Prior art keywords
treatment
forging
finished product
processing
cold forging
Prior art date
Application number
TW99139849A
Other languages
Chinese (zh)
Inventor
Chun-Fang Lin
Original Assignee
Kuen Tong Ind Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kuen Tong Ind Co Ltd filed Critical Kuen Tong Ind Co Ltd
Priority to TW99139849A priority Critical patent/TW201221246A/en
Publication of TW201221246A publication Critical patent/TW201221246A/en

Links

Landscapes

  • Forging (AREA)

Abstract

This invention provides a manufacturing method for bicycle free wheel, in which a lower cost aluminum material is treated with hot forging to make the relative stresses of each tooth of the free wheel more uniform. Then, it is treated with an annealing treatment to lower the hardness. After that, a press punching is carried out to remove the central circular area of the aluminum material so as to preserve the annular area of the aluminum material. The annular area is treated with a surface treatment for forming a protection layer on the surface, followed by a cold forging treatment, a heat treatment, a cold forging treatment and a heat treatment in sequence to form a semi-finished products, which is then machined to form a finished product with increased precision. This manufacturing method enables this invention to make a bicycle free wheel with lower cost, more uniform strength, higher wearing resistance, and having modular common-usage to lower the cost of inventory and having more uniform side tension.

Description

201221246 六、發明說明: 【發明所屬之技術領域】 本發明係與自行車齒盤有關,尤指藉由不同加工 處理方式,製造出有成本較低、強度均勻化,且呈 模組化之共用性,以降低庫存量之成本與提昇產^ 磨度,及具有均勻化側拉力之自行車齒盤之製程方201221246 VI. Description of the Invention: [Technical Field of the Invention] The present invention relates to a bicycle chainring, in particular, a method of manufacturing a lower cost, uniform intensity, and modularity by different processing methods. To reduce the cost of inventory and improve the production and grinding degree, and the process of bicycle sprocket with uniform side tension

