RU2247090C1 - Concrete mixture, additive for concrete mixture and cement modified with same additive (variants) - Google Patents

Concrete mixture, additive for concrete mixture and cement modified with same additive (variants) Download PDF

Info

Publication number
RU2247090C1
RU2247090C1 RU2003134908/03A RU2003134908A RU2247090C1 RU 2247090 C1 RU2247090 C1 RU 2247090C1 RU 2003134908/03 A RU2003134908/03 A RU 2003134908/03A RU 2003134908 A RU2003134908 A RU 2003134908A RU 2247090 C1 RU2247090 C1 RU 2247090C1
Authority
RU
Russia
Prior art keywords
additive
cement
concrete mixture
sand
superplasticizer
Prior art date
Application number
RU2003134908/03A
Other languages
Russian (ru)
Inventor
М.Е. Цельнер (RU)
М.Е. Цельнер
Original Assignee
Цельнер Михаил Ефимович
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Цельнер Михаил Ефимович filed Critical Цельнер Михаил Ефимович
Priority to RU2003134908/03A priority Critical patent/RU2247090C1/en
Application granted granted Critical
Publication of RU2247090C1 publication Critical patent/RU2247090C1/en

Abstract

FIELD: concrete composition, cement modified with additive and additive for concrete mixture.
SUBSTANCE: claimed additive contains silica component (e.g., tripoli or sodium methasilicate); superplasticizer; Lignopane with molecular weight of 10-50 kDa; air-entraining agent (e.g., neutralized air-entraining resin or wood saponificated resin) and additionally carboxymethyl cellulose. Additive is obtained by mixing of dry components in ratio (mass %): tripoli or sodium methasilicate (calculated as Si2O) 20-25; neutralized air-entraining resin or wood saponificated resin 0.005-0.01; superplasticizer 0-20; Lignopane 10-11; carboxymethyl cellulose 1-8. Said additive content is 0.3-2.5 calculated as cement mass. Concrete mixture may comprise (kg/m3) cement 250-600; filler 1590-2030; water 105-190; coarse filler (chip and/or gravel of grade 5-20 mm or 5-40 mm) and/or fine filler (sand of fineness not more than 5 mm). As fine filler at least one component selected from group containing quartz sand, sand from igneous formation, sand from metamorphic formation, haydite sand, and sand from blast-furnace dross is used. As coarse filler at least one component selected from group containing chip from igneous formation, chip from metamorphic formation, chip from sediment, chip from blast-furnace dross, etc. is used. According to one embodiment modified cement is obtained by dry agitation with 0.3-2.5 mass % of above mentioned additives. According to other embodiment modified cement is obtained by simultaneous milling of Portland cement clinker, gypsum and additive of said composition in amount of 0.3-1.0 %. Composition of present invention is useful in building industry for production of monolith and precast concrete and reinforced concrete construction, etc.
EFFECT: concrete mixture of increased water impermeability, freeze resistance, and strength.
11 cl, 3 tbl

Description

Изобретение относится к составам бетонной смеси и добавки для бетонной смеси и может найти применение в строительстве при изготовлении монолитных и сборных бетонных или железобетонных изделий и конструкций, в торкрет-массах, а также в нефтедобывающей отрасли при изготовлении тампонажных и изоляционных цементных материалов.The invention relates to compositions of concrete mixtures and additives for concrete mixtures and can find application in construction in the manufacture of monolithic and prefabricated concrete or reinforced concrete products and structures, in shotcrete masses, as well as in the oil industry in the manufacture of grouting and insulating cement materials.

Известна бетонная смесь, содержащая портландцемент М 500, кварцевый песок, гранитный щебень, воду и добавку - комплексный модификатор, содержащий, мас.%: дисперсный минеральный компонент на основе диоксида кремния из группы: горная порода, продукт газоочистки печей, выплавляющих кристаллический кремний и / или ферросиликохром, и / или силикокальций, и / или сжигающих каменный уголь, 51,9-94,1, соли органических кислот 4,7-45,5 и воду - остальное.Known concrete mixture containing Portland cement M 500, quartz sand, granite crushed stone, water and an additive - complex modifier containing, wt.%: Dispersed mineral component based on silicon dioxide from the group: rock, gas treatment product of furnaces smelting crystalline silicon and / or ferrosilicochrome, and / or silicocalcium, and / or burning coal, 51.9-94.1, salts of organic acids 4.7-45.5, and water - the rest.

