SU148344A1 - Method for removing ferrous compounds from clays and kaolin - Google Patents

Method for removing ferrous compounds from clays and kaolin

Info

Publication number
SU148344A1
SU148344A1 SU695089A SU695089A SU148344A1 SU 148344 A1 SU148344 A1 SU 148344A1 SU 695089 A SU695089 A SU 695089A SU 695089 A SU695089 A SU 695089A SU 148344 A1 SU148344 A1 SU 148344A1
Authority
SU
USSR - Soviet Union
Prior art keywords
clays
kaolin
ferrous compounds
removing ferrous
sulfuric acid
Prior art date
Application number
SU695089A
Other languages
Russian (ru)
Inventor
Н.А. Герасимова
И.П. Романкевич
Original Assignee
Н.А. Герасимова
И.П. Романкевич
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Н.А. Герасимова, И.П. Романкевич filed Critical Н.А. Герасимова
Priority to SU695089A priority Critical patent/SU148344A1/en
Application granted granted Critical
Publication of SU148344A1 publication Critical patent/SU148344A1/en

Description

Известны способы удалени  железистых соединений из глин и каолинов в виде шликера путем обработки его раствором серной кислоты, с последующей промывкой сырьевой массы.Methods are known for removing ferrous compounds from clays and kaolins in the form of a slurry by treating it with a solution of sulfuric acid, followed by washing the raw mass.

Описываемый способ удалени  железистых соединений из глин и каолинов отличаетс  от известных тем, что шликер в смеси с 10%-ным раствором серной кислоты подвергают автоклавной обработке под давлением от 2 до 3 атм и последующей промывке водой.The described method of removing ferrous compounds from clays and kaolins differs from the known ones in that the slurry in a mixture with a 10% solution of sulfuric acid is subjected to autoclave treatment under a pressure of 2 to 3 atm and subsequent washing with water.

Такой способ удалени  железистых соединений из глин и каолинов позвол ет ускорить технологический процесс, а также снизить содержание окислов железа в глине и каолине и получить сьфье, пригодное дл  производства фарфоровых и фа нсовых изделий.Such a method of removing ferrous compounds from clays and kaolin allows for speeding up the technological process, as well as reducing the content of iron oxides in clay and kaolin, and obtaining cfu suitable for the production of porcelain and faience products.

Предлагаемый способ заключаетс  в следующем.The proposed method is as follows.

Глины и каолины обрабатывают 10%-пой серной кислотой. Раствор серной кислоты добавл ют к глинам и каолинам до получени  шликера консистенции густой сметаны. Затем шликер помещают в автоклав, где его выдерживают в течение 2 час под давлением 2-3 атм. При этом процессе железо переходит в растворимое сернокислое железо. После этого шликер промывают несколько раз водой и сернокислое железо удал ют с промывными водами.Clays and kaolins are treated with 10% sulfuric acid. A solution of sulfuric acid is added to the clays and kaolin until a slurry of thick sour cream is obtained. Then the slip is placed in an autoclave, where it is maintained for 2 hours under a pressure of 2-3 atm. In this process, iron passes into soluble iron sulphate. Thereafter, the slurry is washed several times with water and the iron sulfate is removed with wash water.

Предмет изобретени Subject invention

Способ удалени  железистых соединений из глин и каолинов в виде ш.ликера путем обработки его раствором серной кислоты, с последую, шей промывкой сырьевой массы, отличающийс  тем, что, с целью ускорени  технологического процесса, указанный шликер в смеси с 10/%-ным раствором серной кислоты подвергают автоклавной обработке под давлением от 2 до 3 атм и последующей промывке водой.A method of removing ferrous compounds from clays and kaolin in the form of a liquid by treating it with a solution of sulfuric acid, followed by washing the raw material mass, characterized in that, in order to accelerate the process, the slip is mixed with a 10 /% solution. sulfuric acid is subjected to autoclave treatment under pressure from 2 to 3 atm and subsequent washing with water.

SU695089A 1961-01-26 1961-01-26 Method for removing ferrous compounds from clays and kaolin SU148344A1 (en)