TW288074B - Method for producing biaxially oriented polypropylene pearl synthetic paper on which printing ink dries quickly - Google Patents
Method for producing biaxially oriented polypropylene pearl synthetic paper on which printing ink dries quicklyInfo
- Publication number
- TW288074B TW288074B TW85100270A TW85100270A TW288074B TW 288074 B TW288074 B TW 288074B TW 85100270 A TW85100270 A TW 85100270A TW 85100270 A TW85100270 A TW 85100270A TW 288074 B TW288074 B TW 288074B
- Authority
- TW
- Taiwan
- Prior art keywords
- synthetic paper
- sheet
- polypropylene
- printing ink
- agent
- Prior art date
Abstract
A method for producing biaxially extended polypropylene pearl synthetic paper on which printing ink dries quickly, characterized in that a polypropylene resin composition comprising 90-40 wt.% of a high crystallinity polypropylene resin (melt flow index,=2-6) havinga isotacticity greater than 97%, 10-40 wt.% of calcium carbonate composite particles, 0-15 wt.% of titanium dioxide compositeparticles, and 0-5 wt.% of anti-electrostatic agent, and a resin composition comprising 96-99 wt.% of polypropylene and 4-1 wt.% of anti-adhesion agent are extruded separately from a main extruder and two auxiliary extruders (both set at 200-280 deg.C) through one single T-die to give coated sheet of a three-layered structure, the sheet is then cooled by a cooling roller at 15-60 deg.C, longitudinally extended 3-6 times by preheating at 120-150 deg.C, extending and annealing, transversely extended 5-12 times by preheating at 150-190 deg.C, extending and annealing, corona treated under a high frequency wave of 20-150kW, and then winded-up to obtain a coated sheet of thickness under 100(muon)m, and the sheet is then coated with a paper surface treating agent comprising 5-25 wt.% of chlorinated polypropylene resin, 0-10 wt.% of acrylic resin, 15-10 wt.% of calcium carbonate, 5% of white clay, 2-10 wt.% of titanium dioxide, 73-36 wt.% toluene, 0-2 wt.% of anti-electrostatic agent, and 0-2 wt.% ultraviolet light absorber and winded up to give synthetic paper of thickness below 100(muon)m.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW85100270A TW288074B (en) | 1996-01-11 | 1996-01-11 | Method for producing biaxially oriented polypropylene pearl synthetic paper on which printing ink dries quickly |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
TW85100270A TW288074B (en) | 1996-01-11 | 1996-01-11 | Method for producing biaxially oriented polypropylene pearl synthetic paper on which printing ink dries quickly |
Publications (1)
Publication Number | Publication Date |
---|---|
TW288074B true TW288074B (en) | 1996-10-11 |
Family
ID=51398074
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW85100270A TW288074B (en) | 1996-01-11 | 1996-01-11 | Method for producing biaxially oriented polypropylene pearl synthetic paper on which printing ink dries quickly |
Country Status (1)
Country | Link |
---|---|
TW (1) | TW288074B (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0888866A1 (en) * | 1997-07-01 | 1999-01-07 | Nan Ya Plastics Corporation | A process for the production of a biaxially oriented polypropylene synthetic paper of high gloss and easy drying printability |
TWI487822B (en) * | 2012-01-19 | 2015-06-11 | Nanya Plastics Corp | Printing fast - drying environment - friendly biaxially - stretched polypropylene synthetic paper |
-
1996
- 1996-01-11 TW TW85100270A patent/TW288074B/en not_active IP Right Cessation
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
EP0888866A1 (en) * | 1997-07-01 | 1999-01-07 | Nan Ya Plastics Corporation | A process for the production of a biaxially oriented polypropylene synthetic paper of high gloss and easy drying printability |
TWI487822B (en) * | 2012-01-19 | 2015-06-11 | Nanya Plastics Corp | Printing fast - drying environment - friendly biaxially - stretched polypropylene synthetic paper |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US5552011A (en) | Process of 3-layer co-extruded biaxial oriented polypropylene (BOPP) synthetic paper | |
EP0979722B1 (en) | Low temperature heat shrinkable film for labels | |
CA1280867C (en) | Non-blocking film | |
AU679471B2 (en) | Polymeric films | |
KR100304330B1 (en) | Synthetic paper with excellent multi-layered printing characteristics | |
CN1058028C (en) | White resin film with excellent printability | |
US6001290A (en) | Process for the production of a biaxially oriented polypropylene synthetic paper of high gloss and easy-drying printability | |
EP0703071B1 (en) | Composite plastics film or sheet | |
EP1118452A1 (en) | A process for producing a three layers co-extrusion biaxially oriented polypropylene synthetic paper of thickness 25-250 My m | |
EP0651004B1 (en) | Biaxially oriented polyolefinfilm, process for its preparation and use | |
AU2001267417B2 (en) | Transparent, biaxially orientated polyolefinic film with improved bonding properties | |
US20060257628A1 (en) | Watermarked polymeric sheet | |
EP1097805A1 (en) | Stretched film of thermoplastic resin | |
AU663538B2 (en) | In-mould labels | |
EP0862991B1 (en) | Polymeric films | |
US6136439A (en) | Monolayer polymeric film and method of fabrication | |
US6368543B1 (en) | Process using single screw extruder for producing a three layer co-extrusion biaxially oriented polypropylene synthetic paper of thickness 25˜250 μm | |
EP2998096B1 (en) | Formulation and method for making voided plastic film | |
JP3264771B2 (en) | Opaque laminated resin film with excellent printability | |
TW288074B (en) | Method for producing biaxially oriented polypropylene pearl synthetic paper on which printing ink dries quickly | |
US6703447B2 (en) | High bi-directional strength monolayer polymeric film and method of fabrication | |
US7041243B2 (en) | 5-layer co-extruded biaxial-oriented polypropylene synthetic paper and its production process | |
CN106671529A (en) | Biaxially stretched polypropylene touch film | |
US6332940B1 (en) | Process for producing an invisible and writable biaxially oriented polypropylene (BOPP) raw processing film and the product thereof | |
US20030089450A1 (en) | Manufacturing method for improving the yield and production rate of biaxial-oriented polypropylene pearly synthetic paper |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
MK4A | Expiration of patent term of an invention patent |