RU2002108949A - The method of restoration of the rolling roll - Google Patents

The method of restoration of the rolling roll

Info

Publication number
RU2002108949A
RU2002108949A RU2002108949/02A RU2002108949A RU2002108949A RU 2002108949 A RU2002108949 A RU 2002108949A RU 2002108949/02 A RU2002108949/02 A RU 2002108949/02A RU 2002108949 A RU2002108949 A RU 2002108949A RU 2002108949 A RU2002108949 A RU 2002108949A
Authority
RU
Russia
Prior art keywords
temperature
restoration
rolling roll
surfacing
roll
Prior art date
Application number
RU2002108949/02A
Other languages
Russian (ru)
Other versions
RU2218220C1 (en
Inventor
Николай Борисович Скорохватов
Владимир Васильевич Глухов
Александр Васильевич Голованов
Владимир Сергеевич Смирнов
Владимир Федорович Соболев
Александр Иванович Трайно
Олег Вячеславович Тяпаев
Original Assignee
Открытое акционерное общество "Северсталь"
Filing date
Publication date
Application filed by Открытое акционерное общество "Северсталь" filed Critical Открытое акционерное общество "Северсталь"
Priority to RU2002108949A priority Critical patent/RU2218220C1/en
Priority claimed from RU2002108949A external-priority patent/RU2218220C1/en
Publication of RU2002108949A publication Critical patent/RU2002108949A/en
Application granted granted Critical
Publication of RU2218220C1 publication Critical patent/RU2218220C1/en

Links

Claims (1)

Способ восстановления прокатного валка, включающий его нагрев до температуры 400-460°С, многослойную электродуговую наплавку и термическую обработку наплавленного слоя, отличающийся тем, что после наплавки первых 2-3 слоев валок охлаждают до температуры 250-300°С, при которой осуществляют наплавку остальных слоев, а термическую обработку наплавленного валка ведут путем нагрева до температуры 500-600°С с выдержкой при этой температуре в течение 8-10 ч и последующего охлаждения до температуры 50-100°С со скоростью не выше 100°С/ч.A method of restoring a roll, including heating it to a temperature of 400-460 ° C, multilayer electric arc surfacing and heat treatment of the deposited layer, characterized in that after surfacing the first 2-3 layers, the rolls are cooled to a temperature of 250-300 ° C, at which surfacing is carried out the remaining layers, and the heat treatment of the deposited roll is carried out by heating to a temperature of 500-600 ° C with holding at this temperature for 8-10 hours and subsequent cooling to a temperature of 50-100 ° C at a speed not exceeding 100 ° C / h.
RU2002108949A 2002-04-08 2002-04-08 Method of building up rolls RU2218220C1 (en)