SU147731A1 - Способ гидрофобизации волокна - Google Patents

Способ гидрофобизации волокна

Info

Publication number
SU147731A1
SU147731A1 SU742868A SU742868A SU147731A1 SU 147731 A1 SU147731 A1 SU 147731A1 SU 742868 A SU742868 A SU 742868A SU 742868 A SU742868 A SU 742868A SU 147731 A1 SU147731 A1 SU 147731A1
Authority
SU
USSR - Soviet Union
Prior art keywords
fiber
waterproofing
hydrophobization
polyvinyl alcohol
hygroscopicity
Prior art date
Application number
SU742868A
Other languages
English (en)
Inventor
А.И. Меос
Л.А. Вольф
В.И. Полянская
нска В.И. Пол
Original Assignee
А.И. Меос
Л.А. Вольф
нска В.И. Пол
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by А.И. Меос, Л.А. Вольф, нска В.И. Пол filed Critical А.И. Меос
Priority to SU742868A priority Critical patent/SU147731A1/ru
Application granted granted Critical
Publication of SU147731A1 publication Critical patent/SU147731A1/ru

Description

Известны -способы гидрофобизации поливинилспиртового волокна, основанные на обработке термостабилизированного волокна альдегидами или полиальдегидами.
Волокно, гидрофобизированное указанными способами, недостаточно гигроскопично, обладает малой устойчивостью к агрессивным средам и не окрашиваетс  кислотно-протравными красител ми.
В данном изобретении, с целью улучшени  качества готового волокна , в частности повышени  гигроскопичности, устойчивости к агрессивным средам и способности окрашиватьс  кислотно-протравными красител ми , предлагаетс  волокно после предварительной термостабилизации обрабатывать раствором четыреххлористого титана в присутствии серной кислоты.
Полученное в соответствии с предлагаемым способом гидрофобизированное поливинилспиртовое волокно обладает прочностью 26-27 км разрывной длины и удлинением 28-30%. Аналогичные образцы волокна, подвергнутые гидрофобизации форм.альдегидом, имеют прочность 24-- 25 км разрывной длины и удилнение 30%.
Гигроскопичность волокна составл ет 7,5%, в то врем  как гигроскопичность волокна, обработанного известными способами, не превышает 3,5-5%.
Содержание титана в волокне, необходимое дл  его гидрофобизации , составл ет 2,5-3%.
Пример. Свежесформованное поливинилспиртовое волокно подвергают термостабилизации на воздухе при температуре 220° в течение 3-5 мин. Затем волокно погружают в водный раствор, содержащий 1,5-2% четыреххлористого титана и 10%-ную серную кислоту, и выдерживают при температуре 75-80° в течение 20-30 мин. Модуль ванны при этом составл ет 30-40. Обработанное волокно промывают и сушат известными способами.
SU742868A 1961-08-15 1961-08-15 Способ гидрофобизации волокна SU147731A1 (ru)