TH15986B - Reinforced bamboo fiber and its manufacturing methods And an inorganic molded body using reinforced bamboo fiber and its manufacturing method - Google Patents

Reinforced bamboo fiber and its manufacturing methods And an inorganic molded body using reinforced bamboo fiber and its manufacturing method

Info

Publication number
TH15986B
TH15986B TH9601001167A TH9601001167A TH15986B TH 15986 B TH15986 B TH 15986B TH 9601001167 A TH9601001167 A TH 9601001167A TH 9601001167 A TH9601001167 A TH 9601001167A TH 15986 B TH15986 B TH 15986B
Authority
TH
Thailand
Prior art keywords
bamboo
reinforced
moisture content
fibers
inorganic
Prior art date
Application number
TH9601001167A
Other languages
Thai (th)
Other versions
TH25626A (en
Original Assignee
นายชวลิต อัตถศาสตร์
นายชวลิต อัตถศาสตร์ นายไชยวัฒน์ บุนนาค
นายไชยวัฒน์ บุนนาค
Filing date
Publication date
Application filed by นายชวลิต อัตถศาสตร์, นายชวลิต อัตถศาสตร์ นายไชยวัฒน์ บุนนาค, นายไชยวัฒน์ บุนนาค filed Critical นายชวลิต อัตถศาสตร์
Publication of TH25626A publication Critical patent/TH25626A/en
Publication of TH15986B publication Critical patent/TH15986B/en

Abstract

เส้นใยไม้ไผ่ถูกนำมาใช้ทำหน้าที่เป็นวัสดุเสริมให้แข็งแรงและใช้ในการผลิตลำตัว ขึ้นรูปอนินทรีย์ในการผลิตเส้นใยไม้ไผ่ให้มีความคงทนดีเลิศ ในขั้นตอนที่หนึ่ง วัสดุไม้ไผ่จะ ถูกอัดให้ถูกบีบอย่างหยาบๆ และในขั้นตอนที่สอง วัสดุไม้ไผ่ที่ถูกบีบอย่างหยาบๆ จะถูกทำให้ เป็นเส้นใยโดยใช้เครื่องบด ปริมาณความชื้นของวัสดุไม้ไผ่ที่ผ่านขั้นตอนที่หนึ่งจะถูกตั้งไว้ให้ มากกว่า 65% หลังจากสิ้นสุดขั้นตอนที่หนึ่งและที่สอง ขั้นตอนใดขั้นตอนหนึ่งเป็นอย่างน้อยที่ สุดแล้ว จะเริ่มขั้นตอนของการทำแห้ง ดังนั้น ปริมาณความชื้นของวัสดุไม้ไผ่จะถูกปรับให้อยู่ ภายในช่วง 3 ถึง 35% Bamboo fibers are used as reinforcing materials and in the production of bamboo structures. The inorganic process of producing bamboo fibers results in excellent durability. In the first step, the bamboo material is roughly compressed. In the second step, the roughly compressed bamboo material is processed into fibers using a grinder. The moisture content of the bamboo material after the first step is set to over 65%. After the completion of at least one of the first and second steps, the drying process begins. Therefore, the moisture content of the bamboo material is adjusted to be within the range of 3 to 35%.

