TH3553B - Mixture maintains the boiling point of dichloropentafluoropropane and trans-1,2-dichlorethylene with methanol or ethanol. Or isopropanol - Google Patents

Mixture maintains the boiling point of dichloropentafluoropropane and trans-1,2-dichlorethylene with methanol or ethanol. Or isopropanol

Info

Publication number
TH3553B
TH3553B TH9101000231A TH9101000231A TH3553B TH 3553 B TH3553 B TH 3553B TH 9101000231 A TH9101000231 A TH 9101000231A TH 9101000231 A TH9101000231 A TH 9101000231A TH 3553 B TH3553 B TH 3553B
Authority
TH
Thailand
Prior art keywords
weight
approximately
mixture
percent
boiling point
Prior art date
Application number
TH9101000231A
Other languages
Thai (th)
Other versions
TH9512A (en
Inventor
นาซาราลี เมอร์แซนท์ นายอาบิด
Original Assignee
นายโรจน์วิทย์ เปเรร่า
นายโรจน์วิทย์ เปเรร่า นายธเนศ เปเรร่า
นายธเนศ เปเรร่า
Filing date
Publication date
Application filed by นายโรจน์วิทย์ เปเรร่า, นายโรจน์วิทย์ เปเรร่า นายธเนศ เปเรร่า, นายธเนศ เปเรร่า filed Critical นายโรจน์วิทย์ เปเรร่า
Publication of TH9512A publication Critical patent/TH9512A/en
Publication of TH3553B publication Critical patent/TH3553B/en

Abstract

มีการจัดหาวิธีและเครื่องสำหรับการผลิตเทอร์โมพลาสติกเรซินโฟมแบบเชื่อมขวางซึงจัดแจงดังต่อไป อัดรีดสารผสมเรซินซึ่งอย่างน้อยที่สุดมีเทอร์โมพลาสติกเรซิน สารทำให้เป็นโฟมและสารทำให้เกิดการเชื่อมขวางให้เข้าไปในตายที่ปิด ซึ่ง อย่างน้อยที่สุดรวมถึงบริเวณที่อัดแบบบริเวณที่ทำให้ร้อนและบริเวณที่ทำให้เย็น ซึ่งจัดแจงอย่างต่อเนื่องตามชื่อที่ลำดับไว้ อัดแบบสารผสมเรซินให้ได้รูปร่างตามที่ต้องการใน บริเวณที่อัดแบบของดายและแล้วทำให้ร้อนในบริเวณที่ทำให้ร้อนเพื่อให้สารทำให้เกิดการเชื่อมขวางสลายตัวและอย่างน้อยที่สุดให้ส่วนหนึ่งของสารทำให้เป็นโฟมสลายตัวด้วยเพื่อให้ผลิตเซลล์นิวเคลียส ดังนั้น เกิดผลิตภัณฑ์โฟมบางส่วนในบริเวณที่ทำให้เย็นของตาย ทำผลิตภัณฑ์โฟมบางส่วนให้เย็นถึงอุณหภูมิที่ต่ำกว่าจุดอ่อนตัวของผลิตภัณฑ์เพื่อเพิ่มสภาพแข็งเกร็งและได้รับการอัดรีดไปที่ด้านนอกของดาย ขณะที่ได้รับแรงหน่วงขณะที่เคลื่อนที่ในบริเวณที่ทำให้เย็นทำผลิตภัณฑ์โฟมบางส่วนซึ่งอัดรีดแล้วจากดายให้ร้อนภายใต้ความดันปกติเพื่อให้สารทำให้เป็นโฟมขยายตัวเต็มที่ซึ่งได้ผลิต ภัณฑ์สุดท้าย Methods and machines for the production of crosslinked thermoplastic resin foam are provided as follows. Extrusion resin mixtures, which at least contain thermoplastic resins. Foaming agents and crosslinking agents are allowed to enter the enclosed die, which at least includes the compression, heating and cooling zones. which are arranged continuously according to their respective names. Compress the resin mixture to the desired shape in The extruded area of the die and then heated in the heating area to cause the crosslinking agent to decompose and at least part of the foaming agent to decompose to produce nuclei. Thus, a thin foam product is formed. in the cold area of the dead Some foam products are cooled to temperatures below their softening point to increase their rigidity and are extruded to the outside of the die. While subjected to dampening while moving in the cooling area, some extruded foam products from the die are heated under normal pressure so that the foaming agent fully expands to produce the final product.