【先前技術】 傳統製造自行車齒盤之製程方法為,以成本較高 之鋁圓棒經擠壓處理、壓延板材、CNC加工處理等^ 個處理步驟方式形成,由於該方式以_棒先經該擠 壓處理,形成1矩型狀,該扁矩型狀半成品的長轴 與短軸之應力不同,使加工後之成品,存有具有不同 強度’某區段輪齒之強度小於另某區段輪齒之強度。 ^且上述方式為自行車齒盤一次處理二侧面,及在 半成品處料需將外表形狀一次處理到纟,無法模組 化方式處理,相對增加庫存量之成本。 以鋁粉之粉末冶金方式所形成自行車之齒盤由 於自行車在變化車速時,鏈條會在齒盤上向上或向下 移動’而對齒盤上之輪齒產生—側拉力,易使輪齒向 側邊崩潰。 上述傳統自行車齒盤之製程方法,其原料成本較 而,且輪齒之強度不均勻,且無法模組化之共用性, 及輪齒側拉力及耐磨不佳之缺失。 201221246 本發明人有鑑於此,即本著創作之精神,乃思及 不同之技術方法創作而有改進現今缺失之本發明本 創作,進而提出申請。 【發明内容】 本發明之主要發明目的在於:利用原料成本較低 之鋁塊直接鍛造與加工形成,可使輪齒之強度均勻 1匕1且具有模組化之共用性,以降低庫存量之成本與 提昇產品耐磨度,及具有輪齒均勻化側拉力。 、 為達上述目的,本發明提供一冑自行車齒盤之製程 方法,如下: 先將成本較低之較小的鋁塊材料經由一熱鍛處 理,使在自行車齒盤之每個齒相對應力較為均句化, 經一退火處理,使硬度降低,再經一沖壓下料,將一 :間f形區域再予該沖壓下料去除,保留-環狀區 二,再將該環狀區域給予—表面處理,使表面形成一 層保護層,與經一冷鍛處理、一 . 热慝理、一冷鍛處理、 :熱處理,形成一雛形之半成品,最後才予一成品加 工’以對成品提高精密度值。 【實施方式】 所預步!解本發明之構造、運用之技術手段即 兹舉數個較佳實施例並配合圖示 月:下,相信本發明目的、特徵及其他特點, 田了由此而得深入且具體之瞭解。 201221246 敬請參閱第一圖至第二圖,本發明 齒盤之製程方法,係包括: .'、、種自仃車 -熱鍛處理(1 〇 ):先將紹塊 熱鍛處理(10),以中心向外擴散方式沖壓= 之,(12),該熱鍛處理 上)可利用成本較低之較小的鋁塊材料以節省成 本,且經該熱鍛處理(1〇)該粗达( 較為均勻,以德製# ψ + + β J之應Λ 以後製“之成品同樣應 ==盤(51)之每一輪齒(…相對應 …句句及均句化側拉力與提昇產品财磨度。 一退火處理(20):、經由該熱 經該退火處理(2〇),使該 (= 程成品硬度降低。 、丄Ζ )之袈 一沖壓下料(3 〇 ):將兮$ +奋 該粗枉(12)之製程ΛΓ Γ (20)後 :『該沖壓下料(30)去除,保留一環狀區域(3 一表面處理(4 〇 ):將該沖壓 之該環狀區域(3 2 )仏予,下科(3 0 )後 -層保護層。)…表面處理’使表面形成 =料理(50):將該表面處理(4〇)後 成出數齒形,如該自行車齒盤(51)之該輪 齒(5 2),具有模型定型之效果。 熱處理(6 0 ):將該冷鍛處理(5 〇 )後之 201221246 製程成印以固溶處理後直接自然時效方式處理。 一冷鍛處理(7 〇 ):將該熱處理(6 〇 )後之 製程成品經該冷鍛處理(7 〇 ),具有整形加工之效 果。 一熱處理(8 0 ):將該冷鍛處理(7 〇 )後之 製程成品,固溶處理後以人工時效方式處理。 一成品加工(9 〇 ):以CNC加工對該熱處理(8 ◦)後製程成品之一侧做尺寸精確值加工,以提 密度值。 11 π 利用上述加工方式,將一成本較低之該鋁塊(工 1 )經由上述之各項加工處理,形成一自行車齒盤(5 1 ),由於為將該鋁塊(i i )直接加工形成,其原 料成本較上述傳統以壓延板材加工為低。 八 且本發明將该鋁塊(1 1 )以該熱鍛處理(1 〇 ) 方式處理,可使在該自行車齒盤(51)之該輪齒(5 2)相對應力較為均勻化以及均勻化側拉力與提昇產 品耐磨度,不會如上述傳統以擠壓處理方式,、存有某 區段輪齒之強度小於另某區段輪齒之強度,以及不會 如上述傳統以粉末冶金方式,該輪 化,不懼怕鍵條在齒盤上向上或向下移5動=; 力’該輪齒(5 2 )不易側邊崩潰。 以及本發明在經該熱鍛處理(1 〇 )、該退火 處理(2 0 )與該沖壓下料(3 〇 )及該表面處理(4 〇 )之前製程加工後形成一個半成品,再依不同規 格、尺寸再予後續製程加工,因此且具有模組化之共 201221246 用性,以降低庫存量之成本。 綜上所述,本發明誠符合專利法之規定,爰依法 提出申請,盼早日准予專利。 【圖式簡單說明】 第一圖:本發明之過程示意圖。 第一圖.本發明之流程圖。 【主要元件符號說明】 • ( 1 0 )熱鍛處理 (12)粗述 (2 0 )退火處理 (3 0 )沖壓下料 (3 2 )環狀區域 (4 0 )表面處理 (5 0 )冷鍛處理 (5 1 )自行車齒盤 • ( 6 0 )熱處理 (7 0 )冷鍛處理 (8 0 )熱處理 (9 0 )成品加工 (1 1 )鋁塊 (3 1 )中間圓形區域 (5 2 )輪齒[Prior Art] The conventional manufacturing method of the bicycle toothed disc is formed by a high-cost aluminum round bar by extrusion processing, calendering of the sheet, CNC processing, etc., because the method is Extrusion treatment, forming a rectangular shape, the long-axis and short-axis stress of the flat-shaped semi-finished product are different, so that the processed product has different strengths, and the strength of a certain section of the tooth is smaller than another section. The strength of the teeth. ^ The above method is that the bicycle sprocket handles the two sides at a time, and the semi-finished material needs to be processed once to the enamel, which cannot be processed in a modular manner, and the cost of the inventory is relatively increased. The toothed disc of the bicycle formed by the powder metallurgy method of aluminum powder, because the bicycle changes the speed of the vehicle, the chain will move up or down on the toothed disc', and the side teeth of the tooth on the toothed disc generate a side pulling force, which makes the tooth tooth direction easy. The side crashes. The above-mentioned conventional bicycle toothed disc manufacturing method has the advantages of relatively low raw material cost, unevenness of the teeth, and the inability to modularize, and the lack of the side friction and wear resistance. 201221246 The present inventors have in view of this, that is, in the spirit of creation, thinking of different technical methods, and improving the present invention which is lacking in the present invention, and then applying. SUMMARY OF THE INVENTION The main object of the present invention is to directly forge and process aluminum blocks with low raw material cost, so that the strength of the teeth can be uniform 1 匕 1 and have modularity to reduce inventory. Cost and improve product wear resistance, and have uniform tooth side tension. In order to achieve the above object, the present invention provides a method for manufacturing a bicycle chainring, as follows: First, a relatively low cost aluminum block material is subjected to a hot forging process to make the relative stress of each tooth of the bicycle toothed disc relatively Uniformly, after an annealing treatment, the hardness is reduced, and then a stamping and blanking is performed, and the f-shaped region is further removed by the punching, and the ring-shaped region is retained, and then the annular region is given. The surface treatment forms a protective layer on the surface, and is subjected to a cold forging treatment, a heat treatment, a cold forging treatment, a heat treatment, forming a semi-finished product, and finally processing a finished product to improve the precision of the finished product. value. [Embodiment] Pre-step! The technical means for the construction and operation of the present invention will be described with reference to a few preferred embodiments and in conjunction with the drawings. It is believed that the objects, features and other features of the present invention are believed to be intensive and specific. 