SU606847A1 - Method of making arboreous concrete - Google Patents

Method of making arboreous concrete

Info

Publication number
SU606847A1
SU606847A1 SU762325686A SU2325686A SU606847A1 SU 606847 A1 SU606847 A1 SU 606847A1 SU 762325686 A SU762325686 A SU 762325686A SU 2325686 A SU2325686 A SU 2325686A SU 606847 A1 SU606847 A1 SU 606847A1
Authority
SU
USSR - Soviet Union
Prior art keywords
concrete
arboreous
making
buzhevich
literature
Prior art date
Application number
SU762325686A
Other languages
Russian (ru)
Inventor
Анатрлий Сергеевич Щербаков
Владимир Сергеевич Подчуфаров
Вячеслав Михайлович Бутерин
Анатолий Аркадьевич Гуревич
Original Assignee
Московский Лесотехнический Институт
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Московский Лесотехнический Институт filed Critical Московский Лесотехнический Институт
Priority to SU762325686A priority Critical patent/SU606847A1/en
Application granted granted Critical
Publication of SU606847A1 publication Critical patent/SU606847A1/en

Description

(54) СПОСОБ ИЗГОТОВЛЕНИЯ АРБОЛИТА(54) METHOD OF MANUFACTURING ARBOLIT

Прочность в первые сутки кг/смDurability in the first day kg / cm

Прочность в третьи сутки кг/смDurability in the third day kg / cm

Прочность в 28-е сутки кг/смDurability in the 28th day kg / cm

Биостойкость имп/минImpulses / min biostability

Скорость капилл рного подъема влаги (влажность образцов в %)The rate of capillary rise of moisture (moisture content in%)

При обработке органического заполнител  - древесной дробленки растворами хлористого кальци  и сернокислого алюмини  прочность полученного арболита равна 42,1 кг/смг Использование предлагаемого способа изготовлени  арболита позвол ет повысить прочность его на 43-64% по сравнению известным.When processing organic filler - wood shredded with calcium chloride and aluminum sulphate solutions, the strength of arbolite obtained is 42.1 kg / cmg. The use of the proposed method for the manufacture of arbolit improves its strength by 43-64% in comparison with the known.

Claims (2)

1.Бужевич Г. А. Арболит. Издательство литературы по строительству , М., 1968, с. 139-141.1.Buzhevich G. A. Arbolit. Publishing house of literature on construction, M., 1968, p. 139-141. 2.Бужевич Г.А. Технологи  и свойства новых видов и легких бетонов на пористых заполнител х . Издательство литературы по строительству , М., 1971, с. 185-193.2.Buzhevich G.A. Technologists and properties of new types and lightweight concrete on porous aggregates. Publishing house of literature on construction, M., 1971, p. 185-193.
SU762325686A 1976-02-23 1976-02-23 Method of making arboreous concrete SU606847A1 (en)