Известна добавка для бетонной смеси - комплексный модификатор, содержащий, мас.%: дисперсный минеральный компонент на основе диоксида кремния из группы: горная порода, продукт газоочистки печей, выплавляющих кристаллический кремний и / или ферросиликохром, и / или силикокальций, и / или сжигающих каменный уголь, 51,9-94,1, соли органических кислот 4,7-45,5 и воду - остальное (патент РФ №2160723, 20.12.2000).A known additive for concrete mix is a complex modifier containing, wt.%: Dispersed mineral component based on silicon dioxide from the group: rock, gas treatment product of furnaces smelting crystalline silicon and / or ferrosilicochrome, and / or silicocalcium, and / or burning stone coal, 51.9-94.1, salts of organic acids 4.7-45.5, and water - the rest (RF patent No. 2160723, 20.12.2000).

Наиболее близким аналогом для заявленной бетонной смеси является бетонная смесь, включающая цемент, крупный и/или мелкий заполнитель - щебень из изверженных, метаморфических или осадочных горных пород, доменного шлака или шлаковой пемзы, керамзитовый гравий и/или песок, воду и добавку, содержащую мас.ч.: микрокремнезем или перлит, или диатомит, или трепел 50-65, суперпластификатор С-3 15-20, смолу нейтрализованную воздухововлекающую СНВ или гидрофобизирующий кремнийорганический порошок 0,1-0,5, Лигнопан с молекулярной массой 10-50 кДа 10-12, причем содержание добавки в бетонной смеси составляет 1-5% от массы цемента.The closest analogue to the claimed concrete mix is concrete mix, including cement, coarse and / or fine aggregate - crushed stone from igneous, metamorphic or sedimentary rocks, blast furnace slag or pumice slag, expanded clay gravel and / or sand, water and an additive containing mas .h .: silica fume or perlite, or diatomite, or tripoli 50-65, superplasticizer C-3 15-20, neutralized air-entraining START resin or hydrophobizing organosilicon powder 0.1-0.5, Lignopane with a molecular weight of 10-50 kDa 10 -12, with Erzhanov additives in the concrete mixture is 1-5% by weight of cement.

Наиболее близким аналогом для заявленной добавки является добавка для бетонной смеси, содержащая мас.ч.: микрокремнезем или перлит, или диатомит, или трепел 50-65, суперпластификатор С-3 15-20, смолу нейтрализованную воздухововлекающую СНВ или гидрофобизирующий кремнийорганический порошок 0,1-0,5, Лигнопан с молекулярной массой 10-50 кДа 10-12 (патент РФ №2177919, 10.01.2002).The closest analogue for the claimed additive is an additive for concrete mixture containing parts by weight of: silica fume or perlite, or diatomite, or tripoli 50-65, superplasticizer C-3 15-20, neutralized air-entraining START, or hydrophobizing silicone powder 0.1 -0.5, Lignopane with a molecular weight of 10-50 kDa 10-12 (RF patent No. 2177919, 01/10/2002).

Наиболее близким аналогом для заявленного по первому варианту цемента является цемент, модифицированный добавкой, содержащей кремнеземистый компонент - аморфный диоксид кремния, суперпластификатор С-3 (патент РФ №2167114, 20.05.2001).The closest analogue for the cement declared according to the first embodiment is cement modified with an additive containing a siliceous component - amorphous silicon dioxide, C-3 superplasticizer (RF patent No. 2167114, 05.20.2001).