Claims (6)

1. สารผสมคงจุดเดือดที่ประกอบด้วยส่วนที่จำเป็น: (a) ไดคลอโรเพนทาฟลูออโรโทรเพนที่ประกอบด้วยส่วนที่จำเป็นของของผสมของ 1,1-ไดคลอโร -2,2,3,3,3-เพนทาฟลูโรโพรเพนจาก50 ถึง 75 เปอร์เซ็นต์โดยน้ำหนัก และ 1,3-ไดคลอโร-1,1,2,2,3- เพนทาฟลูออโรโพรเทนจากประมาณ 25 ถึง 50เปอร์เซ็นต์โดยน้ำหนักนั้นจากประมาณ 47-57 เปอร์เซ็นต์โดยน้ำหนัก,แทรนส์-1,2-ไดคลอ-โรเอธิลีน ประมาณ 38-48เปอร์เซ็นต์โดยน้ำหนัก และเมธานอลจาก 3-9 เปอร์เซ็นต์โดยน้ำหนัก ซึ่งสารผสมนั้นมีจุดเดือดประมาณ 43.7 องศาเซลเซียลเมื่อปรับความตันให้ถือว่าเท่ากับความดันบรรยากาศ หรือ (b) ไดคลอโรเพนทาฟลูออโรโทรเพนที่ประกอบด้วยส่วนที่จำเป็นของของผสมของ 1,1-ไดคลอโร -2,2,3,3,3-เพนทาฟลูโรโพรเพนจาก50 ถึง 75 เปอร์เซ็นต์โดยน้ำหนัก และ 1,3-ไดคลอโร-1,1,2,2,3- เพนทาฟลูออโรโพรเทนจากประมาณ 25 ถึง 50เปอร์เซ็นต์โดยน้ำหนักนั้นจากประมาณ 47-57 เปอร์เซ็นต์โดยน้ำหนัก,แทรนส์-1,2-ไดคลอ-โรเอธิลีน ประมาณ 40-50เปอร์เซ็นต์โดยน้ำหนัก และเอธานอลประมาณ 1-5 เปอร์เซ็นต์โดยน้ำหนัก ซึ่งสารผสมนั้นมีจุดเดือดประมาณ 46.5 องศาเซลเ ซียล เมื่อปรับความตันให้ถือว่าเท่ากับความดันบรรยากาศหรือ (c) ไดคลอโรเพนทาฟลูออโรโทรเพนที่ประกอบด้วยส่วนที่จำเป็นของของผสมของ 1,1-ไดคลอโร -2,2,3,3,3-เพนทาฟลูโรโพรเพนจาก50 ถึง 75 เปอร์เซ็นต์โดยน้ำหนัก และ 1,3-ไดคลอโร-1,1,2,2,3- เพนทาฟลูออโรโพรเทนจากประมาณ 25 ถึง 50เปอร์เซ็นต์โดยน้ำหนักนั้นจากประมาณ 49-59 เปอร์เซ็นต์โดยน้ำหนัก,แทรนส์-1,2-ไดคลอ-โรเอธิลีน ประมาณ41-51เปอร์เซ็นต์โดยน้ำหนัก และไอโซโพรทานอล ประมาณ 0.1ถึง 1.0 เปอร์เซ็นต์โดยน้ำหนัก ซึ่งสารผสมนั้นมีจุดเดือดประมาณ 47.7 องศาเซลเซียล เมื่อปรับความดันให้เท่ากับความดันบรรยากาศ 2. สารผสมคงจุดเดือดตามข้อถือสิทธิข้อ 1, ซึ่งประกอบด้วยส่วนจำเป็นของของผสมของไดคลอโรเพนทาฟลูออโรโพรเพน ประมาณ47-57 เปอร์เซ็นต์โดยน้ำหนัก, แทรนส์-1,2- ไดคลอโรเอนธิลีนประมาณ 38-48 เปอร์เซ็นต์โดยน้ำหนัก และเอธานอลประมาณ 3-9เปอร์เซ็นต์โดยน้ำหนัก 3. สารผสมคงจุดเดือดตามข้อถือสิทธิข้อ 1, ซึ่งประกอบด้วยส่วนจำเป็นของของผสมของไดคลอโรเพนทาฟลูออโรโพรเพน ประมาณ47-57 เปอร์เซ็นต์โดยน้ำหนัก, แทรนส์-1,2- ไดคลอโรเอนธิลีนประมาณ 40-50 เปอร์เซ็นต์โดยน้ำหนัก และเอธานอลประมาณ 1-5เปอร์เซ็นต์โดยน้ำหนัก 4. สารผสมคงจุดเดือดตามข้อถือสิทธิข้อ 1, ซึ่งประกอบด้วยส่วนจำเป็นของของผสมของไดคลอโรเพนทาฟลูออโรโพรเพน ประมาณ49-59 เปอร์เซ็นต์โดยน้ำหนัก, แทรนส์-1,2- ไดคลอโรเอนธิลีนประมาณ 41-51เปอร์เซ็นต์โดยน้ำหนัก และไอโซโพรทานอล ประมาณ0.1 ถึง 1.0 เปอร์เซ็นต์โดยน้ำหนัก 5. สารผสมคงจุดเดือดตามข้อถือสิทธิข้อ 1, ซึ่งประกอบด้วยส่วนจำเป็นของของผสมของไดคลอโรเพนทาฟลูออโรโพรเพน