RU2007142913A - METHOD FOR REPAIR OF PUMP BAR - Google Patents

METHOD FOR REPAIR OF PUMP BAR Download PDF

Info

Publication number
RU2007142913A
RU2007142913A RU2007142913/03A RU2007142913A RU2007142913A RU 2007142913 A RU2007142913 A RU 2007142913A RU 2007142913/03 A RU2007142913/03 A RU 2007142913/03A RU 2007142913 A RU2007142913 A RU 2007142913A RU 2007142913 A RU2007142913 A RU 2007142913A
Authority
RU
Russia
Prior art keywords
heads
shells
sleeve
sections
mating surfaces
Prior art date
Application number
RU2007142913/03A
Other languages
Russian (ru)
Other versions
RU2359104C2 (en
Inventor
Николай Александрович Богатов (RU)
Николай Александрович Богатов
Original Assignee
Николай Александрович Богатов (RU)
Николай Александрович Богатов
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Николай Александрович Богатов (RU), Николай Александрович Богатов filed Critical Николай Александрович Богатов (RU)
Priority to RU2007142913/03A priority Critical patent/RU2359104C2/en
Publication of RU2007142913A publication Critical patent/RU2007142913A/en
Application granted granted Critical
Publication of RU2359104C2 publication Critical patent/RU2359104C2/en

Abstract

Способ ремонта штанг насосных (ШН), включающий радиационный контроль, очистку их поверхности от отложений парафина, соли и асфальтенов, визуальный и приборный контроль, обрезку головок и участков ШН с недопустимыми дефектами, высадку (изготовление) новых головок, термическую обработку, горячую правку, охлаждение, дробеструйную обработку тела ШН, механическую обработку головок штанг, отличающийся тем, что участки ШН с недопустимыми дефектами не обрезают, а им придают повышенные прочность и коррозионную стойкость наложением на дефектные участки обечаек, сопрягаемые поверхности которых заранее очищают до металлического блеска, наносят на эти поверхности клей с высокой адгезивной способностью, после чего обечайки сдавливают до плотного соприкосновения сопрягаемых поверхностей обечаек и ШН, а после определенной выдержки давление на обечайки снимают и создают условия для полимеризации клея.A method of repairing sucker rods (SH), including radiation monitoring, cleaning their surface from deposits of paraffin, salt and asphaltenes, visual and instrument control, cutting heads and sections of SH with unacceptable defects, planting (manufacturing) of new heads, heat treatment, hot dressing, cooling, bead-blasting of the body of the ШН, machining of the heads of the rods, characterized in that the sections of the ШН with unacceptable defects are not cut, and they are given increased strength and corrosion resistance by superimposing on defective ASTK shells, mating surfaces beforehand purified to metallic luster is applied onto the surface of adhesive with high adhesive ability, whereupon the sleeve is compressed to the dense contact between the mating surfaces of the shells and SHN, and after a certain holding pressure on the sleeve is removed and create conditions for polymerization of the glue.

Claims (1)

Способ ремонта штанг насосных (ШН), включающий радиационный контроль, очистку их поверхности от отложений парафина, соли и асфальтенов, визуальный и приборный контроль, обрезку головок и участков ШН с недопустимыми дефектами, высадку (изготовление) новых головок, термическую обработку, горячую правку, охлаждение, дробеструйную обработку тела ШН, механическую обработку головок штанг, отличающийся тем, что участки ШН с недопустимыми дефектами не обрезают, а им придают повышенные прочность и коррозионную стойкость наложением на дефектные участки обечаек, сопрягаемые поверхности которых заранее очищают до металлического блеска, наносят на эти поверхности клей с высокой адгезивной способностью, после чего обечайки сдавливают до плотного соприкосновения сопрягаемых поверхностей обечаек и ШН, а после определенной выдержки давление на обечайки снимают и создают условия для полимеризации клея.A method of repairing sucker rods (SH), including radiation monitoring, cleaning their surface from deposits of paraffin, salt and asphaltenes, visual and instrument control, cutting heads and sections of SH with unacceptable defects, planting (manufacturing) of new heads, heat treatment, hot dressing, cooling, bead-blasting of the body of the ШН, machining of the heads of the rods, characterized in that the sections of the ШН with unacceptable defects are not cut, and they are given increased strength and corrosion resistance by superimposing on defective ASTK shells, mating surfaces beforehand purified to metallic luster is applied onto the surface of adhesive with high adhesive ability, whereupon the sleeve is compressed to the dense contact between the mating surfaces of the shells and SHN, and after a certain holding pressure on the sleeve is removed and create conditions for polymerization of the glue.
RU2007142913/03A 2007-11-22 2007-11-22 Maintenance method of pumping rod RU2359104C2 (en)