SU626925A1 - Способ восстановлени изношенных внутренних цилиндрических поверхностей деталей - Google Patents

Способ восстановлени изношенных внутренних цилиндрических поверхностей деталей

Info

Publication number
SU626925A1
SU626925A1 SU772466624A SU2466624A SU626925A1 SU 626925 A1 SU626925 A1 SU 626925A1 SU 772466624 A SU772466624 A SU 772466624A SU 2466624 A SU2466624 A SU 2466624A SU 626925 A1 SU626925 A1 SU 626925A1
Authority
SU
USSR - Soviet Union
Prior art keywords
cylindrical surfaces
internal cylindrical
components
worn
parts
Prior art date
Application number
SU772466624A
Other languages
English (en)
Inventor
Анатолий Алексеевич Зуев
Олег Георгиевич Цыплаков
Владимир Георгиевич Цыплаков
Александр Иванович Петров
Original Assignee
Ленинградский Ордена Трудового Красного Знамени Сельскохозяйственный Институт
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ленинградский Ордена Трудового Красного Знамени Сельскохозяйственный Институт filed Critical Ленинградский Ордена Трудового Красного Знамени Сельскохозяйственный Институт
Priority to SU772466624A priority Critical patent/SU626925A1/ru
Application granted granted Critical
Publication of SU626925A1 publication Critical patent/SU626925A1/ru

Links

Landscapes

  • Extrusion Moulding Of Plastics Or The Like (AREA)

Claims (1)

  1. точных напр жений в клеевом соединении после сн ти  подпрессовки, увеличение прочности соединени , улучшаютс  услови дл  механической обработки, повышаетс  точность обработки отверстий. Формула изобретени  Способ восстановлени  изношенных внутренних цилиндрических поверхностей деталей, заключающийс  в том, что изно шенную поверхность детали подвергают м ханической обработке, затем вклеивают ремонтную втулку с последующей требуе мой обработкой, отличающийс тем, что, с целью повынени  качества восстанавливаемых деталей различных типоразмеров , в качестве втулки используют свернутую с тепловым зазором по окружности обработанной поверхности восстанавливаемой детали по крайней мере одну полосу с нанесенными на ее внутренней поверхности по образующей параллельными канав1шми, глубина которых равна припуску на механическую обработку. Источники информации, прин тые во внимание при экспертизе: 1. Гепьберг Б. Т., Пакелис Г. Д. Ре-, моит промьшотенного оборудовани , М., Профтехиздат, 1962, с, 140,
SU772466624A 1977-02-23 1977-02-23 Способ восстановлени изношенных внутренних цилиндрических поверхностей деталей SU626925A1 (ru)