201221246 Please refer to the first to second figures. The method for manufacturing the toothed disc of the present invention includes: ',, the type of self-boring - hot forging treatment (1 〇): first hot-forging processing (10) Pressing the center outward diffusion method, (12), the hot forging treatment can use a lower cost aluminum block material to save cost, and the hot forging treatment (1〇) (More uniform, with the German system # ψ + + β J should be 以后 以后 以后 以后 “ “ 以后 以后 之 之 之 之 成品 成品 成品 成品 成品 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 51 Abrasiveness: An annealing treatment (20): through the heat treatment (2〇), the (= finished product hardness is reduced. 丄Ζ) 袈 a stamping blank (3 〇): will be 兮$ + 奋 ough (12) process ΛΓ 20 (20) after: "The stamping blank (30) is removed, retaining an annular area (3 a surface treatment (4 〇): the annular area of the stamping (3 2 ) 仏 ,, the lower part (3 0 ) after the layer protective layer.) ... surface treatment 'to make the surface formation = cooking (50): the surface treatment (4 〇) into a number of teeth, such as Self The gear teeth (52) of the toothed disc (51) have the effect of model setting. Heat treatment (60): The 201221246 process after the cold forging treatment (5 〇) is printed to form a solid solution after solid solution treatment. Method of treatment: A cold forging treatment (7 〇): After the heat treatment (6 〇), the finished product is subjected to the cold forging treatment (7 〇), which has the effect of shaping processing. A heat treatment (80): the cold forging After the treatment (7 〇), the finished product is treated by artificial aging after solution treatment. A finished product processing (9 〇): CNC machining is used to process the precision of one side of the finished product after the heat treatment (8 ◦). To increase the density value. 11 π Using the above processing method, a lower cost aluminum block (work 1) is processed through the above various processes to form a bicycle chain plate (5 1 ), since the aluminum block is Ii) Direct processing, the raw material cost is lower than that of the above-mentioned conventional calendering sheet processing. 8. The aluminum block (1 1 ) of the present invention is treated by the hot forging (1 〇) method, and the bicycle chainring can be used. (51) The teeth (52) are relatively uniform in relative stress and Homogenizing the side tension and improving the wear resistance of the product, it is not the same as the above-mentioned conventional extrusion treatment, the strength of a certain section of the teeth is less than the strength of the other section of the teeth, and the powder is not as conventional Metallurgical method, the round, not afraid of the key bar moving up or down on the toothed disc 5 movement =; force 'the tooth (5 2) is not easy to side collapse. And the invention is subjected to the hot forging treatment (1 〇 ), the annealing treatment (20) and the stamping blanking (3 〇) and the surface treatment (4 〇) are processed to form a semi-finished product, and then processed according to different specifications and sizes, and thus have a mold Grouped a total of 201221246 usability to reduce the cost of inventory. In summary, the present invention is in line with the provisions of the Patent Law, and is filed in accordance with the law, and is expected to grant patents as soon as possible. BRIEF DESCRIPTION OF THE DRAWINGS First FIG.: A schematic diagram of the process of the present invention. First Figure. Flow chart of the present invention. [Main component symbol description] • (1 0) hot forging treatment (12) rough description (20) annealing treatment (3 0) stamping blanking (3 2) annular region (40) surface treatment (50) cold Forging treatment (5 1 ) bicycle chainring • ( 6 0 ) heat treatment (7 0 ) cold forging treatment (80) heat treatment (90) finished product processing (1 1) aluminum block (3 1) intermediate circular area (5 2 ) teeth