Наиболее близким аналогом для заявленного по второму варианту цемента является цемент, модифицированный добавкой, полученный сухим помолом портландцементного клинкера, гипса и добавки кремнеземистого компонента - туфа, кварцевого песка, полевого шпатового песка, золы-уноса, хвостов обогащения руд, суперпластификатора С-3 и сульфата натрия или калия (патент РФ №2029749, 27.02.1995).The closest analogue for the cement declared in the second embodiment is cement modified with an additive obtained by dry grinding of Portland cement clinker, gypsum and an additive of a siliceous component - tuff, quartz sand, feldspar sand, fly ash, ore dressing tailings, C-3 superplasticizer and sulfate sodium or potassium (RF patent No. 2029749, 02.27.1995).

Задачей настоящего изобретения является повышение водонепроницаемости, морозостойкости, прочности.The objective of the present invention is to increase the water resistance, frost resistance, strength.

Указанная задача решается тем, что в бетонной смеси, включающей цемент, крупный и/или мелкий заполнитель, воду и добавку, содержащую кремнеземистый компонент, суперпластификатор С-3, воздухововлекающую добавку, Лигнопан с молекулярной массой 10-50 кДа, указанная добавка в качестве кремнеземистого компонента содержит трепел или метасиликат натрия, в качестве воздухововлекающей добавки - смолу нейтрализованную воздухововлекающую СНВ или смолу древесную омыленную СДО, дополнительно - карбоксиметилцеллюлозу КМЦ и приготовлена перемешиванием сухих компонентов при следующем их соотношении, мас.ч.:This problem is solved by the fact that in a concrete mixture comprising cement, coarse and / or fine aggregate, water and an additive containing a siliceous component, S-3 superplasticizer, air-entraining additive, Lignopane with a molecular weight of 10-50 kDa, the specified additive as a siliceous the component contains tripoli or sodium metasilicate, as an air-entraining additive - neutralized air-entraining START resin or saponified wood tar, additionally - CMC carboxymethyl cellulose and mixing is prepared m of dry components in the following ratio, parts by weight:

трепел или метасиликат натрия в пересчете на SiО2 20-25Tripoli or sodium metasilicate in terms of SiO 2 20-25

суперпластификатор С-3 0-20superplasticizer S-3 0-20

указанный Лигнопан 10-11specified Lignopan 10-11

СНВ или СДО 0,005-0,01START or LMS 0.005-0.01

КМЦ 1-8,CMC 1-8,

а содержание добавки составляет 0,3-2,5 мас.% от массы цемента. Причем бетонная смесь может содержать указанные компоненты при следующем соотношении, кг/м3: цемент 250-600, заполнитель 1590-2030, вода 105-190, заполнитель крупный и/или мелкий, в качестве заполнителя крупного - щебень и/или гравий, заполнитель крупный фракции 5-20 или 5-40 мм, в качестве заполнителя мелкого - песок крупностью не более 5 мм, в качестве заполнителя мелкого - по крайней мере, один компонент из группы: кварцевый песок, песок из изверженных горных пород, песок из метаморфических горных пород, песок керамзитовый, песок из доменного шлака, в качестве заполнителя крупного - по крайней мере, один компонент из группы: щебень из изверженных горных пород, щебень из метаморфических горных пород, щебень из осадочных горных пород, щебень из доменного шлака, керамзитовый гравий, щебень из шлаковой пемзы.and the content of the additive is 0.3-2.5 wt.% by weight of cement. Moreover, the concrete mixture may contain these components in the following ratio, kg / m 3 : cement 250-600, aggregate 1590-2030, water 105-190, aggregate coarse and / or fine, as aggregate coarse gravel and / or gravel, aggregate coarse fractions of 5-20 or 5-40 mm, as a fine aggregate - sand with a grain size of not more than 5 mm, as a fine aggregate - at least one component from the group: quartz sand, sand from igneous rocks, sand from metamorphic mountain rocks, expanded clay sand, sand from blast furnace slag, as TBE large aggregate - of at least one component from the group: crushed eruptive rocks, rubble from metamorphic rocks, rubble from sedimentary rocks, rubble from blast furnace slag, expanded clay gravel, crushed stone of slag pumice.

