent re-usable bottles, which comprises molding by injection-blow molding copolymers containing units deriving from terephthalic acid and ethylene glycol to prepare an essentially tubular blank and characterized in that the copolymers contain from 0.1 - 10% in moles of units deriving from aromatic diacids different from terephthalic acid which are selected from isophthalic acid, 2,6-naphthalenedicarboxylic acid, 4,4^-biphenyldicarboxylic acid, 4,4^-diphenylmethyl oxide, and from 0.1 - 15% in moles of units deriving from aromatic hydroxy-acids which are selected from p-hydroxy-benzoic acid, salicylic acid, 6-hydroxy-2-naphthoic acid, making reference to the units deriving from terephthalic acid, and the copolymers contain 0.1~5% in moles of 1,2-dioxethylene units, making reference to the units of ethylene glycol; in which the blank being maintained at temperatures from 100 to 120℃ during blow-molding can be mechanically elongated and assembled.
TW084104877A 1994-05-27 1995-05-17 Process for the preparation of re-usable bottles starting from modified PET TW326420B (en)

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
IT9401087 1994-05-27

Publications (1)

Publication Number Publication Date
TW326420B true TW326420B (en) 1998-02-11

Family

ID=58262244

Family Applications (1)

Application Number Title Priority Date Filing Date
TW084104877A TW326420B (en) 1994-05-27 1995-05-17 Process for the preparation of re-usable bottles starting from modified PET

Country Status (1)

Country Link
TW (1) TW326420B (en)

Similar Documents

Publication Publication Date Title
EP0684269A3 (en) Process for the preparation of re-usable bottles starting from modified PET.
CA2190274A1 (en) Process for producing polyethylene terephthalate
WO1999061505A3 (en) Process to prepare a polyester resin
BR0115430A (en) Polyester composition, process for forming a thermostable container and thermostable container
TW227025B (en)
TW200700496A (en) Polyester compositions containing cyclobutanediol and articles made therefrom
ZA971415B (en) Process for preparing copolyesters of terephthalic acid, ethylene glycol, and 1,4-cyclohexanedimethanol exhibiting a neutral hue, high clarity and increased brightness.
MY146045A (en) Polyester compositions containing cyclobutanediol having a certain combination of inherent viscosity and moderate glass transition temperature and articles made therefrom
BR9913787A (en) Liquid crystalline polyester, molding composition and molded article
KR950018138A (en) Polyester manufacturing method
DE69104280D1 (en) Process for the production of high-purity isophthalic acid.
FR2622197B1 (en) TRANSPARENT POLYAMIDES, THEIR MANUFACTURING PROCESS
HK1000063A1 (en) Process for preparing blow molded articles
ES2059108T3 (en) COPOLIESTERS AND ARTICLES OF MOLDING BY BLOWING AND EXTRUSION FROM THESE COPOLIESTERS.
TW422768B (en) Polyethylene-2,6-naphthalene dicarboxylate resin and preform and bottle molded thereof
TW326420B (en) Process for the preparation of re-usable bottles starting from modified PET
EP0899285A3 (en) A copolyester for molding a bottle
AR006022A1 (en) PROCESS TO PRODUCE MOLDED ITEMS.
IT1285525B1 (en) PERFECTED PROCESS FOR THE DIMENSIONAL STABILIZATION OF POLYETHYLENTEREPHTHALATE PRODUCTS
UST954005I4 (en) Process for preparing containers using branched polyesters
EP0640638A3 (en) Low pilling and flame-retardant material modified polyesters, process for their preparation and moulded articles therefrom.
AU778140B2 (en) Recovery of dicarboxylic aromatic acids from polyester-resin contained in articles for recycling
UST954004I4 (en) Process for preparing containers using polyesters
DE69308758D1 (en) Process for the preparation of 2,6-naphthalene dicarboxylic acid
JPS5726632A (en) Purifying method of glycol