ประมาณ51.6 เปอร์เซ็นต์โดยน้ำหนัก, แทรนส์-1,2- ไดคลอโรเอนธิลีนประมาณ 42.6 เปอร์เซ็นต์โดยน้ำหนัก และเอธานอลประมาณ 5.8เปอร์เซ็นต์โดยน้ำหนัก 6. สารผสมคงจุดเดือดตามข้อถือสิทธิข้อ 1, ซึ่งประกอบด้วยส่วนจำเป็นของของผสมของไดคลอโรเพนทาฟลูออโรโพรเพน ประมาณ51.7 เปอร์เซ็นต์โดยน้ำหนัก, แทรนส์-1,2- ไดคลอโรเอนธิลีนประมาณ 45.3 เปอร์เซ็นต์โดยน้ำหนัก และเอธานอลประมาณ 3.0เปอร์เซ็นต์โดยน้ำหนัก 7. สารผสมคงจุดเดือดตามข้อถือสิทธิข้อ 1, ซึ่งประกอบด้วยส่วนจำเป็นของของผสมของไดคลอโรเพนทาฟลูออโรโพรเพน ประมาณ53.9 เปอร์เซ็นต์โดยน้ำหนัก, แทรนส์-1,2- ไดคลอโรเอนธิลีนประมาณเปอร์เซ็นต์โดยน้ำหนัก และไอโซโพรทานอล ประมาณ 0.5เปอร์เซ็นต์โดยน้ำหนัก 8. กรรมวิธีสำหรับทำความสะอาดพื้นผิวของของแข็งซึ่งประกอบด้วยการกระทำกับพื้นผิวดังกล่าวด้วยสารผสมคงจุดเดือดตามข้อถือสิทธิข้อ 1 9. กรรมวิธีตามข้อถือสิทธิข้อ 8 ซึ่งพื้นผิวของของแข็งนั้น คือ แผงวงจรที่พิมพ์ไว้ซึ่งปนเปื้อนด้วยฟลักซ์และกากฟลักซ์ 1 0. กรรมวิธีตามข้อถือสิทธิข้อ 9 ซึ่งพื้นผิวของของแข็งนั้น คือ โลหะ 11. Boiling point stabilizer containing the necessary parts: (a) dichloropentafluorotropane containing the necessary part of a mixture of 1,1-dichloro-2,2,3. , 3,3-pentafluoropane from 50 to 75 percent by weight and 1,3-dichloro-1,1,2,2,3-pentafluoropropane. Ten from about 25 to 50 percent by weight, then from approximately 47-57 percent by weight, about 38-48 percent of trans-1,2-dichlor-dichlorethylene by weight. And methanol from 3-9 percent by weight Where the mixture has a boiling point of approximately 43.7 degrees celsius, when toning is assumed to be equal to atmospheric pressure or (b) dichloropentafluorotropane containing the necessary part of the mixture of 1, 1- dichloro-2,2,3,3,3-pentafluopropane from 50 to 75% by weight and 1,3-dichloro -1,1,2,2, 3-pentafluoroprotein from approximately 25 to 50% by weight, then from approximately 47-57% by weight, about 40- trans -1,2-dichlor-roethylene. 50 percent by weight And about 1-5 percent of ethanol by weight Where the mixture has a boiling point of approximately 46.5 ° C, when toning is assumed to be equal to atmospheric pressure or (c) dichloropentafluorotropane containing the necessary part of the mixture of 1. , 1- dichloro-2,2,3,3,3-pentafluopropane from 50 to 75% by weight and 1,3-dichloro-1,2,3,2,2. , 3-pentafluoroprotane from approximately 25 to 50% by weight, from approximately 49-59% by weight, Trans-1,2-dichlor-dichlorethylene. Approximately 41-51 percent by weight And isoprotanol, approximately 0.1 to 1.0 percent by weight. The mixture had a boiling point of approximately 47.7 degrees celsius when the pressure was adjusted to the atmospheric pressure. 