TW200621944A - Luminous material and method for preparing the same - Google Patents
Luminous material and method for preparing the sameInfo
- Publication number
- TW200621944A TW200621944A TW094126991A TW94126991A TW200621944A TW 200621944 A TW200621944 A TW 200621944A TW 094126991 A TW094126991 A TW 094126991A TW 94126991 A TW94126991 A TW 94126991A TW 200621944 A TW200621944 A TW 200621944A
- Authority
- TW
- Taiwan
- Prior art keywords
- luminous material
- discontinuation
- exhibited
- photo
- irradiation
- Prior art date
Abstract
The present invention relates to an europium-activated alkaline earth metal aluminate luminous material. The europium-activated alkaline earth metal aluminate luminous material is characterized in that the afterglow brightness thereof (Y 23 DEG C and 120 min) exhibited 120 min after photo-irradiation discontinuation at 23 DEG C is at least 0.007 Cd/m<SP>2</SP>, and that the temperature dependence (TD) of afterglow brightness expressed by the ratio of afterglow brightness thereof (Y 80 DEG C) exhibited 10 min after photo-irradiation discontinuation at 80 DEG C to afterglow brightness thereof (Y 23 DEG C) exhibited 10 min after photo-irradiation discontinuation at 23 DEG C, Y 80 DEG C/Y 23 DEG C, is at least 1. This luminous material realizes prolonged afterglow and further exhibits thermoluminescence over a wide temperature range even without the use of an expensive rare earth element, such as dysprosium, as a co-activator. Thus the material can be used over a wide temperature range and the environment for use of the material is almost unlimited.
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2004233649 | 2004-08-10 | ||
JP2004310378 | 2004-10-26 |
Publications (1)
Publication Number | Publication Date |
---|---|
TW200621944A true TW200621944A (en) | 2006-07-01 |
Family
ID=35839336
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
TW094126991A TW200621944A (en) | 2004-08-10 | 2005-08-09 | Luminous material and method for preparing the same |
Country Status (2)
Country | Link |
---|---|
TW (1) | TW200621944A (en) |
WO (1) | WO2006016567A1 (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
TWI712672B (en) * | 2020-01-21 | 2020-12-11 | 國立臺灣大學 | Long afterglow material and preparation method thereof |
Families Citing this family (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2014198758A (en) * | 2013-03-29 | 2014-10-23 | 堺化学工業株式会社 | Stress luminescent material, application of the same, and method for producing stress luminescent material |
JP6135249B2 (en) * | 2013-03-29 | 2017-05-31 | 堺化学工業株式会社 | Raw material composition for stress luminescent material, stress luminescent material, and application thereof |
CN105209572B (en) * | 2013-03-29 | 2018-06-19 | 堺化学工业株式会社 | The manufacturing method of stress light emitting material and its application, stress light emitting material feedstock composition and stress light emitting material |
EP3088488B1 (en) * | 2014-03-11 | 2017-08-23 | Nemoto Lumi-materials Company, Limited | Phosphorescent phosphor |
-
2005
- 2005-08-09 WO PCT/JP2005/014548 patent/WO2006016567A1/en active Application Filing
- 2005-08-09 TW TW094126991A patent/TW200621944A/en unknown
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
TWI712672B (en) * | 2020-01-21 | 2020-12-11 | 國立臺灣大學 | Long afterglow material and preparation method thereof |
Also Published As
Publication number | Publication date |
---|---|
WO2006016567A1 (en) | 2006-02-16 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
TW200730605A (en) | Fluorescence material and manufacture thereof and luminaire | |
WO2010018999A8 (en) | Method for producing a β-sialon phosphor | |
TW200621944A (en) | Luminous material and method for preparing the same | |
CA2572399A1 (en) | Cement compositions comprising high aspect ratio materials and methods of use in subterranean formations | |
EP1861884A4 (en) | Metal silicate-silica-based polymorphous phosphors and lighting devices | |
EP1522534A3 (en) | Aluminate coating for a silicon containing substrate | |
ATE313611T1 (en) | PHOTOLUMINESCENCE PIGMENT MADE OF ALKALINE EARTH ALUMINATE SILICATE ACTIVATED BY RARE EARTH ELEMENTS | |
ATE515552T1 (en) | WATERPROOF MATERIAL COACTIVATED BY MULTIPLE RARE EARTH METALS WITH LONG AFTERGLOW | |
TW200621943A (en) | Barium thioaluminate phosphor materials with novel crystal structures | |
TW200702425A (en) | Phosphor | |
EP1726630A4 (en) | Aluminate phosphor and process for producing the same | |
EP1696224A8 (en) | Standard for referencing luminescence signals | |
AU2003269623A1 (en) | Silicon oxynitride passivated rare earth activated thioaluminate phosphors for electroluminescent displays | |
TW200708190A (en) | Compound, phosphor composition and light-emitting device containing the same | |
TW200514748A (en) | Aluminum hydroxide, aluminum hydroxide slurry and resin composition containing the same, and method for producing the same | |
TW200708595A (en) | Phosphor particle, phosphor paste and light-emitting device | |
TW200704753A (en) | Fluorophor for electron beam excitation light emitting devices | |
EP1215261A3 (en) | Method of producing aluminate phosphor | |
ATE338802T1 (en) | EUROPIUM-DOPED GALLIUM-INDIUM OXIDES AS RED-EMITTING, ELECTROLUMINescent PHOSPHORUS MATERIALS | |
TW200502361A (en) | Ultraviolet excited light-emitting device | |
US20070210282A1 (en) | Phosphorescent compounds | |
AU2003218840A1 (en) | Oxygen substituted barium thioaluminate phosphor materials | |
WO2010016740A3 (en) | Red phosphor and forming method thereof for use in solid state lighting | |
DE60206912D1 (en) | Magnesium kalzium thioaluminate phosphor | |
JP2006306644A (en) | Porous fluorescent ceramic |