Claims (8)

วิธีการของการผลิตเส้นใยไม้ไผ่เสริมให้แข็งแรง ซึ่งประกอบด้วย (1) การอัดวัสดุไม้ไผ่ที่มีปริมาณความชื้นมากกว่า 65% เพื่อบีบมันอย่างหยาบ ๆ (2) การทำเส้นใยวัสดุไม้ไผ่ที่บีบอย่างหยาบ ๆ โดยใช้เครื่องบดเพื่อสร้างเส้นใยไม้ ไผ่ของวัสดุไม้ไผ่ดังกล่าว และ (3) ภายหลังเสร็จสิ้นขั้นตอน (1) ดังกล่าว และขั้นตอน (2) ดังกล่าว ขั้นตอนใด ขั้นตอนหนึ่งเป็นอย่างน้อยที่สุด จะเริ่มการทำแห้งวัสดุไม้ไผ่ดังกล่าวต่อปริมาณความชื้นภายใน ช่วง 3 ถึง 35% โดยที่เส้นใยไม้ไผ่เสริมให้แข็งแรงดังกล่าวถูกก่อขึ้น ที่ซึ่ง ปริมาณความชื้นถูก กำหนดเป็น (น้ำหนักที่มีน้ำ-น้ำหนักแห้ง)/น้ำหนักแห้ง) x 100 2. วิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 1 ที่ซึ่ง เส้นใยไม้ไผ่เสริมให้แข็งแรงยังคง ถูกดำเนินกระบวนการต่อไปเพื่อดูดซับน้ำเพื่อว่าปริมาณความชื้นของมันถึงมากกว่า 100 % ซึ่ง ต่อมา เส้นใยถูกขจัดน้ำเพื่อว่าปริมาณความชื้นของมันจะลดลงโดยมากกว่า 50 % ที่ซึ่ง ปริมาณ ความชื้นที่ได้อยู่ในช่วงของ 50 ถึง 200% 3. วิธีการผลิตเส้นใยไม้ไผ่เสริมให้แข็งแรง ที่ประกอบด้วย (1) การอัดวัสดุไม้ไผ่ที่มีส่วนของผิวบาง ๆ ด้านใน และมีปริมาณความชื้นมากกว่า 65% เพื่อบีบมันอย่างหยาบๆ (2) การทำเส้นใยวัสดุไม้ไผ่ที่บีบอย่างหยาบๆ โดยใช้เครื่องบดเพื่อสร้างเส้นใย ไม้ไผ่ของวัสดุไม้ไผ่ดังกล่าว (3) การแยกส่วนของผิวด้านในของวัสดุไม้ไผ่ดังกล่าวโดยวิธีการแยกทางกล และ (4) ภายหลังเสร็จสิ้นขั้นตอน (1) ดังกล่าว ขั้นตอน (2) ดังกล่าว และขั้นตอน (3) ดังกล่าว ขั้นตอนใดขั้นตอนหนึ่งเป็นอย่างน้อยที่สุด จะเริ่มการทำแห้งวัสดุไม้ไผ่ดังกล่าวต่อ ปริมาณความชื้นภายในช่วง 3 ถึง 35% โดยที่เส้นใยไม้ไผ่เสริมให้แข็งแรงดังกล่าวจะก่อขึ้น ที่ ซึ่ง ปริมาณความชื้นจะถูกกำหนดเป็น ((น้ำหนักที่มีน้ำ-น้ำหนักแห้ง)/น้ำหนักแห้ง) x 100 4. วิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 3 ที่ซึ่ง เส้นใยไม้ไผ่ยังคงถูกดำเนินกระบวน การต่อไปเพื่อดูดซับน้ำ เพื่อว่าปริมาณความชื้นของมันถึงมากกว่า 100% ซึ่งต่อมา เส้นใยจะถูก ขจัดน้ำ เพื่อว่าปริมาณความชื้นของมันจะลดลงโดยมากกว่า 50% ที่ซึ่ง ว่าปริมาณความชื้นที่ได้อยู่ ในช่วง 50 ถึง 200% 5. วิธีการผลิตเส้นใยไม้ไผ่เสริมให้แข็งแรง ที่ซึ่งประกอบด้วย (1) การอัดวัสดุไม้ไผ่ที่มีส่วนของผิวบางๆ ด้านใน และมีปริมาณความชื้นมากกว่า 65% เพื่อบีบมันอย่างหยาบๆ (2) การทำเส้นใยวัสดุไม้ไผ่ที่ถูกบีบอย่างหยาบๆ โดยใช้เครื่องบดเพื่อก่อให้เป็น เส้นใยไม้ไผ่ของวัสดุไม้ไผ่ดังกล่าว (3) การแยกส่วนของผิวบางๆ ด้านในของวัสดุไม้ไผ่ดังกล่าวโดยวิธีการแยกแบบ จุ่มน้ำ (4) ภายหลังเสร็จสิ้นขั้นตอน (1) ดังกล่าว และขั้นตอน (2) ดังกล่าว ขั้นตอนใด ขั้นตอนหนึ่งเป็นอย่างน้อยที่สุด จะเริ่มการทำแห้งวัสดุไม้ไผ่ดังกล่าวต่อปริมาณความชื้นภายใน ช่วง 3 ถึง 35% โดยที่เส้นใยไม้ไผ่เสริมให้แข็งแรงดังกล่าวถูกก่อขึ้น ที่ซึ่ง ปริมาณความชื้นถูก กำหนดเป็น ((น้ำหนักที่มีน้ำ-น้ำหนักแห้ง)/น้ำหนักแห้ง) x 100 6. วิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 5 ที่ซึ่ง ภายหลังการแยกของส่วนของผิวบาง ๆ ด้านในดังกล่าว เส้นใยไม้ไผ่จะถูกขจัดน้ำ เพื่อว่าปริมาณความชื้นของมันจะถูกลดลงโดยมาก กว่า 50% ที่ซึ่ง ปริมาณความชิ้นที่ได้จะอยู่ในช่วง 50 ถึง 200% 7. วิธีการผลิตลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ประกอบด้วย การนวดส่วนผสมวัตถุดิบที่มีเอเจนท์เชื่อมประสานขึ้นรูปด้วยไฮดรอลิคที่เป็นอนินทรีย์ และ เส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตตามวิธีการที่กำหนดในข้อถือสิทธิข้อ 1 ที่มีหรือไม่มีน้ำ เพื่อ สร้างเป็นรูปทรง และต่อมา ทำให้แห้งและแข็งตัว 8. วิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 7 ที่ซึ่ง เอเจนท์เชื่อมประสานใช้ในการขึ้นรูป ด้วยไฮดรอลิคอนินทรีย์ดังกล่าว คือ ซีเมนต์ 9. วิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 7 ที่ซึ่ง ส่วนผสมวัตถุดิบดังกล่าวมีตัวเติมเต็ม 1 0. วิธีการผลิตลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรง ซึ่งประกอบด้วย การนวดส่วนผสมวัตถุดิบที่มีเอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮดรอลิคอนินทรีย์ และ เส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการที่กำหนดไว้ในข้อถือสิทธิข้อ 2 ที่มีหรือไม่มี น้ำเพื่อก่อให้เป็นรูปทรง และต่อมา ทำให้แห้งและแข็งตัว 1 1. วิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 10 ที่ซึ่ง เอเจนท์เชื่อมประสานใช้ในการขึ้น รูปด้วยไฮดรอลิคอนินทรีย์ดังกล่าว คือ ซีเมนต์ 1 2. วิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 10 ที่ซึ่ง ส่วนผสมวัตถุดิบดังกล่าวมีตัวเติม เต็ม 1 3. วิธีการผลิตลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรง ซึ่งประกอบด้วย การนวดส่วนผสมวัตถุดิบที่มีเอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮดรอลิคอนินทรีย์ และ เส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการที่กำหนดไว้ในข้อถือสิทธิข้อ 4 ด้วยปริมาณน้ำ เพื่อก่อให้เป็นรูปทรง และต่อมา ทำให้แห้งและแข็งตัว 1 4. วิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 13 ที่ซึ่ง เอเจนท์เชื่อมประสานใช้ในการขึ้น รูปด้วยไฮดรอลิคอนินทรีย์ดังกล่าว คือ ซีเมนต์ 1 5. วิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 13 ที่ซึ่ง ส่วนผสมวัตถุดิบดังกล่าวมีตัวเติม เต็ม 1 6. วิธีการผลิตลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรง ซึ่งประกอบด้วย การนวดส่วนผสมวัตถุดิบที่มีเอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮดรอลิคอนินทรีย์ และ เส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 5 เพื่อก่อให้เกิด รูปทรง และต่อมา ทำให้แห้งและแข็งตัว 1 7. วิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 16 ที่ซึ่ง ส่วนผสมวัตถุดิบดังกล่าวมีตัวเติม เต็ม 1 8. วิธีการผลิตลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรง ซึ่งประกอบด้วย การนวดส่วนผสมวัตถุดิบที่มีเอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮดรอลิคอนินทรีย์ และ เส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการที่กำหนดไว้ในข้อถือสิทธิข้อ 6 เพื่อก่อให้เป็น รูปทรง และต่อมา ทำให้แห้งและแข็งตัว 1 9. วิธีการตามที่ระบุไว้ในข้อถือสิทธิข้อ 18 ที่ซึ่ง ส่วนผสมวัตถุดิบดังกล่าวมีตัวเติม เต็ม 2 0. เส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตตามวิธีการ ซึ่งประกอบด้วย (1) การอัดวัสดุไม้ไผ่ที่มีปริมาณความชื้นมากกว่า 65% เพื่อบีบมันอย่างหยาบ ๆ (2) การทำเส้นใยวัสดุไม้ไผ่ที่บีบอย่างหยาบๆ โดยใช้เครื่องบด เพื่อสร้างเส้นใย ไม้ไผ่ของวัสดุไม้ไผ่ดังกล่าว และ (3) ภายหลังเสร็จสิ้นขั้นตอน (1) ดังกล่าว และขั้นตอน (2) ดังกล่าว ขั้นตอนใด ขั้นตอนหนึ่งเป็นอย่างน้อยที่สุด จะเริ่มทำแห้งวัสดุไม้ไผ่ดังกล่าวต่อปริมาณความชื้นภายในช่วง 3 ถึง 35% โดยที่เส้นใยไผ่เสริมให้แข็งแรงดังกล่าวถูกก่อขึ้น ที่ซึ่ง ปริมาณความชื้นถูก กำหนดเป็น ((น้ำหนักที่มีน้ำ-น้ำหนักแห้ง)/น้ำหนักแห้ง) x 100 2 1. เส้นใยไม้ไผ่เสริมให้แข็งแรงตามที่ระบุไว้ในข้อถือสิทธิข้อ 20 ที่ซึ่ง เส้นใยไม้ไผ่ เสริมให้แข็งแรงถูกดำเนินกระบวนการต่อไปเพื่อดูดซับน้ำ เพื่อว่าปริมาณความชื้นของมันถึง มากกว่า 100% ซึ่งต่อมา เส้นใยถูกขจัดน้ำเพื่อว่าปริมาณความชื้นของมันถูกลดลงโดยมากกว่า 50% ที่ซึ่ง ปริมาณความชื้นที่ได้อยู่ในช่วง 50 ถึง 200% 2 2. เส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตตามวิธีการ ซึ่งประกอบด้วย (1) การอัดวัสดุไม้ไผ่ที่มีปริมาณความชื้นมากกว่า 65% เพื่อบีบมันอย่างหยาบ ๆ (2) การทำเส้นใยวัตถุไม้ไผ่ที่บีบอย่างหยาบๆ โดยใช้เครื่องบด และ (3) การแยกส่วนของผิวบางๆ ด้านในของวัสดุไม้ไผ่ดังกล่าวโดยวิธีการแยกทาง กล และ (4) ภายหลังเสร็จสิ้นขั้นตอน (1) ดังกล่าว ขั้นตอน (2) ดังกล่าว และขั้นตอน (3) ดังกล่าว ขั้นตอนใดขั้นตอนหนึ่งเป็นอย่างน้อยที่สุด จะเริ่มทำแห้งวัสดุไม้ไผ่ดังกล่าวต่อปริมาณ ความชื้นภายในช่วง 3 ถึง 35% 2 3. เส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการ ซึ่งประกอบด้วย (1) การอัดวัสดุไม้ไผ่ที่มีส่วนของผิวบางๆ ด้านใน และมีปริมาณความชื้นมากกว่า 65% เพื่อบีบมันอย่างหยาบๆ (2) การทำเส้นใยวัสดุไม้ไผ่ที่บีบอย่างหยาบๆ โดยใช้เครื่องบดเพื่อก่อเส้นใยไม้ ไผ่ของวัสดุไม้ไผ่ (3) การแยกส่วนของผิวบางๆ ด้านในของวัสดุไม้ไผ่ดังกล่าวโดยวิธีการแยกแบบ จุ่มน้ำ (4) ภายหลังเสร็จสิ้นขั้นตอน (1) ดังกล่าว และขั้นตอน (2) ดังกล่าว ขั้นตอนใด ขั้นตอนหนึ่งเป็นอย่างน้อยที่สุด จะเริ่มทำแห้งวัสดุไม้ไผ่ดังกล่าวต่อปริมาณความชื้นภายในช่วง 3 ถึง 35% โดยที่เส้นใยไม้ไผ่เสริมให้แข็งแรงดังกล่าวถูกก่อขึ้น ที่ซึ่ง ปริมาณความชื้นถูก กำหนดเป็น ((น้ำหนักที่มีน้ำ-น้ำหนักแห้ง)/น้ำหนักแห้ง) x 100 2 4. เส้นใยไม้ไผ่เสริมให้แข็งแรงตามที่ระบุไว้ในข้อถือสิทธิข้อ 23 ที่ซึ่ง ภายหลังการ แยกส่วนของผิวบางๆ ด้านในดังกล่าว เส้นใยไม้ไผ่ถูกขจัดน้ำ เพื่อว่าปริมาณความชื้นถูกลดลง โดยมากกว่า 50% ที่ซึ่ง ปริมาณความชื้นที่ได้อยู่ภายในช่วง 50 ถึง 200% 2 5. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการซึ่ง ประกอบด้วย การนวดส่วนผสมวัตถุดิบที่มีเอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮครอลิค อนินทรีย์ และเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามข้อถือสิทธิข้อ 20 ที่มีหรือไม่มีน้ำ เพื่อ ก่อให้เป็นรูปทรง และต่อมา ทำให้แห้งและแข็งตัว 2 6. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการซึ่ง ประกอบด้วย การนวดส่วนผสมวัตถุดิบที่มีเอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮดรอลิค อนินทรีย์ และเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามข้อถือสิทธิข้อ 21 ที่มีหรือไม่มีน้ำ เพื่อ ก่อให้เป็นรูปทรง และต่อมา ทำให้แห้งและแข็งตัว 2 7. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามข้อถือสิทธิข้อ 25 ที่ซึ่ง เอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮดรอลิคอนินทรีย์ดังกล่าว คือ ซีเมนต์ 2 8. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตตามข้อถือสิทธิข้อ 26 ที่ซึ่ง เอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮดรอลิคอนินทรีย์ดังกล่าว คือ ซีเมนต์ 2 9. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามข้อถือสิทธิข้อ 25 ที่ซึ่ง ส่วนผสมวัตถุดิบดังกล่าวมีตัวเติมเต็ม 3 0. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามข้อถือสิทธิข้อ 26 ที่ซึ่ง ส่วนผสมของวัตถุดิบดังกล่าวมีตัวเติมเต็ม 3 1. