SU611743A1 - Method of arc butt-welding of aluminium alloys - Google Patents

Method of arc butt-welding of aluminium alloys

Info

Publication number
SU611743A1
SU611743A1 SU762434390A SU2434390A SU611743A1 SU 611743 A1 SU611743 A1 SU 611743A1 SU 762434390 A SU762434390 A SU 762434390A SU 2434390 A SU2434390 A SU 2434390A SU 611743 A1 SU611743 A1 SU 611743A1
Authority
SU
USSR - Soviet Union
Prior art keywords
welding
aluminium alloys
arc butt
butt
arc
Prior art date
Application number
SU762434390A
Other languages
Russian (ru)
Inventor
Валентин Валентинович Цой
Евгений Александрович Алексеев
Геннадий Григорьевич Михайлов
Original Assignee
Предприятие П/Я Г-4361
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я Г-4361 filed Critical Предприятие П/Я Г-4361
Priority to SU762434390A priority Critical patent/SU611743A1/en
Application granted granted Critical
Publication of SU611743A1 publication Critical patent/SU611743A1/en

Description

(54) СПОСОБ ДУГОВОЙ СТЫКОВОЙ СВАРКИ АЛЮМИНИЕВЫХ СПЛАВОВ С ОТБОРТОВКОЙ(54) METHOD OF ARC BUTT WELDING OF ALUMINUM ALLOYS WITH CLEANING

SU762434390A 1976-12-27 1976-12-27 Method of arc butt-welding of aluminium alloys SU611743A1 (en)