SU520784A1 - Method for remelting consumable electrode - Google Patents

Method for remelting consumable electrode Download PDF

Info

Publication number
SU520784A1
SU520784A1 SU742047478A SU2047478A SU520784A1 SU 520784 A1 SU520784 A1 SU 520784A1 SU 742047478 A SU742047478 A SU 742047478A SU 2047478 A SU2047478 A SU 2047478A SU 520784 A1 SU520784 A1 SU 520784A1
Authority
SU
USSR - Soviet Union
Prior art keywords
remelting
consumable electrode
electrode
remelting consumable
arc
Prior art date
Application number
SU742047478A
Other languages
Russian (ru)
Inventor
Б.Е. Петон
Б.И. Медовар
В.И. Лакомский
Г.Э. Цуканов
В.Г. Попов
И.В. Шейко
Л.В. Чекотило
А.И. Букало
Г.М. Григоренко
В.Н. Пахуридзе
Original Assignee
Ордена Ленина И Ордена Трудового Красного Знамени Институт Электросварки Им.Е.О.Патона
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ордена Ленина И Ордена Трудового Красного Знамени Институт Электросварки Им.Е.О.Патона filed Critical Ордена Ленина И Ордена Трудового Красного Знамени Институт Электросварки Им.Е.О.Патона
Priority to SU742047478A priority Critical patent/SU520784A1/en
Application granted granted Critical
Publication of SU520784A1 publication Critical patent/SU520784A1/en

Description

талла, в процессе переплава поддерживают отношение длины дугового промежутка к глубине шлаковой ванны, равным 0,04-0,5.in the process of remelting, the ratio of the length of the arc gap to the depth of the slag bath is maintained at 0.04-0.5.

2. Способ по п. 1, отл и ч а юш,и и с   тем, что в процессе переплава электрод перемеш .ают в зону дуги через флюсовый затвор .2. The method according to p. 1, exc and h and yush, and with the fact that in the process of remelting the electrode is mixed into the arc zone through a flux gate.

Claims (2)

Формула изобретенияClaim 1. Способ переплава расходуемого электрода в герметизированном рабочем пространстве дугой, горящей между электродом и шлаковой ванной, отличающийся тем, что, с целью повышения качества ме3 таяла, в процессе переплава поддерживают отношение длины дугового промежутка к глубине шлаковой ванны, равным 0,04—0,5.1. The method of remelting the consumable electrode in a sealed workspace by an arc burning between the electrode and the slag bath, characterized in that, in order to improve the quality of the metal, during the remelting, the ratio of the length of the arc gap to the depth of the slag bath is 0.04-0 ,5. 2. Способ по π. 1, отличающийся тем, что в процессе переплава электрод перемещают в зону дуги через флюсовый затвор.2. The method according to π. 1, characterized in that in the process of remelting, the electrode is moved into the arc zone through the flux gate.
SU742047478A 1974-08-09 1974-08-09 Method for remelting consumable electrode SU520784A1 (en)