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการซึ่ง ประกอบด้วย การนวดส่วนผสมวัตถุดิบที่มีเอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮดรอลิค อนินทรีย์ และเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามข้อถือสิทธิข้อ 22 ที่มีปริมาณน้ำเพื่อก่อ ให้เป็นรูปทรง และต่อมา ทำให้แห้งและแข็งตัว 3The method of producing reinforced bamboo fibers consists of (1) compressing bamboo material with a moisture content greater than 65% to coarsely squeeze it; (2) fusing the coarsely squeezed bamboo material using a grinder to form bamboo fibers of the said bamboo material; and (3) after the completion of step (1) and step (2), at least one of these steps shall begin drying the said bamboo material to a moisture content in the range of 3 to 35%, where reinforced bamboo fibers are formed, where the moisture content is determined as (Wet Weight - Dry Weight) / Dry Weight) x 100. 2. The method as described in Reputation 1, in which reinforced bamboo fibers are further processed to absorb water so that their moisture content reaches greater than 100%, where the fibers are subsequently dewatered so that their moisture content is reduced to greater than 50%, where the resulting moisture content is in the range of 50 to 200%. 3. The method of producing reinforced bamboo fibers. It consists of (1) the compression of the bamboo material with a thin inner skin and a moisture content greater than 65% to be roughly compressed; (2) the dewatering of the roughly compressed bamboo material using a grinder to create bamboo fibers of the said bamboo material; (3) the separation of the inner skin of the said bamboo material by mechanical separation; and (4) after the completion of step (1), step (2) and step (3), at least one of these steps shall initiate further drying of the said bamboo material to a moisture content in the range of 3 to 35%, in which reinforced bamboo fibers shall be formed, where the moisture content shall be determined as ((weight with water - dry weight) / dry weight) x 100. 4. The method specified in claim 3 in which the bamboo fibers are further processed to absorb water so that their moisture content reaches greater than 100%, in which case the fibers are subsequently dewatered so that their moisture content is reduced to greater than 50%, in which case the resulting moisture content is in the range of 50 to 200%. 5. The method for producing reinforced bamboo fibers. 6. The method described in Claim 5, in which the inner thin layer of bamboo material with a moisture content greater than 65% is roughly compressed; (2) the rough compressed bamboo material is processed using a grinder to form bamboo fibers; (3) the inner thin layer of bamboo material is separated by the immersion method; (4) after the completion of at least one of the above steps (1) and (2), the bamboo material is dried to a moisture content of 3 to 35%, in which the reinforced bamboo fibers are formed, where the moisture content is determined as ((weight with water - dry weight) / dry weight) x 100. 7. The method described in Claim 5, in which, after the separation of the inner thin layer of bamboo fibers, the bamboo fibers are dehydrated so that their moisture content is reduced to more than 50%, in which the resulting moisture content is in the range of 50 to 200%. 