2. The mixture maintained the boiling point according to claim 1, which contained the necessary part of the dichloropentaflu mixture. Oropropane is approximately 47-57% by weight, Trans-1,2-dichlorethylene is approximately 38-48% by weight. And ethanol approximately 3-9% by weight 3. Mixture maintains boiling point according to claim 1, which contains the necessary components of a mixture of approximately 47-57% by weight dichloropentafluoropane. Rhennes-1,2-dichloroethane, approximately 40-50% by weight. And ethanol approximately 1-5% by weight 4. Mixture maintains boiling point according to claim 1, which contains the essential part of the dichloropentafluoropropane mixtures approximately 49-59% by wt. Rhenes-1,2-dichloroethane approx. 41-51 percent by weight And isopotanol approximately 0.1 to 1.0 percent by weight. 5. Mixture maintains boiling point according to claim 1, which contains the necessary components of the dichloropentafluoropane mixture. Approximately 51.6 percent by weight, Trans -1,2-dichlorethylene approximately 42.6 percent by weight. And ethanol approximately 5.8 percent by weight 6. Mixture maintains boiling point according to claim 1, which consists of approximately 51.7 percent by weight of the dichloropentafluoropropane mixture, trans-1. , 2-dichloroethane, approximately 45.3 percent by weight And ethanol approximately 3.0 percent by weight 7. Mixture maintains boiling point according to claim 1, which consists of approximately 53.9 percent by weight of the dichloropentafluoropropane mixture, trans-1. , 2-dichlorethylene, approximately percentage by weight And isopotanol approximately 0.5% by weight. 8. Process for surface cleaning of solids, which consists of action on such surfaces with boiling point stabilizers according to claim No. 1 9. Process according to claim. Clause 8 where the surface of a solid is a printed circuit board contaminated with flux and flux residue 1 0. Treatment according to claim 9 where the surface of the solid is metal 1. 