Claims (1)

201221246 七、申請專利範圍: , 一種自行車齒盤之製程方法,其主要製程如下: 一熱鍛處理··將鋁塊材料經由該熱鍛處理,以 心向外擴散方式沖壓、鍛造,形成-圓形形狀之粗 坯,且經該熱鍛處理粗坯之應力較為均勻化; 理火處理:經由該熱鍛處理後再經該退火處 理,使该粗坯之製程成品硬度降低,· 冲I下料·將該退火處理後該粗坯之製程成品 區=間圓形區域再予該沖壓下料去除,保留一環= 今裘:Π處理··將該沖壓下料後之該環狀區域給予 5亥表面處理,使表面形成一層保護層. ::锻處理··將該表面處理後之製程成 冷锻處理,使該援此P 卫/上、, 、、土 0¾ 型之效果; 出數齒形,具有模型定 -熱處理:將該冷鍛處理後之 處理後直接自然時效方式處理; 成叩以固浴 一冷鍛處理:將該熱處理後 處理,具有整形加工之效果;h成品經該冷锻 一熱處理:,將該冷鍛處理後 處理後以人工時效方式處理; l私成叩,固溶 一成品加工:以CN(:加工 之一側做尺寸精確值加工,以提:二处理後製程成品 人杈阿精密度值。201221246 VII. Patent application scope: The manufacturing method of bicycle toothed disc, the main process of which is as follows: 1. Hot forging treatment · The aluminum block material is punched and forged by the hot forging process, and formed into a circle a rough shape of the shape, and the stress of the rough forging by the hot forging is relatively uniform; the fire treatment: after the hot forging treatment and then the annealing treatment, the hardness of the finished product of the blank is reduced, and After the annealing treatment, the finished product area of the rough blank = the circular area is further removed by the punching blank, and a ring is reserved = 裘: Π treatment · The annular area after the punching is given to 5 The surface treatment of the surface of the sea forms a protective layer on the surface. :: Forging treatment · The surface treatment process is cold forging, so that the effect of this type of P/W, /, and soil type 03⁄4 is obtained; Shape, with model setting-heat treatment: directly after the cold forging treatment, natural aging treatment; forming a solid bath with a cold forging treatment: the heat treatment after treatment, with the effect of shaping processing; h finished product through the cold Forging A heat treatment: after the cold forging treatment and after the artificial aging treatment; l private sputum, solid solution processing of a finished product: with CN (: processing one side to do the exact value processing, to mention: two processing after the process The finished product is a precision value.
TW99139849A 2010-11-18 2010-11-18 Manufacturing method for bicycle chain ring TW201221246A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
TW99139849A TW201221246A (en) 2010-11-18 2010-11-18 Manufacturing method for bicycle chain ring

