SU506631A1 - The mixture to obtain a refining and alloying melt - Google Patents
The mixture to obtain a refining and alloying meltInfo
- Publication number
- SU506631A1 SU506631A1 SU2053544A SU2053544A SU506631A1 SU 506631 A1 SU506631 A1 SU 506631A1 SU 2053544 A SU2053544 A SU 2053544A SU 2053544 A SU2053544 A SU 2053544A SU 506631 A1 SU506631 A1 SU 506631A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- refining
- mixture
- alloying melt
- alloying
- melt
- Prior art date
Description
3 ка, в нее введен углеродсодержащий материал с содержанием углерода не менее 30% при следующем соотношении компонентов, вес. %: Ванадийсодержащий шлак 35,0-65,05 . 4 Металл - восстановитель 3,0-11,0 Углеродсодержащий материал1,0-11,0 Плавиковый шпат0,5-5,0 ИзвестьОстальное.3 ka, it contains carbon-containing material with a carbon content of at least 30% with the following ratio of components, weight. %: Vanadium-containing slag 35.0-65.05. 4 Metal - reducing agent 3.0-11.0 Carbonaceous material1.0-11.0 Fluorspar 0.5-5.0 LimeEstal.