8. The method of producing inorganic reinforced bamboo fiber molded bodies consisting of: The kneading of a hydraulic forming mixture containing an inorganic binding agent and reinforced bamboo fibers produced according to the method specified in Remarks 1, with or without water, to form it, and subsequently drying and hardening it. 8. The method specified in Remarks 7, in which the binding agent used in the hydraulic forming of such inorganic mixture is cement. 9. The method specified in Remarks 7, in which the mixture contains fillers. 10. The method for producing an inorganic forming body reinforced with bamboo fibers, consisting of the kneading of a hydraulic forming mixture containing an inorganic binding agent and reinforced bamboo fibers produced according to the method specified in Remarks 2, with or without water, to form it, and subsequently drying and hardening it. 11. The method specified in Remarks 10, in which the binding agent used in the hydraulic forming of such inorganic mixture is cement. 1. The method specified in Reputation 10, in which the binding agent used in the hydraulic forming of the inorganic body is cement. 1. 2. The method specified in Reputation 10, in which the raw material mixture contains filler. 1. 3. The method for producing inorganic molded bodies reinforced with bamboo fibers, consisting of kneading the raw material mixture containing the binding agent for hydraulic forming and the bamboo fibers reinforced according to the method specified in Reputation 4 with water to form the shape, and subsequently drying and hardening. 1. 4. The method specified in Reputation 13, in which the binding agent used in the hydraulic forming of the inorganic body is cement. 1. 5. The method specified in Reputation 13, in which the raw material mixture contains filler. 1. 6. The method for producing inorganic molded bodies reinforced with bamboo fibers, consisting of... 1 7. The method specified in Reputation 16 in which the mixture of raw materials containing a binding agent is used for hydraulic molding and reinforced with bamboo fibers, produced according to the method specified in Reputation 5 to form the shape and subsequently dried and hardened. 1 8. The method specified in Reputation 18 in which the mixture of raw materials contains a filler. 2 0. Reinforced with bamboo fibers produced according to the method which consists of (1) compression of bamboo material with a moisture content greater than 65% to coarsely compress it; (2) processing of the coarsely compressed bamboo material into fibers using a grinder. 2 1. Reinforced bamboo fibers as described in Reputation 20, in which the reinforced bamboo fibers are further processed to absorb water so that their moisture content reaches more than 100%, in which the fibers are subsequently dewatered so that their moisture content is reduced to more than 50%, in which the resulting moisture content is in the range of 50 to 200%. 