1. สารผสมคงจุดเดือดที่ประกอบด้วยส่วนจำเป็นของ : (a) ไดคลอโรเพนทาฟลูออโรโทรเพนที่ประกอบด้วยส่วนที่จำเป็นของของผสมของ 1,1-ไดคลอโร -2,2,3,3,3-เพนทาฟลูโรโพรเพนจาก50 ถึง 75 เปอร์เซ็นต์โดยน้ำหนัก และ 1,3-ไดคลอโร-1,1,2,2,3- เพนทาฟลูออโรโพรเทนจากประมาณ 25 ถึง 50เปอร์เซ็นต์โดยน้ำหนักนั้น ประมาณ 49-54 เปอร์เซ็นต์โดยน้ำหนัก,แทรนส์-1,2-ไดคลอ-โรเอธิลีน ประมาณ 40-45 เปอร์เซ็นต์โดยน้ำหนัก และเมธานอลประมาณ 4-7 เปอร์เซ็นต์โดยน้ำหนัก,ซึ่งสารผสมนั้นมีจุดเดือดประมาณ 43.7 องศาเซลเซียล ซึ่งได้ ปรับความดันให้เท่ากับความดันบรรยากาศ (b) ไดคลอโรเพนทาฟลูออโรโทรเพนที่ประกอบด้วยส่วนที่จำเป็นของของผสมของ 1,1-ไดคลอโร -2,2,3,3,3-เพนทาฟลูโรโพรเพนจาก50 ถึง 75 เปอร์เซ็นต์โดยน้ำหนัก และ 1,3-ไดคลอโร-1,1,2,2,3- เพนทาฟลูออโรโพรเทนจากประมาณ 25 ถึง 50เปอร์เซ็นต์โดยน้ำหนักนั้น ประมาณ 49-54 เปอร์เซ็นต์โดยน้ำหนัก,แทรนส์-1,2-ไดคลอ-โรเอธิลีน ประมาณ 42-47 เปอร์เซ็นต์โดยน้ำหนัก และเอธานอลประมาณ 2-4 เปอร์เซ็นต์โดยน้ำหนัก,ซึ่งสารผสมนั้นมีจุดเดือดประมาณ 46.5 องศาเซลเซียล ซึ่งได้ ปรับความดันให้เท่ากับความดันบรรยากาศ (c) ไดคลอโรเพนทาฟลูออโรโทรเพนที่ประกอบด้วยส่วนที่จำเป็นของของผสมของ 1,1-ไดคลอโร -2,2,3,3,3-เพนทาฟลูโรโพรเพนจาก50 ถึง 75 เปอร์เซ็นต์โดยน้ำหนัก และ 1,3-ไดคลอโร-1,1,2,2,3- เพนทาฟลูออโรโพรเทนจากประมาณ 25 ถึง 50เปอร์เซ็นต์โดยน้ำหนักนั้น ประมาณ 51-56 เปอร์เซ็นต์โดยน้ำหนัก,แทรนส์-1,2-ไดคลอ-โรเอธิลีน ประมาณ 43-48 เปอร์เซ็นต์โดยน้ำหนัก และไอโซโพรทานอล ประมาณ 0.3-0.7 เปอร์เซ็นต์โดยน้ำหนัก ซึ่งสารผสมนั้นมีจุดเดือดประมาณ 47.7 องศาเซลเซียลเมื่อปรับความดันให้เท่ากับความดันบรรยากาศ 11. Boiling point stabilizer containing the essential parts of: (a) dichloropentafluorotropane containing the necessary part of a mixture of 1,1-dichloro-2,2,3. , 3,3-pentafluoropane from 50 to 75 percent by weight and 1,3-dichloro-1,1,2,2,3-pentafluoropropane. Tane from about 25 to 50% by weight is approximately 49-54% by weight, Trans -1,2-dichlor-dichlorethylene is approximately 40-45% by weight. And methanol by 4-7% by weight, which the mixture has a boiling point of about 43.7 Celsius which is adjusted to the pressure equal to the atmospheric pressure (b) dichloropentafluorotrophae. Containing the required fraction of the mixture of 1,1-dichloro-2,2,3,3,3-pentafluopropane from 50 to 75% by weight and 1,3- Dichloro-1,1,2,2,3-pentafluoroprotein from approximately 25 to 50% by weight approximately 49-54% by weight, Trans -1,2- Dichlor-Roethylene is approximately 42-47% by weight. And