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
TW99139849A TW201221246A (en) 2010-11-18 2010-11-18 Manufacturing method for bicycle chain ring

Publications (1)

Publication Number Publication Date
TW201221246A true TW201221246A (en) 2012-06-01

Family

ID=46724846

Family Applications (1)

Application Number Title Priority Date Filing Date
TW99139849A TW201221246A (en) 2010-11-18 2010-11-18 Manufacturing method for bicycle chain ring

Country Status (1)

Country Link
TW (1) TW201221246A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108971906A (en) * 2018-08-30 2018-12-11 天成车料(深圳)有限公司 A kind of production method and motor cabinet of electric bicycle motor seat

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN108971906A (en) * 2018-08-30 2018-12-11 天成车料(深圳)有限公司 A kind of production method and motor cabinet of electric bicycle motor seat

Similar Documents

Publication Publication Date Title
WO2015188546A1 (en) Method for manufacturing aluminium alloy wheel hub
CN105108457B (en) The processing method of overall driven disc
CN104646975B (en) Wheel rim speed reducer gear ring and manufacturing method thereof
RU2016104070A (en) METHODS FOR PRODUCING FORGED PRODUCTS AND OTHER PROCESSED PRODUCTS
CN104874626B (en) A kind of radial direction reverse Compound Extrusion shaping magnesium alloy heavy burden wheel disc technique and device
CN106734465B (en) Method based on the hot press-formed production automobile B-column of multilayer common metal composite plate
CN107186450A (en) Automobile CVT automatic transmission planet carrier board manufacturing process
CN102441773A (en) Hot precision forging and cold precision shaping compound process for spiral bevel gear
CN103464991A (en) Gear ring machining process
CN102989986A (en) Forging technology of large TC4 alloy drum forged piece
CN108188659A (en) A kind of manufacturing process of steel billet
CN105710620A (en) Manufacturing process for conjunction-tooth gear of car transmission
WO2015188547A1 (en) Method for manufacturing al-mg alloy wheel hub
CN103264265A (en) Extrusion forming process for brake wheel
CN103157758A (en) Precision forging plastic forming process for inner gear ring in planetary reducer
CN104191181A (en) Magnesium alloy wheel forging-spinning composite forming method
KR20150088688A (en) Method of manufacturing gear with double teeth patterns involving forging and two stage cold extrusion process
WO2015188543A1 (en) Method for manufacturing high-magnesium aluminum alloy commercial wheel hub
CN104476145A (en) Gasket manufacturing method
CN209773348U (en) hot forging device
CA2566548A1 (en) Method for manufacturing wrench handle with pressed indentation section
US20150196980A1 (en) Method of manufacturing gear with teeth involving forging
CN105215641B (en) The forging processing method of locking bolt
CN104015012A (en) Manufacturing method of Al-Mg-Si alloy hub
CN106346205A (en) Production method of motorcycle starting rod