Указанная задача решается также тем, что в цементе, модифицированном добавкой, содержащей кремнеземистый компонент и суперпластификатор С-3, указанная добавка содержит в качестве кремнеземистого компонента трепел или метасиликат натрия и дополнительно - Лигнопан с молекулярной массой 10-50 кДа, смолу нейтрализованную воздухововлекающую СНВ или смолу древесную омыленную СДО и карбоксиметилцеллюлозу КМЦ, а цемент получен сухим перемешиванием с 0,3-2,5 мас.% от его массы указанной добавки при следующем соотношении ее компонентов, мас.ч.:This problem is also solved by the fact that in cement modified with an additive containing a siliceous component and C-3 superplasticizer, this additive contains tripoli or sodium metasilicate as a siliceous component and additionally Lignopane with a molecular weight of 10-50 kDa, a neutralized air-entraining START or saponified wood-based resin and CMC carboxymethyl cellulose, and cement obtained by dry mixing with 0.3-2.5 wt.% of its weight of the specified additives in the following ratio of its components, parts by weight:

трепел или метасиликат натрия в пересчете на SiО2 20-25Tripoli or sodium metasilicate in terms of SiO 2 20-25

суперпластификатор С-3 0-20superplasticizer S-3 0-20

указанный Лигнопан 10-11specified Lignopan 10-11

СНВ или СДО 0,005-0,01START or LMS 0.005-0.01

КМЦ 1-8CMC 1-8

Указанная задача решается также тем, что по второму варианту в цементе, модифицированном добавкой, полученном совместным сухим помолом портландцементного клинкера, гипса и добавки, содержащей кремнеземистый компонент и суперпластификатор С-3, указанная добавка содержит в качестве кремнеземистого компонента трепел или метасиликат натрия и дополнительно - Лигнопан с молекулярной массой 10-50 кДа, смолу нейтрализованную воздухововлекающую СНВ или смолу древесную омыленную СДО и карбоксиметилцеллюлозу КМЦ при следующем соотношении компонентов, мас.ч:This problem is also solved by the fact that according to the second variant, in cement modified with an additive obtained by joint dry grinding of Portland cement clinker, gypsum and an additive containing a siliceous component and C-3 superplasticizer, this additive contains tripoli or sodium metasilicate as a siliceous component and additionally - Lignopane with a molecular weight of 10-50 kDa, a neutralized air-entraining START resin or wood-saponified resin SDO and CMC carboxymethyl cellulose in the following ratio of entov, parts by weight:

трепел или метасиликат натрия в пересчете на SiO2 20-25Tripoli or sodium metasilicate in terms of SiO 2 20-25

суперпластификатор С-3 0-20superplasticizer S-3 0-20

указанный Лигнопан 10-11specified Lignopan 10-11

СНВ или СДО 0,005-0,01START or LMS 0.005-0.01

КМЦ 1-8,CMC 1-8,

а содержание добавки составляет 0,3-1,0 мас.% от массы цемента.and the content of the additive is 0.3-1.0 wt.% by weight of cement.

Указанная задача решается также тем, что добавка для бетонной смеси, содержащая кремнеземистый компонент, суперпластификатор С-3, воздухововлекающую добавку, Лигнопан с молекулярной массой 10-50 кДа, содержит в качестве кремнеземистого компонента трепел или метасиликат натрия, в качестве воздухововлекающей добавки смолу нейтрализованную воздухововлекающую СНВ или смолу древесную омыленную СДО и дополнительно - карбоксиметилцеллюлозу КМЦ и приготовлена перемешиванием сухих компонентов при следующем их соотношении, мас.ч.:This problem is also solved by the fact that the concrete mixture additive containing a siliceous component, S-3 superplasticizer, an air-entraining additive, Lignopan with a molecular weight of 10-50 kDa, contains tripoli or sodium metasilicate as a siliceous component, and a neutralized airborne resin as an air-entraining additive START or saponified wood tar, and additionally CMC carboxymethyl cellulose and prepared by mixing dry components in the following ratio, parts by weight:

