SU97094A2 - Method of introduction of softeners in latex - Google Patents

Method of introduction of softeners in latex

Info

Publication number
SU97094A2
SU97094A2 SU446791A SU446791A SU97094A2 SU 97094 A2 SU97094 A2 SU 97094A2 SU 446791 A SU446791 A SU 446791A SU 446791 A SU446791 A SU 446791A SU 97094 A2 SU97094 A2 SU 97094A2
Authority
SU
USSR - Soviet Union
Prior art keywords
latex
softeners
introduction
mixed
hydrophobic
Prior art date
Application number
SU446791A
Other languages
Russian (ru)
Inventor
М.Е. Слепян
н М.Е. Слеп
Original Assignee
М.Е. Слепян
н М.Е. Слеп
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by М.Е. Слепян, н М.Е. Слеп filed Critical М.Е. Слепян
Priority to SU446791A priority Critical patent/SU97094A2/en
Application granted granted Critical
Publication of SU97094A2 publication Critical patent/SU97094A2/en

Description

В ОСНОВНОМ авт. св. 72293 описан способ введени  м гчителей в латекс, заключающийс  в том, что эмульсию м гчител , полученную обычными методами, предварительно смешивают с каким-либо сыпучим нигредиентом резиновой смеси до получени  пасты, которую затем ввод т при перемешивании в латекс.BASIC Auth. St. 72293 describes a method for introducing a softener into latex, which consists in the fact that emulsifier emulsion obtained by conventional methods is pre-mixed with any bulk nigredient rubber compound to form a paste, which is then injected with stirring into latex.

Известно, чти при введении в латексы гидрофобных м гчителей, примен емых в резиновой промышленности , как, напрнмер, вазелина, битумов, парафина, минеральных масел и др., в виде эмульсии, по . учаемых обычными методами, нарушаетс  коллоидна  система латексов и измен ютс  физические свойства с потерей при этом пропиточных свойств.It is known that when hydrophobic grinders used in the rubber industry are introduced into latexes, such as naphtha, petroleum jelly, bitumen, paraffin, mineral oils, etc., as an emulsion, according to. taken into account by conventional methods, the colloidal system of latexes is disturbed and the physical properties change, with the loss of impregnating properties.

Предлагаемый способ обеспечивает стабильность коллоидной системы латексов и сохран ет пропиточные свойства различных латексных композиций.The proposed method ensures the stability of the colloidal system of latexes and preserves the impregnating properties of various latex compositions.

Особенность предлагаемого способа заключаетс  в том, что гидрофобные м гчители предварительно эмульгируют при температуре не выше 25-30° растворами желатины, казеина и т. п. с концентрациейThe peculiarity of the proposed method is that hydrophobic softeners are emulsified beforehand at a temperature not higher than 25-30 ° with solutions of gelatin, casein, etc., with a concentration of

не ниже 30-35%; полученные эмульсии подвергают механической обработке в присутствии сыпучих наполнителей, после чего массу разбавл ют водой и смешивают с латексом.not less than 30-35%; the resulting emulsions are machined in the presence of bulk fillers, after which the mass is diluted with water and mixed with latex.

Предлагаемую латексную смесь примен ют дл  получени  заменителей кожи на основе одно- и многослойных тканей путем пропитки и обработки этих тканей известными технологическими приемами.The proposed latex mixture is used to produce skin substitutes based on single and multi-layer fabrics by impregnating and treating these fabrics with known techniques.

Предмет изобретени Subject invention

Claims (2)

1.Способ введени  м гчителей в латекс по авт. св. ЛЬ 72293, отличающийс  тем, что гидрофобные м гчители предварительно эмульгируют при температуре не выше 25-30° растворами желатины, казеина и т. и. с концентрацией не ниже 30-35%; полученные э.мульсии подвергают механической обработке в присутствии сыпучих наполнителей, после чего массу разбавл ют водой и смешивают с латексом.1. The method of introduction of softeners in latex by the author. St. L72293, characterized in that hydrophobic softeners are emulsified beforehand at a temperature not higher than 25-30 ° with solutions of gelatin, casein, etc., and so on. with a concentration of not less than 30-35%; The resulting emulsions are machined in the presence of bulk fillers, after which the mass is diluted with water and mixed with latex. 2.Применение латексных cMeceii, полученных по п. 1, дл  изготовлени  заменителей кожи на основе одно- и многослойных тканей.2. The use of latex cMeceii, obtained according to claim 1, for the manufacture of skin substitutes based on single and multi-layered fabrics.
SU446791A 1951-09-15 1951-09-15 Method of introduction of softeners in latex SU97094A2 (en)