Красноярский металлургический завод им. В.И.Ленина
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Красноярский металлургический завод им. В.И.ЛенинаfiledCriticalКрасноярский металлургический завод им. В.И.Ленина
Priority to SU4836192/02ApriorityCriticalpatent/SU1714865A1/en
Application grantedgrantedCritical
Publication of SU1714865A1publicationCriticalpatent/SU1714865A1/en
FIELD: thermal treatment of granular alloys. SUBSTANCE: method involves effectuating quench heating at heat rate of 50-250 C/hour with the following two-staged aging at first stage heating temperature of 200-300 C and holding time of 1-3 hours and at second stage heating temperature of 150-170 C and holding time of 12-18 hours. EFFECT: increased plasticity, high strength and improved structure stability of alloys. 1 tbl