трепел или метасиликат натрия в пересчете на SiO2 20-25Tripoli or sodium metasilicate in terms of SiO 2 20-25

суперпластификатор С-3 0-20superplasticizer S-3 0-20

указанный Лигнопан 10-11specified Lignopan 10-11

СНВ или СДО 0,005-0,01START or LMS 0.005-0.01

КМЦ 1-8CMC 1-8

В бетонной смеси может быть использовано:In concrete mix can be used:

Вяжущее - портландцемент, пуццолановый портландцемент, шлакопортландцемент, быстротвердеющий портландцемент, глиноземистый цемент в количестве 250-600 кг/м3;Astringent - Portland cement, pozzolanic portland cement, slag Portland cement, quick-setting Portland cement, alumina cement in an amount of 250-600 kg / m 3 ;

Крупный заполнитель фракций 5-10 мм или 5-20 мм, или 5-40 мм по крайней мере, один компонент из группы, включающей: щебень из изверженных горных пород, из метаморфических горных пород, из осадочных горных пород, из отвального или гранулированного шлака, шлаковой пемзы, керамзитовый гравий;Coarse aggregate of fractions 5-10 mm or 5-20 mm, or 5-40 mm, at least one component from the group including: crushed stone from igneous rocks, from metamorphic rocks, from sedimentary rocks, from dump or granulated slag , slag pumice, expanded clay gravel;

Мелкий заполнитель фракции не более 5 мм - по крайней мере, один компонент из группы, включающей: кварцевый песок, кварцево-полевошпатный песок, известняковый песок, песок из изверженных или метаморфических горных пород, из доменного шлака, песок керамзитовый.Fine aggregate of a fraction of not more than 5 mm is at least one component from the group comprising: quartz sand, quartz-feldspar sand, limestone sand, sand from igneous or metamorphic rocks, from blast furnace slag, expanded clay sand.

Общее содержание заполнителя в составе бетонной смеси 1500-2030 кг/м3;The total content of aggregate in the composition of the concrete mixture is 1500-2030 kg / m 3 ;

Вода в количестве 105-190 кг/м3.Water in an amount of 105-190 kg / m 3 .

Соотношение компонентов в составе бетонной смеси может варьироваться в широких пределах в зависимости от требуемой марки бетона и используемого способа формования изделий.The ratio of the components in the composition of the concrete mix can vary widely depending on the required grade of concrete and the method of molding products used.

Для приготовления добавки используют:To prepare the additive, use:

Трепел Вурнарского месторожденияTripoli Vurnarsky field

Лигнопан - модифицированные электролитами лигносульфонаты с молекулярной массой 10-50 кДа по ТУ 2601-002-20127879-96Lignopan - lignosulfonates modified with electrolytes with a molecular weight of 10-50 kDa according to TU 2601-002-20127879-96

Смола нейтрализованная воздухововлекающая СНВ по ТУ 810575-74Neutralized air-entraining START resin according to TU 810575-74

Смола древесная омыленная СДОSaponified wood resin SDO

Суперпластификатор С-3 по ТУ 6-36-0204229-625-90Superplasticizer S-3 according to TU 6-36-0204229-625-90

КарбоксиметилцеллюлозаCarboxymethyl cellulose

Метасиликат натрия - кристаллический порошокSodium Metasilicate - Crystalline Powder

Добавку готовят путем перемешивания вышеуказанных сухих компонентов.The additive is prepared by mixing the above dry components.

Составы добавки приведены в таблице 1.The compositions of the additives are shown in table 1.

Таблица 1Table 1 компонентыComponents содержание мас.ч.content by weight   11 22 33 44 трепел(в пересчете на SiO2)Tripoli (in terms of SiO 2 ) 20twenty     2525 метасиликат натрия(вsodium metasilicate (in -- 2525 20twenty -- пересчете на SiO2)in terms of SiO 2 )         СНВSTART 0,0060.006 0,010.01   0,0080.008 СДОFROM TO -- -- 0,0070.007 -- С-3S-3 1010 55 -- 20twenty ЛигнопанLignopan 1010 11eleven 11eleven 1010 кмцkmts 44 11 88 66

Добавку используют в количестве 0,3-2,5% от массы цемента.The additive is used in an amount of 0.3-2.5% by weight of cement.

