SU728711A3 - Method of producing water-filled explosive substance - Google Patents

Method of producing water-filled explosive substance Download PDF

Info

Publication number
SU728711A3
SU728711A3 SU782696901A SU2696901A SU728711A3 SU 728711 A3 SU728711 A3 SU 728711A3 SU 782696901 A SU782696901 A SU 782696901A SU 2696901 A SU2696901 A SU 2696901A SU 728711 A3 SU728711 A3 SU 728711A3
Authority
SU
USSR - Soviet Union
Prior art keywords
microspheres
filled
ammonium
urea
guar gum
Prior art date
Application number
SU782696901A
Other languages
Russian (ru)
Inventor
Олоф Экман Гуннар
Original Assignee
Нитро Нобель Аб (Фирма)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Нитро Нобель Аб (Фирма) filed Critical Нитро Нобель Аб (Фирма)
Priority to SU782696901A priority Critical patent/SU728711A3/en
Application granted granted Critical
Publication of SU728711A3 publication Critical patent/SU728711A3/en

Description

Дл  проверки разработанного способа получени  взрывчатого вещества был изготовлен состав, содержащий на 1000 вес.ч. 389,5 вес.ч. нитрата аммони ,.79 вес.ч. нитрата кальци , 120 вес.ч. нитрата натри , 216 вес.ч нитрата метиламмони , 34 вес.ч. мочевины , 55 вес.ч. алюминиевого по-решка , 11 вес.ч. гуаровой смолы, 87 вес.ч. воды и 8,5 вес.ч. микросфер (на сухой материеил) . Изготовленное в различных услови х (по примерам) указанное выше водонаполненное взрывчатое вещество имело плотность 1,12 г/см, скорость детонации в железных трубах диаметром 32 мм и инициировании от к/д № 8 4400 м/с. В услови х повышенного статического давлени  взрывчатое вещество сохран ет посто ннуюг восприимчивость к инициирующему импульсу и стабильно детонирует. По своим характеристикам разработанное водонаполненное взрывчатое вещество равноценно примерно взрывчатому веществу , содержащему сенсибилизатор, например тротил.To test the developed method for producing an explosive, a composition containing 1000 parts by weight was manufactured. 389.5 weight.h. ammonium nitrate, .79 weight.h. calcium nitrate, 120 weight.h. sodium nitrate, 216 weight.h methyl ammonium nitrate, 34 weight.h. urea, 55 weight.h. aluminum on-tail, 11 weight.h. guar gum, 87 weight.h. water and 8.5 wt.h. microspheres (dry matter). Manufactured under various conditions (by examples), the above-mentioned water-filled explosive had a density of 1.12 g / cm, a detonation velocity in iron pipes with a diameter of 32 mm and initiation from k / d No. 8 4400 m / s. Under conditions of increased static pressure, the explosive remains constant susceptibility to the initiating pulse and stably detonates. According to its characteristics, the developed water-filled explosive is equivalent to about an explosive containing a sensitizer, for example, TNT.

Claims (1)

Формула изобретени Invention Formula Способ йолучени  водонаполненного взрывчатого вещества на основе нитратов аммони , кальци  и натри , нитрата метиламмони , мочевины, алюминиевого порошка, загустител  гуаровой смолы, воды и микросфер из сополимера винилиденхлорида с акрилнитрилом , заполненных изобутаном, путем введени  в концентрированный водный раствор нитратов, мочевины или этилен гликол  и гуаровой смолы предварительно смешанных сухих компонентов , алюминиевого порошка, сенсибилизатора и микросфер, размеры которых окончательно довод тс  нагреванием при 85-100с, отличающийс  тем, что, с целью обеспечени  безопасности работы, процесс провод тThe method of obtaining water-filled explosives based on ammonium nitrate, calcium and sodium, methylammonium nitrate, urea, aluminum powder, thickener of guar gum, water, and microspheres of vinylidenechloride-acrylonitrile copolymer filled with isobutane, and placed in a concentrate, a set of 0, 20, etc., in addition to a sample of the concentration of a non-emollium, a sample of the composition, and a volume of nitrite. and guar gum of pre-mixed dry ingredients, aluminum powder, sensitizer and microspheres, the dimensions of which are finally adjusted by heating at 85-100 s , characterized in that, in order to ensure the safety of work, the process is carried out 5 постадийно, вначале термостатируют микросферы при 100-110°С в течение 30 с в концентрированном растворе или эвтектическом расплаве нитратов и мочевины, затем после охлаждени 5 step by step, first incubate microspheres at 100-110 ° C for 30 s in a concentrated solution or eutectic melt of nitrates and urea, then after cooling 0 смеси до 70С добавлением раствора - части нитратов аммони  и метиламмони , ввод т постадийно или сразу остальные сухие компоненты.0 mixtures up to 70 ° C by the addition of a solution — part of ammonium and methyl ammonium nitrates, are introduced step by step or the rest of the dry components immediately. Источники информации,Information sources, 5 прин тые во внимание при экспертизе5 taken into account in the examination 1, Патент США 3773573, кл. С Об В 1/04, кл. 149-21, опублик. 1973 (прототип),1, US Patent 3773573, cl. C About B 1/04, cl. 149-21, published. 1973 (prototype),
SU782696901A 1978-12-15 1978-12-15 Method of producing water-filled explosive substance SU728711A3 (en)