SU514029A1 - Alloy for permanent magnets - Google Patents
Alloy for permanent magnetsInfo
- Publication number
- SU514029A1 SU514029A1 SU2066248A SU2066248A SU514029A1 SU 514029 A1 SU514029 A1 SU 514029A1 SU 2066248 A SU2066248 A SU 2066248A SU 2066248 A SU2066248 A SU 2066248A SU 514029 A1 SU514029 A1 SU 514029A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- alloy
- permanent magnets
- cobalt
- erbium
- thermal stability
- Prior art date
Description
(54) СПЛАВ ДЛЯ ПОСТОЯННЫХ МАГНИТОВ(54) ALLOY FOR PERMANENT MAGNETS
1one
Изобретение относитс к области изыскани новых магнитных сплавов на основ-е кобальта и, в частности, может примен тьс в приборах электронной техники.The invention relates to the field of finding new magnetic alloys based on cobalt and, in particular, can be used in electronic devices.
Известен сплав на основе кобальта, содержащий 35 вес. % самари . Недостатком указанного сплава вл етс пониженна термостабильность , что способствует снижению магнитных свойств в интервале температур от -100 до 150°С.Known alloy based on cobalt, containing 35 wt. % samari. The disadvantage of this alloy is its low thermal stability, which contributes to a decrease in the magnetic properties in the temperature range from -100 to 150 ° C.
Величина температурного коэффициента индукпии сплава в температурном интервале от -50 до +50°С и от -100 до +150°С составл ет соответственно ±30-10 5 и ±42-10-5 110(2The magnitude of the temperature coefficient of induction of the alloy in the temperature range from -50 to + 50 ° C and from -100 to + 150 ° C is respectively ± 30-10 5 and ± 42-10-5 110 (2
С целью повышени термостабильности при сохранении высоких значений максимальной магнитной энергии предлагаемый сплав дл посто нных магнитов дополнительно содержит гадолиний и эрбий при следующем соотношении компонентов, вес. %: Гадолиний5-9In order to increase thermal stability while maintaining high values of the maximum magnetic energy, the proposed alloy for permanent magnets additionally contains gadolinium and erbium in the following ratio of components, weight. %: Gadolinium5-9
Эрбий4,4-6,4Erbiy4,4-6,4
Самарий22,6-26,6Samarium22,6-26,6
КобальтОстальноеCobalt Else
Величина температурного коэффициента индукции сплава в интервале температурThe magnitude of the temperature coefficient of induction of the alloy in the temperature range
от -50 до 50°С и от -100 до 150°С составл ет соответственно -2-10 и -5-10 1/°С.from -50 to 50 ° C and from -100 to 150 ° C, respectively, -2-10 and -5-10 1 / ° C.
Основные характеристики посто нного магнита , приготовлемного из сплава, содержащего 24,6% самари , 7% гадолини , 5,4% эрби , кобальт остальное, следующие:The main characteristics of a permanent magnet prepared from an alloy containing 24.6% samarium, 7% gadolinium, 5.4% erbium, cobalt else are as follows:
Остаточна индукци , Гс7800Residual induction, GS7800
Коэрцитивна сила по намагничности , Э20000Coercive force by magnetization, E20000
Коэрцитивна сила по индукции , Э6000Coercive force by induction, E6000
Максимальна магнитна энерги , Гс-Э15-ЮMaximum Magnetic Energy, Gs-E15-U
Claims (1)