Результаты испытаний цемента, модифицированного добавкой, приведены в таблице 2.The test results of cement modified with the additive are shown in table 2.

Составы бетонной смеси и свойства бетона с указанной добавкой приведены в таблице 3.The composition of the concrete mixture and the properties of concrete with the specified additive are shown in table 3.

Приведенные результаты испытаний свидетельствуют о высокой эффективности добавки, использование которой в бетоне позволяет получить пластифицированный бетон с высокими физико-механическими характеристиками, в том числе с повышенной водонепроницаемостью, прочностью и морозостойкостью.The test results presented indicate the high efficiency of the additive, the use of which in concrete allows to obtain plasticized concrete with high physical and mechanical characteristics, including with increased water resistance, strength and frost resistance.

Результаты испытаний цемента, модифицированного добавкой “Биотех-НМ” Использован цемент Михайловский ПЦ 400 Д20.Test results of cement modified with Biotech-NM additive. Mikhailovsky PC 400 D20 cement was used.

Таблица 2table 2 № п/пNo. p / p содержание добавки, мас.% от цементаthe content of the additive, wt.% from cement Прочность при сжатии в возрасте 28 суток МПАCompression strength at the age of 28 days MPA 11 00 32,132.1 22 0,50.5 41,441,4 33 0,50.5 44,744.7 44 1,01,0 47,547.5 55 1,01,0 50,350.3 66 1,51,5 54,754.7 77 1,51,5 54,854.8 88 2,02.0 59,959.9 9nine 2,52,5 64,864.8 Примечание:
В примерах 2,4,6,9 использовался цемент, полученный смешением с добавкой “ Биотех-НМ”
Note:
In examples 2,4,6,9 used cement obtained by mixing with the additive “Biotech-NM”

В примерах 3, 5, 7 использовался цемент, полученный совместным помолом клинкера с добавкой “Биотех-НМ”. В примерах 2,5 использовалась добавка Биотех-НМ состава 1, приведенного в таблице 1. В примерах 3, 4 использовалась добавка Биотех-НМ состава 2, приведенного в таблице 1. В примерах 6, 7, использовалась добавка Биотех-НМ состава 3, приведенного в таблице 1. В примерах 8,9 использовалась добавка Биотех-НМ состава 4, приведенного в таблице 1.In examples 3, 5, 7, cement was used, obtained by joint grinding of clinker with the addition of “Biotech-NM”. In examples 2.5, we used an additive of Biotech-NM composition 1, shown in table 1. In examples 3, 4 we used an additive of Biotech-NM composition 2, shown in table 1. In examples 6, 7, we used an additive of Biotech-NM composition 3, shown in table 1. In examples 8.9 used the additive Biotech-NM composition 4, are shown in table 1.

Figure 00000001
Figure 00000002
Figure 00000001
Figure 00000002

Claims (11)

