RU1789085C - Composition for protection dried sea bed against wind erosion - Google Patents
Composition for protection dried sea bed against wind erosionInfo
- Publication number
- RU1789085C RU1789085C SU894675174A SU4675174A RU1789085C RU 1789085 C RU1789085 C RU 1789085C SU 894675174 A SU894675174 A SU 894675174A SU 4675174 A SU4675174 A SU 4675174A RU 1789085 C RU1789085 C RU 1789085C
- Authority
- RU
- Russia
- Prior art keywords
- composition
- wind erosion
- sea bed
- against wind
- dried sea
- Prior art date
Abstract
Сущность изобретени : используют состав , содержащий, мас.%: известь 1,5; олифу или стеарат кальци 0,0075-0,2250; воду 10. 1 з.п. ф-лы.SUMMARY OF THE INVENTION: a composition is used comprising, wt.%: Lime 1.5; calcium phosphate drying oil or stearate 0.0075-0.2250; water 10. 1 z.p. f-ly.
Description
Изобретение относитс к охране окружающей среды и может быть использовано дл предотвращени пыле-солевых бурь с осушенных участков дна Аральского мор .The invention relates to environmental protection and can be used to prevent dust and salt storms from drained sections of the bottom of the Aral Sea.
П.р и м е р. 1,5 кг гидравлической извести и 0,1 кг олифы гас т в течение 24 ч в 10 л воды, смесь перемешивают и сплошным равномерным слоем нанос т на закрепл емую поверхность. Поверхность подвергают сушке в естественных услови х в течение 48 ч. Полученную пленку подвергали воздействию капель воды в течение 30 ч. Действие капель воды в течение указанного времени на образовавшуюс пленку не приводит к заметным разрушени м последней. Дл участков дна, содержащих тонкую пыль, в суспензию добавл ют керосин или жидкие фракции газового конденсата в количестве 0,002-0.100 мае.ч.P. p and m. 1.5 kg of hydraulic lime and 0.1 kg of drying oil are quenched for 24 hours in 10 l of water, the mixture is mixed and applied in a uniform uniform layer to the fixed surface. The surface was dried under natural conditions for 48 hours. The resulting film was exposed to water droplets for 30 hours. The action of water droplets during the indicated time on the resulting film did not lead to noticeable destruction of the latter. For areas of the bottom containing fine dust, kerosene or liquid fractions of gas condensate in an amount of 0.002-0.100 wt.h. are added to the suspension.
Ф о р м у л а и з о б р е т е н и FORMULA AND SECTION
Claims (2)