2 2. Reinforced bamboo fibers produced by a method consisting of (1) pressing the bamboo material with a moisture content greater than 65% to coarsely compress it, (2) processing the coarsely compressed bamboo material into fibers using a grinder, and (3) separating the thin layer. The inner layer of the bamboo material is separated by the mechanical separation method, and (4) after the completion of step (1), step (2) and step (3) are at least one of the above steps, the bamboo material is dried to a moisture content of 3 to 35%. 2 3. Reinforced bamboo fibers are produced by the method which consists of (1) pressing the bamboo material with a thin inner layer and a moisture content of more than 65% to coarsely squeeze it; (2) making the coarsely squeezed bamboo material fibers using a grinder to form bamboo fibers of the bamboo material; (3) separating the thin inner layer of the bamboo material by the water separation method; (4) after the completion of step (1) and step (2) are at least one of the above steps, the bamboo material is dried to a moisture content of 3 to 35%. The bamboo material shall be dried to a moisture content of 3 to 35%, where the reinforced bamboo fibers are formed, where the moisture content is determined as ((weight with water - dry weight) / dry weight) x 100. 2 4. The reinforced bamboo fibers are formed as specified in claim 23, where, after separation of the thin inner layer, the bamboo fibers are dehydrated. 2.5. Inorganic molded bodies reinforced with bamboo fibers produced according to a method which involves kneading a mixture of raw materials containing an inorganic hydraulic binding agent and bamboo fibers reinforced according to Reservience Clause 20, with or without water, to form the shape and subsequently drying and hardening. 2.6. Inorganic molded bodies reinforced with bamboo fibers produced according to Reservience Clause 21, with or without water, to form the shape and subsequently drying and hardening. 2.7. Inorganic molded bodies reinforced with bamboo fibers produced according to Reservience Clause 25, where the inorganic hydraulic binding agent is cement. 2.8. An inorganic molded body reinforced with bamboo fibers produced in accordance with Treaty Clause 26 where the binding agent used in the hydraulic molding of such inorganic cement is cement 2 9. An inorganic molded body reinforced with bamboo fibers produced in accordance with Treaty Clause 25 where the raw material mixture contains filler 3 0. An inorganic molded body reinforced with bamboo fibers produced in accordance with Treaty Clause 26 where the raw material mixture contains filler 3 1. An inorganic molded body reinforced with bamboo fibers produced in accordance with Treaty Clause 22 in a method which consists of kneading a raw material mixture containing an inorganic binding agent used in the hydraulic molding and bamboo fibers reinforced in accordance with Treaty Clause 22 with a water content to form the shape and subsequently drying and hardening 3 2. