RS49735B - Aging of aluminium alloy containing magnesium and silicon - Google Patents
Aging of aluminium alloy containing magnesium and siliconInfo
- Publication number
- RS49735B RS49735B YUP-570/01A YU57001A RS49735B RS 49735 B RS49735 B RS 49735B YU 57001 A YU57001 A YU 57001A RS 49735 B RS49735 B RS 49735B
- Authority
- RS
- Serbia
- Prior art keywords
- aging
- silicon
- aluminium alloy
- alloy containing
- containing magnesium
- Prior art date
Abstract
Postupak starenja Al-Mg-Si legure pogodne za termičku obradu, tako da se posle dobijanja oblika i posle hlađenja već izvučenih komada starenje obavlja na taj način što se u prvom koraku izvučeni komad zagreva do temperature između 100°C i 170°C, a u drugom koraku se izvučeni komad zagreva do krajnje održavane temperature između 160°C i 220°C, naznačen time što je brzina zagrevanja u prvom koraku najmanje 100°C/h a u drugom koraku između 5 i 50°C/h, i što se ceo ciklus starenja izvodi se u vremenskom trajanju između 3 i 24 sata. Prijava sadrži još 8 zavisnih patentnih zahteva.The aging process of Al-Mg-Si alloy is suitable for thermal treatment, so that after the shape has been obtained and after the pieces have already been cooled, the aging is carried out in such a way that in the first step the extracted piece is heated to a temperature between 100 ° C and 170 ° C, and in in the second step, the extracted piece is heated to a perfectly maintained temperature between 160 ° C and 220 ° C, characterized in that the first-step heating rate is at least 100 ° C / h in the second step, between 5 and 50 ° C / h, and the whole cycle Aging is performed between 3 and 24 hours. The application contains 8 more dependent patent claims.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
YUP-570/01A RS49735B (en) | 1999-02-12 | 1999-02-12 | Aging of aluminium alloy containing magnesium and silicon |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
YUP-570/01A RS49735B (en) | 1999-02-12 | 1999-02-12 | Aging of aluminium alloy containing magnesium and silicon |
Publications (2)
Publication Number | Publication Date |
---|---|
YU57001A YU57001A (en) | 2004-03-12 |
RS49735B true RS49735B (en) | 2008-04-04 |
Family
ID=47693476
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
YUP-570/01A RS49735B (en) | 1999-02-12 | 1999-02-12 | Aging of aluminium alloy containing magnesium and silicon |
Country Status (1)
Country | Link |
---|---|
RS (1) | RS49735B (en) |
-
1999
- 1999-02-12 RS YUP-570/01A patent/RS49735B/en unknown
Also Published As
Publication number | Publication date |
---|---|
YU57001A (en) | 2004-03-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CA2261994A1 (en) | Frozen food product containing heat stable antifreeze protein | |
BR0212482A (en) | Method for Producing an Electric Grain Oriented Steel Strip | |
DK468489D0 (en) | PROCEDURE FOR THE PREPARATION OF SUBSTANCES OF AN ALUMINUM ALLOY, WHICH MAINTAINS A HIGH EXPENSE STRENGTH AFTER LONG TIME HEAT TREATMENT | |
UA40862A (en) | process of thermal and mechanical treatment of high-strength beta-titanium alloys | |
RS49735B (en) | Aging of aluminium alloy containing magnesium and silicon | |
ATE247181T1 (en) | METHOD FOR PRODUCING AN ALUMINUM ALLOY CONTAINING SILICON AND MAGNESIUM | |
ATE375236T2 (en) | METHOD FOR PRODUCING HARDENED PRODUCTS | |
NO20010079L (en) | Method of manufacturing heat-processable sheet articles | |
UA41975C2 (en) | method for the thermal treatment of alloy aluminium-lithium and method for formation of structure glued with adhesive | |
HUP0101531A2 (en) | Process for the preparation of (r)-or (s)-alpha-hydroxycarboxylic acids with high chemical and optical purity | |
SI1442150T1 (en) | Aluminum-silicon alloys having improved mechanical properties | |
ES2148874T3 (en) | ANTIOXIDANT COMPOSITION AND METHOD FOR ITS PRODUCTION. | |
EP0863115A3 (en) | Process and plant for firing ceramic products containing interlamellar water | |
Wang et al. | The Strengthening of NiAl by TiB sub 2 | |
SE8201778L (en) | PROCEDURE FOR MANUFACTURING ALUMINUM THREADS | |
RS49557B (en) | Aluminium alloy containing magnesium and silicon | |
DK1465757T3 (en) | Thermal process comprising cold RF irradiated liquid as core process for the production of nano-sized particles | |
JPS545896A (en) | Process for producing high temperature reducting gas from light hydrocarbon | |
Rabinovich et al. | Aluminum Alloys Thermal Cycling and Its Application for Residual Stress Decrease | |
Xie et al. | Study on aging strengthening of casting CuNiTiBe alloy by rapid cooling | |
PT102499A (en) | Method for xylophagous wood protection comprises cooling wood to between -20oC and -30C, holding temperature for one to two days and then heating slowly to ambient temperature | |
Kuang et al. | Application of Gas Carbonitriding on Pusher Continuous Furnace Line | |
DE502005007794D1 (en) | METHOD FOR THE PRODUCTION OF PORTION PACKS OF EYE-ACTIVE SUBSTANCES | |
Jinzheng et al. | Heating process of hot-upsetting TC 4 titanium alloy | |
JPS5354169A (en) | Low temperature separating method of thermal cracking gases |