SU455385A1 - The method of training electrolytic capacitors - Google Patents
The method of training electrolytic capacitorsInfo
- Publication number
- SU455385A1 SU455385A1 SU1874630A SU1874630A SU455385A1 SU 455385 A1 SU455385 A1 SU 455385A1 SU 1874630 A SU1874630 A SU 1874630A SU 1874630 A SU1874630 A SU 1874630A SU 455385 A1 SU455385 A1 SU 455385A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- training
- voltage
- electrolytic capacitors
- capacitors
- sections
- Prior art date
Description
1one
Изобретение относитс к изтотовлению алюминиевых электроЛИтически.х конденсаторов и может использоватьс при их тренировке.The invention relates to the manufacture of aluminum electrolytic capacitors and can be used during their training.
Известиы способы тре НИ1ровки электролитических .конденсаторов, .преимущественно накопительных , основанные на включении секций конденсаторов на посто нное напр жение с последующим подъемом напр жени до величины тренировочного и выдержкой секций конденсаторов под этим напр жением.The methods of termination of electrolytic capacitors, mainly accumulative, are based on switching capacitor sections to a constant voltage followed by raising the voltage to the training value and keeping the capacitor sections under this voltage.
Однако эти способы и-меют большое врем тренировки и большое число пробитых конденcaTOipoB .However, these methods have a great workout time and a large number of punctured TOIPOBOBs.
Цель изобретени - уменьшение числа пробитых конденсаторов и сокращение времени тренировки.The purpose of the invention is to reduce the number of punched capacitors and reduce training time.
Эта цель достигаетс тем, что нодъе.м напр жени до .величины тренировочного осуществл ют нри токе, равном 20-50 ма на каждую секцию, делают перерыв в тренировке 20-30 , после чего выдерживают секции конденсаторов под тренировочным напр жением 3-б час.This goal is achieved by the fact that the node voltage to the values of the training is carried out at a current of 20-50 ma per section, a break in the training is 20-30, and then the sections of the capacitors are maintained under the training voltage of 3 bh .
СекЦ.ии накопительных алюминиевых электролитических конденсаторов помещают на тренировочный стенд, подают на них посто нное нанр жение, затем поднимают напр жение до тренировочн.ого при токе на секцию.Sec. And accumulative aluminum electrolytic capacitors are placed on a training stand, they are supplied with a constant voltage, then they raise the voltage to a training one at a current per section.
равном 20-50 ма. Продолжительность подъема напр жени не превышает нескольких часов . Затем тренировка прекращаетс и через 20-30 мнн вновь возобновл етс . После перерыва поднимают напр жение до тренировочного в течение нескольких .минут. Секции конденсаторов выдерживают при тренировочном напр жении 3-6 час. После этого тренировка считаетс законченной. Общее врем тренировки не превышает 8-10 час.equal to 20-50 ma. The duration of the voltage rise does not exceed several hours. Then, the training is stopped and after 20-30 hours the PL is resumed again. After a break, raise the voltage to a training for a few minutes. The sections of the capacitors are kept at a training voltage of 3-6 hours. After this, the training is considered complete. The total training time does not exceed 8-10 hours.
Предмет изобретени Subject invention
Способ тренировки электролитических конденсаторов. преим -щественно накопительных, основанный па включении секций конденсаторов на посто нное напр жение с последующим подъемом напр жени до величины тренировочного и выдержкой секций конденсаторов подэтим напр жением, отличающийс тем, что, с целью уменьшени числа пробитых конденсаторов п сокращени времени тренировки , -подъе.м напр жени до величины тренировочного осуществл ют при токе, равном 20-50 ма на каждую секцию, делают перерыв в тренировке 20-30 .ин, после чего выдерживают секции конденсаторов под тренировочным .напр жением 3-6 час.Method of training electrolytic capacitors. Advantageously, accumulatively based on switching capacitor sections to a constant voltage followed by raising the voltage to the training value and holding the section of capacitors under this voltage, characterized in that, in order to reduce the number of pierced capacitors and reduce the training time, podf. A voltage up to the training value is carried out at a current of 20-50 mA per section, a break in training 20-30 .in is made, after which the sections of the capacitors under the training voltage 3- 6 o'clock