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามข้อถือสิทธิข้อ 31 ที่ซึ่ง เอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮดรอลิคอนินทรีย์ดังกล่าว คือ ซีเมนต์ 32. An inorganic molded body reinforced with bamboo fibers, manufactured pursuant to claim clause 31, whereby the binding agent used in the hydraulic molding of such inorganic body is cement 3. 3. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามข้อถือสิทธิข้อ 32 ที่ซึ่ง ส่วนผสมวัตถุดิบดังกล่าวมีตัวเติมเต็ม 33. An inorganic molded body reinforced with bamboo fibers, manufactured pursuant to claim clause 32, in which the raw material mixture contains three fillers. 4. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการที่ ประกอบด้วย การนวดส่วนผสมวัตถุดิบที่มีเอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮดรอลิค อนินทรีย์ และเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการที่กำหนดในข้อถือสิทธิข้อ 23 เพื่อก่อให้เป็นรูปทรง และต่อมา ทำให้แห้งและแข็งตัว 34. An inorganic, bamboo-reinforced, molded body produced by a method consisting of kneading a mixture of inorganic, hydraulically molded, binding agents and bamboo-reinforced materials produced by the method specified in Patent 23 to form the shape, and subsequently drying and hardening. 3 5. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการที่ ประกอบด้วย การนวดส่วนผสมวัตถุดิบที่มีเอเจนท์เชื่อมประสานใช้ในการขึ้นรูปด้วยไฮดรอลิค อนินทรีย์ และเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามวิธีการที่กำหนดในข้อถือสิทธิข้อ 24 เพื่อก่อให้เป็นรูปทรง และต่อมา ทำให้แห้งและแข็งตัว 35. An inorganic, bamboo-reinforced, molded body produced by a method consisting of a hydraulic kneading of the inorganic, bamboo-reinforced, hydraulically molded mixture of raw materials with binding agents, and subsequently dried and hardened. 3 6. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามข้อถือสิทธิข้อ 34 ที่ซึ่ง ส่วนผสมวัตถุดิบดังกล่าวที่มีตัวเติมเต็ม 36. An inorganic molded body reinforced with bamboo fibers, manufactured pursuant to claim clause 34, in which the raw material mixture contains 3 fillers. 7. ลำตัวขึ้นรูปอนินทรีย์ที่มีเส้นใยไม้ไผ่เสริมให้แข็งแรงที่ผลิตขึ้นตามข้อถือสิทธิข้อ 35 ที่ซึ่ง ส่วนผสมวัตถุดิบดังกล่าวที่มีตัวเติมเต็ม 37. An inorganic molded body reinforced with bamboo fibers, manufactured pursuant to claim clause 35, in which the raw material mixture contains 3 fillers. 8. เส้นใยไม้ไผ่เสริมให้แข็งแรงตามข้อถือสิทธิข้อ 22 ที่ซึ่ง เส้นใยไม้ไผ่เสริมให้ แข็งแรงจะถูกดำเนินกระบวนการต่อไปเพื่อดูดซับน้ำ เพื่อว่าปริมาณความชื้นของมันถึงมากกว่า 100% ซึ่งต่อมา เส้นใยจะถูกขจัดน้ำเพื่อว่าปริมาณความชื้นของมันจะถูกลดโดยมากกว่า 50% ที่ ซึ่ง ปริมาณความชื้นที่ได้อยู่ในช่วง 50 ถึง 200%8. Reinforced bamboo fibers pursuant to claim clause 22, whereby the reinforced bamboo fibers are further processed to absorb water so that their moisture content reaches over 100%, and subsequently the fibers are dewatered so that their moisture content is reduced to over 50%, resulting in a moisture content ranging from 50 to 200%.
TH9601001167A 1996-04-17 Reinforced bamboo fiber and its manufacturing methods And an inorganic molded body using reinforced bamboo fiber and its manufacturing method TH15986B (en)