1. Бетонная смесь, включающая цемент, заполнитель, воду и добавку, содержащую кремнеземистый компонент, суперпластификатор С-3, воздухововлекающую добавку, Лигнопан с молекулярной массой 10-50 кДа, отличающаяся тем, что добавка в качестве кремнеземистого компонента содержит трепел или метасиликат натрия, в качестве воздухововлекающей добавки - смолу нейтрализованную воздухововлекающую СНВ или смолу древесную омыленную СДО, дополнительно карбоксиметилцеллюлозу КМЦ и приготовлена перемешиванием сухих компонентов при следующем их соотношении, мас.ч.:1. A concrete mixture comprising cement, aggregate, water and an additive containing a siliceous component, a C-3 superplasticizer, an air-entraining additive, Lignopane with a molecular weight of 10-50 kDa, characterized in that the additive contains tripoli or sodium metasilicate as a siliceous component, as an air-entraining additive - neutralized air-entraining START resin or saponified wood-based resin, additionally CMC carboxymethyl cellulose and prepared by mixing dry components in the following ratio SRI, in parts by weight .: Трепел или метасиликат натрия в пересчете на SiО2 20-25Tripoli or sodium metasilicate in terms of SiO 2 20-25 Суперпластификатор С-3 0-20Superplasticizer S-3 0-20 Указанный Лигнопан 10-11Specified Lignopan 10-11 СНВ или СДО 0,005-0,01START or LMS 0.005-0.01 КМЦ 1-8CMC 1-8 причем содержание добавки составляет 0,3- 2,5 мас.% от цемента.moreover, the content of the additive is 0.3 to 2.5 wt.% from cement. 2. Бетонная смесь по п.1, отличающаяся тем, что она содержит цемент, заполнитель и воду при следующем соотношении, кг/м:2. The concrete mixture according to claim 1, characterized in that it contains cement, aggregate and water in the following ratio, kg / m: Цемент 250-600Cement 250-600 Заполнитель 1590-2030Placeholder 1590-2030 Вода 105-190Water 105-190 3. Бетонная смесь по п.1 или 2, отличающаяся тем, что она содержит заполнитель крупный и/или мелкий.3. The concrete mixture according to claim 1 or 2, characterized in that it contains a large and / or small aggregate. 4. Бетонная смесь по любому из пп.1-3, отличающаяся тем, что она содержит в качестве заполнителя крупного щебень и/или гравий.4. Concrete mixture according to any one of claims 1 to 3, characterized in that it contains coarse gravel and / or gravel as an aggregate. 5. Бетонная смесь по п.3 или 4, отличающаяся тем, что она содержит заполнитель крупный фракции 5-20 или 5-40 мм.5. The concrete mixture according to claim 3 or 4, characterized in that it contains a coarse aggregate fraction 5-20 or 5-40 mm 6. Бетонная смесь по любому из пп.3-5, отличающаяся тем, что она содержит в качестве заполнителя мелкого песок крупностью не более 5 мм.6. Concrete mixture according to any one of claims 3 to 5, characterized in that it contains fine sand with a particle size of not more than 5 mm as aggregate. 7. Бетонная смесь по любому из пп.3-6, отличающаяся тем, что она содержит в качестве заполнителя мелкого, по крайней мере, один компонент из группы: кварцевый песок, песок из изверженных горных пород, песок из метаморфических горных пород, песок керамзитовый, песок из доменного шлака.7. Concrete mixture according to any one of claims 3 to 6, characterized in that it contains at least one component from the group as fine aggregate: quartz sand, sand from igneous rocks, sand from metamorphic rocks, expanded clay sand sand from blast furnace slag. 8. Бетонная смесь по любому из пп.3-7, отличающаяся тем, что она содержит в качестве заполнителя крупного, по крайней мере, один компонент из группы: щебень из изверженных горных пород, щебень из метаморфических горных пород, щебень из осадочных горных пород, щебень из доменного шлака, керамзитовый гравий, щебень из шлаковой пемзы.8. Concrete mixture according to any one of claims 3 to 7, characterized in that it contains a large aggregate of at least one component from the group: crushed stone from igneous rocks, crushed stone from metamorphic rocks, crushed stone from sedimentary rocks , crushed stone from blast furnace slag, expanded clay gravel, crushed stone from slag pumice. 