SU396220A1 - DEVICE FOR TREATMENT OF DETAILS BY PRESSURE - Google Patents
DEVICE FOR TREATMENT OF DETAILS BY PRESSUREInfo
- Publication number
- SU396220A1 SU396220A1 SU1447985A SU1447985A SU396220A1 SU 396220 A1 SU396220 A1 SU 396220A1 SU 1447985 A SU1447985 A SU 1447985A SU 1447985 A SU1447985 A SU 1447985A SU 396220 A1 SU396220 A1 SU 396220A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- pressure
- details
- treatment
- coil
- welding
- Prior art date
Description
1one
Известно устройство дл обработки деталей давлением, содержащее нагревательный элемент , электромагнитный датчик температуры точки Кюри, выполненный в виде двух катушек , одна из которых св зана с источником переменного тока, а друга - с приводом давлени .A device for processing parts by pressure is known, which contains a heating element, an electromagnetic temperature sensor of the Curie point, made in the form of two coils, one of which is connected to an alternating current source and the other is driven by pressure.
Дл повышени качества издели при получении сварного соединени в предлагаемом устройстве катушки датчика расположены по разные стороны от свариваемого стыка, при этом катушка, св занна с приводом давлени , электрически св зана с нагревательным элементом.To improve the quality of the product upon receipt of the welded joint in the proposed device, the coil of the sensor is located on opposite sides of the welded joint, while the coil connected to the pressure drive is electrically connected to the heating element.
Использование в данном устройстве при сварке состо ни сверхпластичности материала , которое отличаетс увеличенной способностью к деформированию, позвол ет снизить усилие осадки и температуру нагрева.The use in this device of the state of superplasticity of a material, which is distinguished by an increased deformability, allows to reduce the slump force and the heating temperature.
Это позвол ет использовать менее мощное оборудование, т. е. снизить габариты и вес сварочных машин, что особенно важно, например , при сварке труб в полевых услови х или в несколько раз увеличить предельные размеры свариваемых деталей. Повышение пластичности в зоне соединени позвол ет также снизить припуски на выдавливание металла в грат, что особенно важно при сварке дорогосто ших и дефицитных сталей, например при сварке инструмента.This makes it possible to use less powerful equipment, i.e., reduce the size and weight of welding machines, which is especially important, for example, when welding pipes in field conditions or to increase the size limits of the parts to be welded several times. Increased ductility in the joint zone also allows reducing allowances for metal extrusion, which is especially important when welding expensive and scarce steels, for example when welding tools.
На чертеже схематично показано предлагаемое устройство.The drawing schematically shows the proposed device.
Устройство состоит из неподвижного упора / с возбуждающей катушкой 2, питаемой отThe device consists of a fixed stop / with excitation coil 2, fed from
источника переменного напр жени ; подвижного упора 3, соединенного с приводом 4 осадки . На подвижном упоре о закреплена измерительна катушка 5, св занна со входом усилител 6. Выход усилител 6 св зан с системой включени привода осадки и со входом блока 7 сравнени . Вход последнего также св зан с источником 8 эталонного напр жени , напр жение которого соответствует напр жению при качественно выполненном сварном соединении. Свариваемые детали 9 и 10 нагревают от генератора 11 индуктором 12.source of alternating voltage; movable stop 3 connected to the drive 4 precipitation. A measuring coil 5 connected to the input of the amplifier 6 is fixed on the movable stop. The output of the amplifier 6 is connected with the system for switching on the drive of the draft and with the input of the comparison unit 7. The input of the latter is also connected to the source 8 of the reference voltage, the voltage of which corresponds to the voltage at a well-made welded joint. Weldable parts 9 and 10 are heated from generator 11 by inductor 12.
Генератор // св зан с выходами усилител 6 и блока 7 сравнени .The generator // is connected to the outputs of amplifier 6 and unit 7 of the comparison.
Устройство работает следующим образом.The device works as follows.
Свариваемые детали 9 и 10, зажатые между упорами 1 и 3, нагревают индуктором 12 до температуры несколько выше интервала фазового превращени . Объемы металла, прилегающие к свариваемым поверхност м, расположенные под индуктором и нагретые несколько выше интервала фазового превращени , переход т в парамагнитное состо ние. На возбуждающую катушку 2 подают переменноеThe parts to be welded 9 and 10, clamped between the lugs 1 and 3, are heated by the inductor 12 to a temperature slightly above the phase transition interval. The volumes of the metal adjacent to the surfaces to be welded, located under the inductor and heated slightly above the phase transition interval, become paramagnetic. On the exciting coil 2 serves variable
напр жение.voltage.
В измерительной катушке 5, индуктивно с ней св занной, возникает ток, иропорциональный магнитной ироницаемости и величине парамагнитного объема в зоне соединени . По мере естественного остывани нарамагиитный объем нереходит в ферромагнитное состо ние , в результате чего резко увеличиваетс его магнитна проницаемость и, как результат , ток в измерительной катушке 5. Этот ток усиливаетс усилителем 6, выход которо:го св зан с системой включени привода 4 осадки и систеА10й кратковременного включени генератора // дл циклического изменени температуры с переходом через область фазовых превращений. Затем привод осадки осуществл ет деформирование остальных деталей в зоне соединени в состо нии сверхпластичности . После этого в блоке 7 сравниваютс два напр жени : с выхода усилител 5 и от источника 8 эталонного напр жени . Если по вл етс результирующа разница.In the measuring coil 5, inductively coupled to it, a current arises, proportional to the magnetic permeability and the magnitude of the paramagnetic volume in the junction zone. As the natural cooling cools, the paramagitic volume does not go to a ferromagnetic state, as a result of which its magnetic permeability increases and, as a result, the current in the measuring coil 5. This current is amplified by the amplifier 6, the output of which is connected to the drive system of system of short-term switching on of the generator // for cyclic temperature change with transition through the area of phase transformations. The sediment drive is then deformed of the remaining parts in the joint zone in the state of superplasticity. Thereafter, in block 7, two voltages are compared: from the output of the amplifier 5 and from the source 8 of the reference voltage. If the resulting difference appears.
свидетельствующа о наличии дефекта, например непровара, то она управл ет повторением циклов сварки. Отсутствие результирующей разницы свидетельствует об окончании цикла сварки.indicating a defect, such as lack of penetration, it controls the repetition of welding cycles. The absence of the resulting difference indicates the end of the welding cycle.
Предмет изобретени Subject invention
Устройство дл обработки деталей давлением , содержащее нагревательный элемент и электромагнитный датчик температуры точки Кюри, выполненный в виде двух катущек, одна из которых св зана с источником неременного тока, а друга - с приводом давлени , . отличающеес тем, что, с целью повыщени качества издели , преимущественно при получении сварного соединени , катушки датчика расположены но разные стороны от свариваемого стыка, при этом катущка, св занна с приводом давлени , электрически св зана с нагревательным элементом.A device for processing parts by pressure, containing a heating element and a Curie point temperature electromagnetic sensor, made in the form of two coils, one of which is connected to a non-temporal current source and the other is driven by pressure,. characterized in that, in order to increase the quality of the product, mainly in obtaining a welded joint, the coils of the sensor are located but different sides of the welded joint, while the coil associated with the pressure drive is electrically connected with the heating element.