about 2-4 percent ethanol by weight, where the mixture has a boiling point of approximately 46.5 degrees celsius, which has been adjusted to equal atmospheric pressure (c) dichloropentafluorotro. The pen contains the necessary part of the mixture of 1,1-dichloro-2,2,3,3,3-pentafluopropane from 50 to 75% by weight and 1,3. - dichloro-1,1,2,2,3-pentafluoroprotein from approximately 25 to 50% by weight approximately 51-56% by weight, Trans -1,2. - Dichlor-Roethylene approximately 43-48 percent by weight. And isoprotanol approximately 0.3-0.7 percent by weight. The mixture has a boiling point of approximately 47.7 degrees Celsius when adjusted to the atmospheric pressure 1. 2. กรรมวิธีสำหรับทำให้เกิดการทำความเย็นซึ่งประกอบด้วยการระเหยของผสมตามข้อถือสิทธิข้อ 1 ในบริเวณติดๆ กับส่วนที่จะทำให้เย็นลงนั้น 12. A process for cooling which consists of the evaporation of the mixture according to claim 1, adjacent to the cooling part 1. 3. กรรมวิธีสำหรับทำความร้อนซึ่งประกอบด้วยการควบแน่นสารผสมตามข้อถือสิทธิข้อ 1 ในบริเวณติดๆ กับส่วนที่จะทำให้ร้อนขึ้น 13. Heating process consisting of condensation of the mixture according to claim 1 in the area adjacent to the heated part 1. 4. กรรมวิธีสำหรับครียมโพลิเมอร์โฟม ซึ่งประกอบด้วยการขยายตัวโพลิเมอร์ด้วยสารทำให้ฟู การปรับปรุงนั้ซึ่งสารทำให้ฟูขึ้นนั้น คือสารผสมตามข้อถือสิทธิข้อ 1 14.Process for Cremolymer Foam Which consists of polymer expansion with reagents The improvement of the substance that makes it rise Is a mixture according to claim 1 1 5. สารผสแอโรซอล ซึ่งประกอบด้วยสารผลักดันและสารแสดงฤทธิ์ การปรับปรุงนี้ซึ่งสารผลักดันนั้นคือ สารผสมตามข้อถือสิทธิข้อ 1 15. Aerosol containing substances, pushers and active substances This improvement, which the driving force is Mixture according to claim 1 1 6. กรรมวิธีสำหรับเตรียมสารสูตรผสมแอโรซอล ซึ่งประกอบด้วยการควบแน่นสารแสดงฤทธิ์ในภาชนะบรรจุแอโรซอลที่ประกอบด้วย สารผสมตามข้อถือสิทธิข้อ 1 ในปริมาณ ที่ใช้ได้ผลนั้นเป็นสารผลักดัน6. Process for preparing aerosol formulations Which consists of condensation of active substance in an aerosol container containing The mixture according to claim 1 in the effective quantity is a driving agent.
TH9101000231A 1991-02-26 Mixture maintains the boiling point of dichloropentafluoropropane and trans-1,2-dichlorethylene with methanol or ethanol. Or isopropanol TH3553B (en)