9. Цемент, модифицированный добавкой, содержащей кремнеземистый компонент и суперпластификатор С-3, отличающийся тем, что указанная добавка содержит в качестве кремнеземистого компонента трепел или метасиликат натрия и дополнительно - Лигнопан с молекулярной массой 10-50 кДа, смолу воздухововлекающую нейтрализованную СНВ или смолу древесную омыленную СДО, карбоксиметилцеллюлозу КМЦ и получен сухим перемешиванием с 0,3-2,5 мас.% от его массы указанной добавки при следующем соотношении ее компонентов, мас.%:9. Cement modified with an additive containing a siliceous component and C-3 superplasticizer, characterized in that the additive contains tripoli or sodium metasilicate as a siliceous component and, additionally, Lignopane with a molecular weight of 10-50 kDa, an air-entraining neutralized START resin or wood resin saponified SDO, CMC carboxymethyl cellulose and obtained by dry mixing with 0.3-2.5 wt.% of its weight of the specified additives in the following ratio of its components, wt.%: Трепел или метасиликат натрия в пересчете на SiО2 20-25Tripoli or sodium metasilicate in terms of SiO 2 20-25 Суперпластификатор С-3 0-20Superplasticizer S-3 0-20 Указанный Лигнопан 10-11Specified Lignopan 10-11 СНВ или СДО 0,005-0,01START or LMS 0.005-0.01 КМЦ 1-8CMC 1-8 10. Цемент, модифицированный добавкой, полученный совместным сухим помолом портландцементного клинкера, гипса и добавки, содержащей кремнеземистый компонент и суперпластификатор С-3, отличающийся тем, что указанная добавка содержит в качестве кремнеземистого компонента трепел или метасиликат натрия и дополнительно - Лигнопан с молекулярной массой 10-50 кДа, смолу нейтрализованную воздухововлекающую СНВ или смолу древесную омыленную СДО, карбоксиметилцеллюлозу КМЦ при следующем соотношении компонентов, мас.%:10. Cement modified by the additive obtained by co-dry grinding of Portland cement clinker, gypsum and an additive containing a siliceous component and C-3 superplasticizer, characterized in that the additive contains tripoli or sodium metasilicate as a siliceous component and additionally Lignopane with a molecular weight of 10 -50 kDa, neutralized air-entraining START resin or wood-saponified resin SDO, CMC carboxymethyl cellulose in the following ratio, wt.%: Трепел или метасиликат натрия в пересчете на SiO2 20-25Tripoli or sodium metasilicate in terms of SiO 2 20-25 Суперпластификатор С-3 0-20Superplasticizer S-3 0-20 Указанный Лигнопан 10-11Specified Lignopan 10-11 СНВ или СДО 0,005-0,01START or LMS 0.005-0.01 КМЦ 1-8CMC 1-8 причем содержание добавки составляет 0,3-1,0 мас.% от массы цемента.moreover, the content of the additive is 0.3-1.0 wt.% by weight of cement. 11. Добавка для бетонной смеси, содержащая кремнеземистый компонент, суперпластификатор С-3, воздухововлекающую добавку, Лигнопан с молекулярной массой 10-50 кДа, отличающаяся тем, что она содержит в качестве кремнеземистого компонента трепел или порошок метасиликата натрия, в качестве воздухововлекающей добавки смолу нейтрализованную воздухововлекающую или смолу древесную омыленную и дополнительно карбоксиметилцеллюлозу КМЦ и приготовлена перемешиванием сухих компонентов при следующем их соотношении, мас.ч.:11. Additive for concrete mixture containing a siliceous component, C-3 superplasticizer, air-entraining additive, Lignopan with a molecular weight of 10-50 kDa, characterized in that it contains tripoli or sodium metasilicate powder as a siliceous component, neutralized resin as an air-entraining additive saponified air or wood resin and optionally CMC carboxymethyl cellulose and prepared by mixing dry components in the following ratio, wt.h .: Трепел или метасиликат натрия в пересчете на SiO2 20-25Tripoli or sodium metasilicate in terms of SiO 2 20-25 Суперпластификатор С-3 0-20Superplasticizer S-3 0-20 Указанный Лигнопан 10-11Specified Lignopan 10-11 СНВ или СДО 0,005-0,01START or LMS 0.005-0.01 КМЦ 1-8CMC 1-8 причем содержание добавки составляет 0,3-2,5 мас.% от цемента.moreover, the content of the additive is 0.3-2.5 wt.% from cement.
RU2003134908/03A 2003-12-03 2003-12-03 Concrete mixture, additive for concrete mixture and cement modified with same additive (variants) RU2247090C1 (en)